Influence of enzymatic and chemical degradation on zirconia resin bond strength after different surface treatments

Author keywords

[No Author keywords available]

Indexed keywords

ALCOHOL; ESTERASE; FILTEK Z250; RELY X UNICEM; RESIN; RESIN CEMENT; SODIUM HYDROXIDE; WATER; ZIRCONIUM; ZIRCONIUM OXIDE;

EID: 79952456427     PISSN: 08948275     EISSN: None     Source Type: Journal    
DOI: None     Document Type: Article
Times cited : (7)

References (36)
  • 1
    • 9944229063 scopus 로고    scopus 로고
    • Contemporary materials and technologies for all-ceramic fixed partial dentures: A review of the literature
    • DOI 10.1016/j.prosdent.2004.09.015, PII S0022391304006158
    • Raigrodski AJ. Contemporary materials and technologies for all-ceramic fixed partial dentures: A review of the literature. J Prosthet Dent 2004;92:557-562. (Pubitemid 39593586)
    • (2004) Journal of Prosthetic Dentistry , vol.92 , Issue.6 , pp. 557-562
    • Raigrodski, A.J.1
  • 2
    • 20444408006 scopus 로고    scopus 로고
    • In vitro retentive strength of zirconium oxide ceramic crowns using different luting agents
    • DOI 10.1016/j.prosdent.2005.04.011, PII S0022391305002362
    • Ernst CP, Cohnen U, Stender E, Willershausen B. In vitro retentive strength of zirconium oxide ceramic crowns using different luting agents. J Prosthet 4Dent 2005;93:551-558. (Pubitemid 40798345)
    • (2005) Journal of Prosthetic Dentistry , vol.93 , Issue.6 , pp. 551-558
    • Ernst, C.-P.1    Cohnen, U.2    Stender, E.3    Willershausen, B.4
  • 3
    • 59349112720 scopus 로고    scopus 로고
    • Effect of water aging on microtensile bond strength of dual-cured resin cements to pre-treated sintered zirconium-oxide ceramics
    • Oyague RC, Monticelli F, Toledano M, Osorio E, Ferrari M, Osorio R. Effect of water aging on microtensile bond strength of dual-cured resin cements to pre-treated sintered zirconium-oxide ceramics. Dent Mater 2009;25:392-399.
    • (2009) Dent Mater , vol.25 , pp. 392-399
    • Oyague, R.C.1    Monticelli, F.2    Toledano, M.3    Osorio, E.4    Ferrari, M.5    Osorio, R.6
  • 4
    • 33749677224 scopus 로고    scopus 로고
    • The efficacy of posterior three-unit zirconium-oxide-based ceramic fixed partial dental prostheses: A prospective clinical pilot study
    • DOI 10.1016/j.prosdent.2006.08.010, PII S0022391306004033
    • Raigrodski AJ, Chiche GJ, Potiket N, Hochstedler JL, Mohamed SE, Billiot S, Mercante DE. The efficacy of posterior three-unit zirconium-oxidebased ceramic fixed partial dental prostheses: A prospective clinical pilot study. J Prosthet Dent 2006;96:237-244. (Pubitemid 44556711)
    • (2006) Journal of Prosthetic Dentistry , vol.96 , Issue.4 , pp. 237-244
    • Raigrodski, A.J.1    Chiche, G.J.2    Potiket, N.3    Hochstedler, J.L.4    Mohamed, S.E.5    Billiot, S.6    Mercante, D.E.7
  • 5
    • 36749072559 scopus 로고    scopus 로고
    • The effect of surface preparation and luting agent on bond strength to a zirconium-based ceramic
    • Senyilmaz DP, Palin WM, Shortall AC, Burke FJ. The effect of surface preparation and luting agent on bond strength to a zirconium-based ceramic. Oper Dent 2007;32:623-630.
    • (2007) Oper Dent , vol.32 , pp. 623-630
    • Senyilmaz, D.P.1    Palin, W.M.2    Shortall, A.C.3    Burke, F.J.4
  • 6
    • 0033222358 scopus 로고    scopus 로고
    • The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic
    • PII S0109564199000706
    • Kosmac T, Oblak C, Jevnikar P, Funduk N, Marion L. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic. Dent Mater 1999;15:426-433. (Pubitemid 129586772)
    • (1999) Dental Materials , vol.15 , Issue.6 , pp. 426-433
    • Kosmac, T.1    Oblak, C.2    Jevnikar, P.3    Funduk, N.4    Marion, L.5
  • 7
    • 50349096922 scopus 로고    scopus 로고
    • The effect of hydrofluoric acid surface treatment and bond strength of a zirconia veneering ceramic
    • Chaiyabutr Y, McGowan S, Phillips KM, Kois JC, Giordano RA. The effect of hydrofluoric acid surface treatment and bond strength of a zirconia veneering ceramic. J Prosthet Dent 2008; 100:194-202.
    • (2008) J Prosthet Dent , vol.100 , pp. 194-202
    • Chaiyabutr, Y.1    McGowan, S.2    Phillips, K.M.3    Kois, J.C.4    Giordano, R.A.5
  • 8
    • 34548648100 scopus 로고    scopus 로고
    • Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia
    • Blatz MB, Chiche G, Holst S, Sadan A. Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia. Quintessence Int 2007;38:745-753.
    • (2007) Quintessence Int , vol.38 , pp. 745-753
    • Blatz, M.B.1    Chiche, G.2    Holst, S.3    Sadan, A.4
  • 9
    • 0031598657 scopus 로고    scopus 로고
    • Bonding to zirconia ceramic: Adhesion methods and their durability
    • PII S01095641980000116
    • Kern M, Wegner SM. Bonding to zirconia ceramic: Adhesion methods and their durability. Dent Mater 1998;14:64-71. (Pubitemid 128419490)
    • (1998) Dental Materials , vol.14 , Issue.1 , pp. 64-71
    • Kern, M.1    Wegner, S.M.2
  • 10
    • 36049040304 scopus 로고    scopus 로고
    • Selective infiltration-etching technique for a strong and durable bond of resin cements to zirconia-based materials
    • Aboushelib MN, Kleverlaan CJ, Feilzer AJ. Selective infiltration-etching technique for a strong and durable bond of resin cements to zirconia-based materials. J Prosthet Dent 2007;98:379-388.
    • (2007) J Prosthet Dent , vol.98 , pp. 379-388
    • Aboushelib, M.N.1    Kleverlaan, C.J.2    Feilzer, A.J.3
  • 13
    • 30344433724 scopus 로고    scopus 로고
    • Effect of thermocycling on bond strength of luting cements to zirconia ceramic
    • Luthy H, Loeffel O, Hammerle CH. Effect of thermocycling on bond strength of luting cements to zirconia ceramic. Dent Mater 2006;22:195-200.
    • (2006) Dent Mater , vol.22 , pp. 195-200
    • Luthy, H.1    Loeffel, O.2    Hammerle, C.H.3
  • 14
    • 0030307272 scopus 로고    scopus 로고
    • Filler leachability of composites stored in distilled water or artificial saliva
    • Soderholm KJ, Mukherjee R, Longmate J. Filler leachability of composites stored in distilled water or artificial saliva. J Dent Res 1996;75:1692-1699. (Pubitemid 32770415)
    • (1996) Journal of Dental Research , vol.75 , Issue.9 , pp. 1692-1699
    • Soderholm, K.-J.M.1    Mukherjee, R.2    Longmate, J.3
  • 15
    • 58149326616 scopus 로고
    • Properties of heat-treated composites after aging in water
    • Ferracane JL, Hopkin JK, Condon JR. Properties of heat-treated composites after aging in water. Dent Mater 1995;11:354-358.
    • (1995) Dent Mater , vol.11 , pp. 354-358
    • Ferracane, J.L.1    Hopkin, J.K.2    Condon, J.R.3
  • 16
    • 15944425354 scopus 로고    scopus 로고
    • Influence of pH environment on polymer based dental material properties
    • DOI 10.1016/j.jdent.2004.08.004
    • Prakki A, Cilli R, Mondelli RF, Kalachandra S, Pereira JC. Influence of pH environment on polymer based dental material properties. J Dent 2005;33:91-98. (Pubitemid 40431300)
    • (2005) Journal of Dentistry , vol.33 , Issue.2 , pp. 91-98
    • Prakki, A.1    Cilli, R.2    Lia, M.R.F.3    Kalachandra, S.4    Pereira, J.C.5
  • 17
    • 1542652361 scopus 로고    scopus 로고
    • Salivary esterase activity and its association with the biodegradation of dental composites
    • Finer Y, Santerre JP. Salivary esterase activity and its association with the biodegradation of dental composites. J Dent Res 2004;83:22-26. (Pubitemid 41756853)
    • (2004) Journal of Dental Research , vol.83 , Issue.1 , pp. 22-26
    • Finer, Y.1    Santerre, J.P.2
  • 18
    • 0017356168 scopus 로고
    • Origin of esterases in human whole saliva
    • Lindqvist L, Nord CE, Soder PO. Origin of esterases in human whole saliva. Enzyme 1977;22:166-175. (Pubitemid 8089439)
    • (1977) Enzyme , vol.22 , Issue.3 , pp. 166-175
    • Lindqvist, L.1    Nord, C.E.2    Soder, P.O.3
  • 19
    • 0029335996 scopus 로고
    • Fracture toughness of experimental dental composites aged in ethanol
    • Ferracane JL, Berge HX. Fracture toughness of experimental dental composites aged in ethanol. J Dent Res 1995;74:1418-1423.
    • (1995) J Dent Res , vol.74 , pp. 1418-1423
    • Ferracane, J.L.1    Berge, H.X.2
  • 20
    • 0026198113 scopus 로고
    • Residual monomers (TEGDMA and Bis-GMA) of a set visible-light-cured dental composite resin when immersed in water
    • Tanaka K, Taira M, Shintani H, Wakasa K, Yamaki M. Residual monomers (TEGDMA and Bis-GMA) of a set visible-light-cured dental composite resin when immersed in water. J Oral Rehabil 1991 ; 18:353-362.
    • (1991) J Oral Rehabil , vol.18 , pp. 353-362
    • Tanaka, K.1    Taira, M.2    Shintani, H.3    Wakasa, K.4    Yamaki, M.5
  • 21
    • 0141592642 scopus 로고    scopus 로고
    • Biodegradation of a dental composite by esterases: Dependence on enzyme concentration and specificity
    • DOI 10.1163/156856203768366558
    • Finer Y, Santerre JP. Biodegradation of a dental composite by esterases: Dependence on enzyme concentration and specificity. J Biomater Sci Polym Ed 2003;14:837-849. (Pubitemid 37160562)
    • (2003) Journal of Biomaterials Science, Polymer Edition , vol.14 , Issue.8 , pp. 837-849
    • Finer, Y.1    Santerre, J.P.2
  • 22
    • 33748460089 scopus 로고    scopus 로고
    • Comparison of wire loop and shear blade as the 2 most common methods for testing orthodontic shear bond strength
    • DOI 10.1016/j.ajodo.2006.03.021, PII S0889540606008249
    • Mojtahedzadeh F, Akhoundi MS, Noroozi H. Comparison of wire loop and shear blade as the 2 most common methods for testing orthodontic shear bond strength. Am J Orthod Dentofacial Orthop 2006;130:385-387. (Pubitemid 44354040)
    • (2006) American Journal of Orthodontics and Dentofacial Orthopedics , vol.130 , Issue.3 , pp. 385-387
    • Mojtahedzadeh, F.1    Akhoundi, M.S.A.2    Noroozi, H.3
  • 23
    • 0022358205 scopus 로고
    • Chemical softening and wear of dental composites
    • McKinney JE, Wu W. Chemical softening and wear of dental composites. J Dent Res 1985;64:1326-1331. (Pubitemid 16227212)
    • (1985) Journal of Dental Research , vol.64 , Issue.11 , pp. 1326-1331
    • McKinney, J.E.1    Wu, W.2
  • 24
    • 34250196404 scopus 로고    scopus 로고
    • Subsurface degradation of resin-based composites
    • DOI 10.1016/j.dental.2006.06.035, PII S010956410600220X
    • Bagheri R, Tyas MJ, Burrow MF. Subsurface degradation of resin-based composites. Dent Mater 2007;23:944-951. (Pubitemid 46907958)
    • (2007) Dental Materials , vol.23 , Issue.8 , pp. 944-951
    • Bagheri, R.1    Tyas, M.J.2    Burrow, M.F.3
  • 25
    • 0033852622 scopus 로고    scopus 로고
    • Internal corrosion in dental composite wear
    • Sarkar NK. Internal corrosion in dental composite wear. J Biomed Mater Res 2000;53:371-380.
    • (2000) J Biomed Mater Res , vol.53 , pp. 371-380
    • Sarkar, N.K.1
  • 26
    • 0028719867 scopus 로고
    • Effect of food and oral simulating fluids on dentine bond and composite strength
    • Lee SY, Greener EH, Mueller HJ, Chiu CH. Effect of food and oral simulating fluids on dentine bond and composite strength. J Dent 1994;22:352-359.
    • (1994) J Dent , vol.22 , pp. 352-359
    • Lee, S.Y.1    Greener, E.H.2    Mueller, H.J.3    Chiu, C.H.4
  • 29
  • 31
    • 32044466739 scopus 로고    scopus 로고
    • The influence of surface modification techniques on the performance of a Y-TZP dental ceramic
    • DOI 10.1016/j.jdent.2005.06.006, PII S030057120500120X
    • Curtis AR, Wright AJ, Fleming GJ. The influence of surface modification techniques on the performance of a Y-TZP dental ceramic. J Dent 2006;34:195-206. (Pubitemid 43199800)
    • (2006) Journal of Dentistry , vol.34 , Issue.3 , pp. 195-206
    • Curtis, A.R.1    Wright, A.J.2    Fleming, G.J.P.3
  • 32
    • 11844264547 scopus 로고    scopus 로고
    • Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic
    • DOI 10.1016/j.jdent.2004.07.001, PII S0300571204001125
    • Guazzato M, Quach L, Albakry M, Swain MV. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic. J Dent 2005;33:9-18. (Pubitemid 40093557)
    • (2005) Journal of Dentistry , vol.33 , Issue.1 , pp. 9-18
    • Guazzato, M.1    Quach, L.2    Albakry, M.3    Swain, M.V.4
  • 36
    • 40749115551 scopus 로고    scopus 로고
    • Strength influencing variables on CAD/CAM zirconia frameworks
    • DOI 10.1016/j.dental.2007.06.030, PII S0109564107001765
    • Wang H, Aboushelib MN, Feilzer AJ. Strength influencing variables on CAD/CAM zirconia frameworks. Dent Mater 2008;24:633-638. (Pubitemid 351389493)
    • (2008) Dental Materials , vol.24 , Issue.5 , pp. 633-638
    • Wang, H.1    Aboushelib, M.N.2    Feilzer, A.J.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.