Fracture toughness of veneering ceramics for fused to metal (PFM) and zirconia dental restorative materials

Author keywords

Dental restorations; Fracture toughness; Hardness; PFM; Surface crack in flexure; Veneering ceramic; Zirconia

Indexed keywords

CERAMIC MATERIALS; CRACKS; DENTAL MATERIALS; FILLING; HARDNESS; PORCELAIN; RESTORATION; SURFACE DEFECTS; VENEERS; ZEOLITES; ZIRCONIA;

EID: 77958198019     PISSN: 1044677X     EISSN: None     Source Type: Journal    
DOI: 10.6028/jres.115.024     Document Type: Article
Times cited : (40)

References (30)
  • 1
    • 0019708313 scopus 로고
    • Zirconia: An overview
    • Science and Technology of Zirconia, eds. A. H. Heuer L. W. Hobbs (Elsevier, Amsterdam)
    • E. C. Subbarao, Zirconia: an overview, in Advances in Ceramics, vol. 3. Science and Technology of Zirconia, eds. A. H. Heuer, L. W. Hobbs (Elsevier, Amsterdam) (1981).
    • (1981) Advances in Ceramics , vol.3
    • Subbarao, E.C.1
  • 2
    • 0032917811 scopus 로고    scopus 로고
    • Zirconia as a ceramic biomaterial
    • C. Piconi and G. Maccauro, Zirconia as a ceramic biomaterial, Biomater. 20, 1-25 (1999).
    • (1999) Biomater. , vol.20 , pp. 1-25
    • Piconi, C.1    MacCauro, G.2
  • 3
    • 0034264517 scopus 로고    scopus 로고
    • Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia- based ceramics
    • J. Tinschert, D. Zwez, R. Marx, and K. J. Anusavice, Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia- based ceramics, J. Dent. 28 [7], 529-35 (2000).
    • (2000) J. Dent. , vol.28 , Issue.7 , pp. 529-535
    • Tinschert, J.1    Zwez, D.2    Marx, R.3    Anusavice, K.J.4
  • 4
    • 71349085938 scopus 로고    scopus 로고
    • Clinical behavior of zirconia based bridges: Two-years results
    • Abst. No. 0901
    • F. Beuer, H. Aggstaller, T. Fishcher, K. Spiegl, J. Schweiger, and W. Gernet, Clinical behavior of zirconia based bridges: Two-years results, J. Dent. Res. 86, (Spec Iss A), Abst. No. 0901 (2007).
    • (2007) J. Dent. Res. , vol.86 , Issue.SPEC ISS A
    • Beuer, F.1    Aggstaller, H.2    Fishcher, T.3    Spiegl, K.4    Schweiger, J.5    Gernet, W.6
  • 5
    • 71349086000 scopus 로고    scopus 로고
    • Outcome of posterior FPDs of veneered zirconia ceramic (Cercon)
    • Abst. No. 0292
    • S. Wolfart, S. Eschbach, and M. Kern, Outcome of posterior FPDs of veneered zirconia ceramic (Cercon), J. Dent. Res. 86 (Spec Iss A), Abst. No. 0292 (2007).
    • (2007) J. Dent. Res. , vol.86 , Issue.SPEC ISS A
    • Wolfart, S.1    Eschbach, S.2    Kern, M.3
  • 6
    • 14844364021 scopus 로고    scopus 로고
    • All-ceramic fixed partial dentures designed according to the DC-Zirkon® technique: A 2-year clinical study
    • P. Vult Von Steyern, P. Carlson, and K. Nilner, All-ceramic fixed partial dentures designed according to the DC-Zirkon® technique: A 2-year clinical study, J. Oral Rehab. 32 [3], 180-187 (2005).
    • (2005) J. Oral Rehab. , vol.32 , Issue.3 , pp. 180-187
    • Von S.P.Vult1    Carlson, P.2    Nilner, K.3
  • 8
    • 71349087426 scopus 로고    scopus 로고
    • Clinical long-term behavior of zirconia-based bridges (LAVA): Five years results
    • Abst. No. 0312
    • F. P. Nothdurft, P. R. Rountree, and P. R. Pospiech. Clinical long-term behavior of zirconia-based bridges (LAVA): Five years results, J. Dent. Res. 85 (Spec Iss C), Abst. No. 0312 (2006).
    • (2006) J. Dent. Res. , vol.85 , Issue.SPEC ISS C
    • Nothdurft, F.P.1    Rountree, P.R.2    Pospiech, P.R.3
  • 9
    • 71349087621 scopus 로고    scopus 로고
    • 3-year results of zirconia posterior fixed partial dentures made by Direct Ceramic Machining (DCM)
    • Abst. No. 0074
    • I. Sailer, H. Liithy, A. Feher, M. Schumacher, P. Schärer, and C. Hämmerle, 3-year results of zirconia posterior fixed partial dentures made by Direct Ceramic Machining (DCM), J. Dent. Res. 82 (Spec Iss B), Abst. No. 0074 (2003).
    • (2003) J. Dent. Res. , vol.82 , Issue.SPEC ISS B
    • Sailer, I.1    Liithy, H.2    Feher, A.3    Schumacher, M.4    Schärer, P.5    Hämmerle, C.6
  • 10
    • 61649114194 scopus 로고    scopus 로고
    • Trends in materials science from the point of view of a practicing dentist
    • R. Hickel, Trends in materials science from the point of view of a practicing dentist, J. Eur. Cer. Soc. 29, 1283-1289 (2009).
    • (2009) J. Eur. Cer. Soc. , vol.29 , pp. 1283-1289
    • Hickel, R.1
  • 11
    • 30144443459 scopus 로고    scopus 로고
    • Resistance to fracture of two all- ceramic crown materials following endodontic access
    • K. C. Wood, D. W. Berzins, Q. Luo, G. A. Thompson, J. M. Toth, and W. W. Nagy, Resistance to fracture of two all- ceramic crown materials following endodontic access, J. Prosthet. Dent. 95 [1], 33-41 (2006).
    • (2006) J. Prosthet. Dent. , vol.95 , Issue.1 , pp. 33-41
    • Wood, K.C.1    Berzins, D.W.2    Luo, Q.3    Thompson, G.A.4    Toth, J.M.5    Nagy, W.W.6
  • 12
    • 0034204345 scopus 로고    scopus 로고
    • Porcelain esthetics for the 21st century
    • K. F. Leinfelder, Porcelain esthetics for the 21st century, J. Am. Dent. Assoc. 131 [1], 47S-51S (2000).
    • (2000) J. Am. Dent. Assoc. , vol.131 , Issue.1
    • Leinfelder, K.F.1
  • 13
    • 77953556773 scopus 로고    scopus 로고
    • ISO 6872, International Organization for Standardization, Geneva, SW
    • ISO 6872. Dentistry - Ceramic Materials, International Organization for Standardization, Geneva, SW (2008).
    • (2008) Dentistry - Ceramic Materials
  • 14
    • 71349085544 scopus 로고    scopus 로고
    • Comparison of edge chipping resistance of PFM and veneered zirconia specimens
    • J. B. Quinn, V. Sundar, E. E. Parry, and G. D. Quinn, Comparison of Edge Chipping Resistance of PFM and Veneered Zirconia Specimens, Dental Materials. 26 [1], 13-20 (2010).
    • (2010) Dental Materials , vol.26 , Issue.1 , pp. 13-20
    • Quinn, J.B.1    Sundar, V.2    Parry, E.E.3    Quinn, G.D.4
  • 16
    • 84965080618 scopus 로고    scopus 로고
    • Standard test method for determination of fracture toughness of advanced ceramics at ambient temperature
    • ASTM C 1421-99, Vol. 15.01, ASTM, West Conshohocken, PA
    • ASTM C 1421-99, Standard Test Method for Determination of Fracture Toughness of Advanced Ceramics at Ambient Temperature. Annual Book of Standards, Vol. 15.01, ASTM, West Conshohocken, PA, (1999).
    • (1999) Annual Book of Standards
  • 17
    • 77953808354 scopus 로고    scopus 로고
    • Measuring the real fracture toughness of ceramics - ASTM C 1421
    • R. C. Bradt, D. Munz, M. Sakai, and K. W. White, eds., 2005, Springer, USA
    • J. A. Salem, G. D. Quinn, M. G. Jenkins, Measuring the Real Fracture Toughness of Ceramics - ASTM C 1421, pp. 531- 554 in Fracture Mechanics of Ceramics, Vol. 14, R. C. Bradt, D. Munz, M. Sakai, and K. W. White, eds., 2005, Springer, USA, (2005).
    • (2005) Fracture Mechanics of Ceramics , vol.14 , pp. 531-554
    • Salem, J.A.1    Quinn, G.D.2    Jenkins, M.G.3
  • 20
    • 0028514531 scopus 로고
    • Fracture toughness of ceramics by the Surface Crack in Flexure (SCF) Method: Results of the VAMAS round robin
    • G. D. Quinn, R. J. Gettings, and J. J. Kübler, Fracture Toughness of Ceramics by the Surface Crack in Flexure (SCF) Method: Results of the VAMAS Round Robin, Ceramic Engineering and Science Proceedings, 15 [5], 846-855 (1994).
    • (1994) Ceramic Engineering and Science Proceedings , vol.15 , Issue.5 , pp. 846-855
    • Quinn, G.D.1    Gettings, R.J.2    Kübler, J.J.3
  • 21
    • 0003966062 scopus 로고
    • Fracture toughness of advanced ceramics by the Surface Crack in Flexure (SCF) Method: A VAMAS round robin
    • National Institute of Standards and Technology, Gaithersburg, MD 20899
    • G. D. Quinn, J. J. KÜbler, and R. J. Gettings, Fracture Toughness of Advanced Ceramics by the Surface Crack in Flexure (SCF) Method: A VAMAS Round Robin, VAMAS Technical Report #17, National Institute of Standards and Technology, Gaithersburg, MD 20899, (1994).
    • (1994) VAMAS Technical Report #17
    • Quinn, G.D.1    Kübler, J.J.2    Gettings, R.J.3
  • 22
    • 8844224884 scopus 로고    scopus 로고
    • The fracture toughness round robins in VAMAS: What we have learned
    • ASTM STP 1409, J. A. Salem, G. D. Quinn, M. G. Jenkins, eds., (ASTM, West Conshohocken, PA)
    • G. D. Quinn, The Fracture Toughness Round Robins in VAMAS: What We Have Learned, pp. 107-126 in Fracture Resistance Testing of Monolithic and Composite Brittle Materials, ASTM STP 1409, J. A. Salem, G. D. Quinn, M. G. Jenkins, eds., (ASTM, West Conshohocken, PA) (2002).
    • (2002) Fracture Resistance Testing of Monolithic and Composite Brittle Materials , pp. 107-126
    • Quinn, G.D.1
  • 23
    • 77958173560 scopus 로고    scopus 로고
    • SRM 2100, Standard Reference Material Office, National Institute of Standards and Technology, Gaithersburg, MD
    • SRM 2100, Fracture Toughness of Ceramics, Standard Reference Material Office, National Institute of Standards and Technology, Gaithersburg, MD, (1999).
    • (1999) Fracture Toughness of Ceramics
  • 24
    • 77958162250 scopus 로고    scopus 로고
    • SRM 2100: Fracture toughness of ceramics
    • R. C. Bradt, D. Munz, M. Sakai, and K. W. White, eds., Springer, USA
    • G. D. Quinn, K. Xu, R. Gettings, J. A. Salem, and J. J. Swab, SRM 2100: Fracture Toughness of Ceramics, pp. 499-530 in Fracture Mechanics of Ceramics, Vol. 14, R. C. Bradt, D. Munz, M. Sakai, and K. W. White, eds., Springer, USA (2005).
    • (2005) Fracture Mechanics of Ceramics , vol.14 , pp. 499-530
    • Quinn, G.D.1    Xu, K.2    Gettings, R.3    Salem, J.A.4    Swab, J.J.5
  • 25
    • 0001457039 scopus 로고    scopus 로고
    • Fracture toughness of ceramics by the Surface Crack in Flexure (SCF) method
    • R. C. Bradt, D. P. H. Hasselman, D. Munz, M. Sakai, and V. Yashevchenko, eds., (Plenum, NY)
    • G. D. Quinn, R. J. Gettings, and J. J. Kiibler, Fracture Toughness of Ceramics by the Surface Crack in Flexure (SCF) Method, pp. 203-218 in Fracture Mechanics of Ceramics, Vol.11, R. C. Bradt, D. P. H. Hasselman, D. Munz, M. Sakai, and V. Yashevchenko, eds., (Plenum, NY) (1996).
    • (1996) Fracture Mechanics of Ceramics , vol.11 , pp. 203-218
    • Quinn, G.D.1    Gettings, R.J.2    Kiibler, J.J.3
  • 27
    • 0019658622 scopus 로고
    • An empirical stress-intensity factor equation for the surface crack
    • J. C. Newman, Jr., and I. S. Raju, An Empirical Stress-Intensity Factor Equation for the Surface Crack, Eng. Fract. Mech. 15 [1-2], 185-92 (1981).
    • (1981) Eng. Fract. Mech. , vol.15 , Issue.1-2 , pp. 185-192
    • Newman Jr., J.C.1    Raju, I.S.2
  • 28
    • 0042128698 scopus 로고    scopus 로고
    • Influence of micro- structure and chemistry on the fracture toughness of dental ceramics
    • J. B. Quinn, V. Sundar, and I. K Lloyd, Influence of micro- structure and chemistry on the fracture toughness of dental ceramics, Dental Materials 19 (7), 603-11 (2003).
    • (2003) Dental Materials , vol.19 , Issue.7 , pp. 603-611
    • Quinn, J.B.1    Sundar, V.2    Lloyd, I.K.3
  • 29
    • 60449083274 scopus 로고    scopus 로고
    • Impact of thermal misfit on shear strength of veneering ceramic/zirconia composites
    • J. Fischer, B. Stawarzcyk, A. Trottmann, and C. H. F. Hämmerle, Impact of thermal misfit on shear strength of veneering ceramic/zirconia composites, Dental Materials 25 [4], 419-423 (2009).
    • (2009) Dental Materials , vol.25 , Issue.4 , pp. 419-423
    • Fischer, J.1    Stawarzcyk, B.2    Trottmann, A.3    Hämmerle, C.H.F.4
  • 30
    • 67349133480 scopus 로고    scopus 로고
    • Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures
    • M. V. Swain, Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures, Acta Biomater. 5, 1668-1677 (2009).
    • (2009) Acta Biomater. , vol.5 , pp. 1668-1677
    • Swain, M.V.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.