메뉴 건너뛰기




Volumn 28, Issue 5, 2008, Pages 1085-1090

The effects of dental grinding and sandblasting on ageing and fatigue behavior of dental zirconia (Y-TZP) ceramics

Author keywords

Ageing; Dental zirconia; Fatigue

Indexed keywords

DENTAL MATERIALS; FATIGUE OF MATERIALS; GRINDING (COMMINUTION); PLASTIC DEFORMATION; STRESS CORROSION CRACKING; THERMAL AGING;

EID: 38149012120     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2007.09.013     Document Type: Article
Times cited : (152)

References (24)
  • 1
    • 0026877704 scopus 로고
    • A review of strength properties of dental ceramics
    • Hondrum S.O. A review of strength properties of dental ceramics. J. Prosthet. Dent. 67 (1992) 859-865
    • (1992) J. Prosthet. Dent. , vol.67 , pp. 859-865
    • Hondrum, S.O.1
  • 2
    • 0030691360 scopus 로고    scopus 로고
    • Ceramics in restorative and prosthetic dentistry
    • Kelly J.R. Ceramics in restorative and prosthetic dentistry. Annu. Rev. Mater. Sci. 27 (1997) 443-468
    • (1997) Annu. Rev. Mater. Sci. , vol.27 , pp. 443-468
    • Kelly, J.R.1
  • 3
    • 0029436750 scopus 로고
    • Zirconium post. A new all-ceramic concept for nonvital abutment teeth
    • Meyeberg K.H., Lüthy H., and Schärer P. Zirconium post. A new all-ceramic concept for nonvital abutment teeth. J. Esthet. Dent. 7 (1995) 73-80
    • (1995) J. Esthet. Dent. , vol.7 , pp. 73-80
    • Meyeberg, K.H.1    Lüthy, H.2    Schärer, P.3
  • 4
    • 0002438153 scopus 로고    scopus 로고
    • The zirconium oxide abutment: an all-ceramic abutment for the esthetic improvement of implant superstructures Quintessence
    • Wohlwend A., Studer S., and Schärer P. The zirconium oxide abutment: an all-ceramic abutment for the esthetic improvement of implant superstructures Quintessence. Dent. Technol. 1 (1997) 63-74
    • (1997) Dent. Technol. , vol.1 , pp. 63-74
    • Wohlwend, A.1    Studer, S.2    Schärer, P.3
  • 6
    • 84979438879 scopus 로고
    • Strengthening by surface damage in metastable tetragonal zirconia
    • Gupta T.K. Strengthening by surface damage in metastable tetragonal zirconia. J. Am. Ceram. Soc. 63 (1980) 117-121
    • (1980) J. Am. Ceram. Soc. , vol.63 , pp. 117-121
    • Gupta, T.K.1
  • 7
    • 0033278142 scopus 로고    scopus 로고
    • Influence of clenching intensity on bite force balance, occlusal contact area, and average bite pressure
    • Hidaka O., Iwasaki M., Saito M., and Morimoto T. Influence of clenching intensity on bite force balance, occlusal contact area, and average bite pressure. J. Dent. Res. 78 (1999) 1336-1344
    • (1999) J. Dent. Res. , vol.78 , pp. 1336-1344
    • Hidaka, O.1    Iwasaki, M.2    Saito, M.3    Morimoto, T.4
  • 8
    • 0041491423 scopus 로고    scopus 로고
    • The effect of thermocycling on the strength of porcelain laminate veneer materials
    • Addison O., Fleming G.J., and Marquis P.M. The effect of thermocycling on the strength of porcelain laminate veneer materials. Dent. Mater. 19 (2003) 291-297
    • (2003) Dent. Mater. , vol.19 , pp. 291-297
    • Addison, O.1    Fleming, G.J.2    Marquis, P.M.3
  • 11
    • 0029237462 scopus 로고
    • Environmental degradation of zirconia ceramics
    • Lawson S. Environmental degradation of zirconia ceramics. J. Eur. Ceram. Soc. 15 (1995) 485-502
    • (1995) J. Eur. Ceram. Soc. , vol.15 , pp. 485-502
    • Lawson, S.1
  • 13
    • 26844583254 scopus 로고    scopus 로고
    • What future for zirconia as a biomaterial?
    • Chevalier J. What future for zirconia as a biomaterial?. Biomaterials 27 (2006) 535-543
    • (2006) Biomaterials , vol.27 , pp. 535-543
    • Chevalier, J.1
  • 14
    • 0033762148 scopus 로고    scopus 로고
    • Effect of surface coating on water migration into resin-modified glass ionomer cements: a magnetic resonance micro-imaging study
    • Jevnikar P., Sersa I., Sepe A., Jarh O., and Funduk N. Effect of surface coating on water migration into resin-modified glass ionomer cements: a magnetic resonance micro-imaging study. Magn. Reson. Med. 44 (2000) 686-691
    • (2000) Magn. Reson. Med. , vol.44 , pp. 686-691
    • Jevnikar, P.1    Sersa, I.2    Sepe, A.3    Jarh, O.4    Funduk, N.5
  • 15
  • 16
    • 0030244480 scopus 로고    scopus 로고
    • Effect of heat treatment on grain size, phase assemblage, and mechanical properties of 3 mol% Y-TZP
    • Ruiz L., and Readey M.J. Effect of heat treatment on grain size, phase assemblage, and mechanical properties of 3 mol% Y-TZP. J. Am. Ceram. Soc. 79 (1996) 2331-2340
    • (1996) J. Am. Ceram. Soc. , vol.79 , pp. 2331-2340
    • Ruiz, L.1    Readey, M.J.2
  • 17
    • 2342500842 scopus 로고    scopus 로고
    • Critical effect of cubic phase on aging in 3 mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis
    • Chevalier J., Deville S., Münch E., Jullian R., and Lair F. Critical effect of cubic phase on aging in 3 mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis. Biomaterials 25 (2004) 5539-5545
    • (2004) Biomaterials , vol.25 , pp. 5539-5545
    • Chevalier, J.1    Deville, S.2    Münch, E.3    Jullian, R.4    Lair, F.5
  • 18
    • 0024715577 scopus 로고
    • Metastability of the mertensitic tranformation in a 12 mol% ceria-zirconia alloy. II. Grinding studies
    • Swain M.V., and Hannink R.H.J. Metastability of the mertensitic tranformation in a 12 mol% ceria-zirconia alloy. II. Grinding studies. J. Am. Ceram. Soc. 72 (1989) 1358-1364
    • (1989) J. Am. Ceram. Soc. , vol.72 , pp. 1358-1364
    • Swain, M.V.1    Hannink, R.H.J.2
  • 19
    • 0033222358 scopus 로고    scopus 로고
    • The effect of grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic
    • Kosmač T., Oblak C., Jevnikar P., Funduk N., and Marion L. The effect of grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic. Dent. Mater. 15 (1999) 426-433
    • (1999) Dent. Mater. , vol.15 , pp. 426-433
    • Kosmač, T.1    Oblak, C.2    Jevnikar, P.3    Funduk, N.4    Marion, L.5
  • 20
    • 34250164925 scopus 로고    scopus 로고
    • The biaxial flexural strength and fatigue property of Lava™ Y-TZP dental ceramic
    • Pittayachawan P., McDonald A., Petrie A., and Knowles J.C. The biaxial flexural strength and fatigue property of Lava™ Y-TZP dental ceramic. Dent. Mater. 23 (2007) 1018-1029
    • (2007) Dent. Mater. , vol.23 , pp. 1018-1029
    • Pittayachawan, P.1    McDonald, A.2    Petrie, A.3    Knowles, J.C.4
  • 21
    • 0033225415 scopus 로고    scopus 로고
    • Subcritical crack propagation in 3Y-TZP ceramics: static and cycling fatigue
    • Chevalier J., Olagnon C., and Fantozzi G. Subcritical crack propagation in 3Y-TZP ceramics: static and cycling fatigue. J. Am. Ceram. Soc. 82 (1999) 3129-3138
    • (1999) J. Am. Ceram. Soc. , vol.82 , pp. 3129-3138
    • Chevalier, J.1    Olagnon, C.2    Fantozzi, G.3
  • 23
    • 32044466739 scopus 로고    scopus 로고
    • The influence of surface modification techniques on the performance of a Y-TZP dental ceramic
    • Curtis A.R., Wright A.J., and Fleming G.J.P. The influence of surface modification techniques on the performance of a Y-TZP dental ceramic. J. Dent. 34 (2006) 195-206
    • (2006) J. Dent. , vol.34 , pp. 195-206
    • Curtis, A.R.1    Wright, A.J.2    Fleming, G.J.P.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.