Evolution of the γ/γ′ interface width in a commercial nickel base superalloy studied by three-dimensional atom probe tomography

Author keywords

Interfaces; Nickel superalloy; Three dimensional atom probe (3DAP)

Indexed keywords

COMMERCIAL NICKEL BASE SUPERALLOYS; CONTINUOUS COOLING; DIFFUSE INTERFACES; INTERFACES; ISOTHERMAL AGING; NICKEL SUPERALLOY; SHARP INTERFACES; THREE-DIMENSIONAL ATOM PROBE (3DAP); THREE-DIMENSIONAL ATOM PROBES;

EID: 64849086679     PISSN: 13596462     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.scriptamat.2009.03.011     Document Type: Article
Times cited : (52)

References (23)
  • 2
    • 0004247029 scopus 로고    scopus 로고
    • Kissinger R.D., Deye D.J., Anton D.L., Cetel A.D., Nathal M.V., Pollock T.M., and Woodford D.A. (Eds), TMS, Warrendale, PA
    • Wlodek S.T., Kelly M., and Alden D.A. In: Kissinger R.D., Deye D.J., Anton D.L., Cetel A.D., Nathal M.V., Pollock T.M., and Woodford D.A. (Eds). Superalloys 1996 (1996), TMS, Warrendale, PA 129-136
    • (1996) Superalloys 1996 , pp. 129-136
    • Wlodek, S.T.1    Kelly, M.2    Alden, D.A.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.