메뉴 건너뛰기




Volumn 27, Issue 1, 1997, Pages 443-468

Ceramics in restorative and prosthetic dentistry

Author keywords

Aesthetics; Ceramics; Clinical failure; Dentistry; Feldspar; Fracture; History; Leucite; Prostheses; Wear

Indexed keywords

BONDING; COMPOSITION; DENTAL CEMENT; DENTAL PROSTHESES; FELDSPAR; FRACTURE; MICROSTRUCTURE; SURFACE TREATMENT; WEAR OF MATERIALS;

EID: 0030691360     PISSN: 00846600     EISSN: None     Source Type: Journal    
DOI: 10.1146/annurev.matsci.27.1.443     Document Type: Article
Times cited : (260)

References (145)
  • 5
    • 0030203769 scopus 로고    scopus 로고
    • Dental ceramic restorative systems
    • Giordano RA. 1996. Dental ceramic restorative systems. Compendium 17: 779-802
    • (1996) Compendium , vol.17 , pp. 779-802
    • Giordano, R.A.1
  • 7
    • 0022140086 scopus 로고
    • Development of dental ceramics
    • Jones DW. 1985. Development of dental ceramics. Dent. Clin. North Am. 29:621-44
    • (1985) Dent. Clin. North Am. , vol.29 , pp. 621-644
    • Jones, D.W.1
  • 8
    • 9644290506 scopus 로고
    • Dental porcelain
    • ed. JA von Fraunhofer, London: Butterworths
    • Southan DE. 1975. Dental porcelain. In Scientific Aspects of Dental Materials, ed. JA von Fraunhofer, pp. 277-305. London: Butterworths
    • (1975) Scientific Aspects of Dental Materials , pp. 277-305
    • Southan, D.E.1
  • 11
    • 0014548805 scopus 로고
    • X-ray diffraction analysis of dental porcelain
    • Lehman ML, Isard JO. 1969. X-ray diffraction analysis of dental porcelain. J. Dent. Res. 48:543-45
    • (1969) J. Dent. Res. , vol.48 , pp. 543-545
    • Lehman, M.L.1    Isard, J.O.2
  • 13
    • 9644256802 scopus 로고
    • Phase composition of crown and inlay porcelains
    • Hodson JT. 1959. Phase composition of crown and inlay porcelains. J. Dent. Res. 38:483-90
    • (1959) J. Dent. Res. , vol.38 , pp. 483-490
    • Hodson, J.T.1
  • 15
    • 0017921276 scopus 로고
    • On the crystallization of the glassy phases in whitewares
    • Hermansson L, Carlsson R. 1978. On the crystallization of the glassy phases in whitewares. Trans. Br. Ceram. Soc. 77(2):32-35
    • (1978) Trans. Br. Ceram. Soc. , vol.77 , Issue.2 , pp. 32-35
    • Hermansson, L.1    Carlsson, R.2
  • 16
    • 0017907682 scopus 로고
    • Crystallization of glasses in the primary phase field of leucite in the potassium oxide-aluminum oxide-silicon dioxide system
    • Rouf MA, Hermansson L, Carlsson R. 1978. Crystallization of glasses in the primary phase field of leucite in the potassium oxide-aluminum oxide-silicon dioxide system. Trans. Br. Ceram. Soc. 77(2):36-39
    • (1978) Trans. Br. Ceram. Soc. , vol.77 , Issue.2 , pp. 36-39
    • Rouf, M.A.1    Hermansson, L.2    Carlsson, R.3
  • 21
    • 9644288998 scopus 로고
    • Thermal expansion of silicate fluxes in the crystalline and glassy states
    • 20a. Orlowski HJ, Koenig CJ. 1941. Thermal expansion of silicate fluxes in the crystalline and glassy states. J. Am. Ceram. Soc. 24:80-84
    • (1941) J. Am. Ceram. Soc. , vol.24 , pp. 80-84
    • Orlowski, H.J.1    Koenig, C.J.2
  • 22
    • 0022671798 scopus 로고
    • The effect of the leucite transformation on dental porcelain expansion
    • Mackert JR, Butts MB, Fairhurst CW. 1986. The effect of the leucite transformation on dental porcelain expansion. Dent. Mater. 2:32-36
    • (1986) Dent. Mater. , vol.2 , pp. 32-36
    • Mackert, J.R.1    Butts, M.B.2    Fairhurst, C.W.3
  • 23
    • 0024388304 scopus 로고
    • Phase identification in dental porcelains for ceramo-metallic restorations
    • Barreiro MM, Riesgo O, Vincente EE. 1989. Phase identification in dental porcelains for ceramo-metallic restorations. Dent. Mater. 5:51-57
    • (1989) Dent. Mater. , vol.5 , pp. 51-57
    • Barreiro, M.M.1    Riesgo, O.2    Vincente, E.E.3
  • 25
    • 0028381562 scopus 로고
    • The effect of microstructural features on the biaxial flexural strength of leucite reinforced glass-ceramics
    • Shareef MY, Van Noort R, Messer PF, Piddock V. 1994. The effect of microstructural features on the biaxial flexural strength of leucite reinforced glass-ceramics. J. Mater. Sci. Mater. Med. 5:113-18
    • (1994) J. Mater. Sci. Mater. Med. , vol.5 , pp. 113-118
    • Shareef, M.Y.1    Van Noort, R.2    Messer, P.F.3    Piddock, V.4
  • 26
    • 84979340076 scopus 로고
    • Machinable glass-ceramics based upon tetrasilicic mica
    • Grossman DG. 1972. Machinable glass-ceramics based upon tetrasilicic mica. J. Am. Ceram. Soc. 55:446-49
    • (1972) J. Am. Ceram. Soc. , vol.55 , pp. 446-449
    • Grossman, D.G.1
  • 27
    • 0014420096 scopus 로고
    • Advances in dental ceramics
    • MacCulloch WT. 1968. Advances in dental ceramics. Br. Dent. J. 124:361-65
    • (1968) Br. Dent. J. , vol.124 , pp. 361-365
    • MacCulloch, W.T.1
  • 29
    • 0348164095 scopus 로고
    • Processing a dental ceramic by casting methods
    • ed. WJ O'Brien, RG Craig, Westerville, OH: Am. Ceram. Soc.
    • Grossman DG. 1985. Processing a dental ceramic by casting methods. In Proc. Conf. Recent Developments in Dental Ceramics, ed. WJ O'Brien, RG Craig, pp. 19-40. Westerville, OH: Am. Ceram. Soc.
    • (1985) Proc. Conf. Recent Developments in Dental Ceramics , pp. 19-40
    • Grossman, D.G.1
  • 30
  • 31
    • 0000653434 scopus 로고
    • The reinforcement of dental porcelain with ceramic oxides
    • McLean JW, Hughs TH. 1965. The reinforcement of dental porcelain with ceramic oxides. Br. Dent. J. 119:251-67
    • (1965) Br. Dent. J. , vol.119 , pp. 251-267
    • McLean, J.W.1    Hughs, T.H.2
  • 33
    • 9644252417 scopus 로고
    • Transfer molded "all ceramic crowns": The Cerestore system
    • ed. WJ O'Brien, RG Craig, Columbus, OH: Am. Ceram. Soc.
    • Starling LB. 1985. Transfer molded "all ceramic crowns": the Cerestore system. In Proc. Conf. Recent Developments in Dental Ceramics: Ceramic Engineering and Science, ed. WJ O'Brien, RG Craig, 6(1-2):41-56. Columbus, OH: Am. Ceram. Soc.
    • (1985) Proc. Conf. Recent Developments in Dental Ceramics: Ceramic Engineering and Science , vol.6 , Issue.1-2 , pp. 41-56
    • Starling, L.B.1
  • 34
    • 0024986205 scopus 로고
    • Vita In-Ceram, a new system for producing aluminum oxide crown and bridge substructures
    • Clause H. 1990. Vita In-Ceram, a new system for producing aluminum oxide crown and bridge substructures (Ger-man). Quint. Zahntech. 16:35-46
    • (1990) Quint. Zahntech. , vol.16 , pp. 35-46
    • Clause, H.1
  • 36
    • 0029327839 scopus 로고
    • Mechanical properties and microstructure of In-Ceram, a ceramic-glass composite for dental crowns
    • Hornberger H, Marquis PM. 1995. Mechanical properties and microstructure of In-Ceram, a ceramic-glass composite for dental crowns. Glastech. Ber. Sci. Technol. 68:188-94
    • (1995) Glastech. Ber. Sci. Technol. , vol.68 , pp. 188-194
    • Hornberger, H.1    Marquis, P.M.2
  • 37
    • 0029294815 scopus 로고
    • Relative flexural strength of six new ceramic materials
    • Seghi RR, Sorensen JA. 1995. Relative flexural strength of six new ceramic materials. Int. J. Prosthodont. 8:239-46
    • (1995) Int. J. Prosthodont. , vol.8 , pp. 239-246
    • Seghi, R.R.1    Sorensen, J.A.2
  • 38
    • 9544221770 scopus 로고
    • Highstrength alumina crowns and fixed partial dentures generated by copy-milling technology
    • McLaren EA, Sorensen JA. 1995. Highstrength alumina crowns and fixed partial dentures generated by copy-milling technology. Quint. Dent. Technol. 18:31-38
    • (1995) Quint. Dent. Technol. , vol.18 , pp. 31-38
    • McLaren, E.A.1    Sorensen, J.A.2
  • 39
    • 1842721165 scopus 로고    scopus 로고
    • Clinical and technical aspects of the CEREC In-Ceram crown
    • WH Mörmann, Chicago: Quintessence
    • Bindl A, Mörmann WH. 1996. Clinical and technical aspects of the CEREC In-Ceram crown. In CAD/CIM in Aesthetic Dentistry, ed. WH Mörmann, pp. 441-62. Chicago: Quintessence
    • (1996) CAD/CIM in Aesthetic Dentistry , pp. 441-462
    • Bindl, A.1    Mörmann, W.H.2
  • 40
    • 0027546239 scopus 로고
    • A new all-ceramic crown. A dense-sintered, high purity alumina coping with porcelain
    • Andersson M, Oden A. 1993. A new all-ceramic crown. A dense-sintered, high purity alumina coping with porcelain. Acta Odont. Scand. 51:59-64
    • (1993) Acta Odont. Scand. , vol.51 , pp. 59-64
    • Andersson, M.1    Oden, A.2
  • 41
    • 0005063671 scopus 로고    scopus 로고
    • Procera aluminum oxide ceramics: A new way to achieve stability, precision, and aesthetics in all-ceramic restorations
    • Heganbarth EA. 1996. Procera aluminum oxide ceramics: a new way to achieve stability, precision, and aesthetics in all-ceramic restorations. Quint. Dent. Technol. 20:21-34
    • (1996) Quint. Dent. Technol. , vol.20 , pp. 21-34
    • Heganbarth, E.A.1
  • 44
    • 0342731052 scopus 로고
    • Development and testing of ceramics for dental restorations
    • ed. G Fischman, A Clare, L Hench, Westerville, OH: Am. Ceram. Soc.
    • Anusavice KJ. 1995. Development and testing of ceramics for dental restorations. In Bioceramics: Materials and Applications, ed. G Fischman, A Clare, L Hench, 48:101-24. Westerville, OH: Am. Ceram. Soc.
    • (1995) Bioceramics: Materials and Applications , vol.48 , pp. 101-124
    • Anusavice, K.J.1
  • 46
    • 0027638565 scopus 로고
    • Kinetics of isothermal phase transformations in a dental porcelain
    • Barreiro MM, Vincente EE. 1993. Kinetics of isothermal phase transformations in a dental porcelain. J. Mater. Sci. Mater. Med. 4:431-36
    • (1993) J. Mater. Sci. Mater. Med. , vol.4 , pp. 431-436
    • Barreiro, M.M.1    Vincente, E.E.2
  • 48
    • 0026115101 scopus 로고
    • Quantitative X-ray diffraction determination of leucite thermal instability in dental porcelain
    • Mackert JR, Evans AL. 1991. Quantitative X-ray diffraction determination of leucite thermal instability in dental porcelain. J. Am. Ceram. Soc. 74:450-53
    • (1991) J. Am. Ceram. Soc. , vol.74 , pp. 450-453
    • Mackert, J.R.1    Evans, A.L.2
  • 50
    • 0015371484 scopus 로고
    • Calculation of interfacial stresses in dental porcelain bonded to gold alloy substrate
    • Nielsen JP, Tuccillo JJ. 1972. Calculation of interfacial stresses in dental porcelain bonded to gold alloy substrate. J. Dent. Res. 51:1043-47
    • (1972) J. Dent. Res. , vol.51 , pp. 1043-1047
    • Nielsen, J.P.1    Tuccillo, J.J.2
  • 51
    • 0026112383 scopus 로고
    • Effect of cooling rate on leucite volume fraction in dental porcelains
    • Mackert JR, Evans AL. 1991. Effect of cooling rate on leucite volume fraction in dental porcelains. J. Dent. Res. 70:137-39
    • (1991) J. Dent. Res. , vol.70 , pp. 137-139
    • Mackert, J.R.1    Evans, A.L.2
  • 52
    • 0029318140 scopus 로고
    • Isothermal anneal effect on leucite content in dental porcelains
    • Mackert JR, Twiggs SW, Evans AL. 1995. Isothermal anneal effect on leucite content in dental porcelains. J. Dent. Res. 74:1259-65
    • (1995) J. Dent. Res. , vol.74 , pp. 1259-1265
    • Mackert, J.R.1    Twiggs, S.W.2    Evans, A.L.3
  • 53
    • 0022671798 scopus 로고
    • The effect of leucite transformation on dental porcelain expansion
    • Mackert JR, Butts MB, Fairhurst CW. 1986. The effect of leucite transformation on dental porcelain expansion. Dent. Mater. 2:32-36
    • (1986) Dent. Mater. , vol.2 , pp. 32-36
    • Mackert, J.R.1    Butts, M.B.2    Fairhurst, C.W.3
  • 54
    • 0024399223 scopus 로고
    • Influence of framework design, contraction mismatch, and thermal history on porcelain checking in fixed partial dentures
    • Anusavice KJ, Gray AE. 1989. Influence of framework design, contraction mismatch, and thermal history on porcelain checking in fixed partial dentures. Dent. Mater. 5:58-63
    • (1989) Dent. Mater. , vol.5 , pp. 58-63
    • Anusavice, K.J.1    Gray, A.E.2
  • 56
    • 0028381562 scopus 로고
    • The effect of microstructural features on the biaxial flexure strength of leucite reinforced glass-ceramics
    • Shareef MY, Van Noort R, Messer PF, Piddock V. 1994. The effect of microstructural features on the biaxial flexure strength of leucite reinforced glass-ceramics. J. Mater. Sci. Mater. Med. 5:113-18
    • (1994) J. Mater. Sci. Mater. Med. , vol.5 , pp. 113-118
    • Shareef, M.Y.1    Van Noort, R.2    Messer, P.F.3    Piddock, V.4
  • 57
    • 0346535808 scopus 로고    scopus 로고
    • Evidence of a critical leucite particle radius for microcracking in dental porcelains
    • IADR Abstr.
    • Mackert JR, Russell CM, Evans-Williams AL. 1996. Evidence of a critical leucite particle radius for microcracking in dental porcelains. J. Dent. Rex. 75(IADR Abstr.):126:A866
    • (1996) J. Dent. Rex. , vol.75 , pp. 126
    • Mackert, J.R.1    Russell, C.M.2    Evans-Williams, A.L.3
  • 59
    • 0025492382 scopus 로고
    • Fracture surface analysis of dental ceramics, clinically-failed restorations
    • Kelly JR, Giordano R, Pober R, Cima MJ. 1990. Fracture surface analysis of dental ceramics, clinically-failed restorations. Int. J. Prosthodont. 3:430-40
    • (1990) Int. J. Prosthodont. , vol.3 , pp. 430-440
    • Kelly, J.R.1    Giordano, R.2    Pober, R.3    Cima, M.J.4
  • 60
    • 0028709614 scopus 로고
    • Fracture surface characterization of clinically failed all-ceramic crowns
    • Thompson JY, Anusavice KJ, Morris H. 1994. Fracture surface characterization of clinically failed all-ceramic crowns. J. Dent. Res. 73:1824-32
    • (1994) J. Dent. Res. , vol.73 , pp. 1824-1832
    • Thompson, J.Y.1    Anusavice, K.J.2    Morris, H.3
  • 61
    • 0026891764 scopus 로고
    • Tensile stresses in glass-ceramic crowns: Effect of flaws and cement voids
    • Anusavice KJ, Hojjatie B. 1992. Tensile stresses in glass-ceramic crowns: effect of flaws and cement voids. Int. J. Prosthodont. 5:351-58
    • (1992) Int. J. Prosthodont. , vol.5 , pp. 351-358
    • Anusavice, K.J.1    Hojjatie, B.2
  • 62
    • 9644282611 scopus 로고
    • Failure loads of bonded ceramics influenced by hydrostatic compressive stresses
    • Abstr.
    • Morris DR, Kelly JR. 1995. Failure loads of bonded ceramics influenced by hydrostatic compressive stresses. J. Dent. Res. 74(Abstr.):220:A666
    • (1995) J. Dent. Res. , vol.74 , pp. 220
    • Morris, D.R.1    Kelly, J.R.2
  • 63
    • 9644308956 scopus 로고    scopus 로고
    • All-ceramic crown failure as a function of occlusal contact location
    • IADR Abstr.
    • Ellert DO, Kelly JR. 1997. All-ceramic crown failure as a function of occlusal contact location. J. Dent. Res. 76(IADR Abstr.) 392:A3030
    • (1997) J. Dent. Res. , vol.76 , pp. 392
    • Ellert, D.O.1    Kelly, J.R.2
  • 64
    • 0346212703 scopus 로고
    • Clinical evaluation of dental restorative materials - Final report
    • San Francisco: Letterman Army Inst. Res.
    • Moffa JP. 1988. Clinical evaluation of dental restorative materials - final report. Interagency Agreement No. IYOI-DE40001-05, San Francisco: Letterman Army Inst. Res.
    • (1988) Interagency Agreement No. IYOI-DE40001-05
    • Moffa, J.P.1
  • 65
    • 0142261200 scopus 로고
    • Clinical application of bonded Dicor crowns: A two year report
    • IADR Abstr.
    • Malament KA, Grossman DG. 1990. Clinical application of bonded Dicor crowns: a two year report. J. Dent. Res. 69(IADR Abstr.) 299:A1523
    • (1990) J. Dent. Res. , vol.69 , pp. 299
    • Malament, K.A.1    Grossman, D.G.2
  • 66
    • 0042836087 scopus 로고
    • Bonded vs non-bonded Dicor crowns
    • AADR Abstr.
    • Malament KA, Grossman DG. 1992. Bonded vs non-bonded Dicor crowns. J. Dent Res. 71(AADR Abstr.) 321:A1720
    • (1992) J. Dent Res. , vol.71 , pp. 321
    • Malament, K.A.1    Grossman, D.G.2
  • 67
    • 0004842604 scopus 로고
    • The strength and weakness of brittle materials
    • Phillips CJ. 1965. The strength and weakness of brittle materials. Am. Sci. 53:20-51
    • (1965) Am. Sci. , vol.53 , pp. 20-51
    • Phillips, C.J.1
  • 68
    • 0026136085 scopus 로고
    • Effect of polymer coatings on the strength of indented soda-lime glass
    • Ritter JE, Lin MR. 1991. Effect of polymer coatings on the strength of indented soda-lime glass. Glass Technol. 32:51-4
    • (1991) Glass Technol. , vol.32 , pp. 51-54
    • Ritter, J.E.1    Lin, M.R.2
  • 70
    • 0030154926 scopus 로고    scopus 로고
    • Contact damage as a failure mode during in vitro testing
    • Harvey CK, Kelly JR. 1996. Contact damage as a failure mode during in vitro testing. J. Prosthadont. 5:95-100
    • (1996) J. Prosthadont. , vol.5 , pp. 95-100
    • Harvey, C.K.1    Kelly, J.R.2
  • 71
    • 0029318343 scopus 로고
    • Failure of all-ceramic fixed partial dentures in vitro and in vivo: Analysis and modeling
    • Kelly JR, Tesk JA, Sorensen JA. 1995. Failure of all-ceramic fixed partial dentures in vitro and in vivo: analysis and modeling. J. Dent. Res. 74:1253-58
    • (1995) J. Dent. Res. , vol.74 , pp. 1253-1258
    • Kelly, J.R.1    Tesk, J.A.2    Sorensen, J.A.3
  • 72
    • 9644271351 scopus 로고
    • Clinically relevant all-ceramic FPD mechanical test analogs
    • Abstr.
    • Kelly JR, Tesk JA. 1995. Clinically relevant all-ceramic FPD mechanical test analogs. J. Dent. Res. 74(Abstr.):159:A1184
    • (1995) J. Dent. Res. , vol.74 , pp. 159
    • Kelly, J.R.1    Tesk, J.A.2
  • 73
    • 0345990869 scopus 로고
    • Fabrication and failure behavior of an all-ceramic FPD test analog
    • Abstr.
    • Grant GT, Kelly JR. 1995. Fabrication and failure behavior of an all-ceramic FPD test analog. J. Dent. Res. 74(Abstr.):160:A1185
    • (1995) J. Dent. Res. , vol.74 , pp. 160
    • Grant, G.T.1    Kelly, J.R.2
  • 74
    • 9644255352 scopus 로고    scopus 로고
    • Influence of veneering material on failure of In-Ceram FPD analogs
    • IADR Abstr.
    • Fahncke CR, Kelly JR, Antonucci JM. 1997. Influence of veneering material on failure of In-Ceram FPD analogs. J. Dent. Res. 76(IADR Abstr.) 311:A2378
    • (1997) J. Dent. Res. , vol.76 , pp. 311
    • Fahncke, C.R.1    Kelly, J.R.2    Antonucci, J.M.3
  • 76
    • 0015026649 scopus 로고
    • Studies on the wear of porcelain, enamel and gold
    • Monasky GE. 1971. Studies on the wear of porcelain, enamel and gold. J. Prosthet. Dent. 25:299-306
    • (1971) J. Prosthet. Dent. , vol.25 , pp. 299-306
    • Monasky, G.E.1
  • 78
    • 0024024131 scopus 로고
    • Occlusal contact wear of prosthodontic materials: An in vivo study
    • Ekfeldt A, Ilo G. 1988. Occlusal contact wear of prosthodontic materials: an in vivo study. Acta Odontol Scand. 46:159-69
    • (1988) Acta Odontol Scand. , vol.46 , pp. 159-169
    • Ekfeldt, A.1    Ilo, G.2
  • 79
    • 0024619009 scopus 로고
    • Effects of porcelain on occluding surfaces of restored teeth
    • Wiley MG. 1989. Effects of porcelain on occluding surfaces of restored teeth. J. Prosthet. Dent. 61:133-37
    • (1989) J. Prosthet. Dent. , vol.61 , pp. 133-137
    • Wiley, M.G.1
  • 80
    • 0029678297 scopus 로고    scopus 로고
    • An in vitro investigation of the wear of enamel on porcelain and gold in saliva
    • Hacker CH, Wagner WC, Razzoog ME. 1996. An in vitro investigation of the wear of enamel on porcelain and gold in saliva. J. Prothel. Dent. 75:14-17
    • (1996) J. Prothel. Dent. , vol.75 , pp. 14-17
    • Hacker, C.H.1    Wagner, W.C.2    Razzoog, M.E.3
  • 81
    • 0001862685 scopus 로고
    • Abrasive wear of ceramics
    • ed. S Jahanmir, New York: Dekker
    • Larsen-Basse J. 1994. Abrasive wear of ceramics. In Friction and Wear of Ceramics, ed. S Jahanmir, pp. 99-115. New York: Dekker
    • (1994) Friction and Wear of Ceramics , pp. 99-115
    • Larsen-Basse, J.1
  • 82
    • 0029678682 scopus 로고
    • Ceramics in dentistry: Historical roots and current perspectives
    • Kelly JR, Nishimura I, Campbell SD. 1995. Ceramics in dentistry: historical roots and current perspectives. J. Prosthet. Dent. 75:18-32
    • (1995) J. Prosthet. Dent. , vol.75 , pp. 18-32
    • Kelly, J.R.1    Nishimura, I.2    Campbell, S.D.3
  • 83
    • 9644280649 scopus 로고    scopus 로고
    • Intra-oral wear mechanisms on dental ceramics
    • Abstr.
    • Gentile MJ, Kelly JR. 1996. Intra-oral wear mechanisms on dental ceramics. J. Dent. Res. 75(Abstr.):50:A264
    • (1996) J. Dent. Res. , vol.75 , pp. 50
    • Gentile, M.J.1    Kelly, J.R.2
  • 84
    • 0026133066 scopus 로고
    • Abrasion of human enamel by different dental ceramics in vitro
    • Seghi RR, Rosenstiel SF, Bauer P. 1991. Abrasion of human enamel by different dental ceramics in vitro. J. Dent. Res. 70:221-25
    • (1991) J. Dent. Res. , vol.70 , pp. 221-225
    • Seghi, R.R.1    Rosenstiel, S.F.2    Bauer, P.3
  • 85
    • 9644263625 scopus 로고
    • Enamel wear against In-Ceram and Vitadur-N with various finishes
    • IADR Abstr.
    • Reeves N, Gore K, Meiers JC, Kelly JR. 1993. Enamel wear against In-Ceram and Vitadur-N with various finishes. J. Dent. Res. 72(IADR Abstr.) 187:665
    • (1993) J. Dent. Res. , vol.72 , pp. 187
    • Reeves, N.1    Gore, K.2    Meiers, J.C.3    Kelly, J.R.4
  • 87
    • 0026217002 scopus 로고
    • A comparison of the abrasiveness of six ceramic surfaces and gold
    • Jacobi R, Shillingburg HT, Duncanson MG. 1991. A comparison of the abrasiveness of six ceramic surfaces and gold. J. Prosthet. Dent. 66:303-9
    • (1991) J. Prosthet. Dent. , vol.66 , pp. 303-309
    • Jacobi, R.1    Shillingburg, H.T.2    Duncanson, M.G.3
  • 88
    • 0024729005 scopus 로고
    • The influence of surface preparation on the strength and surface microstructure of a cast dental ceramic
    • Campbell SD, Kelly JR. 1989. The influence of surface preparation on the strength and surface microstructure of a cast dental ceramic. Int. J. Prosthodont. 2:459-66
    • (1989) Int. J. Prosthodont. , vol.2 , pp. 459-466
    • Campbell, S.D.1    Kelly, J.R.2
  • 89
    • 0027562622 scopus 로고
    • Flexural strength and fracture toughness of Dicorglass-ceramic after embedment modification
    • Denry IL, Rosenstiel SF. 1993. Flexural strength and fracture toughness of Dicorglass-ceramic after embedment modification. J. Dent. Res. 72:572-76
    • (1993) J. Dent. Res. , vol.72 , pp. 572-576
    • Denry, I.L.1    Rosenstiel, S.F.2
  • 90
    • 0028394042 scopus 로고
    • Wear of CAD/CAM ceramic inlays: Restorations, opposing cusps, and luting cements
    • Krejci I, Lutz F, Reimer M. 1994. Wear of CAD/CAM ceramic inlays: restorations, opposing cusps, and luting cements. Quint. Int. 25:199-207
    • (1994) Quint. Int. , vol.25 , pp. 199-207
    • Krejci, I.1    Lutz, F.2    Reimer, M.3
  • 91
    • 0026892510 scopus 로고
    • The wear of enamel opposing shaded ceramic restorative materials: An in vitro study
    • DeLong R, Pintado MR, Douglass WH. 1992. The wear of enamel opposing shaded ceramic restorative materials: an in vitro study. J. Prosthet. Dent. 68:42-48
    • (1992) J. Prosthet. Dent. , vol.68 , pp. 42-48
    • Delong, R.1    Pintado, M.R.2    Douglass, W.H.3
  • 93
    • 0021481427 scopus 로고
    • Effect of sliding friction forces on the strength of brittle materials
    • Lawn BR, Wiederhorn SE, Roberts DE. 1984. Effect of sliding friction forces on the strength of brittle materials. J. Mater. Sci. 19:2561-69
    • (1984) J. Mater. Sci. , vol.19 , pp. 2561-2569
    • Lawn, B.R.1    Wiederhorn, S.E.2    Roberts, D.E.3
  • 94
    • 0024611244 scopus 로고
    • Influence of fracture toughness on the wear resistance of yttria-doped zirconium oxide
    • Fischer TE, Anderson MP, Jahnmir S. 1989. Influence of fracture toughness on the wear resistance of yttria-doped zirconium oxide. J. Am. Ceram. Soc. 72:252-57
    • (1989) J. Am. Ceram. Soc. , vol.72 , pp. 252-257
    • Fischer, T.E.1    Anderson, M.P.2    Jahnmir, S.3
  • 96
    • 0016966278 scopus 로고
    • Wear of dental tissues and materials
    • Craig RG, Powers JM. 1976. Wear of dental tissues and materials. Int. J. Dent 26:121-33
    • (1976) Int. J. Dent , vol.26 , pp. 121-133
    • Craig, R.G.1    Powers, J.M.2
  • 98
    • 0029257028 scopus 로고
    • Wear mechanism of a dental glass-ceramic
    • Jahanmir S, Dong X. 1995. Wear mechanism of a dental glass-ceramic. Wear 181-83:821-25
    • (1995) Wear , vol.181 , Issue.83 , pp. 821-825
    • Jahanmir, S.1    Dong, X.2
  • 99
    • 0014903392 scopus 로고
    • Strengthening modern dental porcelain by ion exchange
    • Southan DE. 1970. Strengthening modern dental porcelain by ion exchange. Aust. Dent. J. 15:507-10
    • (1970) Aust. Dent. J. , vol.15 , pp. 507-510
    • Southan, D.E.1
  • 100
    • 0017544171 scopus 로고
    • Improving the fracture resistance of dental ceramics
    • Dunn B, Levy MN, Reisbeck MH. 1977. Improving the fracture resistance of dental ceramics. J. Dent. Res. 56:1209-13
    • (1977) J. Dent. Res. , vol.56 , pp. 1209-1213
    • Dunn, B.1    Levy, M.N.2    Reisbeck, M.H.3
  • 101
    • 0025389073 scopus 로고
    • The effect of ion exchange on the flexural strength of dental porcelains
    • Seghi RR, Crispin BC, Mito W. 1990. The effect of ion exchange on the flexural strength of dental porcelains. Int. J. Prosthodont. 3:130-34
    • (1990) Int. J. Prosthodont. , vol.3 , pp. 130-134
    • Seghi, R.R.1    Crispin, B.C.2    Mito, W.3
  • 102
    • 0026115440 scopus 로고
    • An investigation of an ion strengthening paste for dental porcelains
    • Piddock V, Qualtrough AJE, Brough I. 1991. An investigation of an ion strengthening paste for dental porcelains. Int. J. Prosthodont. 4:132-37
    • (1991) Int. J. Prosthodont. , vol.4 , pp. 132-137
    • Piddock, V.1    Qualtrough, A.J.E.2    Brough, I.3
  • 103
    • 0028438171 scopus 로고
    • Flexural strength of feldspathic porcelain treated with ion exchange, overglaze, and polishing
    • Giordano RA, Campbell S, Pober R. 1994. Flexural strength of feldspathic porcelain treated with ion exchange, overglaze, and polishing. J. Prosthet. Dent. 71:468-72
    • (1994) J. Prosthet. Dent. , vol.71 , pp. 468-472
    • Giordano, R.A.1    Campbell, S.2    Pober, R.3
  • 104
    • 0026891164 scopus 로고
    • Effects of ion exchange on hardness and fracture toughness of dental ceramics
    • Seghi RR, Denry I, Brajevic F. 1992. Effects of ion exchange on hardness and fracture toughness of dental ceramics. Int. J. Prosthodont. 5:309-14
    • (1992) Int. J. Prosthodont. , vol.5 , pp. 309-314
    • Seghi, R.R.1    Denry, I.2    Brajevic, F.3
  • 106
    • 9644265052 scopus 로고
    • Effect of abrasion on the flexural strength of ion-exchanged porcelain
    • IADR Abstr.
    • Osborn GD, Denry IL, Rosenstiel SF, Holloway JA. 1994. Effect of abrasion on the flexural strength of ion-exchanged porcelain. J. Dent. Res. 73(IADR Abstr.) 320:A1745
    • (1994) J. Dent. Res. , vol.73 , pp. 320
    • Osborn, G.D.1    Denry, I.L.2    Rosenstiel, S.F.3    Holloway, J.A.4
  • 107
    • 0039274140 scopus 로고
    • Strengthening of feldspathic porcelain by one-step dual ion-exchange
    • IADR Abstr
    • Holloway JA, Denry IL, Rosenstiel SF. 1994. Strengthening of feldspathic porcelain by one-step dual ion-exchange. J. Dent. Res. 73(IADR Abstr.) 320:A1746
    • (1994) J. Dent. Res. , vol.73 , pp. 320
    • Holloway, J.A.1    Denry, I.L.2    Rosenstiel, S.F.3
  • 108
    • 0026180417 scopus 로고
    • Effect of thermal tempering on strength and crack propagation behavior of feldspathic porcelains
    • Anusavice KJ, Hojjatie B. 1991. Effect of thermal tempering on strength and crack propagation behavior of feldspathic porcelains. J. Dent. Res. 70:1009-13
    • (1991) J. Dent. Res. , vol.70 , pp. 1009-1013
    • Anusavice, K.J.1    Hojjatie, B.2
  • 109
    • 0027569625 scopus 로고
    • Effects of initial temperature and tempering medium on thermal tempering of dental porcelains
    • Hojjatie B, Anusavice KJ. 1993. Effects of initial temperature and tempering medium on thermal tempering of dental porcelains. J. Dent. Res. 72:566-71
    • (1993) J. Dent. Res. , vol.72 , pp. 566-571
    • Hojjatie, B.1    Anusavice, K.J.2
  • 110
    • 0026112382 scopus 로고
    • Influence of initial flaw size on crack growth in air-tempered porcelain
    • Anusavice KJ, Gray A, Shen C. 1991. Influence of initial flaw size on crack growth in air-tempered porcelain. J. Dent. Res. 70:131-36
    • (1991) J. Dent. Res. , vol.70 , pp. 131-136
    • Anusavice, K.J.1    Gray, A.2    Shen, C.3
  • 111
    • 0026859460 scopus 로고
    • Strengthening of porcelain by ion exchange subsequent to thermal tempering
    • Anusavice KJ, Shen C, Vermost B, Chow B. 1992. Strengthening of porcelain by ion exchange subsequent to thermal tempering. Dent. Mater. 8:149-52
    • (1992) Dent. Mater. , vol.8 , pp. 149-152
    • Anusavice, K.J.1    Shen, C.2    Vermost, B.3    Chow, B.4
  • 112
    • 9644255353 scopus 로고
    • Effect of abrasion on strength of thermally tempered dental ceramics
    • AADR Abstr.
    • Hojjatie B, Anusavice KJ, Hsiao LI. 1992. Effect of abrasion on strength of thermally tempered dental ceramics. J. Dent. Res. 71(AADR Abstr.) 208:A817
    • (1992) J. Dent. Res. , vol.71 , pp. 208
    • Hojjatie, B.1    Anusavice, K.J.2    Hsiao, L.I.3
  • 113
    • 9644279150 scopus 로고
    • Viscoelastic analysis of PFM crowns using finite element methods
    • IADR Abstr.
    • DeHoff PH, Vontivillu SB, Anusavice KJ, Wang Z. 1994. Viscoelastic analysis of PFM crowns using finite element methods. J. Dent. Res. 73(IADR Abstr.) 369.A2141
    • (1994) J. Dent. Res. , vol.73 , pp. 369
    • Dehoff, P.H.1    Vontivillu, S.B.2    Anusavice, K.J.3    Wang, Z.4
  • 114
  • 115
    • 0002924196 scopus 로고
    • Effect of thermally induced changes on porcelain-metal compatibility
    • ed. JD Preston, Chicago: Quintessence
    • Mackert JR. 1988. Effect of thermally induced changes on porcelain-metal compatibility. In Proc. 4th Int. Symp. on Ceramics, ed. JD Preston, pp. 53-64. Chicago: Quintessence
    • (1988) Proc. 4th Int. Symp. on Ceramics , pp. 53-64
    • Mackert, J.R.1
  • 116
    • 9644284078 scopus 로고
    • Leucite stabilization in feldspathic dental porcelain
    • ed. RP Rusin, GS Fischman, Westerville, OH: Am. Ceram. Soc.
    • Denry IL, Rosenstiel SF. 1995. Leucite stabilization in feldspathic dental porcelain. In Bioceramics; Materials and Applications II. Ceramic Transactions, ed. RP Rusin, GS Fischman, 63:115-21. Westerville, OH: Am. Ceram. Soc.
    • (1995) Bioceramics; Materials and Applications II. Ceramic Transactions , vol.63 , pp. 115-121
    • Denry, I.L.1    Rosenstiel, S.F.2
  • 117
    • 84972047859 scopus 로고
    • Properties of leucite-glass composites prepared by a coprecipitation process
    • Yoon CK, Rasmussen ST, O'Brien WJ, Tien T-Y. 1994. Properties of leucite-glass composites prepared by a coprecipitation process. J. Mater. Res. 9:2285-89
    • (1994) J. Mater. Res. , vol.9 , pp. 2285-2289
    • Yoon, C.K.1    Rasmussen, S.T.2    O'Brien, W.J.3    Tien, T.-Y.4
  • 118
    • 0028317853 scopus 로고
    • Mechanical properties and thermal expansion behavior in leucite containing materials
    • Sheu T-S, O'Brien WJ, Rasmussen ST, Tien T-Y. 1994. Mechanical properties and thermal expansion behavior in leucite containing materials. J. Mater. Sci. 29:125-28
    • (1994) J. Mater. Sci. , vol.29 , pp. 125-128
    • Sheu, T.-S.1    O'Brien, W.J.2    Rasmussen, S.T.3    Tien, T.-Y.4
  • 119
    • 9644263624 scopus 로고    scopus 로고
    • Effect of ion-exchange on the thermal expansion behavior of leucite-reinforced dental porcelain
    • Abstr.
    • Denry IL, Rosenstiel SF. 1996. Effect of ion-exchange on the thermal expansion behavior of leucite-reinforced dental porcelain. Presented at Am. Ceram. Soc. Annu. Meet. Indianapolis, IN. Abstr. p. 24
    • (1996) Am. Ceram. Soc. Annu. Meet. Indianapolis, IN , pp. 24
    • Denry, I.L.1    Rosenstiel, S.F.2
  • 120
    • 9644291141 scopus 로고    scopus 로고
    • Effect of ion-exchange on the crystallization behavior of a low expansion feldspar glass
    • IADR Abstr
    • Denry IL, Holloway JA, Rosenstiel SF. 1997. Effect of ion-exchange on the crystallization behavior of a low expansion feldspar glass. J. Dent. Res. 76(IADR Abstr.) 138:A993
    • (1997) J. Dent. Res. , vol.76 , pp. 138
    • Denry, I.L.1    Holloway, J.A.2    Rosenstiel, S.F.3
  • 121
    • 0027075823 scopus 로고
    • Chemical strengthening of leucite-containing dental ceramics
    • Fischer J, Pospiech P, Gernet W. 1992. Chemical strengthening of leucite-containing dental ceramics. J. Eur. Ceram. Soc. 10:221-27
    • (1992) J. Eur. Ceram. Soc. , vol.10 , pp. 221-227
    • Fischer, J.1    Pospiech, P.2    Gernet, W.3
  • 124
    • 0022141704 scopus 로고
    • Magnesia ceramic jacket crowns
    • O'Brien WJ. 1985. Magnesia ceramic jacket crowns. Dent. Clin. North Am. 29:719-23
    • (1985) Dent. Clin. North Am. , vol.29 , pp. 719-723
    • O'Brien, W.J.1
  • 125
    • 0028439191 scopus 로고
    • Preparation of nepheline glass-ceramics and their application as dental porcelain
    • Wang M-C, Wu N-C, Hon M-H. 1994. Preparation of nepheline glass-ceramics and their application as dental porcelain. Mater. Chem. Phys. 37:370-75
    • (1994) Mater. Chem. Phys. , vol.37 , pp. 370-375
    • Wang, M.-C.1    Wu, N.-C.2    Hon, M.-H.3
  • 126
    • 9644253850 scopus 로고
    • Influence of colorants on crystallization and properties of lithia-based glass ceramics
    • IADR Abstr.
    • Anusavice KJ, Zhang N-Z, Moorhead JE. 1993. Influence of colorants on crystallization and properties of lithia-based glass ceramics. J. Dent. Res. 72(IADR Abstr.) 262:A1271
    • (1993) J. Dent. Res. , vol.72 , pp. 262
    • Anusavice, K.J.1    Zhang, N.-Z.2    Moorhead, J.E.3
  • 128
    • 0004205930 scopus 로고    scopus 로고
    • Effect of nucleation temperature on toughness and flexural strength of canasite glass-ceramic
    • IADR Abstr.
    • Anusavice KJ, Zhang N-Z. 1996. Effect of nucleation temperature on toughness and flexural strength of canasite glass-ceramic. J. Dent. Res. 75(IADR Abstr.): 67
    • (1996) J. Dent. Res. , vol.75 , pp. 67
    • Anusavice, K.J.1    Zhang, N.-Z.2
  • 129
    • 0011425333 scopus 로고
    • An intrinsically colored microcrystalline glass-ceramic for use in dental restorations
    • George LA, Eichmiller FC, Bowen RL. 1992. An intrinsically colored microcrystalline glass-ceramic for use in dental restorations. Bull. Am. Ceram. Soc. 71:1073-76
    • (1992) Bull. Am. Ceram. Soc. , vol.71 , pp. 1073-1076
    • George, L.A.1    Eichmiller, F.C.2    Bowen, R.L.3
  • 130
    • 0030308994 scopus 로고    scopus 로고
    • The new creativity in ceramic restorations: Dental CAD-CIM
    • Mörmann WH, Bindl A, 1996. The new creativity in ceramic restorations: dental CAD-CIM. Quint. Int. 27:821-28
    • (1996) Quint. Int. , vol.27 , pp. 821-828
    • Mörmann, W.H.1    Bindl, A.2
  • 131
    • 0346242565 scopus 로고
    • Fabrication of conservative ceramic restorations using copy milling technology
    • McLaren EA, Sorensen JA. 1994. Fabrication of conservative ceramic restorations using copy milling technology. Quint. Dent. Technol. 17:19-25
    • (1994) Quint. Dent. Technol. , vol.17 , pp. 19-25
    • McLaren, E.A.1    Sorensen, J.A.2
  • 133
    • 2442491367 scopus 로고    scopus 로고
    • Strength and toughness of dental ceramics
    • ed. WH Mörmann, Chicago: Quintessence
    • Luthy H. 1996. Strength and toughness of dental ceramics. In CAD/CIM in Aesthetic Dentistry, ed. WH Mörmann, pp. 229-39. Chicago: Quintessence
    • (1996) CAD/CIM in Aesthetic Dentistry , pp. 229-239
    • Luthy, H.1
  • 135
    • 0021727646 scopus 로고
    • Fracture properties of human enamel and dentin in an aqueous environment
    • Rasmussen ST, Patchin RE. 1984. Fracture properties of human enamel and dentin in an aqueous environment. J. Dent. Res. 63:1362-68
    • (1984) J. Dent. Res. , vol.63 , pp. 1362-1368
    • Rasmussen, S.T.1    Patchin, R.E.2
  • 138
    • 0030107011 scopus 로고    scopus 로고
    • Crack suppression in strongly bonded homogeneous/heterogeneous laminates: A study on glass/glass-ceramic bilayers
    • Wuttiphan S, Lawn BR, Padture NP. 1996. Crack suppression in strongly bonded homogeneous/heterogeneous laminates: a study on glass/glass-ceramic bilayers. J. Am. Ceram. Soc. 79:634-40
    • (1996) J. Am. Ceram. Soc. , vol.79 , pp. 634-640
    • Wuttiphan, S.1    Lawn, B.R.2    Padture, N.P.3
  • 139
    • 0030126078 scopus 로고    scopus 로고
    • Hertzian contact response of tailored silicon nitride multilayers
    • Liu H, Lawn BR, Hsu SM. 1996. Hertzian contact response of tailored silicon nitride multilayers. J. Am. Ceram. Soc. 79:10009-14
    • (1996) J. Am. Ceram. Soc. , vol.79 , pp. 10009-10014
    • Liu, H.1    Lawn, B.R.2    Hsu, S.M.3
  • 140
    • 0017918175 scopus 로고
    • Engineering design and fatigue failure of brittle materials
    • ed. RC Bradt, DPH Hasselman, FF Lange, New York: Plenum
    • Ritter JE. 1978. Engineering design and fatigue failure of brittle materials. In Fracture Mechanics of Ceramics, ed. RC Bradt, DPH Hasselman, FF Lange, 4:667-86. New York: Plenum
    • (1978) Fracture Mechanics of Ceramics , vol.4 , pp. 667-686
    • Ritter, J.E.1
  • 141
    • 0023314812 scopus 로고
    • Stress corrosion failure of dental porcelain
    • Jones DW, Sutow EJ. 1987. Stress corrosion failure of dental porcelain. Br. Ceram. Trans. J. 86:40-43
    • (1987) Br. Ceram. Trans. J. , vol.86 , pp. 40-43
    • Jones, D.W.1    Sutow, E.J.2
  • 142
    • 84970306303 scopus 로고
    • Transverse strength of aluminous and feldspathic porcelain
    • Sherrill CA, O'Brien WJ. 1974. Transverse strength of aluminous and feldspathic porcelain. J. Dent. Res. 53:683-90
    • (1974) J. Dent. Res. , vol.53 , pp. 683-690
    • Sherrill, C.A.1    O'Brien, W.J.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.