Volumn 40, Issue 7 PART A, 2014, Pages 9009-9016

Mechanical and microwave dielectric properties of KD-I SiCf/SiC composites fabricated through precursor infiltration and pyrolysis

Author keywords

C. Dielectric properties; C. Mechanical properties; Precursor infiltration and pyrolysis

Indexed keywords

AUGER ELECTRON SPECTROSCOPY; COATINGS; DIELECTRIC PROPERTIES OF SOLIDS; FIBERS; MECHANICAL PROPERTIES; PHOTOELECTRONS; SCANNING ELECTRON MICROSCOPY; TRANSMISSION ELECTRON MICROSCOPY; X RAY PHOTOELECTRON SPECTROSCOPY;

EID: 84900497883     PISSN: 02728842     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.ceramint.2014.01.113     Document Type: Article
Times cited : (42)

References (48)
  • 1
    • 9344222773 scopus 로고    scopus 로고
    • Microwave absorbing materials
    • V.M. Petrov, and V.V. Gagulin Microwave absorbing materials Inorg. Mater. 37 2 2001 93 98
    • (2001) Inorg. Mater. , vol.37 , Issue.2 , pp. 93-98
    • Petrov, V.M.1    Gagulin, V.V.2
  • 2
    • 37849189742 scopus 로고    scopus 로고
    • A two-layer dielectric absorber covering a wide frequency range
    • F. Luo, D.M. Zhu, and W.C. Zhou A two-layer dielectric absorber covering a wide frequency range Ceram. Int. 33 2007 197 200
    • (2007) Ceram. Int. , vol.33 , pp. 197-200
    • Luo, F.1    Zhu, D.M.2    Zhou, W.C.3
  • 3
    • 33646346106 scopus 로고    scopus 로고
    • Application research and prospects of new and light mass radar absorbing materials
    • E.H. Ha, D.Q. Huang, and H.Y. Ding Application research and prospects of new and light mass radar absorbing materials J. Mater Eng. 3 2006 55 59
    • (2006) J. Mater Eng. , vol.3 , pp. 55-59
    • Ha, E.H.1    Huang, D.Q.2    Ding, H.Y.3
  • 4
    • 1842588034 scopus 로고    scopus 로고
    • Microwave absorption enhancement and complex permittivity and permeability of Fe encapsulated within carbon nanotubes
    • R.C. Che, L.M. Peng, X.F. Duan, Q. Chen, and X.L. Liang Microwave absorption enhancement and complex permittivity and permeability of Fe encapsulated within carbon nanotubes Adv. Mater. 16 5 2004 401 405
    • (2004) Adv. Mater. , vol.16 , Issue.5 , pp. 401-405
    • Che, R.C.1    Peng, L.M.2    Duan, X.F.3    Chen, Q.4    Liang, X.L.5
  • 5
    • 17644372364 scopus 로고    scopus 로고
    • SiC-matrix composites: Non brittle ceramics for thermostructural application
    • R. Naslain SiC-matrix composites: non brittle ceramics for thermostructural application Int. J. Appl. Ceram. Technol. 2 2005 75 84
    • (2005) Int. J. Appl. Ceram. Technol. , vol.2 , pp. 75-84
    • Naslain, R.1
  • 6
    • 0348013351 scopus 로고    scopus 로고
    • Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: An overview
    • R. Naslain Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview Compos. Sci. Technol. 64 2004 155 170
    • (2004) Compos. Sci. Technol. , vol.64 , pp. 155-170
    • Naslain, R.1
  • 7
    • 84866852746 scopus 로고    scopus 로고
    • Dielectric properties of SiC fiber-reinforced SiC matrix composites in the temperature range from 25 to 700 °c at frequencies between 8.2 and 18 GHz
    • H.T. Liu, H. Tian, and H.F. Cheng Dielectric properties of SiC fiber-reinforced SiC matrix composites in the temperature range from 25 to 700 °C at frequencies between 8.2 and 18 GHz J. Nucl. Mater. 432 2013 57 60
    • (2013) J. Nucl. Mater. , vol.432 , pp. 57-60
    • Liu, H.T.1    Tian, H.2    Cheng, H.F.3
  • 8
    • 84875250672 scopus 로고    scopus 로고
    • Ni-decorated SiC powders: Enhanced high-temperature dielectric properties and microwave absorption performance
    • J. Yuan, H.J. Yang, Z.L. Hou, W.L. Song, H. Xu, Y.Q. Kang, H.B. Jin, X.Y. Fang, and M.S. Cao Ni-decorated SiC powders: enhanced high-temperature dielectric properties and microwave absorption performance Powder Technol. 237 2012 309 313
    • (2012) Powder Technol. , vol.237 , pp. 309-313
    • Yuan, J.1    Yang, H.J.2    Hou, Z.L.3    Song, W.L.4    Xu, H.5    Kang, Y.Q.6    Jin, H.B.7    Fang, X.Y.8    Cao, M.S.9
  • 9
    • 84890280773 scopus 로고    scopus 로고
    • A high-temperature radar absorbing structure: Design, fabrication and characterization
    • H. Tian, H.T. Liu, H.F. Cheng, A high-temperature radar absorbing structure: design, fabrication and characterization, Compos. Sci. Technol. 90 (2014) 202-208.
    • (2014) Compos. Sci. Technol. , vol.90 , pp. 202-208
    • Tian, H.1    Liu, H.T.2    Cheng, H.F.3
  • 11
    • 0036500241 scopus 로고    scopus 로고
    • The influence of an interphase on the deflection of a matrix crack in a ceramic-matrix composite
    • C. Lacroix, D. Leguillon, and E. Martin The influence of an interphase on the deflection of a matrix crack in a ceramic-matrix composite Compos. Sci. Technol 62 4 2002 519 523
    • (2002) Compos. Sci. Technol , vol.62 , Issue.4 , pp. 519-523
    • Lacroix, C.1    Leguillon, D.2    Martin, E.3
  • 12
    • 84865630187 scopus 로고    scopus 로고
    • f/SiC composites with alternating PyC/SiC multilayer interphases
    • f/SiC composites with alternating PyC/SiC multilayer interphases Mater. Des. 44 2013 320 324
    • (2013) Mater. Des. , vol.44 , pp. 320-324
    • Yu, H.J.1    Zhou, X.G.2    Zhang, W.3
  • 13
    • 84862817354 scopus 로고    scopus 로고
    • f/SiC composites with BN interphase prepared by dip-coating process
    • f/SiC composites with BN interphase prepared by dip-coating process J. Eur. Ceram. Soc. 32 2012 2505 2512
    • (2012) J. Eur. Ceram. Soc. , vol.32 , pp. 2505-2512
    • Liu, H.T.1    Tian, H.2
  • 14
    • 77955514909 scopus 로고    scopus 로고
    • f/SiC composites fabricated by PIP process
    • f/SiC composites fabricated by PIP process Ceram. Int. 36 2010 2033 2037
    • (2010) Ceram. Int. , vol.36 , pp. 2033-2037
    • Liu, H.T.1    Cheng, H.F.2    Wang, J.3
  • 15
    • 3342960901 scopus 로고    scopus 로고
    • Preparation of silicon-based oxide layer on high-crystalline SiC fiber as an interphase in SiC/SiC composites
    • N. Igawa, T. Taguchi, R. Yamada, Y. Ishii, and S. Jitsukawa Preparation of silicon-based oxide layer on high-crystalline SiC fiber as an interphase in SiC/SiC composites J. Nucl. Mater. 329-333 2004 554 557
    • (2004) J. Nucl. Mater. , vol.329-333 , pp. 554-557
    • Igawa, N.1    Taguchi, T.2    Yamada, R.3    Ishii, Y.4    Jitsukawa, S.5
  • 18
    • 29844434507 scopus 로고    scopus 로고
    • Chemical vapor infiltrated SiC/SiC composites (CVI SiC/SiC)
    • N.P. Bansal, Kluwer
    • J. Lamon Chemical vapor infiltrated SiC/SiC composites (CVI SiC/SiC) N.P. Bansal, Handbook of Ceramic Composites 2005 Kluwer 55 76
    • (2005) Handbook of Ceramic Composites , pp. 55-76
    • Lamon, J.1
  • 20
    • 11144258701 scopus 로고    scopus 로고
    • Preparation of SiC fiber-reinforced SiC composites
    • X.B. He, and H. Yang Preparation of SiC fiber-reinforced SiC composites J. Mater. Process. Technol. 159 2005 135 138
    • (2005) J. Mater. Process. Technol. , vol.159 , pp. 135-138
    • He, X.B.1    Yang, H.2
  • 21
    • 0041734601 scopus 로고    scopus 로고
    • Effect of ageing treatments at high temperatures on the microstructure and mechanical behaviour of 2D Nicalon/C/SiC composites. 1: Ageing under vacuum or argon
    • C. Labrugkre, A. Guette, and R. Naslain Effect of ageing treatments at high temperatures on the microstructure and mechanical behaviour of 2D Nicalon/C/SiC composites. 1: Ageing under vacuum or argon J. Eur. Ceram. Soc. 17 1997 623 640
    • (1997) J. Eur. Ceram. Soc. , vol.17 , pp. 623-640
    • Labrugkre, C.1    Guette, A.2    Naslain, R.3
  • 22
    • 0035980513 scopus 로고    scopus 로고
    • Influence of fiber coating thickness on fracture behavior of continuous woven Nicalon fabric-reinforced silicon-carbide matrix ceramic composites
    • J.H. Miller, P.K. Liaw, and J.D. Landes Influence of fiber coating thickness on fracture behavior of continuous woven Nicalon fabric-reinforced silicon-carbide matrix ceramic composites Mater. Sci. Eng. A 317 2001 49 58
    • (2001) Mater. Sci. Eng. A , vol.317 , pp. 49-58
    • Miller, J.H.1    Liaw, P.K.2    Landes, J.D.3
  • 23
    • 0033945255 scopus 로고    scopus 로고
    • High-temperature thermal stability of Hi-Nicalon™ SiC fiber/SiC matrix composites under long term cyclic heating
    • M. Takeda, Y. Imai, Y. Kagawa, and S.Q. Guo High-temperature thermal stability of Hi-Nicalon™ SiC fiber/SiC matrix composites under long term cyclic heating Mater. Sci. Eng. A 286 2000 312 323
    • (2000) Mater. Sci. Eng. A , vol.286 , pp. 312-323
    • Takeda, M.1    Imai, Y.2    Kagawa, Y.3    Guo, S.Q.4
  • 24
    • 0036883753 scopus 로고    scopus 로고
    • Tensile fracture behavior of continuous SiC fiber-reinforced SiC matrix composites at elevated temperatures and correlation to in situ constituent properties
    • S. Guo, and Y. Kagawa Tensile fracture behavior of continuous SiC fiber-reinforced SiC matrix composites at elevated temperatures and correlation to in situ constituent properties J. Eur. Ceram. Soc 22 2002 2349 2356
    • (2002) J. Eur. Ceram. Soc , vol.22 , pp. 2349-2356
    • Guo, S.1    Kagawa, Y.2
  • 25
    • 0034818330 scopus 로고    scopus 로고
    • Improvement of mechanical properties of SiC/SiC composites by various surface treatments of fibers
    • T. Hinoki, W. Yang, T. Nozawa, T. Shibayama, and Y. Katoh Improvement of mechanical properties of SiC/SiC composites by various surface treatments of fibers J. Nucl. Mater. 289 2001 23 29
    • (2001) J. Nucl. Mater. , vol.289 , pp. 23-29
    • Hinoki, T.1    Yang, W.2    Nozawa, T.3    Shibayama, T.4    Katoh, Y.5
  • 27
    • 33751523794 scopus 로고    scopus 로고
    • Effects of heat treatment on the microstructure and flexural properties of CVI-Tyranno-SA/SiC composite
    • Wen Yang, H. Araki, A. Kohyama, Q. Yang, and T. Noda Effects of heat treatment on the microstructure and flexural properties of CVI-Tyranno-SA/SiC composite Ceram Int. 33 2007 141 146
    • (2007) Ceram Int. , vol.33 , pp. 141-146
    • Yang, W.1    Araki, H.2    Kohyama, A.3    Yang, Q.4    Noda, T.5
  • 29
    • 0037465963 scopus 로고    scopus 로고
    • Mechanical properties of several advanced Tyranno-SA fiber-reinforced CVI-SiC/SiC composites
    • W. Yang, T. Noda, H. Araki, J. Yu, and A. Kohyama Mechanical properties of several advanced Tyranno-SA fiber-reinforced CVI-SiC/SiC composites Mater. Sci. Eng. A 345 2003 28 35
    • (2003) Mater. Sci. Eng. A , vol.345 , pp. 28-35
    • Yang, W.1    Noda, T.2    Araki, H.3    Yu, J.4    Kohyama, A.5
  • 31
    • 0016974220 scopus 로고
    • Synthesis of continuous SiC fibers with high tensile strength
    • S. Yajima, K. Okamura, J. Hayashi., and M. Omori Synthesis of continuous SiC fibers with high tensile strength J. Am. Ceram. Soc. 59 1976 324 327
    • (1976) J. Am. Ceram. Soc. , vol.59 , pp. 324-327
    • Yajima, S.1    Okamura, K.2    Hayashi, J.3    Omori, M.4
  • 32
    • 79955601048 scopus 로고    scopus 로고
    • SiC fibers with controllable thickness of carbon layer prepared directly by preceramic polymer pyrolysis routes
    • T.J. Hu, X.D. Li, G.Y. Li, D.Y. Wang, and J. Wang SiC fibers with controllable thickness of carbon layer prepared directly by preceramic polymer pyrolysis routes Mater. Sci. Eng. B 176 2011 706 710
    • (2011) Mater. Sci. Eng. B , vol.176 , pp. 706-710
    • Hu, T.J.1    Li, X.D.2    Li, G.Y.3    Wang, D.Y.4    Wang, J.5
  • 33
    • 77953607685 scopus 로고    scopus 로고
    • SiC fiber with low electrical resistivity and oxygen content
    • D.Y. Wang, X.H. Mao, Y.C. Song, and Y.D. Wang SiC fiber with low electrical resistivity and oxygen content Sci. China Technol. Sci. 53 2010 1038 1044
    • (2010) Sci. China Technol. Sci. , vol.53 , pp. 1038-1044
    • Wang, D.Y.1    Mao, X.H.2    Song, Y.C.3    Wang, Y.D.4
  • 34
    • 84861943618 scopus 로고    scopus 로고
    • Effect of composition and structure on specific resistivity of SiC fibers
    • D.Y. Wang, Y.C. Song, and Y.Q. Li Effect of composition and structure on specific resistivity of SiC fibers Trans. Nonferr. Metal Soc. China 22 2012 1133 1139
    • (2012) Trans. Nonferr. Metal Soc. China , vol.22 , pp. 1133-1139
    • Wang, D.Y.1    Song, Y.C.2    Li, Y.Q.3
  • 35
    • 0344468183 scopus 로고    scopus 로고
    • Determination of carbon and oxygen in silicon carbide fibers
    • R. He, D. Jiang, and X. Li Determination of carbon and oxygen in silicon carbide fibers J. Chin Ceram. Soc. 31 4 2003 386 388
    • (2003) J. Chin Ceram. Soc. , vol.31 , Issue.4 , pp. 386-388
    • He, R.1    Jiang, D.2    Li, X.3
  • 36
    • 69649096236 scopus 로고    scopus 로고
    • Oxidation of silicon carbide fibers during static fatigue in air at intermediate temperatures
    • W. Gauthier, F. Pailler, J. Lamon, and R. Pailler Oxidation of silicon carbide fibers during static fatigue in air at intermediate temperatures J. Am. Ceram. Soc. 92 9 2009 2067 2073
    • (2009) J. Am. Ceram. Soc. , vol.92 , Issue.9 , pp. 2067-2073
    • Gauthier, W.1    Pailler, F.2    Lamon, J.3    Pailler, R.4
  • 37
    • 34247092013 scopus 로고    scopus 로고
    • Tensile creep behavior of SiC-based fibers with a low oxygen content
    • C. Sauder, and J. Lamon Tensile creep behavior of SiC-based fibers with a low oxygen content J. Am. Ceram. Soc. 90 4 2007 1146 1156
    • (2007) J. Am. Ceram. Soc. , vol.90 , Issue.4 , pp. 1146-1156
    • Sauder, C.1    Lamon, J.2
  • 38
    • 0033740018 scopus 로고    scopus 로고
    • Characterization of interfaces in C fiber-renforced laminated C-SiC matrix composites
    • K.A. Appiah, Z.L. Wang, and W.J. Lackey Characterization of interfaces in C fiber-renforced laminated C-SiC matrix composites Carbon 38 2000 831 838
    • (2000) Carbon , vol.38 , pp. 831-838
    • Appiah, K.A.1    Wang, Z.L.2    Lackey, W.J.3
  • 39
    • 33748533488 scopus 로고    scopus 로고
    • The analysis of carbon bonding environment in HWCVD deposited a-SiC:H films by XPS and Raman spectroscopy
    • P.B. Swain The analysis of carbon bonding environment in HWCVD deposited a-SiC:H films by XPS and Raman spectroscopy Surf. Coat. Technol. 201 2006 1589 1593
    • (2006) Surf. Coat. Technol. , vol.201 , pp. 1589-1593
    • Swain, P.B.1
  • 40
    • 67651017506 scopus 로고    scopus 로고
    • Microstructural investigations of the pyrocarbon interphase in SiC fiber-reinforced SiC matrix composites
    • H.T. Liu, H.F. Cheng, J. Wang, R.C. Che, G.P. Tang, and Q.S. Ma Microstructural investigations of the pyrocarbon interphase in SiC fiber-reinforced SiC matrix composites Mater. Lett. 63 2009 2029 2031
    • (2009) Mater. Lett. , vol.63 , pp. 2029-2031
    • Liu, H.T.1    Cheng, H.F.2    Wang, J.3    Che, R.C.4    Tang, G.P.5    Ma, Q.S.6
  • 41
    • 79953767935 scopus 로고    scopus 로고
    • In situ growth of a carbon interphase between carbon fibres and a polycarbosilane-derived silicon carbide matrix
    • Y. Ma, S. Wang, and Z.H. Chen In situ growth of a carbon interphase between carbon fibres and a polycarbosilane-derived silicon carbide matrix Carbon 49 2011 2869 2877
    • (2011) Carbon , vol.49 , pp. 2869-2877
    • Ma, Y.1    Wang, S.2    Chen, Z.H.3
  • 42
    • 0032620745 scopus 로고    scopus 로고
    • A TEM study of microstructure of carbon fiber/polycarbosilane-derived SiC composites
    • G.B. Zheng, H. Sano, K. Suzuki, K. Kazuo, U. Yasuo, and H.M. Cheng A TEM study of microstructure of carbon fiber/polycarbosilane-derived SiC composites Carbon 37 1999 2057 2062
    • (1999) Carbon , vol.37 , pp. 2057-2062
    • Zheng, G.B.1    Sano, H.2    Suzuki, K.3    Kazuo, K.4    Yasuo, U.5    Cheng, H.M.6
  • 43
    • 84900495458 scopus 로고    scopus 로고
    • Microstructual investigation of interfaces in CMCs
    • G. Boitier, S. Darzens, J.L. Chermant, and J. Vicens Microstructual investigation of interfaces in CMCs Compos. A 331 2002 1467 1470
    • (2002) Compos. A , vol.331 , pp. 1467-1470
    • Boitier, G.1    Darzens, S.2    Chermant, J.L.3    Vicens, J.4
  • 44
    • 67649111355 scopus 로고    scopus 로고
    • High dielectric loss and its monotonic dependence of conducting-dominated multiwalled carbon nanotubes/silica nanocomposite on temperature ranging from 373 to 873 K in X-band
    • W.L. Song, M.S. Cao, Z.L. Hou, X.Y. Fang, X.L. Shi, and J. Yuan High dielectric loss and its monotonic dependence of conducting-dominated multiwalled carbon nanotubes/silica nanocomposite on temperature ranging from 373 to 873 K in X-band Appl. Phys. Lett. 94 23 2009 233110
    • (2009) Appl. Phys. Lett. , vol.94 , Issue.23 , pp. 233110
    • Song, W.L.1    Cao, M.S.2    Hou, Z.L.3    Fang, X.Y.4    Shi, X.L.5    Yuan, J.6
  • 45
    • 0036132917 scopus 로고    scopus 로고
    • Nanometer silicon carbide powder synthesis and its dielectric behavior in the GHz range
    • B. Zhang, J.B. Li, J.J. Sun, S.X. Zhang, H.Z. Zhai, and Z.W. Du Nanometer silicon carbide powder synthesis and its dielectric behavior in the GHz range J. Eur. Ceram. Soc. 22 2002 93 99
    • (2002) J. Eur. Ceram. Soc. , vol.22 , pp. 93-99
    • Zhang, B.1    Li, J.B.2    Sun, J.J.3    Zhang, S.X.4    Zhai, H.Z.5    Du, Z.W.6
  • 48
    • 84875029361 scopus 로고    scopus 로고
    • 2 composites fabricated through a sol-gel process
    • 2 composites fabricated through a sol-gel process Powder Technol. 239 2013 374 380
    • (2013) Powder Technol. , vol.239 , pp. 374-380
    • Tian, H.1    Liu, H.T.2    Cheng, H.F.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.