메뉴 건너뛰기




Volumn 87, Issue , 2014, Pages 504-516

Corrosion mechanism of Al, Al-Zn and Al-Zn-Sn alloys in 3wt.% NaCl solution

Author keywords

A. Alloy; A. Aluminum; B. EIS; B. Polarization; B. SEM

Indexed keywords

ALUMINUM ALLOYS; CORROSION; ELECTROCHEMICAL IMPEDANCE SPECTROSCOPY; GRAIN BOUNDARIES; SCANNING ELECTRON MICROSCOPY; TIN; TIN ALLOYS; X RAY SPECTROSCOPY; ZINC; ELECTROCHEMICAL CORROSION; ENERGY DISPERSIVE SPECTROSCOPY;

EID: 84905380123     PISSN: 0010938X     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.corsci.2014.07.018     Document Type: Article
Times cited : (169)

References (77)
  • 1
    • 77950298398 scopus 로고    scopus 로고
    • Electrochemical behavior of aluminium alloys containing indium and tin in NaCl solution
    • Gudić S., Smoljko I., Kliškić M. Electrochemical behavior of aluminium alloys containing indium and tin in NaCl solution. Mater. Chem. Phys. 2010, 121:561.
    • (2010) Mater. Chem. Phys. , vol.121 , pp. 561
    • Gudić, S.1    Smoljko, I.2    Kliškić, M.3
  • 3
    • 0025383096 scopus 로고
    • Evolution of the chemistry of passive films of sputter-deposited, supersaturated Al alloys
    • Davis G.D., Moshier W.C., Fritz T.L., Cote G.O. Evolution of the chemistry of passive films of sputter-deposited, supersaturated Al alloys. J. Electrochem. Soc. 1990, 137:422.
    • (1990) J. Electrochem. Soc. , vol.137 , pp. 422
    • Davis, G.D.1    Moshier, W.C.2    Fritz, T.L.3    Cote, G.O.4
  • 4
    • 0026906125 scopus 로고
    • Insight into the pitting corrosion behavior of aluminum alloys
    • Szklarska-Smialowska Z. Insight into the pitting corrosion behavior of aluminum alloys. Corros. Sci. 1992, 33:1193.
    • (1992) Corros. Sci. , vol.33 , pp. 1193
    • Szklarska-Smialowska, Z.1
  • 5
    • 0030735125 scopus 로고    scopus 로고
    • Activation of aluminium by indium ions in chloride solutions
    • Saidman S.B., Bessone J.B. Activation of aluminium by indium ions in chloride solutions. Electrochim. Acta 1997, 42:413.
    • (1997) Electrochim. Acta , vol.42 , pp. 413
    • Saidman, S.B.1    Bessone, J.B.2
  • 7
    • 4744346431 scopus 로고    scopus 로고
    • Comprehensive model for the activation mechanism of Al-Zn alloys produced by indium
    • Bessone J.B., Flamini D.O., Saidman S.B. Comprehensive model for the activation mechanism of Al-Zn alloys produced by indium. Corros. Sci. 2005, 47:95.
    • (2005) Corros. Sci. , vol.47 , pp. 95
    • Bessone, J.B.1    Flamini, D.O.2    Saidman, S.B.3
  • 8
    • 0027588631 scopus 로고
    • Studies on the anodic behavior of aluminum electrodes in alkaline solution
    • Pengfei S., Geping Y., Baojia X., Guoqi L.U. Studies on the anodic behavior of aluminum electrodes in alkaline solution. J. Power Sources 1993, 45:105.
    • (1993) J. Power Sources , vol.45 , pp. 105
    • Pengfei, S.1    Geping, Y.2    Baojia, X.3    Guoqi, L.U.4
  • 9
    • 0030717784 scopus 로고    scopus 로고
    • Activation of aluminium anodes by the presence of intermetallic compounds
    • Barbucci A., Cerisola G., Bruzzone G., Saccone A. Activation of aluminium anodes by the presence of intermetallic compounds. Electrochim. Acta 1997, 42:2369.
    • (1997) Electrochim. Acta , vol.42 , pp. 2369
    • Barbucci, A.1    Cerisola, G.2    Bruzzone, G.3    Saccone, A.4
  • 11
    • 84885174398 scopus 로고    scopus 로고
    • The performance of Al-Zn-In-Mg-Ti sacrificial anode in simulated deep water environment
    • Sun H., Liu L., Li Y., Ma L., Yan Y. The performance of Al-Zn-In-Mg-Ti sacrificial anode in simulated deep water environment. Corros. Sci. 2013, 77:77.
    • (2013) Corros. Sci. , vol.77 , pp. 77
    • Sun, H.1    Liu, L.2    Li, Y.3    Ma, L.4    Yan, Y.5
  • 12
    • 0036778768 scopus 로고    scopus 로고
    • Corrosion of an Al-Zn-In alloy in chloride media
    • Muñoz A.G., Saidman S.B., Bessone J.B. Corrosion of an Al-Zn-In alloy in chloride media. Corros. Sci. 2002, 44:2171.
    • (2002) Corros. Sci. , vol.44 , pp. 2171
    • Muñoz, A.G.1    Saidman, S.B.2    Bessone, J.B.3
  • 13
    • 0037662275 scopus 로고    scopus 로고
    • Corrosion mechanism of Al-Zn-In alloys in chloride solutions
    • Muñoz A.G., Saidman S.B., Bessone J.B. Corrosion mechanism of Al-Zn-In alloys in chloride solutions. Latin Am. Appl. Res. 2003, 33:275.
    • (2003) Latin Am. Appl. Res. , vol.33 , pp. 275
    • Muñoz, A.G.1    Saidman, S.B.2    Bessone, J.B.3
  • 14
    • 38949116256 scopus 로고    scopus 로고
    • An investigation on the use of indium to increase dissolution of AlZn anodes in sea water
    • Zazoua A., Azzouz N. An investigation on the use of indium to increase dissolution of AlZn anodes in sea water. Mater. Des. 2008, 29:806.
    • (2008) Mater. Des. , vol.29 , pp. 806
    • Zazoua, A.1    Azzouz, N.2
  • 15
    • 80054860059 scopus 로고    scopus 로고
    • Optimization of manganese and magnesium contents in As-cast aluminium-zinc-indium alloy as sacrificial anode
    • Saeri† M.R., Keyvani A. Optimization of manganese and magnesium contents in As-cast aluminium-zinc-indium alloy as sacrificial anode. J. Mater. Sci. Technol. 2011, 27:785.
    • (2011) J. Mater. Sci. Technol. , vol.27 , pp. 785
    • Saeri, M.R.1    Keyvani, A.2
  • 16
    • 0031338764 scopus 로고    scopus 로고
    • AC impedance study on the activation mechanism of aluminium by indium and zinc in 3.5% NaCl medium
    • Venugopal A., Raja V.S. AC impedance study on the activation mechanism of aluminium by indium and zinc in 3.5% NaCl medium. Corros. Sci. 1997, 39:2053.
    • (1997) Corros. Sci. , vol.39 , pp. 2053
    • Venugopal, A.1    Raja, V.S.2
  • 17
    • 0029274701 scopus 로고
    • Electrochemical behaviour of Al-In alloys in chloride solutions
    • Saidman S.B., Garcia S.G., Bessone J.B. Electrochemical behaviour of Al-In alloys in chloride solutions. J. Appl. Electrochm. 1995, 25:252.
    • (1995) J. Appl. Electrochm. , vol.25 , pp. 252
    • Saidman, S.B.1    Garcia, S.G.2    Bessone, J.B.3
  • 18
    • 0032687310 scopus 로고    scopus 로고
    • Electrochemical behaviour of Al, Al-Sn, Al-Zn and Al-Zn-Sn alloys in chloride solutions containing indium ions
    • El Shayaeb H.A., Abd El Wahab F.M., Zein El Abedin S. Electrochemical behaviour of Al, Al-Sn, Al-Zn and Al-Zn-Sn alloys in chloride solutions containing indium ions. J. Appl. Electrochem. 1999, 29:473.
    • (1999) J. Appl. Electrochem. , vol.29 , pp. 473
    • El Shayaeb, H.A.1    Abd El Wahab, F.M.2    Zein El Abedin, S.3
  • 20
    • 0035314059 scopus 로고    scopus 로고
    • Effect of gallium ions on the electrochemical behavior of Al, Al-Sn, Al-Zn and Al-Zn-Sn alloys in chloride solutions
    • El Shayeb H.A., Abd El Wahab F.M., Zein El Abidin S. Effect of gallium ions on the electrochemical behavior of Al, Al-Sn, Al-Zn and Al-Zn-Sn alloys in chloride solutions. Corros. Sci. 2001, 43:643.
    • (2001) Corros. Sci. , vol.43 , pp. 643
    • El Shayeb, H.A.1    Abd El Wahab, F.M.2    Zein El Abidin, S.3
  • 21
    • 0035312752 scopus 로고    scopus 로고
    • Electrochemical behavior of Al, Al-Sn, Al-Zn and Al-Zn-Sn alloys in chloride solutions containing stannous ions
    • El Shayeb H.A., Abd El Wahab F.M., Zein El Abidin S. Electrochemical behavior of Al, Al-Sn, Al-Zn and Al-Zn-Sn alloys in chloride solutions containing stannous ions. Corros. Sci. 2001, 43:655.
    • (2001) Corros. Sci. , vol.43 , pp. 655
    • El Shayeb, H.A.1    Abd El Wahab, F.M.2    Zein El Abidin, S.3
  • 22
    • 0026225719 scopus 로고
    • Electrochemical behavior of Al-5%Zn-0.1%Sn sacrificial anode in aggressive Media: influence of its alloying elements and the solidification structure
    • Salinas D.R., Bessone J.B. Electrochemical behavior of Al-5%Zn-0.1%Sn sacrificial anode in aggressive Media: influence of its alloying elements and the solidification structure. Corrosion 1991, 47:665.
    • (1991) Corrosion , vol.47 , pp. 665
    • Salinas, D.R.1    Bessone, J.B.2
  • 23
    • 0028481096 scopus 로고
    • Behaviour of Al-Sn alloy on the negative side of the open-circuit potential
    • Kliskić M., Radosević J., Aljinovic L.J. Behaviour of Al-Sn alloy on the negative side of the open-circuit potential. J. Appl. Electrochem. 1994, 24:814.
    • (1994) J. Appl. Electrochem. , vol.24 , pp. 814
    • Kliskić, M.1    Radosević, J.2    Aljinovic, L.J.3
  • 24
    • 0030264855 scopus 로고    scopus 로고
    • Impedance and transient study of aluminium barrier-type oxide films
    • Gudić S., Radosević J., Kliskić M. Impedance and transient study of aluminium barrier-type oxide films. J. Appl. Electrochem. 1996, 26:1027.
    • (1996) J. Appl. Electrochem. , vol.26 , pp. 1027
    • Gudić, S.1    Radosević, J.2    Kliskić, M.3
  • 25
    • 0005396640 scopus 로고    scopus 로고
    • Impedance transient study of barrier films on aluminium and Al-Sn alloys
    • Proceeding of Symposium on Passivity and its Breakdown, Electrochemical Society, INC, New Jersey
    • S. Gudić, J. Radosević, M. Kliskić, Impedance transient study of barrier films on aluminium and Al-Sn alloys, in: Proceeding of Symposium on Passivity and its Breakdown, Electrochemical Society, INC, New Jersey, 1997, p. 689.
    • (1997) , pp. 689
    • Gudić, S.1    Radosević, J.2    Kliskić, M.3
  • 26
    • 80053239721 scopus 로고    scopus 로고
    • Influence of Ga and Bi on electrochemical performance of Al-Zn-Sn sacrificial anodes
    • He J.-G., Wen J.-B., Li X.-D., Wang G.-W., Xu C.-H. Influence of Ga and Bi on electrochemical performance of Al-Zn-Sn sacrificial anodes. Trans. Nonferr. Metal. Soc. 2011, 21:1580.
    • (2011) Trans. Nonferr. Metal. Soc. , vol.21 , pp. 1580
    • He, J.-G.1    Wen, J.-B.2    Li, X.-D.3    Wang, G.-W.4    Xu, C.-H.5
  • 27
    • 77955586472 scopus 로고    scopus 로고
    • The effect of small addition of tin and indium on the corrosion behavior of aluminium in chloride solution
    • Gudić S., Smoljko I., Kliškić M. The effect of small addition of tin and indium on the corrosion behavior of aluminium in chloride solution. J. Alloys Compd. 2010, 505:54.
    • (2010) J. Alloys Compd. , vol.505 , pp. 54
    • Gudić, S.1    Smoljko, I.2    Kliškić, M.3
  • 28
    • 84865471864 scopus 로고    scopus 로고
    • Electrochemical behavior of Al-Zn-Ga and Al-In-Ga in chloride media
    • O Flamini D., Saidman S.B. Electrochemical behavior of Al-Zn-Ga and Al-In-Ga in chloride media. Mater. Chem. Phys. 2012, 136:103.
    • (2012) Mater. Chem. Phys. , vol.136 , pp. 103
    • Flamini, D.O.1    Saidman, S.B.2
  • 29
    • 84897115293 scopus 로고    scopus 로고
    • The corrosion of two aluminium sacrificial anode alloys in SRB-containing sea mud
    • Liu F., Zhang J., Sun C., Yu Z., Hou B. The corrosion of two aluminium sacrificial anode alloys in SRB-containing sea mud. Corros. Sci. 2014, 83:375-381.
    • (2014) Corros. Sci. , vol.83 , pp. 375-381
    • Liu, F.1    Zhang, J.2    Sun, C.3    Yu, Z.4    Hou, B.5
  • 31
    • 79952899218 scopus 로고    scopus 로고
    • Effects of precipitates on electrochemical performance of Al sacrificial anode
    • He J.-G., Wen J.-B., Li X.-D. Effects of precipitates on electrochemical performance of Al sacrificial anode. Corros. Sci. 2011, 53:1948-1953.
    • (2011) Corros. Sci. , vol.53 , pp. 1948-1953
    • He, J.-G.1    Wen, J.-B.2    Li, X.-D.3
  • 32
    • 0017635660 scopus 로고
    • Pitting potential of high purity binary aluminium alloys-II. Al-Mg and Al-Zn alloys
    • Muller J.C., Galvele J.R. Pitting potential of high purity binary aluminium alloys-II. Al-Mg and Al-Zn alloys. Corros. Sci. 1977, 17:995.
    • (1977) Corros. Sci. , vol.17 , pp. 995
    • Muller, J.C.1    Galvele, J.R.2
  • 33
    • 0037143420 scopus 로고    scopus 로고
    • Aluminum as anode for energy storage and conversion: a review
    • Li Q., Bjerrum N.J. Aluminum as anode for energy storage and conversion: a review. J. Power Sources 2002, 110:1.
    • (2002) J. Power Sources , vol.110 , pp. 1
    • Li, Q.1    Bjerrum, N.J.2
  • 35
    • 0026892935 scopus 로고
    • Activation of aluminium in halide solutions containing 'activator ions'
    • Carroll W.M., Breslin C.B. Activation of aluminium in halide solutions containing 'activator ions'. Corros. Sci. 1992, 33:1161.
    • (1992) Corros. Sci. , vol.33 , pp. 1161
    • Carroll, W.M.1    Breslin, C.B.2
  • 36
    • 0027545107 scopus 로고
    • The activation of aluminium by indium ions in chloride, bromide and iodide solutions
    • Breslin C.B., Carroll W.M. The activation of aluminium by indium ions in chloride, bromide and iodide solutions. Corros. Sci. 1993, 34:327.
    • (1993) Corros. Sci. , vol.34 , pp. 327
    • Breslin, C.B.1    Carroll, W.M.2
  • 37
    • 0031187712 scopus 로고    scopus 로고
    • The self regulating nature of In on the potential of Al in 3.5% NaCl solution
    • Venugopal A., Raja V.S. The self regulating nature of In on the potential of Al in 3.5% NaCl solution. Corros. Sci. 1997, 39:1285.
    • (1997) Corros. Sci. , vol.39 , pp. 1285
    • Venugopal, A.1    Raja, V.S.2
  • 38
    • 0034101338 scopus 로고    scopus 로고
    • Activation of pure Al in an indium-containing electrolyte - an electrochemical noise and impedance study
    • Breslin C.B., Rudd A.L. Activation of pure Al in an indium-containing electrolyte - an electrochemical noise and impedance study. Corros. Sci. 2000, 42:1023.
    • (2000) Corros. Sci. , vol.42 , pp. 1023
    • Breslin, C.B.1    Rudd, A.L.2
  • 40
    • 0032636184 scopus 로고    scopus 로고
    • Influence of alloying elements and microstructure on aluminium sacrificial anode performance: case of Al-Zn
    • Salinas D.R., Garcia S.G., Bessone J.B. Influence of alloying elements and microstructure on aluminium sacrificial anode performance: case of Al-Zn. J. Appl. Electrochem. 1999, 29:1063.
    • (1999) J. Appl. Electrochem. , vol.29 , pp. 1063
    • Salinas, D.R.1    Garcia, S.G.2    Bessone, J.B.3
  • 41
    • 0035241899 scopus 로고    scopus 로고
    • - ion incorporation into native oxide film on pure aluminium in neutral chloride solution on pit initiation
    • - ion incorporation into native oxide film on pure aluminium in neutral chloride solution on pit initiation. Corros. Sci. 2001, 43:353.
    • (2001) Corros. Sci. , vol.43 , pp. 353
    • Pyun, S.-I.1    Lee, W.-J.2
  • 42
    • 65349167280 scopus 로고    scopus 로고
    • The attack initiation of Al-Zn-In-Sn anode by the segregation concentrating Zn, Sn and In
    • Qi G.T., Qiu Y.B., Zhao Y.N., Cai Q.Z. The attack initiation of Al-Zn-In-Sn anode by the segregation concentrating Zn, Sn and In. Mater. Corros. 2009, 60:206.
    • (2009) Mater. Corros. , vol.60 , pp. 206
    • Qi, G.T.1    Qiu, Y.B.2    Zhao, Y.N.3    Cai, Q.Z.4
  • 43
    • 68049137317 scopus 로고    scopus 로고
    • The effects of lanthanum on microstructure and electrochemical properties of Al-Zn-In based sacrificial anode alloys
    • Ma J., Wen J. The effects of lanthanum on microstructure and electrochemical properties of Al-Zn-In based sacrificial anode alloys. Corros. Sci. 2009, 51:2115.
    • (2009) Corros. Sci. , vol.51 , pp. 2115
    • Ma, J.1    Wen, J.2
  • 44
    • 84883242800 scopus 로고    scopus 로고
    • Effect of small amounts of alloyed tin on the electrochemical behavior of aluminium in sodium chloride solution
    • Tan J., Nisancioglu K. Effect of small amounts of alloyed tin on the electrochemical behavior of aluminium in sodium chloride solution. Corros. Sci. 2013, 76:219-230.
    • (2013) Corros. Sci. , vol.76 , pp. 219-230
    • Tan, J.1    Nisancioglu, K.2
  • 45
    • 84887996516 scopus 로고    scopus 로고
    • Corrosion behavior of Mg-2.4Zn alloy micro-alloyed with Ag and Ca
    • Mandal M., Moon A.P., Deo G., Mendis C.L., Mondal K. Corrosion behavior of Mg-2.4Zn alloy micro-alloyed with Ag and Ca. Corros. Sci. 2014, 78:172-182.
    • (2014) Corros. Sci. , vol.78 , pp. 172-182
    • Mandal, M.1    Moon, A.P.2    Deo, G.3    Mendis, C.L.4    Mondal, K.5
  • 46
    • 84905398708 scopus 로고    scopus 로고
    • Thesis of Doctor, Comportement à la corrosion des alliages d'aluminium utilisés dans l'industrie automobile pour la fabrication de radiateur de chauffage
    • Romania, Lyon-France
    • E.L. Din-Stirbu, Thesis of Doctor, Comportement à la corrosion des alliages d'aluminium utilisés dans l'industrie automobile pour la fabrication de radiateur de chauffage, Romania, Lyon-France 2005.
    • (2005)
    • Din-Stirbu, E.L.1
  • 48
    • 0035241902 scopus 로고    scopus 로고
    • Surface reactions during pickling of an aluminium-magnesium-silicon alloy in phosphoric acid
    • Mizuno K., Nylund A., Olefjord I. Surface reactions during pickling of an aluminium-magnesium-silicon alloy in phosphoric acid. Corros. Sci. 2001, 43:381-396.
    • (2001) Corros. Sci. , vol.43 , pp. 381-396
    • Mizuno, K.1    Nylund, A.2    Olefjord, I.3
  • 50
    • 0033428306 scopus 로고    scopus 로고
    • Pitting corrosion of aluminum
    • Szklarska-Smialowska Z. Pitting corrosion of aluminum. Corros. Sci. 1999, 41:1743-1767.
    • (1999) Corros. Sci. , vol.41 , pp. 1743-1767
    • Szklarska-Smialowska, Z.1
  • 51
    • 0003583287 scopus 로고
    • Atlas d'équilibres électrochimiques
    • Cebelcor, Ed. Gauthier-Villars
    • M. Pourbaix, Atlas d'équilibres électrochimiques, Cebelcor, Ed. Gauthier-Villars, 1963.
    • (1963)
    • Pourbaix, M.1
  • 52
    • 77957664305 scopus 로고    scopus 로고
    • Comparison of corrosion behaviour of zinc in NaCl and in NaOH solutions. Part I: corrosion layer characterization
    • Mouanga M., Berçot P., Rauch J.Y. Comparison of corrosion behaviour of zinc in NaCl and in NaOH solutions. Part I: corrosion layer characterization. Corros. Sci. 2010, 52:3984-3992.
    • (2010) Corros. Sci. , vol.52 , pp. 3984-3992
    • Mouanga, M.1    Berçot, P.2    Rauch, J.Y.3
  • 53
    • 84862811068 scopus 로고    scopus 로고
    • In situ corrosion analysis of Al-Zn-In-Mg-Ti-Ce sacrificial anode alloy
    • Ma J., Wen J., Zhai W., Li Q. In situ corrosion analysis of Al-Zn-In-Mg-Ti-Ce sacrificial anode alloy. Mater. Charact. 2012, 65:86.
    • (2012) Mater. Charact. , vol.65 , pp. 86
    • Ma, J.1    Wen, J.2    Zhai, W.3    Li, Q.4
  • 54
    • 84869506053 scopus 로고    scopus 로고
    • Effect of aluminium on the passivation of zinc-aluminium alloys in artificial seawater at 80 C
    • Kaewmaneekul T., Lothongkum G. Effect of aluminium on the passivation of zinc-aluminium alloys in artificial seawater at 80 C. Corros. Sci. 2013, 66:67.
    • (2013) Corros. Sci. , vol.66 , pp. 67
    • Kaewmaneekul, T.1    Lothongkum, G.2
  • 56
    • 84880947652 scopus 로고    scopus 로고
    • Environmentally assisted cracking behavior of Al-Zn-Mg-Cu-Cr alloy bonded with polymer matrix composite stiffener
    • Kale S.S., Raja V.S., Bakare A.K. Environmentally assisted cracking behavior of Al-Zn-Mg-Cu-Cr alloy bonded with polymer matrix composite stiffener. Corros. Sci. 2013, 75:318-325.
    • (2013) Corros. Sci. , vol.75 , pp. 318-325
    • Kale, S.S.1    Raja, V.S.2    Bakare, A.K.3
  • 57
    • 0022721588 scopus 로고
    • Localized corrosion of aluminum alloys - a review
    • Foley R.T. Localized corrosion of aluminum alloys - a review. Corrosion 1986, 42:277-288.
    • (1986) Corrosion , vol.42 , pp. 277-288
    • Foley, R.T.1
  • 58
    • 26944454422 scopus 로고    scopus 로고
    • Electrochemical corrosion behaviour of lead-free Sn-8.5 Zn-x Ag-0.1 Al-0.5 Ga solder in 3.5% NaCl solution
    • Mohanty U.S., Lin K.-L. Electrochemical corrosion behaviour of lead-free Sn-8.5 Zn-x Ag-0.1 Al-0.5 Ga solder in 3.5% NaCl solution. Mater. Sci. Eng. A 2005, 406:34.
    • (2005) Mater. Sci. Eng. A , vol.406 , pp. 34
    • Mohanty, U.S.1    Lin, K.-L.2
  • 60
    • 84878375987 scopus 로고    scopus 로고
    • Atmospheric corrosion of Galfan coating on steel in chloride-riche environments
    • Zhang X., Leygraf C., Wallinder I.O. Atmospheric corrosion of Galfan coating on steel in chloride-riche environments. Corros. Sci. 2013, 73:62-71.
    • (2013) Corros. Sci. , vol.73 , pp. 62-71
    • Zhang, X.1    Leygraf, C.2    Wallinder, I.O.3
  • 62
    • 0037769361 scopus 로고    scopus 로고
    • Pitting of aluminium in non-aqueous chloride media
    • Muñoz A.G., Bessone J.B. Pitting of aluminium in non-aqueous chloride media. Corros. Sci. 1999, 41:1447.
    • (1999) Corros. Sci. , vol.41 , pp. 1447
    • Muñoz, A.G.1    Bessone, J.B.2
  • 64
    • 0002577382 scopus 로고
    • Impedance spectroscopy and its use in analyzing the steady-state AC response of solid and liquid electrolytes
    • Macdonald J.R. Impedance spectroscopy and its use in analyzing the steady-state AC response of solid and liquid electrolytes. J. Electroanal. Chem. 1987, 223:25.
    • (1987) J. Electroanal. Chem. , vol.223 , pp. 25
    • Macdonald, J.R.1
  • 66
    • 0036295450 scopus 로고    scopus 로고
    • Deviations of capacitive and inductive loops in the electrochemical impedance of a dissolving iron electrode
    • Itagaki M., Taya A., Watanabe K., Noda K. Deviations of capacitive and inductive loops in the electrochemical impedance of a dissolving iron electrode. Anal. Sci. 2002, 18:641.
    • (2002) Anal. Sci. , vol.18 , pp. 641
    • Itagaki, M.1    Taya, A.2    Watanabe, K.3    Noda, K.4
  • 68
    • 0345246198 scopus 로고
    • Faraday impedances and intermediates in electrochemical reactions
    • Epelboin I., Keddam M., Lestrade J.C. Faraday impedances and intermediates in electrochemical reactions. Faraday Disc. Chem. Soc. 1973, 56:264.
    • (1973) Faraday Disc. Chem. Soc. , vol.56 , pp. 264
    • Epelboin, I.1    Keddam, M.2    Lestrade, J.C.3
  • 69
    • 59149100917 scopus 로고    scopus 로고
    • Evaluation of inhibitive action of some quaternary N-heterocyclic compounds on the corrosion of Al-Cu alloy in hydrochloric acid
    • Ehteram A.N. Evaluation of inhibitive action of some quaternary N-heterocyclic compounds on the corrosion of Al-Cu alloy in hydrochloric acid. Mater. Chem. Phys. 2009, 114:533.
    • (2009) Mater. Chem. Phys. , vol.114 , pp. 533
    • Ehteram, A.N.1
  • 70
    • 0037197585 scopus 로고    scopus 로고
    • Negative capacitance for polyaniline - an analysis via electrochemical impedance spectroscopy
    • Chen W.-C., Wen T.-C., Copalan A. Negative capacitance for polyaniline - an analysis via electrochemical impedance spectroscopy. Synth. Met. 2002, 128:179.
    • (2002) Synth. Met. , vol.128 , pp. 179
    • Chen, W.-C.1    Wen, T.-C.2    Copalan, A.3
  • 71
    • 0036472001 scopus 로고    scopus 로고
    • Identification of inductive behavior for polyaniline via electrochemical impedance spectroscopy
    • Chen W.-C., Wen T.-C., Hu C.-C., Copalan A. Identification of inductive behavior for polyaniline via electrochemical impedance spectroscopy. Electrochim. Acta 2002, 47:1305.
    • (2002) Electrochim. Acta , vol.47 , pp. 1305
    • Chen, W.-C.1    Wen, T.-C.2    Hu, C.-C.3    Copalan, A.4
  • 72
    • 0000058779 scopus 로고
    • J.C. Scully (Ed.), Treatise on Material Science and Technology
    • Academic Press, New York
    • G.E. Thompson, G.C. Wood, in: J.C. Scully (Ed.), Treatise on Material Science and Technology, Academic Press, New York, vol. 23, 1983, p. 18.
    • (1983) , vol.23 , pp. 18
    • Thompson, G.E.1    Wood, G.C.2
  • 73
    • 0035263470 scopus 로고    scopus 로고
    • The role of alloyed molybdenum in the inhibition of pitting corrosion in stainless steels
    • Ilevbare G.O., Burstein G.T. The role of alloyed molybdenum in the inhibition of pitting corrosion in stainless steels. Corros. Sci. 2001, 43:485.
    • (2001) Corros. Sci. , vol.43 , pp. 485
    • Ilevbare, G.O.1    Burstein, G.T.2
  • 74
    • 0035127057 scopus 로고    scopus 로고
    • Microelectrochemical studies of pit initiation at single inclusions in Al 2024-T3
    • Suter T., Alkir R.C. Microelectrochemical studies of pit initiation at single inclusions in Al 2024-T3. J. Electrochem. Soc. 2001, 148:B36-B42.
    • (2001) J. Electrochem. Soc. , vol.148
    • Suter, T.1    Alkir, R.C.2
  • 75
    • 84892319682 scopus 로고    scopus 로고
    • Introduction to Corrosion Science
    • New York-USA
    • E. McCafferty, Introduction to Corrosion Science, New York-USA, 2010.
    • (2010)
    • McCafferty, E.1
  • 76
    • 76449119437 scopus 로고    scopus 로고
    • Corrosion behavior of ultra-fine grained industrial pure Al fabricated by ECAP
    • Song D., Ma A.-B., Jiang J.-H. Corrosion behavior of ultra-fine grained industrial pure Al fabricated by ECAP. Trans. Nonferrous Met. Soc. China 2009, 19:1065-1070.
    • (2009) Trans. Nonferrous Met. Soc. China , vol.19 , pp. 1065-1070
    • Song, D.1    Ma, A.-B.2    Jiang, J.-H.3
  • 77
    • 0017635660 scopus 로고
    • Pitting of high purity binary aluminium alloys - II. Al-Mg and Al-Zn alloys
    • Muller I.L., Galvele J.R. Pitting of high purity binary aluminium alloys - II. Al-Mg and Al-Zn alloys. Corros. Sci. 1977, 17:995-1007.
    • (1977) Corros. Sci. , vol.17 , pp. 995-1007
    • Muller, I.L.1    Galvele, J.R.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.