메뉴 건너뛰기




Volumn 101, Issue 4, 2013, Pages 485-497

In vitro study on newly designed biodegradable Fe-X composites (X = W, CNT) prepared by spark plasma sintering

Author keywords

Biocompatibility; Biodegradable metal; Corrosion; Fe X composite; Spark plasma sintering

Indexed keywords

BIODEGRADABLE METALS; CANDIDATE MATERIALS; CORROSION BEHAVIOR; ELECTROCHEMICAL MEASUREMENTS; LOCALIZED CORROSION; PHYSIOLOGICAL ENVIRONMENT; SPARK PLASMA SINTERING METHOD; ULTIMATE COMPRESSIVE STRENGTH;

EID: 84879605324     PISSN: 15524973     EISSN: 15524981     Source Type: Journal    
DOI: 10.1002/jbm.b.32783     Document Type: Article
Times cited : (75)

References (41)
  • 2
    • 33749451169 scopus 로고    scopus 로고
    • Update on bioabsorbable stents: From bench to clinical
    • DOI 10.1111/j.1540-8183.2006.00187.x
    • Waksman R. Update on bioabsorbable stents: From bench to clinical. J Interv Cardiol 2006;19:414-421. (Pubitemid 44511072)
    • (2006) Journal of Interventional Cardiology , vol.19 , Issue.5 , pp. 414-421
    • Waksman, R.1
  • 3
    • 28844481103 scopus 로고    scopus 로고
    • Magnesium and its alloys as orthopedic biomaterials: A review
    • DOI 10.1016/j.biomaterials.2005.10.003, PII S0142961205009014
    • Staiger MP, Pietak AM, Huadmai J, Dias G. Magnesium and its alloys as orthopedic biomaterials: A review. Biomaterials 2006;27: 1728-1734. (Pubitemid 41760433)
    • (2006) Biomaterials , vol.27 , Issue.9 , pp. 1728-1734
    • Staiger, M.P.1    Pietak, A.M.2    Huadmai, J.3    Dias, G.4
  • 5
    • 56549090894 scopus 로고    scopus 로고
    • In vitro corrosion and biocompatibility of binary magnesium alloys
    • Gu X, Zheng Y, Cheng Y, Zhong S, Xi T. In vitro corrosion and biocompatibility of binary magnesium alloys. Biomaterials 2009; 30:484-498.
    • (2009) Biomaterials , vol.30 , pp. 484-498
    • Gu, X.1    Zheng, Y.2    Cheng, Y.3    Zhong, S.4    Xi, T.5
  • 6
    • 34248224956 scopus 로고    scopus 로고
    • A possible biodegradable magnesium implant material
    • DOI 10.1002/adem.200600252
    • Song G, Song S. A possible biodegradable magnesium implant material. Adv Eng Mater 2007;9:298-302. (Pubitemid 46707090)
    • (2007) Advanced Engineering Materials , vol.9 , Issue.4 , pp. 298-302
    • Song, G.1    Song, S.2
  • 7
    • 34249744766 scopus 로고    scopus 로고
    • Magnesium and its alloys as degradable biomaterials. Corrosion studies using potentiodynamic and EIS electrochemical techniques
    • Muller WD, Nascimento ML, Zeddies M, Corsico M, Gassa LM, Mele MAFL. Magnesium and its alloys as degradable biomaterials: Corrosion studies using potentiodynamic and EIS electrochemical techniques. Mater Res 2007;10:5-10. (Pubitemid 46830253)
    • (2007) Materials Research , vol.10 , Issue.1 , pp. 5-10
    • Muller, W.D.1    Nascimento, M.L.2    Zeddies, M.3    Corsico, M.4    Gassa, L.M.5    De Mele, M.A.F.L.6
  • 8
    • 53449099699 scopus 로고    scopus 로고
    • Optical coherence tomography and intravascular ultrasound imaging of bioabsorbable magnesium stent degradation in porcine coronary arteries
    • Slottow T, Pakala R, Okabe T, Hellinga D, Lovec R, Tio F, Bui A, Waksman R. Optical coherence tomography and intravascular ultrasound imaging of bioabsorbable magnesium stent degradation in porcine coronary arteries. Cardiovasc Revasc Med 2008;9: 248-254.
    • (2008) Cardiovasc Revasc Med , vol.9 , pp. 248-254
    • Slottow, T.1    Pakala, R.2    Okabe, T.3    Hellinga, D.4    Lovec, R.5    Tio, F.6    Bui, A.7    Waksman, R.8
  • 9
    • 77954685452 scopus 로고    scopus 로고
    • Design strategy for biodegradable Fe-based alloys for medical applications
    • Schinhammer M, Hanzi AC, Loffler JF, Uggowitzer PJ. Design strategy for biodegradable Fe-based alloys for medical applications. Acta Biomater 2010;6:1705-1713.
    • (2010) Acta Biomater , vol.6 , pp. 1705-1713
    • Schinhammer, M.1    Hanzi, A.C.2    Loffler, J.F.3    Uggowitzer, P.J.4
  • 10
    • 77954673809 scopus 로고    scopus 로고
    • Developments in metallic biodegradable stents
    • Hermawan H, Dube D, Mantovani D. Developments in metallic biodegradable stents. Acta Biomater 2010;6:1693-1697.
    • (2010) Acta Biomater , vol.6 , pp. 1693-1697
    • Hermawan, H.1    Dube, D.2    Mantovani, D.3
  • 11
    • 79251648817 scopus 로고    scopus 로고
    • Effects of alloying elements (Mn, Co, Al, W, Sn, B, C and S) on biodegradability and in vitro biocompatibility of pure iron
    • Liu B, Zheng YF. Effects of alloying elements (Mn, Co, Al, W, Sn, B, C and S) on biodegradability and in vitro biocompatibility of pure iron. Acta Biomater 2011;7:1407-1420.
    • (2011) Acta Biomater , vol.7 , pp. 1407-1420
    • Liu, B.1    Zheng, Y.F.2
  • 12
    • 33747740694 scopus 로고    scopus 로고
    • Are resorbable implants about to become a reality?
    • DOI 10.1017/S1047951106000011, PII S1047951106000011
    • Peuster M, Beerbaum P, Bach FW, Hauser H. Are resorbable implants about to become a reality? Cardiol Young 2006;16: 107-116. (Pubitemid 44269389)
    • (2006) Cardiology in the Young , vol.16 , Issue.2 , pp. 107-116
    • Peuster, M.1    Beerbaum, P.2    Bach, F.-W.3    Hauser, H.4
  • 13
    • 77954684596 scopus 로고    scopus 로고
    • Fe-Mn alloys for metallic biodegradable stents: Degradation and cell viability studies
    • Hermawan H, Purnama A, Dube D, Couet J, Mantovani D. Fe-Mn alloys for metallic biodegradable stents: Degradation and cell viability studies. Acta Biomater 2010;6:1852-1860.
    • (2010) Acta Biomater , vol.6 , pp. 1852-1860
    • Hermawan, H.1    Purnama, A.2    Dube, D.3    Couet, J.4    Mantovani, D.5
  • 14
    • 0034778878 scopus 로고    scopus 로고
    • A novel approach to temporary stenting: Degradable cardiovascular stents produced from corrodible metal - Results 6-18 months after implantation into New Zealand white rabbits
    • Peuster M, Wohlsein P, Brugmann M, Ehlerding M, Seidler K, Fink C, Brauer H, Fischer A, Hausdorf G. A novel approach to temporary stenting: Degradable cardiovascular stents produced from corrodible metal-results 6-18 months after implantation into New Zealand white rabbits. Heart 2001;86:563-569. (Pubitemid 32999872)
    • (2001) Heart , vol.86 , Issue.5 , pp. 563-569
    • Peuster, M.1    Wohlsein, P.2    Brugmann, M.3    Ehlerding, M.4    Seidler, K.5    Fink, C.6    Brauer, H.7    Fischer, A.8    Hausdorf, G.9
  • 15
    • 33744988409 scopus 로고    scopus 로고
    • Long-term biocompatibility of a corrodible peripheral iron stent in the porcine descending aorta
    • DOI 10.1016/j.biomaterials.2006.05.029, PII S0142961206004923
    • Peuster M, Hesse C, Schloo T, Fink C, Beerbaum P, von Schnakenburg C. Long-term biocompatibility of a corrodible peripheral iron stent in the porcine descending aorta. Biomaterials 2006;27: 4955-4962. (Pubitemid 43866928)
    • (2006) Biomaterials , vol.27 , Issue.28 , pp. 4955-4962
    • Peuster, M.1    Hesse, C.2    Schloo, T.3    Fink, C.4    Beerbaum, P.5    Von Schnakenburg, C.6
  • 17
    • 58549103551 scopus 로고    scopus 로고
    • Biocompatibility of Fe-O films synthesized by plasma immersion ion implantation and deposition
    • Zhu S, Huang N, Xu L, Zhang Y, Liu H, Lei Y, Sun H, Yao Y. Biocompatibility of Fe-O films synthesized by plasma immersion ion implantation and deposition. Surf Coat Technol 2009;203: 1523-1529.
    • (2009) Surf Coat Technol , vol.203 , pp. 1523-1529
    • Zhu, S.1    Huang, N.2    Xu, L.3    Zhang, Y.4    Liu, H.5    Lei, Y.6    Sun, H.7    Yao, Y.8
  • 18
    • 77954667713 scopus 로고    scopus 로고
    • Electroformed iron as new biomaterial for degradable stents: Development process and structure-properties relationship
    • Moravej M, Prima F, Fiset M, Mantovani D. Electroformed iron as new biomaterial for degradable stents: Development process and structure-properties relationship. Acta Biomater 2010;6: 1726-1735.
    • (2010) Acta Biomater , vol.6 , pp. 1726-1735
    • Moravej, M.1    Prima, F.2    Fiset, M.3    Mantovani, D.4
  • 19
    • 77954665666 scopus 로고    scopus 로고
    • Electroformed pure iron as a new biomaterial for degradable stents: In vitro degradation and preliminary cell viability studies
    • Moravej M, Purnama A, Fiset M, Couet J, Mantovani D. Electroformed pure iron as a new biomaterial for degradable stents: In vitro degradation and preliminary cell viability studies. Acta Biomater 2010;6:1843-1851.
    • (2010) Acta Biomater , vol.6 , pp. 1843-1851
    • Moravej, M.1    Purnama, A.2    Fiset, M.3    Couet, J.4    Mantovani, D.5
  • 20
    • 0034554828 scopus 로고    scopus 로고
    • Rapid sintering of nanocrystalline ZrO2 (3Y) by spark plasma sintering
    • Li W, Gao L. Rapid sintering of nanocrystalline ZrO2 (3Y) by spark plasma sintering. J Eur Ceram Soc 2000;20:2441-2445.
    • (2000) J Eur Ceram Soc , vol.20 , pp. 2441-2445
    • Li, W.1    Gao, L.2
  • 22
    • 39749148359 scopus 로고    scopus 로고
    • Mechanical properties of nanostructured and ultrafine-grained iron alloys produced by spark plasma sintering of ball milled powders
    • DOI 10.1016/j.msea.2007.05.111, PII S0921509307012920
    • Libardi S, Zadra M, Casari F, Molinari A. Mechanical properties of nanostructured and ultrafine-grained iron alloys produced by spark plasma sintering of ball milled powders. Mater Sci Eng A 2008;478:243-250. (Pubitemid 351292494)
    • (2008) Materials Science and Engineering A , vol.478 , Issue.1-2 , pp. 243-250
    • Libardi, S.1    Zadra, M.2    Casari, F.3    Molinari, A.4
  • 23
    • 79954414783 scopus 로고    scopus 로고
    • Microstructure and mechanical properties of magnesium composites prepared by spark plasma sintering technology
    • Muhammad WNAW, Sajuri Z, Mutoh Y, Miyashita Y. Microstructure and mechanical properties of magnesium composites prepared by spark plasma sintering technology. J Alloys Compd 2011;509:6021-6029.
    • (2011) J Alloys Compd , vol.509 , pp. 6021-6029
    • Wnaw, M.1    Sajuri, Z.2    Mutoh, Y.3    Miyashita, Y.4
  • 26
    • 0037290055 scopus 로고    scopus 로고
    • Degradation of tungsten coils implanted into the subclavian artery of New Zealand white rabbits is not associated with local or systemic toxicity
    • DOI 10.1016/S0142-9612(02)00352-6, PII S0142961202003526
    • Peuster M, Fink C, Wohlsein P, Bruegmann M, Gunther A, Kaese V, Niemeyer M, Haferkamp H, Schnakenburg C. Degradation of tungsten coils implanted into the subclavian artery of New Zealand white rabbits is not associated with local or systemic toxicity. Biomaterials 2003;24:393-399. (Pubitemid 35287512)
    • (2003) Biomaterials , vol.24 , Issue.3 , pp. 393-399
    • Peuster, M.1    Fink, C.2    Wohlsein, P.3    Bruegmann, M.4    Gunther, A.5    Kaese, V.6    Niemeyer, M.7    Haferkamp, H.8    Schnakenburg, C.V.9
  • 27
    • 58849160335 scopus 로고    scopus 로고
    • Tubular micro-scale multiwalled carbon nanotube-based scaffolds for tissue engineering
    • Edwards SL, Church JS, Werkmeister JA, Ramshaw JAM. Tubular micro-scale multiwalled carbon nanotube-based scaffolds for tissue engineering. Biomaterials 2009;30:1725-1731.
    • (2009) Biomaterials , vol.30 , pp. 1725-1731
    • Edwards, S.L.1    Church, J.S.2    Werkmeister, J.A.3    Ramshaw, J.A.M.4
  • 28
    • 32144456766 scopus 로고    scopus 로고
    • In vitro studies of carbon nanotubes biocompatibility
    • DOI 10.1016/j.carbon.2005.11.022, PII S0008622305006998, Toxicology of Carbon Nanimaterials
    • Chlopek J, Czajkowska B, Szaraniec B, Frackowiak E, Szostak K, Beguin F. In vitro studies of carbon nanotubes biocompatibility. Carbon 2006;44:1106-1111. (Pubitemid 43204500)
    • (2006) Carbon , vol.44 , Issue.6 , pp. 1106-1111
    • Chlopek, J.1    Czajkowska, B.2    Szaraniec, B.3    Frackowiak, E.4    Szostak, K.5    Beguin, F.6
  • 29
    • 84879602142 scopus 로고    scopus 로고
    • ASTM E. E 9-89a,Standard Test Methods of Compression Testing of Metallic Materials at Room Temperature. Annual Book of ASTM Standards 2000; 3
    • ASTM E. E 9-89a,Standard Test Methods of Compression Testing of Metallic Materials at Room Temperature. Annual Book of ASTM Standards 2000; 3.
  • 30
    • 0036013929 scopus 로고    scopus 로고
    • Effect of surface chemistries and characteristics of Ti6Al4V on the Ca and P adsorption and ion dissolution in Hank's ethylene diamine tetra-acetic acid solution
    • DOI 10.1016/S0142-9612(01)00420-3, PII S0142961201004203
    • Chang E, Lee T. Effect of surface chemistries and characteristics of Ti6Al4V on the Ca and P adsorption and ion dissolution in Hank's ethylene diamine tetra-acetic acid solution. Biomaterials 2002;23:2917-2925. (Pubitemid 34497083)
    • (2002) Biomaterials , vol.23 , Issue.14 , pp. 2917-2925
    • Chang, E.1    Lee, T.M.2
  • 31
    • 84879603811 scopus 로고    scopus 로고
    • ASTM G. G 31-72, Standard Practice for Laboratory Immersion Corrosion Testing of Metals, ASTM Book of Standards, Philadelphia, PA
    • ASTM G. G 31-72, Standard Practice for Laboratory Immersion Corrosion Testing of Metals, ASTM Book of Standards, Philadelphia, PA.
  • 32
    • 33845437441 scopus 로고    scopus 로고
    • Protection of iron corrosion by stearic acid and stearic imidazoline self-assembled monolayers
    • DOI 10.1016/j.apsusc.2006.01.038, PII S0169433206000560
    • Liu X, Chen S, Ma H, Liu G, Shen L. Protection of iron corrosion by stearic acid and stearic imidazoline self-assembled monolayers. Appl Surf Sci 2006;253:814-820. (Pubitemid 44894211)
    • (2006) Applied Surface Science , vol.253 , Issue.2 , pp. 814-820
    • Liu, X.1    Chen, S.2    Ma, H.3    Liu, G.4    Shen, L.5
  • 33
    • 28844497993 scopus 로고    scopus 로고
    • Control of smooth muscle cell proliferation by ferrous iron
    • DOI 10.1016/j.biomaterials.2005.10.042, PII S0142961205010173
    • Mueller PP, May T, Perz A, Hauser H, Peuster M. Control of smooth muscle cell proliferation by ferrous iron. Biomaterials 2006;27:2193-2200. (Pubitemid 41774531)
    • (2006) Biomaterials , vol.27 , Issue.10 , pp. 2193-2200
    • Mueller, P.P.1    May, T.2    Perz, A.3    Hauser, H.4    Peuster, M.5
  • 34
    • 67349109411 scopus 로고    scopus 로고
    • Biocompatibility of pure iron: In vitro assessment of degradation kinetics and cytotoxicity on endothelial cells
    • Zhu S, Huang N, Xu L, Zhang Y, Liu H, Sun H, Leng Y. Biocompatibility of pure iron: In vitro assessment of degradation kinetics and cytotoxicity on endothelial cells. Mater Sci Eng C 2009;29: 1589-1592.
    • (2009) Mater Sci Eng C , vol.29 , pp. 1589-1592
    • Zhu, S.1    Huang, N.2    Xu, L.3    Zhang, Y.4    Liu, H.5    Sun, H.6    Leng, Y.7
  • 35
    • 84879603497 scopus 로고    scopus 로고
    • ASTM F756-08. Standard Practice for Assessment of Hemolytic Properties of Materials, Annual Book of ASTM Standards, American Society for Testing and Materials, Philadelphia, Pennsylvania, USA 2008
    • ASTM F756-08. Standard Practice for Assessment of Hemolytic Properties of Materials, Annual Book of ASTM Standards, American Society for Testing and Materials, Philadelphia, Pennsylvania, USA 2008.
  • 36
    • 38349153562 scopus 로고    scopus 로고
    • The development of binary Mg-Ca alloys for use as biodegradable materials within bone
    • Li Z, Gu X, Lou S, Zheng Y. The development of binary Mg-Ca alloys for use as biodegradable materials within bone. Biomaterials 2008;29:1329-1344.
    • (2008) Biomaterials , vol.29 , pp. 1329-1344
    • Li, Z.1    Gu, X.2    Lou, S.3    Zheng, Y.4
  • 37
    • 0032008208 scopus 로고    scopus 로고
    • Cytotoxicity evaluation of 43 metal salts using murine fibroblasts and osteoblastic cells
    • DOI 10.1002/(SICI)1097-4636(199802)39:2<331::AID-JBM22>3.0.CO;2-E
    • Yamamoto A, Honma R, Sumita M. Cytotoxicity evaluation of 43 metal salts using murine fibroblasts and osteoblastic cells. J Biomed Mater Res 1998;39:331-340. (Pubitemid 28060368)
    • (1998) Journal of Biomedical Materials Research , vol.39 , Issue.2 , pp. 331-340
    • Yamamoto, A.1    Honma, R.2    Sumita, M.3
  • 39
    • 0038486163 scopus 로고    scopus 로고
    • Biocorrosion of magnesium alloys: A new principle in cardiovascular implant technology?
    • Heublein B, Rohde R, Kaese V, Niemeyer M, Hartung W, Haverich A. Biocorrosion of magnesium alloys: A new principle in cardiovascular implant technology? Heart 2003;89:651.
    • (2003) Heart , vol.89 , pp. 651
    • Heublein, B.1    Rohde, R.2    Kaese, V.3    Niemeyer, M.4    Hartung, W.5    Haverich, A.6
  • 40
    • 0038354711 scopus 로고    scopus 로고
    • Biocompatibility of corroding tungsten coils: In vitro assessment of degradation kinetics and cytotoxicity on human cells
    • DOI 10.1016/S0142-9612(03)00274-6
    • Peuster M. Biocompatibility of corroding tungsten coils: In vitro assessment of degradation kinetics and cytotoxicity on human cells. Biomaterials 2003;24:4057-4061. (Pubitemid 36794408)
    • (2003) Biomaterials , vol.24 , Issue.22 , pp. 4057-4061
    • Peuster, M.1    Fink, C.2    Von Schnakenburg, C.3
  • 41
    • 32044445744 scopus 로고    scopus 로고
    • Investigation of the cytotoxicity of CCVD carbon nanotubes towards human umbilical vein endothelial cells
    • DOI 10.1016/j.carbon.2005.11.007, PII S000862230500672X, Toxicology of Carbon Nanimaterials
    • Flahaut E, Durrieu M, Remyzolghadri M, Bareille R, Baquey C. Investigation of the cytotoxicity of CCVD carbon nanotubes towards human umbilical vein endothelial cells. Carbon 2006;44:1093-1099. (Pubitemid 43202166)
    • (2006) Carbon , vol.44 , Issue.6 , pp. 1093-1099
    • Flahaut, E.1    Durrieu, M.C.2    Remy-Zolghadri, M.3    Bareille, R.4    Baquey, Ch.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.