메뉴 건너뛰기




Volumn 23, Issue 8, 2007, Pages 1042-1049

Numerical modeling of the fracture process in a three-unit all-ceramic fixed partial denture

Author keywords

Dental ceramic; Fixed partial denture; Fracture; Numerical modeling; Zirconia

Indexed keywords

COMPUTER SIMULATION; FRACTURE; PHOTOELASTICITY; POLYCRYSTALS; STRESS ANALYSIS; ZIRCONIA;

EID: 34250222382     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.dental.2006.06.039     Document Type: Article
Times cited : (34)

References (23)
  • 1
    • 0347540993 scopus 로고    scopus 로고
    • Mechanical properties of commercial high strength ceramic core materials
    • Rizkalla A.S., and Jones D.W. Mechanical properties of commercial high strength ceramic core materials. Dent Mater 20 (2004) 207-212
    • (2004) Dent Mater , vol.20 , pp. 207-212
    • Rizkalla, A.S.1    Jones, D.W.2
  • 2
    • 0035348308 scopus 로고    scopus 로고
    • Resistance to staining, flexural strength, and chemical solubility of core porcelains for all-ceramic crowns
    • Esquivel-Upshaw J.F., Chai J., Sansano S., and Shonberg D. Resistance to staining, flexural strength, and chemical solubility of core porcelains for all-ceramic crowns. Int J Prosthodont 14 (2001) 284-288
    • (2001) Int J Prosthodont , vol.14 , pp. 284-288
    • Esquivel-Upshaw, J.F.1    Chai, J.2    Sansano, S.3    Shonberg, D.4
  • 3
    • 0035348103 scopus 로고    scopus 로고
    • Flexural strength of Cerec 2 machined and jointed InCeram-Alumina and InCeram-Zirconia bars
    • Apholt W., Bindl A., Luthy H., and Mörmann W.H. Flexural strength of Cerec 2 machined and jointed InCeram-Alumina and InCeram-Zirconia bars. Dent Mater 17 (2001) 260-267
    • (2001) Dent Mater , vol.17 , pp. 260-267
    • Apholt, W.1    Bindl, A.2    Luthy, H.3    Mörmann, W.H.4
  • 4
    • 0007285056 scopus 로고    scopus 로고
    • A comparison of the microstructure and properties of the IPS Empress 2 and the IPS Empress glass-ceramics
    • Höland W., Schweiger M., Frank M., and Rheinberger V. A comparison of the microstructure and properties of the IPS Empress 2 and the IPS Empress glass-ceramics. J Biomed Mater Res 53 (2000) 297-303
    • (2000) J Biomed Mater Res , vol.53 , pp. 297-303
    • Höland, W.1    Schweiger, M.2    Frank, M.3    Rheinberger, V.4
  • 5
    • 0027546239 scopus 로고
    • A new all-ceramic crown. A dense-sintered, high-purity alumina coping with porcelain
    • Andersson M., and Odén A. A new all-ceramic crown. A dense-sintered, high-purity alumina coping with porcelain. Acta Odontol Scand 51 (1993) 59-64
    • (1993) Acta Odontol Scand , vol.51 , pp. 59-64
    • Andersson, M.1    Odén, A.2
  • 6
    • 16344387546 scopus 로고    scopus 로고
    • Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing
    • Sundh A., Molin M., and Sjögren G. Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing. Dent Mater 21 (2005) 476-482
    • (2005) Dent Mater , vol.21 , pp. 476-482
    • Sundh, A.1    Molin, M.2    Sjögren, G.3
  • 8
    • 0029318343 scopus 로고
    • Failure of all-ceramic fixed partial dentures in vitro and in vivo: analysis and modeling
    • Kelly J.R., Tesk J.A., and Sorensen J.A. Failure of all-ceramic fixed partial dentures in vitro and in vivo: analysis and modeling. J Dent Res 74 (1995) 1253-1258
    • (1995) J Dent Res , vol.74 , pp. 1253-1258
    • Kelly, J.R.1    Tesk, J.A.2    Sorensen, J.A.3
  • 9
    • 0037364513 scopus 로고    scopus 로고
    • Lifetime prediction of all-ceramic bridges by computational methods
    • (Erratum in J Dent Res 2003;406)
    • Fischer H., Weber M., and Marx R. Lifetime prediction of all-ceramic bridges by computational methods. J Dent Res 82 (2003) 238-242 (Erratum in J Dent Res 2003;406)
    • (2003) J Dent Res , vol.82 , pp. 238-242
    • Fischer, H.1    Weber, M.2    Marx, R.3
  • 10
    • 0141890840 scopus 로고    scopus 로고
    • 3-D Finite element analysis of all-ceramic posterior crowns
    • Imanishi A., Nakamura T., Ohyama T., and Nakamura T. 3-D Finite element analysis of all-ceramic posterior crowns. J Oral Rehabil 30 (2003) 818-822
    • (2003) J Oral Rehabil , vol.30 , pp. 818-822
    • Imanishi, A.1    Nakamura, T.2    Ohyama, T.3    Nakamura, T.4
  • 11
    • 0742321994 scopus 로고    scopus 로고
    • Finite element and experimental analyses of polymer-based dental bridges reinforced by ceramic bars
    • Fischer H., Weber M., Eck M., Erdrich A., and Marx R. Finite element and experimental analyses of polymer-based dental bridges reinforced by ceramic bars. J Biomech 37 (2004) 289-294
    • (2004) J Biomech , vol.37 , pp. 289-294
    • Fischer, H.1    Weber, M.2    Eck, M.3    Erdrich, A.4    Marx, R.5
  • 12
    • 34250199055 scopus 로고    scopus 로고
    • Liu HY. Numerical modeling of the rock fragmentation process by mechanical tools. Doctoral thesis. Luleå University of Technology, Luleå, Sweden. 2004 (ISSN: 1402-1544).
  • 13
    • 0031079848 scopus 로고    scopus 로고
    • Numerical simulation of progressive rock failure and associated seismicity
    • Tang C.A. Numerical simulation of progressive rock failure and associated seismicity. Int J Rock Mech Min Sci 34 (1997) 249-261
    • (1997) Int J Rock Mech Min Sci , vol.34 , pp. 249-261
    • Tang, C.A.1
  • 14
    • 1342267203 scopus 로고    scopus 로고
    • Characterization of rock heterogeneity and numerical verification
    • Liu H.Y., Roquete M., Kou S.Q., and Lindqvist P.A. Characterization of rock heterogeneity and numerical verification. Eng Geol 72 (2004) 89-119
    • (2004) Eng Geol , vol.72 , pp. 89-119
    • Liu, H.Y.1    Roquete, M.2    Kou, S.Q.3    Lindqvist, P.A.4
  • 15
    • 1842783267 scopus 로고    scopus 로고
    • Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics
    • Guazzato M., Albakry M., Ringer S.P., and Swain M.V. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics. Dent Mater 20 (2004) 449-456
    • (2004) Dent Mater , vol.20 , pp. 449-456
    • Guazzato, M.1    Albakry, M.2    Ringer, S.P.3    Swain, M.V.4
  • 16
    • 11844264547 scopus 로고    scopus 로고
    • Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic
    • Guazzato M., Quach L., Albakry M., and Swain M.V. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic. J Dent 33 (2005) 9-18
    • (2005) J Dent , vol.33 , pp. 9-18
    • Guazzato, M.1    Quach, L.2    Albakry, M.3    Swain, M.V.4
  • 19
    • 0034441675 scopus 로고    scopus 로고
    • Crack initiation modes in bilayered alumina/porcelain disks as a function of core/veneer thickness ratio and supporting substrate stiffness
    • Wakabayashi N., and Anusavice K.J. Crack initiation modes in bilayered alumina/porcelain disks as a function of core/veneer thickness ratio and supporting substrate stiffness. J Dent Res 79 (2000) 1398-1404
    • (2000) J Dent Res , vol.79 , pp. 1398-1404
    • Wakabayashi, N.1    Anusavice, K.J.2
  • 20
    • 1942468620 scopus 로고    scopus 로고
    • Strength, reliability and mode of fracture of bilayered porcelain/zirconia (Y-TZP) dental ceramics
    • Guazzato M., Proos K., Quach L., and Swain M.V. Strength, reliability and mode of fracture of bilayered porcelain/zirconia (Y-TZP) dental ceramics. Biomaterials 25 (2004) 5045-5052
    • (2004) Biomaterials , vol.25 , pp. 5045-5052
    • Guazzato, M.1    Proos, K.2    Quach, L.3    Swain, M.V.4
  • 21
    • 30344459124 scopus 로고    scopus 로고
    • Influence of stress simulation parameters on the fracture strength of all-ceramic fixed-partial dentures
    • Rosentritt M., Behr M., Gebhard R., and Handel G. Influence of stress simulation parameters on the fracture strength of all-ceramic fixed-partial dentures. Dent Mater 22 (2006) 176-182
    • (2006) Dent Mater , vol.22 , pp. 176-182
    • Rosentritt, M.1    Behr, M.2    Gebhard, R.3    Handel, G.4
  • 22
    • 0036716828 scopus 로고    scopus 로고
    • Influence of connector design on fracture probability of ceramic fixed-partial dentures
    • Oh W., Gotzen N., and Anusavice K.J. Influence of connector design on fracture probability of ceramic fixed-partial dentures. J Dent Res 81 (2002) 623-627
    • (2002) J Dent Res , vol.81 , pp. 623-627
    • Oh, W.1    Gotzen, N.2    Anusavice, K.J.3
  • 23
    • 33645356680 scopus 로고    scopus 로고
    • Surface roughness of five different dental ceramic core materials after grinding and polishing
    • Kou W., Molin M., and Sjögren G. Surface roughness of five different dental ceramic core materials after grinding and polishing. J Oral Rehabil 33 (2006) 117-124
    • (2006) J Oral Rehabil , vol.33 , pp. 117-124
    • Kou, W.1    Molin, M.2    Sjögren, G.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.