Effect of the sintering additive content on the non-protective oxidation behaviour of pressureless liquid-phase-sintered α-SiC in air

Author keywords

Liquid phase sintering; Oxidation; SiC

Indexed keywords

EUTECTIC PHASE; HIGH TEMPERATURE; LIQUID-PHASE-SINTERED; OXIDATION BEHAVIOURS; OXIDATION PROCESS; OXIDE SCALE; PRESSURELESS; RATE LAWS; SIC CERAMICS; SIC GRAINS; SINTERING ADDITIVES; YAG;

EID: 75749150058     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2009.10.008     Document Type: Article
Times cited : (25)

References (25)
  • 2
    • 0028382729 scopus 로고
    • In situ-toughened silicon-carbide
    • Padture N.P. In situ-toughened silicon-carbide. J. Am. Ceram. Soc. 77 2 (1994) 519-523
    • (1994) J. Am. Ceram. Soc. , vol.77 , Issue.2 , pp. 519-523
    • Padture, N.P.1
  • 3
    • 0035470704 scopus 로고    scopus 로고
    • Heat-resistant silicon carbide with aluminum nitride and erbium oxide
    • Kim Y.-W., Mitomo M., and Nishimura T. Heat-resistant silicon carbide with aluminum nitride and erbium oxide. J. Am. Ceram. Soc. 84 9 (2001) 2060-2064
    • (2001) J. Am. Ceram. Soc. , vol.84 , Issue.9 , pp. 2060-2064
    • Kim, Y.-W.1    Mitomo, M.2    Nishimura, T.3
  • 4
    • 0037410803 scopus 로고    scopus 로고
    • Thermal conductivity of liquid-phase-sintered silicon carbide
    • Sigl L.S. Thermal conductivity of liquid-phase-sintered silicon carbide. J. Eur. Ceram. Soc. 23 7 (2003) 1115-1122
    • (2003) J. Eur. Ceram. Soc. , vol.23 , Issue.7 , pp. 1115-1122
    • Sigl, L.S.1
  • 7
    • 33846382729 scopus 로고    scopus 로고
    • Effect of liquid-phase content on the contact mechanical properties of liquid-phase-sintered α-SiC
    • Borrero-López O., Ortiz A.L., Guiberteau F., and Padture N.P. Effect of liquid-phase content on the contact mechanical properties of liquid-phase-sintered α-SiC. J. Eur. Ceram. Soc. 27 6 (2007) 2521-2527
    • (2007) J. Eur. Ceram. Soc. , vol.27 , Issue.6 , pp. 2521-2527
    • Borrero-López, O.1    Ortiz, A.L.2    Guiberteau, F.3    Padture, N.P.4
  • 8
    • 34248582292 scopus 로고    scopus 로고
    • Microstructural design of sliding-wear-resistant liquid-phase-sintered SiC: an overview
    • Borrero-López O., Ortiz A.L., Guiberteau F., and Padture N.P. Microstructural design of sliding-wear-resistant liquid-phase-sintered SiC: an overview. J. Eur. Ceram. Soc. 27 11 (2007) 3351-3357
    • (2007) J. Eur. Ceram. Soc. , vol.27 , Issue.11 , pp. 3351-3357
    • Borrero-López, O.1    Ortiz, A.L.2    Guiberteau, F.3    Padture, N.P.4
  • 11
    • 33644682295 scopus 로고    scopus 로고
    • Correlation between microstructure and creep behavior in liquid-phase-sintered α-silicon carbide
    • Castillo-Rodríguez M., Muñoz A., and Domínguez-Rodríguez A. Correlation between microstructure and creep behavior in liquid-phase-sintered α-silicon carbide. J. Am. Ceram. Soc. 89 3 (2006) 960-967
    • (2006) J. Am. Ceram. Soc. , vol.89 , Issue.3 , pp. 960-967
    • Castillo-Rodríguez, M.1    Muñoz, A.2    Domínguez-Rodríguez, A.3
  • 13
    • 33750969652 scopus 로고    scopus 로고
    • Relationships between microstructure and electrical properties of liquid-phase-sintered silicon carbide materials using impedance spectroscopy
    • Can A., McLachlan D.S., Sauti G., and Herrmann M. Relationships between microstructure and electrical properties of liquid-phase-sintered silicon carbide materials using impedance spectroscopy. J. Eur. Ceram. Soc. 27 2-3 (2005) 1361-1363
    • (2005) J. Eur. Ceram. Soc. , vol.27 , Issue.2-3 , pp. 1361-1363
    • Can, A.1    McLachlan, D.S.2    Sauti, G.3    Herrmann, M.4
  • 14
    • 0034893838 scopus 로고    scopus 로고
    • Electrical and thermal conductivity of liquid phase sintered SiC
    • Volz E., Roosen A., Hartung W., and Winnacker A. Electrical and thermal conductivity of liquid phase sintered SiC. J. Eur. Ceram. Soc. 21 10-11 (2001) 2089-2093
    • (2001) J. Eur. Ceram. Soc. , vol.21 , Issue.10-11 , pp. 2089-2093
    • Volz, E.1    Roosen, A.2    Hartung, W.3    Winnacker, A.4
  • 15
    • 0033746134 scopus 로고    scopus 로고
    • Densification of liquid-phase-sintered silicon carbide
    • Pujar V.V., Jensen R.P., and Padture N.P. Densification of liquid-phase-sintered silicon carbide. J. Mater. Sci. Lett. 19 (2000) 1011-1014
    • (2000) J. Mater. Sci. Lett. , vol.19 , pp. 1011-1014
    • Pujar, V.V.1    Jensen, R.P.2    Padture, N.P.3
  • 16
    • 0032714756 scopus 로고    scopus 로고
    • Coarsening in liquid-phase-sintered α-SiC
    • Ye H., Pujar V.V., and Padture N.P. Coarsening in liquid-phase-sintered α-SiC. Acta Mater. 47 2 (1999) 481-487
    • (1999) Acta Mater. , vol.47 , Issue.2 , pp. 481-487
    • Ye, H.1    Pujar, V.V.2    Padture, N.P.3
  • 17
    • 0030718703 scopus 로고    scopus 로고
    • Oxidation of polycrystalline α-silicon carbide ceramic
    • Liu D.-M. Oxidation of polycrystalline α-silicon carbide ceramic. Ceram. Int. 23 5 (1997) 425-436
    • (1997) Ceram. Int. , vol.23 , Issue.5 , pp. 425-436
    • Liu, D.-M.1
  • 18
    • 36849138946 scopus 로고
    • Passivity during the oxidation of silicon at elevated temperatures
    • Wagner C. Passivity during the oxidation of silicon at elevated temperatures. J. Appl. Phys. 29 9 (1958) 1295-1297
    • (1958) J. Appl. Phys. , vol.29 , Issue.9 , pp. 1295-1297
    • Wagner, C.1
  • 19
    • 24944508406 scopus 로고
    • The effect of oxide volatilization on the oxidation kinetics of Cr and Fe-Cr alloys
    • Tedmon C.S.J. The effect of oxide volatilization on the oxidation kinetics of Cr and Fe-Cr alloys. J. Electrochem. Soc. 113 8 (1966) 766-768
    • (1966) J. Electrochem. Soc. , vol.113 , Issue.8 , pp. 766-768
    • Tedmon, C.S.J.1
  • 20
    • 0030868046 scopus 로고    scopus 로고
    • Paralinear oxidation of CVD SiC in water vapor
    • Opila E.J., and Hann Jr. R.E. Paralinear oxidation of CVD SiC in water vapor. J. Am. Ceram. Soc. 80 1 (1997) 197-205
    • (1997) J. Am. Ceram. Soc. , vol.80 , Issue.1 , pp. 197-205
    • Opila, E.J.1    Hann Jr., R.E.2
  • 21
    • 18144389366 scopus 로고    scopus 로고
    • Ceramic matrix composite corrosion models
    • Nickel K.G. Ceramic matrix composite corrosion models. J. Eur. Ceram. Soc. 25 10 (2005) 1699-1704
    • (2005) J. Eur. Ceram. Soc. , vol.25 , Issue.10 , pp. 1699-1704
    • Nickel, K.G.1
  • 22
    • 48949117347 scopus 로고    scopus 로고
    • Oxidation kinetics of pressureless liquid-phase-sintered α-SiC in ambient air at elevated temperatures
    • Rodríguez-Rojas F., Borrero-López O., Ortiz A.L., and Guiberteau F. Oxidation kinetics of pressureless liquid-phase-sintered α-SiC in ambient air at elevated temperatures. J. Mater. Res. 23 6 (2008) 1689-1700
    • (2008) J. Mater. Res. , vol.23 , Issue.6 , pp. 1689-1700
    • Rodríguez-Rojas, F.1    Borrero-López, O.2    Ortiz, A.L.3    Guiberteau, F.4
  • 23
    • 70349973859 scopus 로고    scopus 로고
    • 2 sintering atmosphere on the high-temperature oxidation behaviour of pressureless liquid-phase-sintered α-SiC in air
    • 2 sintering atmosphere on the high-temperature oxidation behaviour of pressureless liquid-phase-sintered α-SiC in air. J. Eur. Ceram. Soc. 30 1 (2010) 119-128
    • (2010) J. Eur. Ceram. Soc. , vol.30 , Issue.1 , pp. 119-128
    • Rodríguez-Rojas, F.1    Ortiz, A.L.2    Borrero-López, O.3    Guiberteau, F.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.