메뉴 건너뛰기




Volumn 99, Issue 11, 2011, Pages

Defect migration and recombination in nanoindentation of silica glass

Author keywords

[No Author keywords available]

Indexed keywords

ATOMISTIC MECHANISM; DEFECT ANNIHILATION; HYDROSTATIC TENSION; INDENTERS; MECHANICAL PROCESS; MOLECULAR DYNAMICS SIMULATIONS; OXYGEN DEFECT; PLASTIC REGIONS; SILICA-BASED GLASS;

EID: 80053193430     PISSN: 00036951     EISSN: None     Source Type: Journal    
DOI: 10.1063/1.3637052     Document Type: Article
Times cited : (40)

References (31)
  • 1
    • 78649707639 scopus 로고    scopus 로고
    • 10.1557/mrs2010.717
    • W. C. Oliver and G. M. Pharr, MRS Bull. 35 (11), 897 (2010). 10.1557/mrs2010.717
    • (2010) MRS Bull. , vol.35 , Issue.11 , pp. 897
    • Oliver, W.C.1    Pharr, G.M.2
  • 4
    • 0026875935 scopus 로고
    • 10.1557/JMR.1992.1564
    • W. C. Oliver and G. M. Pharr, J. Mater. Res. 7 (6), 1564 (1992). 10.1557/JMR.1992.1564
    • (1992) J. Mater. Res. , vol.7 , Issue.6 , pp. 1564
    • Oliver, W.C.1    Pharr, G.M.2
  • 5
    • 0040633110 scopus 로고    scopus 로고
    • 10.1016/S0921-5093(98)00724-2
    • G. M. Pharr, Mater. Sci. Eng., A 253 (1-2), 151 (1998). 10.1016/S0921-5093(98)00724-2
    • (1998) Mater. Sci. Eng., A , vol.253 , Issue.12 , pp. 151
    • Pharr, G.M.1
  • 8
    • 0027666487 scopus 로고
    • 10.1016/0043-1648(93)90192-O
    • C. M. Mate, Wear 168 (1-2), 17 (1993). 10.1016/0043-1648(93)90192-O
    • (1993) Wear , vol.168 , Issue.12 , pp. 17
    • Mate, C.M.1
  • 9
    • 21544451468 scopus 로고
    • 10.1063/1.103950
    • G. Meyer and N. M. Amer, Appl. Phys. Lett. 57 (20), 2089 (1990). 10.1063/1.103950
    • (1990) Appl. Phys. Lett. , vol.57 , Issue.20 , pp. 2089
    • Meyer, G.1    Amer, N.M.2
  • 14
  • 16
    • 80053183864 scopus 로고    scopus 로고
    • See supplementary material at E-APPLAB-99-058137 for the indenter-substrate potential. Silicon nitride or diamond is used as a nanoindenter ti Since these are hard materials (Refs.), we use a rigid indenter.
    • See supplementary material at http://dx.doi.org/10.1063/1.3637052 E-APPLAB-99-058137 for the indenter-substrate potential. Silicon nitride or diamond is used as a nanoindenter tip. Since these are hard materials (Refs.,), we use a rigid indenter.
  • 19
    • 0026312020 scopus 로고
    • 10.1038/353344a0
    • N. Binggeli and J. R. Chelikowsky, Nature 353 (6342), 344 (1991). 10.1038/353344a0
    • (1991) Nature , vol.353 , Issue.6342 , pp. 344
    • Binggeli, N.1    Chelikowsky, J.R.2
  • 23
    • 0024528301 scopus 로고
    • 10.1038/340217a0
    • Y. Tsuchida and T. Yagi, Nature 340 (6230), 217 (1989). 10.1038/340217a0
    • (1989) Nature , vol.340 , Issue.6230 , pp. 217
    • Tsuchida, Y.1    Yagi, T.2
  • 24
    • 55649083894 scopus 로고    scopus 로고
    • 10.1016/j.jnoncrysol.2008.09.015
    • T. M. Gross and M. Tomozawa, J. Non-Cryst. Solids 354 (52-54), 5567 (2008). 10.1016/j.jnoncrysol.2008.09.015
    • (2008) J. Non-Cryst. Solids , vol.354 , Issue.5254 , pp. 5567
    • Gross, T.M.1    Tomozawa, M.2
  • 28
  • 29
    • 0012281922 scopus 로고
    • 10.1080/13642818708208532
    • N. F. Mott, Philos. Mag. B 56 (2), 257 (1987). 10.1080/13642818708208532
    • (1987) Philos. Mag. B , vol.56 , Issue.2 , pp. 257
    • Mott, N.F.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.