Volumn 5, Issue 4, 2010, Pages 189-200

Elemental release and surface changes of fluorapatite-leucite porcelain upon immersion in acidic agents

Author keywords

Acidic agent; Fluorapatite leucite porcelain; Ion leaching; Surface roughness

Indexed keywords


EID: 79952818316     PISSN: 19917902     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jds.2010.11.003     Document Type: Article
Times cited : (11)

References (40)
  • 1
    • 0037104975 scopus 로고    scopus 로고
    • Ion leaching from dental ceramics during static in vitro corrosion testing
    • DOI 10.1002/jbm.10109
    • Milleding P, Haraldsson C, Karlsson S. Ion leaching from dental ceramics during static in vitro corrosion testing. J Biomed Mater Res 2002;61:541-50. (Pubitemid 34721498)
    • (2002) Journal of Biomedical Materials Research , vol.61 , Issue.4 , pp. 541-550
    • Milleding, P.1    Haraldsson, C.2    Karlsson, S.3
  • 2
    • 0026922763 scopus 로고
    • Degradability of dental ceramics
    • Anusavice KJ. Degradability of dental ceramics. Adv Dent Res 1992;6:82-9.
    • (1992) Adv Dent Res , vol.6 , pp. 82-89
    • Anusavice, K.J.1
  • 3
    • 0030621975 scopus 로고    scopus 로고
    • Chemical durability of Dicor and lithia-based glass-ceramics
    • Anusavice KJ, Zhang NZ. Chemical durability of Dicor and Lithia-based glass-ceramics. Dent Mater 1997;13:13-9. (Pubitemid 127752784)
    • (1997) Dental Materials , vol.13 , Issue.1 , pp. 13-19
    • Anusavice, K.J.1    Zhang, N.-Z.2
  • 4
    • 0038356543 scopus 로고    scopus 로고
    • On the surface elemental composition of non-corroded and corroded dental ceramic materials in vitro
    • DOI 10.1023/A:1023416232222
    • Milleding P, Karlsson S, Nyborg L. On the surface elemental composition of non-corroded and corroded dental ceramic materials in vitro. J Mater Sci Mater Med 2003;14:557-66. (Pubitemid 36649186)
    • (2003) Journal of Materials Science: Materials in Medicine , vol.14 , Issue.6 , pp. 557-566
    • Milleding, P.1    Karlsson, S.2    Nyborg, L.3
  • 7
    • 0033118163 scopus 로고    scopus 로고
    • Surface corrosion of dental ceramics in vitro
    • DOI 10.1016/S0142-9612(98)00223-3, PII S0142961298002233
    • Milleding P, Wennerberg A, Aladdin S, Karlsson S, Simon E. Surface corrosion of dental ceramics in vitro. Biomaterials 1999;20:733-46. (Pubitemid 29176702)
    • (1999) Biomaterials , vol.20 , Issue.8 , pp. 733-746
    • Milleding, P.1    Wennerberg, A.2    Alaeddin, S.3    Karlsson, S.4    Simon, E.5
  • 8
    • 74049112939 scopus 로고    scopus 로고
    • Vicker's microhardness and energy dispersive x-ray analysis of fluorapatite-leucite and fluorapatite ceramics cyclically immersed in acidic agents
    • Kukiattrakoon B, Junpoom P, Hengtrakool C. Vicker's microhardness and energy dispersive x-ray analysis of fluorapatite-leucite and fluorapatite ceramics cyclically immersed in acidic agents. J Oral Sci 2009;51:443-50.
    • (2009) J Oral Sci , vol.51 , pp. 443-450
    • Kukiattrakoon, B.1    Junpoom, P.2    Hengtrakool, C.3
  • 9
    • 0003673876 scopus 로고
    • th ed.Washington,DC: National Academy Press. Available at: Date accessed 28.01.10
    • th ed.Washington,DC: National Academy Press. Available at: http://www.nap.edu/openbook.php?record-idZ1349; 1989 [Date accessed 28.01.10].
    • (1989) Recommended Dietary Allowance
  • 10
    • 0003824141 scopus 로고    scopus 로고
    • Agency for Toxic Substances and Disease Registry. Atlanta, GA: U.S. Department of Health and Human Service. Available at: Date accessed 28.01.10
    • Agency for Toxic Substances and Disease Registry. Minimal Risk Levels (MRLs) for Hazardous Substances. Atlanta, GA: U.S. Department of Health and Human Service. Available at: http://www.atsdr.cdc.gov/mrls/mrls-list.html; 2008 [Date accessed 28.01.10].
    • (2008) Minimal Risk Levels (MRLs) for Hazardous Substances
  • 12
    • 0032730157 scopus 로고    scopus 로고
    • A molecular mechanism of aluminium-induced Alzheimer's disease?
    • Exley C. A molecular mechanism of aluminium-induced Alzheimer's disease? J Inorg Biochem 1999;76:133-40.
    • (1999) J Inorg Biochem , vol.76 , pp. 133-140
    • Exley, C.1
  • 14
    • 0026921420 scopus 로고
    • Effect of topical fluorides and citric acid on overglazed and autoglazed porcelain surfaces
    • Demirhanoǧlu ŞT, Şahin E. Effect of topical fluorides and citric acid on overglazed and autoglazed porcelain surfaces. Int J Prosthodont 1992;5:434-40.
    • (1992) Int J Prosthodont , vol.5 , pp. 434-440
    • Demirhanoǧlu, Ş.T.1    Şahin, E.2
  • 15
    • 0034331731 scopus 로고    scopus 로고
    • The influence of surface roughness on porcelain strength
    • De Jager N, Feilzer AJ, Davidson CL. The influence of surface roughness on porcelain strength. Dent Mater 2000;16:381-8.
    • (2000) Dent Mater , vol.16 , pp. 381-388
    • De Jager, N.1    Feilzer, A.J.2    Davidson, C.L.3
  • 16
    • 4344646079 scopus 로고    scopus 로고
    • Effect of surface roughness on flexural strength of veneer ceramics
    • Fischer H, Schafer M, Marx R. Effect of surface roughness on flexural strength of veneer ceramics. J Dent Res 2003;82:972-5.
    • (2003) J Dent Res , vol.82 , pp. 972-975
    • Fischer, H.1    Schafer, M.2    Marx, R.3
  • 19
    • 33745864031 scopus 로고    scopus 로고
    • Physical properties and microstructural characterization of dental porcelains mixed with distilled water and modeling liquid
    • DOI 10.1016/j.dental.2005.08.007, PII S0109564105002708
    • Sinmazişik G, Oveçoǧlu ML. Physical properties and microstructural characterization of dental porcelains mixed with distilled water and modeling liquid. Dent Mater 2006;22:735-45. (Pubitemid 44026524)
    • (2006) Dental Materials , vol.22 , Issue.8 , pp. 735-745
    • Sinmazisik, G.1    Ovecoglu, M.L.2
  • 20
    • 0029294815 scopus 로고
    • Relative flexural strength of six new ceramics materials
    • Seghi RR, Sorensen JA. Relative flexural strength of six new ceramics materials. Int J Prosthodont 1995;8:239-46.
    • (1995) Int J Prosthodont , vol.8 , pp. 239-246
    • Seghi, R.R.1    Sorensen, J.A.2
  • 22
    • 0032081997 scopus 로고    scopus 로고
    • Stress induced phase transformation of a cesium stabilized leucite porcelain and associated properties
    • PII S0109564198000335
    • Rasmussen ST, Groh CL, O'Brien WJ. Stress induced phase transformation of a cesium stabilized leucite porcelain and associated properties. Dent Mater 1998;14:202-11. (Pubitemid 128421203)
    • (1998) Dental Materials , vol.14 , Issue.3 , pp. 202-211
    • Rasmussen, S.T.1    Groh, C.L.2    O'Brien, W.J.3
  • 23
    • 0031324457 scopus 로고    scopus 로고
    • 2O in a Glass Matrix on the Strength of Leucite-Containing Porcelains
    • Lee HH, Kon M, Asaoka K. Influence of modification of Na2O in a glass matrix on the strength of leucite-containing porcelains. Dent Mater J 1997;16:134-43. (Pubitemid 127489122)
    • (1997) Dental Materials Journal , vol.16 , Issue.2 , pp. 134-143
    • Lee, H.-H.1    Kon, M.2    Asaoka, K.3
  • 24
    • 33746538494 scopus 로고    scopus 로고
    • Prevalence, incidence and distribution of erosion
    • Jaeggi T, Lussi A. Prevalence, incidence and distribution of erosion. Monogr Oral Sci 2006;20:44-65.
    • (2006) Monogr Oral Sci , vol.20 , pp. 44-65
    • Jaeggi, T.1    Lussi, A.2
  • 25
    • 0035375452 scopus 로고    scopus 로고
    • Cupped lesions of early onset dental erosion in young southeast Queensland adults
    • Khan F, Young WG, Law V, Priest J, Daley TJ. Cupped lesions of early onset dental erosion in young southeast Queensland adults. Aust Dent J 2001;46:100-7. (Pubitemid 33633262)
    • (2001) Australian Dental Journal , vol.46 , Issue.2 , pp. 100-107
    • Khan, F.1    Young, W.G.2    Law, V.3    Priest, J.4    Daley, T.J.5
  • 26
    • 18544400001 scopus 로고    scopus 로고
    • Dental erosion. Definition, classification and links
    • Imfeld T. Dental erosion. Definition, classification and links. Eur J Oral Sci 1996;104:151-5.
    • (1996) Eur J Oral Sci , vol.104 , pp. 151-155
    • Imfeld, T.1
  • 29
    • 48749114754 scopus 로고    scopus 로고
    • Twenty-year follow-up of metal-ceramic single crown: A retrospective study
    • Napankangas R, Raustia A. Twenty-year follow-up of metal-ceramic single crown: a retrospective study. Int J Prosthodont 2008;21:307-11.
    • (2008) Int J Prosthodont , vol.21 , pp. 307-311
    • Napankangas, R.1    Raustia, A.2
  • 31
    • 0019662986 scopus 로고
    • Surface roughness: Measurement, interpretation and significance of data
    • Stout KJ. Surface roughness: measurement, interpretation and significance of data. Mater Eng 1981;2:260-0-5.
    • (1981) Mater Eng , vol.2
    • Stout, K.J.1
  • 32
    • 0038601691 scopus 로고    scopus 로고
    • Surface roughness of a novel "ceramic restorative cement" after treatment with different polishing techniques in vitro
    • Sunnegårdh-Grönberg K, van Dijken JW. Surface roughness of a novel "ceramic restorative cement" after treatment with different polishing techniques in vitro. Clin Oral Investig 2003;7:27-31.
    • (2003) Clin Oral Investig , vol.7 , pp. 27-31
    • Sunnegårdh-Grönberg, K.1    Van Dijken, J.W.2
  • 35
    • 33845944460 scopus 로고    scopus 로고
    • Evaluation of surface roughness of glazed and polished ceramic surface on exposure to fluoride gel, bleaching agent and aerated drink: An in vitro study
    • Kamala K, Annapurni H. Evaluation of surface roughness of glazed and polished ceramic surface on exposure to fluoride gel, bleaching agent and aerated drink: an in vitro study. J Indian Prosthodont Soc 2006;61:28-32.
    • (2006) J Indian Prosthodont Soc , vol.61 , pp. 28-32
    • Kamala, K.1    Annapurni, H.2
  • 36
    • 0025492382 scopus 로고
    • Fracture surface analysis of dental ceramics: Clinically failed restorations
    • Kelly R, Giordano R, Pober R, Cima MJ. Fracture surface analysis of dental ceramics: clinically failed restorations. Int J Prosthodont 1990;3:430-40.
    • (1990) Int J Prosthodont , vol.3 , pp. 430-440
    • Kelly, R.1    Giordano, R.2    Pober, R.3    Cima, M.J.4
  • 37
    • 0031173323 scopus 로고    scopus 로고
    • Comparison of surface roughness of oral hard materials to the threshold surface roughness for bacterial plaque retention: A review of the literature
    • Bollen CM, Lambrechts P, Quirynen M. Comparison of surface roughness of oral hard materials to the threshold surface roughness for bacterial plaque retention: a review of the literature. Dent Mater 1997;13:258-69.
    • (1997) Dent Mater , vol.13 , pp. 258-269
    • Bollen, C.M.1    Lambrechts, P.2    Quirynen, M.3
  • 38
    • 0028949846 scopus 로고
    • Pineapple fruit: Morphological characteristics, chemical composition and sensory analysis of Red Spanish and Smooth Cayenne cultivars
    • Bartolomé AP, Rupérez P, Fúster C. Pineapple fruit: morphological characteristics, chemical composition and sensory analysis of Red Spanish and Smooth Cayenne cultivars. Food Chem 1995;53:75-9.
    • (1995) Food Chem , vol.53 , pp. 75-79
    • Bartolomé, A.P.1    Rupérez, P.2    Fúster, C.3
  • 39
    • 0030119212 scopus 로고    scopus 로고
    • Pathogenesis and modifying factors of dental erosion
    • Meurman JH, ten Cate JM. Pathogenesis and modifying factors of dental erosion. Eur J Oral Sci 1996;104:199-206.
    • (1996) Eur J Oral Sci , vol.104 , pp. 199-206
    • Meurman, J.H.1    Ten Cate, J.M.2
  • 40
    • 70349783445 scopus 로고    scopus 로고
    • The effect of salivary factors on dental erosion in various age groups and tooth surfaces
    • Piangprach T, Hengtrakool C, Kukiattrakoon B, Kedjarune-Leggat U. The effect of salivary factors on dental erosion in various age groups and tooth surfaces. J Am Dent Assoc 2009;140:1137-43.
    • (2009) J Am Dent Assoc , vol.140 , pp. 1137-1143
    • Piangprach, T.1    Hengtrakool, C.2    Kukiattrakoon, B.3    Kedjarune-Leggat, U.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.