메뉴 건너뛰기




Volumn 50, Issue 1, 2015, Pages 38-46

Towards long lasting zirconia-based composites for dental implants: Part I: Innovative synthesis, microstructural characterization and invitro stability

Author keywords

Ageing; Alumina; Composite; Dental implant; Microstructure; Zirconia

Indexed keywords

ALUMINA; ALUMINUM OXIDE; CERIUM OXIDE; COATINGS; COMPOSITE MATERIALS; DENTAL PROSTHESES; ENVIRONMENTAL IMPACT; MICROSTRUCTURE; POWDERS; STRONTIUM COMPOUNDS;

EID: 84932602783     PISSN: 01429612     EISSN: 18785905     Source Type: Journal    
DOI: 10.1016/j.biomaterials.2015.01.018     Document Type: Article
Times cited : (100)

References (46)
  • 1
    • 35548955463 scopus 로고    scopus 로고
    • 3 nanocomposite and a veneering ceramic
    • 3 nanocomposite and a veneering ceramic. Dent Mater 2007, 23:1500-1505.
    • (2007) Dent Mater , vol.23 , pp. 1500-1505
    • Fisher, J.1    Stawarczyk, B.2
  • 2
    • 79953299288 scopus 로고    scopus 로고
    • Ceramics for dental applications: a review
    • Denry I., Holloway J.A. Ceramics for dental applications: a review. Materials 2010, 3:351-368.
    • (2010) Materials , vol.3 , pp. 351-368
    • Denry, I.1    Holloway, J.A.2
  • 3
    • 69649085444 scopus 로고    scopus 로고
    • The tetragonal-monoclinic transformation in zirconia: lesson learned and future trends
    • Chevalier J., Gremillard L., Virkar A.V., Clarke D.R. The tetragonal-monoclinic transformation in zirconia: lesson learned and future trends. JAm Ceram Soc 2009, 92:1901-1920.
    • (2009) JAm Ceram Soc , vol.92 , pp. 1901-1920
    • Chevalier, J.1    Gremillard, L.2    Virkar, A.V.3    Clarke, D.R.4
  • 4
    • 0029237462 scopus 로고
    • Environmental degradation of zirconia ceramics
    • Lawson S. Environmental degradation of zirconia ceramics. JEur Ceram Soc 1995, 15:485-502.
    • (1995) JEur Ceram Soc , vol.15 , pp. 485-502
    • Lawson, S.1
  • 5
    • 77953685176 scopus 로고    scopus 로고
    • Low temperature degradation -aging- of zirconia: a critical review of the relevant aspects in dentistry
    • Lughi V., Sergo V. Low temperature degradation -aging- of zirconia: a critical review of the relevant aspects in dentistry. Dent Mater 2010, 26:807-820.
    • (2010) Dent Mater , vol.26 , pp. 807-820
    • Lughi, V.1    Sergo, V.2
  • 6
    • 26844583254 scopus 로고    scopus 로고
    • What future for zirconia as a biomaterial?
    • Chevalier J. What future for zirconia as a biomaterial?. Biomaterials 2006, 27:535-543.
    • (2006) Biomaterials , vol.27 , pp. 535-543
    • Chevalier, J.1
  • 9
    • 84875212608 scopus 로고    scopus 로고
    • Low temperature degradation and reliability of one-piece ceramic oral implants with a porous surface
    • Sanon C., Chevalier J., Douillard T., Kohal R.J., Coelho P.G., Hjerppe J., et al. Low temperature degradation and reliability of one-piece ceramic oral implants with a porous surface. Dent Mater 2013, 29:389-397.
    • (2013) Dent Mater , vol.29 , pp. 389-397
    • Sanon, C.1    Chevalier, J.2    Douillard, T.3    Kohal, R.J.4    Coelho, P.G.5    Hjerppe, J.6
  • 10
    • 84856531797 scopus 로고    scopus 로고
    • Low-temperature degradation of different zirconia ceramics for dental applications
    • Kohorst P., Borchers L., Strempel J., Stiesch M., Hassel T., Bach F.W., et al. Low-temperature degradation of different zirconia ceramics for dental applications. Acta Biomater 2012, 8:1213-1220.
    • (2012) Acta Biomater , vol.8 , pp. 1213-1220
    • Kohorst, P.1    Borchers, L.2    Strempel, J.3    Stiesch, M.4    Hassel, T.5    Bach, F.W.6
  • 12
  • 13
    • 38349192796 scopus 로고    scopus 로고
    • State of the art of zirconia for dental applications
    • Denry I., Kelly J.R. State of the art of zirconia for dental applications. Dent Mater 2008, 24:299-307.
    • (2008) Dent Mater , vol.24 , pp. 299-307
    • Denry, I.1    Kelly, J.R.2
  • 14
    • 0036132150 scopus 로고    scopus 로고
    • Crack growth resistance of alumina, zirconia and zirconia toughened alumina ceramics for joint prostheses
    • De Aza A.H., Chevalier J., Fantozzi G., Schehl M., Torrecillas R. Crack growth resistance of alumina, zirconia and zirconia toughened alumina ceramics for joint prostheses. Biomaterials 2002, 23:937-945.
    • (2002) Biomaterials , vol.23 , pp. 937-945
    • De Aza, A.H.1    Chevalier, J.2    Fantozzi, G.3    Schehl, M.4    Torrecillas, R.5
  • 15
    • 68549083371 scopus 로고    scopus 로고
    • On the kinetics and impact of tetragonal to monoclinic transformation in an alumina/zirconia composite for arthroplasty applications
    • Chevalier J., Grandjean S., Kuntz M., Pezzotti G. On the kinetics and impact of tetragonal to monoclinic transformation in an alumina/zirconia composite for arthroplasty applications. Biomaterials 2009, 30:5279-5282.
    • (2009) Biomaterials , vol.30 , pp. 5279-5282
    • Chevalier, J.1    Grandjean, S.2    Kuntz, M.3    Pezzotti, G.4
  • 16
  • 18
    • 61649127532 scopus 로고    scopus 로고
    • Ceramics for medical applications: a picture for the next 20 years
    • Chevalier J., Gremillard L. Ceramics for medical applications: a picture for the next 20 years. JEur Ceram Soc 2009, 29:1245-1255.
    • (2009) JEur Ceram Soc , vol.29 , pp. 1245-1255
    • Chevalier, J.1    Gremillard, L.2
  • 19
    • 33750975872 scopus 로고    scopus 로고
    • Static and cyclic crack propagation in Ce-TZP ceramics with different amounts of transformation toughening
    • El Attaoui H., Saâdaoui M., Chevalier J., Fantozzi G. Static and cyclic crack propagation in Ce-TZP ceramics with different amounts of transformation toughening. JEur Ceram Soc 2007, 27:483-486.
    • (2007) JEur Ceram Soc , vol.27 , pp. 483-486
    • El Attaoui, H.1    Saâdaoui, M.2    Chevalier, J.3    Fantozzi, G.4
  • 20
    • 0032290602 scopus 로고    scopus 로고
    • Tough and strong Ce-TZP/alumina nanocomposites doped with titania
    • Nawa M., Nakamoto S., Sekino T., Niihara K. Tough and strong Ce-TZP/alumina nanocomposites doped with titania. Cer Int 1998, 24:497-506.
    • (1998) Cer Int , vol.24 , pp. 497-506
    • Nawa, M.1    Nakamoto, S.2    Sekino, T.3    Niihara, K.4
  • 24
    • 56049113455 scopus 로고    scopus 로고
    • Properties of zirconia-toughened-alumina prepared via powder processing and colloidal processing routes
    • Rafferty A., Alsebaie A.M., Olabi A.G., Prescott T. Properties of zirconia-toughened-alumina prepared via powder processing and colloidal processing routes. JColloid Interf S C 2009, 329:310-315.
    • (2009) JColloid Interf S C , vol.329 , pp. 310-315
    • Rafferty, A.1    Alsebaie, A.M.2    Olabi, A.G.3    Prescott, T.4
  • 25
    • 0036533926 scopus 로고    scopus 로고
    • Preparation of alumina-high zirconia microcomposite by combined gel-precipitation
    • Bhattacharyya S., Pratihar S.K., Sinha R.K., Behera R.C., Ganguly R.I. Preparation of alumina-high zirconia microcomposite by combined gel-precipitation. Mater Lett 2002, 53:425-431.
    • (2002) Mater Lett , vol.53 , pp. 425-431
    • Bhattacharyya, S.1    Pratihar, S.K.2    Sinha, R.K.3    Behera, R.C.4    Ganguly, R.I.5
  • 26
    • 0037075766 scopus 로고    scopus 로고
    • Alumina nanocomposites from powder-alkoxide mixtures
    • Schehl M., Diaz J.A., Torrecillas R. Alumina nanocomposites from powder-alkoxide mixtures. Acta Mater 2002, 50:1125-1139.
    • (2002) Acta Mater , vol.50 , pp. 1125-1139
    • Schehl, M.1    Diaz, J.A.2    Torrecillas, R.3
  • 28
    • 53349117628 scopus 로고    scopus 로고
    • Alumina-based nanocomposites obtained by doping with inorganic salt solutions: application to immiscible and reactive systems
    • Palmero P., Naglieri V., Chevalier J., Fantozzi G., Montanaro L. Alumina-based nanocomposites obtained by doping with inorganic salt solutions: application to immiscible and reactive systems. JEur Ceram Soc 2009, 29:59-66.
    • (2009) JEur Ceram Soc , vol.29 , pp. 59-66
    • Palmero, P.1    Naglieri, V.2    Chevalier, J.3    Fantozzi, G.4    Montanaro, L.5
  • 30
    • 46749123800 scopus 로고    scopus 로고
    • Fracture toughness, strength and slow crack growth in a ceria stabilized zirconia-alumina nanocomposite for medical applications
    • Benzaid R., Chevalier J., Saâdaoui M., Fantozzi G., Nawa M., Diaz L.A., et al. Fracture toughness, strength and slow crack growth in a ceria stabilized zirconia-alumina nanocomposite for medical applications. Biomaterials 2008, 29:3636-3641.
    • (2008) Biomaterials , vol.29 , pp. 3636-3641
    • Benzaid, R.1    Chevalier, J.2    Saâdaoui, M.3    Fantozzi, G.4    Nawa, M.5    Diaz, L.A.6
  • 31
    • 0022755218 scopus 로고
    • Strength limitations of transformation-toughened zirconia alloys
    • Swain M.V., Rose L.R.F. Strength limitations of transformation-toughened zirconia alloys. JAm Ceram Soc 1986, 69:511-518.
    • (1986) JAm Ceram Soc , vol.69 , pp. 511-518
    • Swain, M.V.1    Rose, L.R.F.2
  • 33
    • 0035157050 scopus 로고    scopus 로고
    • High strength and toughness alumina matrix composites by transformation toughening and "in situ" platelets reinformcement (ZPTA)-the new generation of bioceramics
    • Burger W., Richter H.G. High strength and toughness alumina matrix composites by transformation toughening and "in situ" platelets reinformcement (ZPTA)-the new generation of bioceramics. Key Eng Mat 2011, 192:545-548.
    • (2011) Key Eng Mat , vol.192 , pp. 545-548
    • Burger, W.1    Richter, H.G.2
  • 34
    • 84887196433 scopus 로고    scopus 로고
    • Acomparison of microstructure and mechanical properties of 12Ce-TZP reinforced with alumina and in situ formed strontium- or lanthanum-hexaaluminate precipitates
    • Kern F. Acomparison of microstructure and mechanical properties of 12Ce-TZP reinforced with alumina and in situ formed strontium- or lanthanum-hexaaluminate precipitates. JEur Ceram Soc 2014, 34:413-423.
    • (2014) JEur Ceram Soc , vol.34 , pp. 413-423
    • Kern, F.1
  • 36
    • 84890287526 scopus 로고    scopus 로고
    • Initial bacterial adhesion on different yttria-stabilized tetragonal zirconia implant surfaces invitro
    • Karygianni L., Jähnig A., Schienle S., Bernsmann F., Adolfsson E., Kohal R.J., et al. Initial bacterial adhesion on different yttria-stabilized tetragonal zirconia implant surfaces invitro. Materials 2013, 6:5659-5674.
    • (2013) Materials , vol.6 , pp. 5659-5674
    • Karygianni, L.1    Jähnig, A.2    Schienle, S.3    Bernsmann, F.4    Adolfsson, E.5    Kohal, R.J.6
  • 38
    • 84932637266 scopus 로고    scopus 로고
    • http://www.dkkk.co.jp/english.
  • 39
    • 84932622409 scopus 로고    scopus 로고
    • http://www.tosoh.com/our-products/advanced-materials/zirconia-grinding%13dispersion-media.
  • 42
    • 79954993042 scopus 로고    scopus 로고
    • Evaluation of precipitates used in strainer head loss testing: part III. Long-term aluminum hydroxide precipitation tests in borated water
    • Bahn C.B., Kasza K.E., Shack W.J., Natesan K., Klein P. Evaluation of precipitates used in strainer head loss testing: part III. Long-term aluminum hydroxide precipitation tests in borated water. Nucl Eng Des 2011, 241:1914-1925.
    • (2011) Nucl Eng Des , vol.241 , pp. 1914-1925
    • Bahn, C.B.1    Kasza, K.E.2    Shack, W.J.3    Natesan, K.4    Klein, P.5
  • 44
    • 84875465277 scopus 로고    scopus 로고
    • Thermal analyses applied to ceramic nanopowders: from synthesis to sintering. A review on transition alumina powder-based materials
    • Montanaro L., Palmero P., Lombardi M., Esnouf C., Chevalier J., Cardinal S. Thermal analyses applied to ceramic nanopowders: from synthesis to sintering. A review on transition alumina powder-based materials. JTherm Anal Calorim 2013, 112:437-445.
    • (2013) JTherm Anal Calorim , vol.112 , pp. 437-445
    • Montanaro, L.1    Palmero, P.2    Lombardi, M.3    Esnouf, C.4    Chevalier, J.5    Cardinal, S.6
  • 45
    • 0029271623 scopus 로고
    • Deformation bands in ceria-stabilized tetragonal zirconia/alumina: II. Stress-induced aging at room temperature
    • Sergo V., Clarke D.R. Deformation bands in ceria-stabilized tetragonal zirconia/alumina: II. Stress-induced aging at room temperature. JAmer Ceram Soc 1995, 78:641-644.
    • (1995) JAmer Ceram Soc , vol.78 , pp. 641-644
    • Sergo, V.1    Clarke, D.R.2
  • 46
    • 34547381199 scopus 로고    scopus 로고
    • Low-temperature degradation of zirconia and implications for biomedical implants
    • Chevalier J., Gremillard L., Deville S. Low-temperature degradation of zirconia and implications for biomedical implants. Ann Rev Mat Res 2007, 37:1-32.
    • (2007) Ann Rev Mat Res , vol.37 , pp. 1-32
    • Chevalier, J.1    Gremillard, L.2    Deville, S.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.