Volumn 95, Issue 1, 2006, Pages 33-41

Resistance to fracture of two all-ceramic crown materials following endodontic access

Author keywords

[No Author keywords available]

Indexed keywords

ALUMINUM OXIDE; ZIRCONIUM; ZIRCONIUM OXIDE;

EID: 30144443459     PISSN: 00223913     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.prosdent.2005.11.003     Document Type: Article
Times cited : (51)

References (31)
  • 1
    • 0034328440 scopus 로고    scopus 로고
    • Restoring teeth that are endodontically treated through existing crowns. Part II: Survey of restorative materials commonly used
    • G. Trautmann, J.L. Gutmann, M.E. Nunn, D.E. Witherspoon, and J.D. Shulman Restoring teeth that are endodontically treated through existing crowns. Part II: survey of restorative materials commonly used Quintessence Int 31 2000 719 728
    • (2000) Quintessence Int , vol.31 , pp. 719-728
    • Trautmann, G.1    Gutmann, J.L.2    Nunn, M.E.3    Witherspoon, D.E.4    Shulman, J.D.5
  • 2
    • 0026934955 scopus 로고
    • Microleakage-full crowns and the dental pulp
    • M. Goldman, P. Laosonthorn, and R.R. White Microleakage-full crowns and the dental pulp J Endod 18 1992 473 475
    • (1992) J Endod , vol.18 , pp. 473-475
    • Goldman, M.1    Laosonthorn, P.2    White, R.R.3
  • 3
    • 0021381133 scopus 로고
    • Endodontic complications following periodontal and prosthetic treatment of patients with advanced periodontal disease
    • G. Bergenholtz, and S. Nyman Endodontic complications following periodontal and prosthetic treatment of patients with advanced periodontal disease J Periodontol 55 1984 63 68
    • (1984) J Periodontol , vol.55 , pp. 63-68
    • Bergenholtz, G.1    Nyman, S.2
  • 4
    • 0022300356 scopus 로고
    • Endodontic access of Cerestore crowns
    • P.E. Teplitsky, and J.K. Sutherland Endodontic access of Cerestore crowns J Endod 11 1985 555 558
    • (1985) J Endod , vol.11 , pp. 555-558
    • Teplitsky, P.E.1    Sutherland, J.K.2
  • 5
    • 0032407845 scopus 로고    scopus 로고
    • Providing endodontic care for teeth with ceramic crowns
    • M.W. Davis Providing endodontic care for teeth with ceramic crowns J Am Dent Assoc 129 1998 1746 1747
    • (1998) J Am Dent Assoc , vol.129 , pp. 1746-1747
    • Davis, M.W.1
  • 6
    • 0025814887 scopus 로고
    • Castable glass ceramic crowns and their reaction to endodontic therapy
    • B.D. Cohen, and J.A. Wallace Castable glass ceramic crowns and their reaction to endodontic therapy Oral Surg Oral Med Oral Pathol 72 1991 108 110
    • (1991) Oral Surg Oral Med Oral Pathol , vol.72 , pp. 108-110
    • Cohen, B.D.1    Wallace, J.A.2
  • 9
    • 0028709614 scopus 로고
    • Fracture surface characterization of clinically failed all-ceramic crowns
    • J.Y. Thompson, K.J. Anusavice, A. Naman, and H.F. Morris Fracture surface characterization of clinically failed all-ceramic crowns J Dent Res 73 1994 1824 1832
    • (1994) J Dent Res , vol.73 , pp. 1824-1832
    • Thompson, J.Y.1    Anusavice, K.J.2    Naman, A.3    Morris, H.F.4
  • 10
    • 3242748246 scopus 로고    scopus 로고
    • Dental ceramics: Current thinking and trends
    • J.R. Kelly Dental ceramics: current thinking and trends Dent Clin N Am 48 2004 513 530
    • (2004) Dent Clin N Am , vol.48 , pp. 513-530
    • Kelly, J.R.1
  • 11
    • 0024057893 scopus 로고
    • Endodontic access cavities in porcelain jacket crowns - Two methods of repair compared
    • A.N. Stokes, J.A. Hood, P.B. Casley, R.M. Cawley, and G.J. Cho Endodontic access cavities in porcelain jacket crowns - two methods of repair compared Restorative Dent 4 1988 56 58
    • (1988) Restorative Dent , vol.4 , pp. 56-58
    • Stokes, A.N.1    Hood, J.A.2    Casley, P.B.3    Cawley, R.M.4    Cho, G.J.5
  • 12
    • 0036580814 scopus 로고    scopus 로고
    • Fracture strength of amalgam crowns with repaired endodontic access
    • K.A. Hachmeister, W.J. Dunn, D.F. Murchison, and R.B. Larsen Fracture strength of amalgam crowns with repaired endodontic access Oper Dent 27 2002 254 258
    • (2002) Oper Dent , vol.27 , pp. 254-258
    • Hachmeister, K.A.1    Dunn, W.J.2    Murchison, D.F.3    Larsen, R.B.4
  • 13
    • 2942551095 scopus 로고    scopus 로고
    • A comparison of the porcelain fracture resistance of screw-retained and cement-retained implant-supported metal-ceramic crowns
    • E. Torrado, C. Ercoli, M.A. Mardini, G.N. Graser, R.H. Tallents, and L. Cordaro A comparison of the porcelain fracture resistance of screw-retained and cement-retained implant-supported metal-ceramic crowns J Prosthet Dent 91 2004 532 537
    • (2004) J Prosthet Dent , vol.91 , pp. 532-537
    • Torrado, E.1    Ercoli, C.2    Mardini, M.A.3    Graser, G.N.4    Tallents, R.H.5    Cordaro, L.6
  • 14
    • 0028491971 scopus 로고
    • Relative frequency of teeth needing endodontic treatment in 3350 consecutive endodontic patients
    • B.E. Wayman, J.A. Patten, and S.E. Dazey Relative frequency of teeth needing endodontic treatment in 3350 consecutive endodontic patients J Endod 20 1994 399 401
    • (1994) J Endod , vol.20 , pp. 399-401
    • Wayman, B.E.1    Patten, J.A.2    Dazey, S.E.3
  • 15
    • 0035502392 scopus 로고    scopus 로고
    • Procera AllCeram crowns followed for 5 to 10.5 years: A prospective clinical study
    • P. Odman, and B. Andersson Procera AllCeram crowns followed for 5 to 10.5 years: a prospective clinical study Int J Prosthodont 14 2001 504 509
    • (2001) Int J Prosthodont , vol.14 , pp. 504-509
    • Odman, P.1    Andersson, B.2
  • 20
    • 0037629915 scopus 로고    scopus 로고
    • An in vitro study to investigate the load at fracture of Procera AllCeram crowns with various thickness of occlusal veneer porcelain
    • Z. Harrington, A. McDonald, and J. Knowles An in vitro study to investigate the load at fracture of Procera AllCeram crowns with various thickness of occlusal veneer porcelain Int J Prosthodont 16 2003 54 58
    • (2003) Int J Prosthodont , vol.16 , pp. 54-58
    • Harrington, Z.1    McDonald, A.2    Knowles, J.3
  • 21
    • 2942547986 scopus 로고    scopus 로고
    • Fracture resistance of three all-ceramic restorative systems for posterior applications
    • K. Pallis, J.A. Griggs, R.D. Woody, G.E. Guillen, and A.W. Miller Fracture resistance of three all-ceramic restorative systems for posterior applications J Prosthet Dent 91 2004 561 569
    • (2004) J Prosthet Dent , vol.91 , pp. 561-569
    • Pallis, K.1    Griggs, J.A.2    Woody, R.D.3    Guillen, G.E.4    Miller, A.W.5
  • 22
    • 0030207640 scopus 로고    scopus 로고
    • Evaluation of porcelain surface treatments and agents for composite-to-porcelain repair
    • K.A. Kupiec, K.M. Wuertz, W.W. Barkmeier, and T.M. Wilwerding Evaluation of porcelain surface treatments and agents for composite-to-porcelain repair J Prosthet Dent 76 1996 119 124
    • (1996) J Prosthet Dent , vol.76 , pp. 119-124
    • Kupiec, K.A.1    Wuertz, K.M.2    Barkmeier, W.W.3    Wilwerding, T.M.4
  • 23
    • 0034251885 scopus 로고    scopus 로고
    • Approaches for intraoral repair of ceramic restorations
    • M.A. Latta, and W.W. Barkmeier Approaches for intraoral repair of ceramic restorations Compend Contin Educ Dent 21 2000 635 639 642-4
    • (2000) Compend Contin Educ Dent , vol.21 , pp. 635-639
    • Latta, M.A.1    Barkmeier, W.W.2
  • 25
    • 0032171898 scopus 로고    scopus 로고
    • Effect of etchant, etching period, and silane priming on bond strength to porcelain of composite resin
    • J.H. Chen, H. Matsumura, and M. Atsuta Effect of etchant, etching period, and silane priming on bond strength to porcelain of composite resin Oper Dent 23 1998 250 257
    • (1998) Oper Dent , vol.23 , pp. 250-257
    • Chen, J.H.1    Matsumura, H.2    Atsuta, M.3
  • 26
    • 0033146116 scopus 로고    scopus 로고
    • Clinically relevant approach to failure testing of all-ceramic restorations
    • J.R. Kelly Clinically relevant approach to failure testing of all-ceramic restorations J Prosthet Dent 81 1999 652 661
    • (1999) J Prosthet Dent , vol.81 , pp. 652-661
    • Kelly, J.R.1
  • 27
    • 0041491460 scopus 로고    scopus 로고
    • Stress distribution and failure mode of dental ceramic structures under Hertzian indentation
    • X.D. Dong, and B.W. Darvell Stress distribution and failure mode of dental ceramic structures under Hertzian indentation Dent Mater 19 2003 542 551
    • (2003) Dent Mater , vol.19 , pp. 542-551
    • Dong, X.D.1    Darvell, B.W.2
  • 28
    • 0038727300 scopus 로고    scopus 로고
    • An in vitro study of the compressive load at fracture of Procera AllCeram crowns with varying thickness of veneer porcelain
    • B. Webber, A. McDonald, and J. Knowles An in vitro study of the compressive load at fracture of Procera AllCeram crowns with varying thickness of veneer porcelain J Prosthet Dent 89 2003 154 160
    • (2003) J Prosthet Dent , vol.89 , pp. 154-160
    • Webber, B.1    McDonald, A.2    Knowles, J.3
  • 30
    • 0025492382 scopus 로고
    • Fracture surface analysis of dental ceramics: Clinically failed restorations
    • J.R. Kelly, R. Giordano, R. Pober, and M.J. Cima Fracture surface analysis of dental ceramics: clinically failed restorations Int J Prosthodont 3 1990 430 440
    • (1990) Int J Prosthodont , vol.3 , pp. 430-440
    • Kelly, J.R.1    Giordano, R.2    Pober, R.3    Cima, M.J.4
  • 31
    • 0034439683 scopus 로고    scopus 로고
    • Lifetime-limiting strength degradation from contact fatigue in dental ceramics
    • Y.G. Jung, I.M. Peterson, D.K. Kim, and B.R. Lawn Lifetime-limiting strength degradation from contact fatigue in dental ceramics J Dent Res 79 2000 722 731
    • (2000) J Dent Res , vol.79 , pp. 722-731
    • Jung, Y.G.1    Peterson, I.M.2    Kim, D.K.3    Lawn, B.R.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.