1
-
-
85133099738
-
-
CRC Press, Taylor & Francis Group, Boca Raton, London, New York, Singapore
-
Anderson T.L. Fracture Mechanics - Fundamentals and Applications. third ed. (2005), CRC Press, Taylor & Francis Group, Boca Raton, London, New York, Singapore
-
(2005)
Fracture Mechanics - Fundamentals and Applications. third ed.
-
-
Anderson, T.L.1
-
3
-
-
0023859641
-
Design and analysis of the crack rail shear specimen for mode III interlaminar fracture
-
Becht G., and Gillespie Jr. J.W. Design and analysis of the crack rail shear specimen for mode III interlaminar fracture. Composites Science and Technology 31 (1988) 143-157
-
(1988)
Composites Science and Technology
, vol.31
, pp. 143-157
-
-
Becht, G.1
Gillespie Jr., J.W.2
-
4
-
-
0022241748
-
-
Bradley, W.L., Cohen, R.N. 1985. Matrix deformation and fracture in graphite-reinforced epoxies. In: Johnson, S.W. (Ed.), Delamination and Debonding of Materials, American Society for Testing and Materials, Philadelphia, ASTM STP 876, pp. 389-410.
-
-
-
-
5
-
-
0022810345
-
On the analysis and design of the end notched flexure (ENF) specimen for mode II testing
-
Carlsson L.A., Gillespie J.W., and Pipes R.B. On the analysis and design of the end notched flexure (ENF) specimen for mode II testing. Journal of Composite Materials 20 (1986) 594-604
-
(1986)
Journal of Composite Materials
, vol.20
, pp. 594-604
-
-
Carlsson, L.A.1
Gillespie, J.W.2
Pipes, R.B.3
-
7
-
-
0025422074
-
Interlaminar shear fracture of laminated composites
-
Chai H. Interlaminar shear fracture of laminated composites. International Journal of Fracture 43 (1990) 117-131
-
(1990)
International Journal of Fracture
, vol.43
, pp. 117-131
-
-
Chai, H.1
-
8
-
-
84896887132
-
-
Chen, L., Sankar, B.V., Ifju, P.G. 2003. Mixed-Mode Fracture Toughness Tests for Stitched Composite Laminates. AIAA Paper 2003-1874. In: Proceedings of the 44th AIAA Structures, Structural Dynamics and Materials Conference, Norfolk, Virginia, April 7-10, 2003, 10 pages.
-
-
-
-
9
-
-
33947157174
-
-
Cicci, D., Sharif, F., Kortschot, M.T. 1995. Data reduction for the split cantilever beam mode III delamination test. In: Proceedings, ACCM 10, Whistler, British Columbia, Canada, August 14-18.
-
-
-
-
10
-
-
0041136638
-
A mixed-mode bending apparatus for delamination testing
-
Crews Jr. J.H., and Reeder J.R. A mixed-mode bending apparatus for delamination testing. NASA Technical Memorandum 100662 (1988) 1-37
-
(1988)
NASA Technical Memorandum
, vol.100662
, pp. 1-37
-
-
Crews Jr., J.H.1
Reeder, J.R.2
-
11
-
-
0029539060
-
Three-dimensional analysis of center-delaminated unidirectional and multidirectional single-leg bending specimens
-
Davidson B.D., Krüger R., and König M. Three-dimensional analysis of center-delaminated unidirectional and multidirectional single-leg bending specimens. Composites Science and Technology 54 (1995) 385-394
-
(1995)
Composites Science and Technology
, vol.54
, pp. 385-394
-
-
Davidson, B.D.1
Krüger, R.2
König, M.3
-
12
-
-
0001844390
-
A single leg bending test for interfacial fracture toughness determination
-
Davidson B.D., and Sundararaman V. A single leg bending test for interfacial fracture toughness determination. International Journal of Fracture 78 (1996) 193-210
-
(1996)
International Journal of Fracture
, vol.78
, pp. 193-210
-
-
Davidson, B.D.1
Sundararaman, V.2
-
13
-
-
33947122150
-
-
Davies, P., Ducept, F., Brunner, A.J., Blackman, B.R.K., Morais, de A.B. 1996. Development of a standard mode II shear fracture test procedure. In: Proceedings of the 7th European Conference on Composite Materials (ECCM-7), vol. 2, London, May, pp. 9-15.
-
-
-
-
14
-
-
0024142425
-
Mode III intelaminar fracture characterization of composite materials
-
Donaldson S.L. Mode III intelaminar fracture characterization of composite materials. Composites Science and Technology 32 (1988) 225-249
-
(1988)
Composites Science and Technology
, vol.32
, pp. 225-249
-
-
Donaldson, S.L.1
-
15
-
-
0030692336
-
An experimental study to validate tests used to determine mixed mode failure criteria of glass/epoxy composites
-
Ducept F., Davies P., and Gamby D. An experimental study to validate tests used to determine mixed mode failure criteria of glass/epoxy composites. Composites Part A: Applied Science and Manufacturing 28A (1997) 719-729
-
(1997)
Composites Part A: Applied Science and Manufacturing
, vol.28 A
, pp. 719-729
-
-
Ducept, F.1
Davies, P.2
Gamby, D.3
-
16
-
-
0029209158
-
Nominally constant strain energy release rate specimen for the study of mode II fracture and fatigue in adhesively bonded joints
-
Edde F.C., and Verreman Y. Nominally constant strain energy release rate specimen for the study of mode II fracture and fatigue in adhesively bonded joints. International Journal of Adhesion and Adhesives 15 (1995) 29-32
-
(1995)
International Journal of Adhesion and Adhesives
, vol.15
, pp. 29-32
-
-
Edde, F.C.1
Verreman, Y.2
-
17
-
-
0032173209
-
Crack face interaction and mixed.mode fracture of wood composites during mode III loading
-
Ehart R.J.A., Stanzl-Tschegg S.E., and Tschegg E.K. Crack face interaction and mixed.mode fracture of wood composites during mode III loading. Engineering Fracture Mechanics 61 (1998) 253-278
-
(1998)
Engineering Fracture Mechanics
, vol.61
, pp. 253-278
-
-
Ehart, R.J.A.1
Stanzl-Tschegg, S.E.2
Tschegg, E.K.3
-
19
-
-
0032108194
-
Investigation of mode III fracture toughness using an anti-clastic plate bending method
-
Farshad M., and Flüeler P. Investigation of mode III fracture toughness using an anti-clastic plate bending method. Engineering Fracture Mechanics 60 (1998) 5-6
-
(1998)
Engineering Fracture Mechanics
, vol.60
, pp. 5-6
-
-
Farshad, M.1
Flüeler, P.2
-
22
-
-
84970675276
-
The effects of geometry, rate and temperature on mode I, mode II and mixed-mode I/II interlaminar fracture toughness of carbon-fibre/poly(ether-ether ketone) composites
-
Hashemi S., Kinloch J., and Williams J.G. The effects of geometry, rate and temperature on mode I, mode II and mixed-mode I/II interlaminar fracture toughness of carbon-fibre/poly(ether-ether ketone) composites. Journal of Composite Materials 24 (1990) 918-956
-
(1990)
Journal of Composite Materials
, vol.24
, pp. 918-956
-
-
Hashemi, S.1
Kinloch, J.2
Williams, J.G.3
-
23
-
-
0025205711
-
Mechanics and mechanisms of delamination in a poly(ether sulphone)-fibre composite
-
Hashemi S., Kinloch J., and Williams J.G. Mechanics and mechanisms of delamination in a poly(ether sulphone)-fibre composite. Composites Science and Technology 37 (1990) 429-462
-
(1990)
Composites Science and Technology
, vol.37
, pp. 429-462
-
-
Hashemi, S.1
Kinloch, J.2
Williams, J.G.3
-
24
-
-
0035244892
-
Tearing mode interlaminar fracture toughness of composite materials
-
Hwang S.-F., and Hu C.-L. Tearing mode interlaminar fracture toughness of composite materials. Polymer Composites 22 (2001) 57-64
-
(2001)
Polymer Composites
, vol.22
, pp. 57-64
-
-
Hwang, S.-F.1
Hu, C.-L.2
-
25
-
-
33947131185
-
-
Ifju, P.G., Chen, L.-S., Sankar, B.V. 2002. Mixed-mode fracture toughness for stitched composites. SEM Annual Conference, Milwaukee, WI 2002, paper number 173.
-
-
-
-
26
-
-
0032157287
-
Mixed mode I/III fracture toughness of armco iron
-
Kamat S.V., Srinivas M., and Rao P.R. Mixed mode I/III fracture toughness of armco iron. Acta Materialia 46 14 (1998) 4985-4992
-
(1998)
Acta Materialia
, vol.46
, Issue.14
, pp. 4985-4992
-
-
Kamat, S.V.1
Srinivas, M.2
Rao, P.R.3
-
27
-
-
0037388856
-
Influence of fiber direction and mixed-mode ratio on delamination fracture toughness of carbon/epoxy laminates
-
Kim B.W., and Mayer A.H. Influence of fiber direction and mixed-mode ratio on delamination fracture toughness of carbon/epoxy laminates. Composites Science and Technology 63 (2003) 695-713
-
(2003)
Composites Science and Technology
, vol.63
, pp. 695-713
-
-
Kim, B.W.1
Mayer, A.H.2
-
28
-
-
0035400611
-
Crack fornt rotation and segmentation in mixed mode I+III or I+II+III. Part II: Comparison with experiments
-
Lazarus V., Leblond J.-B., and Mouschrif S.-E. Crack fornt rotation and segmentation in mixed mode I+III or I+II+III. Part II: Comparison with experiments. Journal of the Mechanics and Physics of Solids 49 (2001) 1421-1443
-
(2001)
Journal of the Mechanics and Physics of Solids
, vol.49
, pp. 1421-1443
-
-
Lazarus, V.1
Leblond, J.-B.2
Mouschrif, S.-E.3
-
29
-
-
0027660606
-
An edge crack torsion method for mode III delamination fracture testing
-
Lee S.M. An edge crack torsion method for mode III delamination fracture testing. Journal of Composites Technology and Research 15 3 (1993) 193-201
-
(1993)
Journal of Composites Technology and Research
, vol.15
, Issue.3
, pp. 193-201
-
-
Lee, S.M.1
-
30
-
-
0029244583
-
Mixed mode I/III fracture toughness of a V-5Cr-5Ti alloy at 100 °C
-
Li H., Jones R.H., and Hirth J.P. Mixed mode I/III fracture toughness of a V-5Cr-5Ti alloy at 100 °C. Scripta Metallurgica et Materialia 32 4 (1995) 611-616
-
(1995)
Scripta Metallurgica et Materialia
, vol.32
, Issue.4
, pp. 611-616
-
-
Li, H.1
Jones, R.H.2
Hirth, J.P.3
-
31
-
-
0030124795
-
The determination of mode III fracture toughness in thick composite laminates
-
Liao W.C., and Sun C.T. The determination of mode III fracture toughness in thick composite laminates. Composites Science and Technology 56 (1996) 489-499
-
(1996)
Composites Science and Technology
, vol.56
, pp. 489-499
-
-
Liao, W.C.1
Sun, C.T.2
-
32
-
-
0037100333
-
Interlaminar fracture characterization for plain weave fabric composites
-
Naik N.K., Reddy K.S., Meduri S., Raju N.B., Prasad P.D., Azad S.K.N.M., Ogde P.A., and Reddy B.C.K. Interlaminar fracture characterization for plain weave fabric composites. Journal of Materials Science 37 (2002) 2983-2987
-
(2002)
Journal of Materials Science
, vol.37
, pp. 2983-2987
-
-
Naik, N.K.1
Reddy, K.S.2
Meduri, S.3
Raju, N.B.4
Prasad, P.D.5
Azad, S.K.N.M.6
Ogde, P.A.7
Reddy, B.C.K.8
-
33
-
-
0026652164
-
A simplified improved beam analysis of the DCB specimen
-
Olsson R. A simplified improved beam analysis of the DCB specimen. Composites Science and Technology 43 (1992) 329-338
-
(1992)
Composites Science and Technology
, vol.43
, pp. 329-338
-
-
Olsson, R.1
-
35
-
-
0035807449
-
The determination of fracture mechanics properties of pharmaceutical materials in mode III loading using an anti-clastic plate bending method
-
Podczeck F. The determination of fracture mechanics properties of pharmaceutical materials in mode III loading using an anti-clastic plate bending method. International Journal of Pharmaceutics 227 (2001) 39-46
-
(2001)
International Journal of Pharmaceutics
, vol.227
, pp. 39-46
-
-
Podczeck, F.1
-
36
-
-
0037376149
-
Analysis of tapered ENF specimen and characterization of bonded interface fracture under mode-II loading
-
Qiao P., Wang J., and Davalos J.F. Analysis of tapered ENF specimen and characterization of bonded interface fracture under mode-II loading. International Journal of Solids and Structures 40 (2003) 1865-1884
-
(2003)
International Journal of Solids and Structures
, vol.40
, pp. 1865-1884
-
-
Qiao, P.1
Wang, J.2
Davalos, J.F.3
-
37
-
-
0004026023
-
An evaluation of mixed-mode delamination failure criterion
-
Reeder J.R. An evaluation of mixed-mode delamination failure criterion. NASA Technical Memorandum 104210 (1992) 1-49
-
(1992)
NASA Technical Memorandum
, vol.104210
, pp. 1-49
-
-
Reeder, J.R.1
-
38
-
-
0025465054
-
Mixed-mode bending method for delamination testing
-
Reeder J.R., and Crews Jr. J.H. Mixed-mode bending method for delamination testing. AIAA Journal 28 (1990) 1270-1276
-
(1990)
AIAA Journal
, vol.28
, pp. 1270-1276
-
-
Reeder, J.R.1
Crews Jr., J.H.2
-
39
-
-
0032173023
-
Investigation of mixed mode I/II interlaminar fracture toughness of laminated composites by using a CTS type specimen
-
Rikards R., Buchholz F.G., Wang H., Bledzki A.K., Korjakin A., and Richard H.-A. Investigation of mixed mode I/II interlaminar fracture toughness of laminated composites by using a CTS type specimen. Engineering Fracture Mechanics 61 (1998) 325-342
-
(1998)
Engineering Fracture Mechanics
, vol.61
, pp. 325-342
-
-
Rikards, R.1
Buchholz, F.G.2
Wang, H.3
Bledzki, A.K.4
Korjakin, A.5
Richard, H.-A.6
-
40
-
-
0017561766
-
A finite element calculation of stress intensity factors by a modified crack closure integral
-
Rybicki E.F., and Kanninen M.F. A finite element calculation of stress intensity factors by a modified crack closure integral. Engineering Fracture Mechanics 9 (1977) 931-938
-
(1977)
Engineering Fracture Mechanics
, vol.9
, pp. 931-938
-
-
Rybicki, E.F.1
Kanninen, M.F.2
-
42
-
-
0034250054
-
Evaluation of the accuracy of the four-point bend end-notched flexure test for mode II delamination toughness determination
-
Schuecker C., and Davidson B.D. Evaluation of the accuracy of the four-point bend end-notched flexure test for mode II delamination toughness determination. Composites Science and Technology 60 (2000) 2137-2146
-
(2000)
Composites Science and Technology
, vol.60
, pp. 2137-2146
-
-
Schuecker, C.1
Davidson, B.D.2
-
43
-
-
0029386283
-
-
Sharif, F., Kortschot, M.T., Martin, R.H. 1995. Mode III delamination using a split cantilever beam. In: Martin, R.H. (Ed.), Composite Materials: Fatigue and Fracture, vol. 5, ASTM STP 1230, ASTM, Philadelphia, pp. 85-99.
-
-
-
-
44
-
-
33947165749
-
-
Sørensen, B.F., Jørgensen, K., Jacobsen, T.K., Østergaard, R.C. 2004. A general mixed-mode fracture specimen: the DCB specimen loaded with uneven bending moments. Print. Pitney Bowes Management Services A/S - Risø-R-1394(EN), 1-35.
-
-
-
-
45
-
-
0032837191
-
An experimental method to measure the mode-III interlaminar fracture toughness of composite materials"
-
Suemasu H. An experimental method to measure the mode-III interlaminar fracture toughness of composite materials". Composites Science and Technology 59 (1999) 1015-1021
-
(1999)
Composites Science and Technology
, vol.59
, pp. 1015-1021
-
-
Suemasu, H.1
-
46
-
-
33947185260
-
-
Szekrényes, A. 2005. Delamination of composite specimens. Ph.D. Thesis, Budapest University of Technology and Economics, Faculty of Mechanical Engineering, Department of Applied Mechanics, Budapest, PhD-261/2004.
-
-
-
-
47
-
-
33746479200
-
Prestressed fracture specimen for delamination testing of composites
-
Szekrényes A. Prestressed fracture specimen for delamination testing of composites. International Journal of Fracture 139 (2006) 213-237
-
(2006)
International Journal of Fracture
, vol.139
, pp. 213-237
-
-
Szekrényes, A.1
-
48
-
-
33947167754
-
-
Szekrényes, A., submitted for publication, 2006b. Improved analysis of the modified split-cantilever beam for mode-III fracture. Cement and Concrete Composites.
-
-
-
-
49
-
-
27544507926
-
Mode-II fracture in E-glass/polyester composite
-
Szekrényes A., and Uj J. Mode-II fracture in E-glass/polyester composite. Journal of Composite Materials 39 19 (2005) 1747-1768
-
(2005)
Journal of Composite Materials
, vol.39
, Issue.19
, pp. 1747-1768
-
-
Szekrényes, A.1
Uj, J.2
-
50
-
-
30944455661
-
Comparison of some improved solutions for mixed-mode composite delamination coupons
-
Szekrényes A., and Uj J. Comparison of some improved solutions for mixed-mode composite delamination coupons. Composite Structures 72 (2006) 321-329
-
(2006)
Composite Structures
, vol.72
, pp. 321-329
-
-
Szekrényes, A.1
Uj, J.2
-
51
-
-
0030609352
-
-
Trakas, K., Kortschot, M.T. 1997. The relationship between critical strain energy release rate and fracture mode multidirectional carbon-fiber/epoxy laminates. In: Armanios, E.A. (Ed.), Composite Materials: Fatigue and Fracture, vol. 6, ASTM STP 1285, ASTM, pp. 283-304.
-
-
-
-
52
-
-
0030230641
-
Use of end-loaded-split (ELS) test to study stable fracture behaviour of composites under mode-II loading
-
Wang H., and Vu-Khanh T. Use of end-loaded-split (ELS) test to study stable fracture behaviour of composites under mode-II loading. Composite Structures 36 (1996) 71-79
-
(1996)
Composite Structures
, vol.36
, pp. 71-79
-
-
Wang, H.1
Vu-Khanh, T.2
-
53
-
-
0142216018
-
Novel beam analysis of the end notched flexure specimen for mode-II fracture
-
Wang J., and Qiao P. Novel beam analysis of the end notched flexure specimen for mode-II fracture. Engineering Fracture Mechanics 71 (2004) 219-231
-
(2004)
Engineering Fracture Mechanics
, vol.71
, pp. 219-231
-
-
Wang, J.1
Qiao, P.2
-
54
-
-
33947124560
-
-
Wang, W.-X., Takao, Y., Nakata, M. 2003. Effects of friction on the measurement of the mode II interlaminar fracture toughness of composite laminates. In: Proceedings of the 14th International Conference on Composite Materials (CD-ROM), Manuscript No.: 1429, July 14-18, San Diego, California, USA.
-
-
-
-
55
-
-
0024864238
-
End corrections for orthotropic DCB specimens
-
Williams J.G. End corrections for orthotropic DCB specimens. Composites Science and Technology 35 (1989) 367-376
-
(1989)
Composites Science and Technology
, vol.35
, pp. 367-376
-
-
Williams, J.G.1
-
56
-
-
27144471408
-
Examination of the 4-ENF test for measuring the mode III R-curve of wood
-
Yoshihara H. Examination of the 4-ENF test for measuring the mode III R-curve of wood. Engineering Fracture Mechanics 73 (2006) 42-63
-
(2006)
Engineering Fracture Mechanics
, vol.73
, pp. 42-63
-
-
Yoshihara, H.1
|