3
-
-
0347673782
-
-
Marcel Dekker Inc., New York
-
W. G. Kuryla, A. J. Papa, Flame Retardancy of Polymeric Materials, Vol. 1. Marcel Dekker Inc., New York, 1973, 134.
-
(1973)
Flame Retardancy of Polymeric Materials
, vol.1
, pp. 134
-
-
Kuryla, W.G.1
Papa, A.J.2
-
4
-
-
0347043068
-
Historical aspects of polymer fire retardancy
-
Chap 7, ACS Symposium Series
-
R. B. Hindersinn, Historical aspects of polymer fire retardancy. In: Fire and Polymers, Hazards Identification and Prvention, Chap 7, ACS Symposium Series, 1989, 425.
-
(1989)
Fire and Polymers, Hazards Identification and Prvention
, pp. 425
-
-
Hindersinn, R.B.1
-
5
-
-
84869163083
-
-
J. M. Church, R. W. Little, A. Coppick, Ind. Eng. Chem. 1950, 42, 41.
-
(1950)
Ind. Eng. Chem.
, vol.42
, pp. 41
-
-
Church, J.M.1
Little, R.W.2
Coppick, A.3
-
6
-
-
0036340541
-
-
C. S. Wu, Y. L. Liu, Y. C. Chiu, Y. S. Chiu, Polym. Degrad. Stab. 2002, 78, 41.
-
(2002)
Polym. Degrad. Stab.
, vol.78
, pp. 41
-
-
Wu, C.S.1
Liu, Y.L.2
Chiu, Y.C.3
Chiu, Y.S.4
-
7
-
-
0037161891
-
-
C. S. Wu, Y. L. Liu, Y. S. Chiu, Polymer 2002, 43, 4277.
-
(2002)
Polymer
, vol.43
, pp. 4277
-
-
Wu, C.S.1
Liu, Y.L.2
Chiu, Y.S.3
-
8
-
-
0034301467
-
-
G. H. Hsiue, Y. L. Liu, J. Tsiao, J. Appl. Polym. Sci. 2000, 78, 1.
-
(2000)
J. Appl. Polym. Sci.
, vol.78
, pp. 1
-
-
Hsiue, G.H.1
Liu, Y.L.2
Tsiao, J.3
-
9
-
-
0343183941
-
-
W. J. Wang, L. H. Perng, G. H. Hsiue, F. C. Chang, Polymer 2000, 41, 6113.
-
(2000)
Polymer
, vol.41
, pp. 6113
-
-
Wang, W.J.1
Perng, L.H.2
Hsiue, G.H.3
Chang, F.C.4
-
10
-
-
0030287792
-
-
J. R. Ebdon, B. J. Hunt, M. S. Jones, F. G. Thorpe, Polym. Degrad. Stab. 1996, 54, 395.
-
(1996)
Polym. Degrad. Stab.
, vol.54
, pp. 395
-
-
Ebdon, J.R.1
Hunt, B.J.2
Jones, M.S.3
Thorpe, F.G.4
-
11
-
-
84964166171
-
-
G. C. Tesoro, S. B. Sello, J. J. Willard, Text. Res. J. 1968, 38, 245.
-
(1968)
Text. Res. J.
, vol.38
, pp. 245
-
-
Tesoro, G.C.1
Sello, S.B.2
Willard, J.J.3
-
14
-
-
0018985340
-
-
J. T. Langley, M. J. Drews, R. H. Barker, J. Appl. Polym. Sci. 1980, 25, 243.
-
(1980)
J. Appl. Polym. Sci.
, vol.25
, pp. 243
-
-
Langley, J.T.1
Drews, M.J.2
Barker, R.H.3
-
15
-
-
0018981214
-
-
S. K. Brauman, R. Swidler, P. V. Trescony, A. S. Brolly, J. Fire Retard. Chem. 1980, 7, 15.
-
(1980)
J. Fire Retard. Chem.
, vol.7
, pp. 15
-
-
Brauman, S.K.1
Swidler, R.2
Trescony, P.V.3
Brolly, A.S.4
-
17
-
-
33751249572
-
-
K. J. Calzia, A. Forcum, A. J. Lesser, J. Appl. Polym. Sci. 2006, 102, 4606.
-
(2006)
J. Appl. Polym. Sci.
, vol.102
, pp. 4606
-
-
Calzia, K.J.1
Forcum, A.2
Lesser, A.J.3
-
20
-
-
77949336670
-
-
S. Gaan, P. Rupper, V. Salimova, M. J. Heuberger, Anal. Appl. Pyrolysis 2010, 87, 93.
-
(2010)
Anal. Appl. Pyrolysis
, vol.87
, pp. 93
-
-
Gaan, S.1
Rupper, P.2
Salimova, V.3
Heuberger, M.J.4
-
21
-
-
0942300958
-
-
H. L. Lee, G. C. Chen, R. M. Rowell, J. Appl. Polym. Sci. 2004, 91, 2465.
-
(2004)
J. Appl. Polym. Sci.
, vol.91
, pp. 2465
-
-
Lee, H.L.1
Chen, G.C.2
Rowell, R.M.3
-
22
-
-
84869188550
-
-
Standard test method for flame resistance of textiles (vertical flame test), American Society for Standards and Testing, ASTM D-6413-08
-
Standard test method for flame resistance of textiles (vertical flame test), American Society for Standards and Testing, ASTM D-6413-08, 2008.
-
(2008)
-
-
-
23
-
-
84869163084
-
-
Standard test method for measuring the minimum oxygen concentration..., American Society for Standards and Testing, ASTM D-2863-09
-
Standard test method for measuring the minimum oxygen concentration..., American Society for Standards and Testing, ASTM D-2863-09, 2009.
-
(2009)
-
-
-
24
-
-
0029196914
-
-
N. D. Sachinvala, R. F. Ju, M. H. Litt, W. P. Niemczura, J. Polym. Sci. Pol. Chem. 1995, 33, 15.
-
(1995)
J. Polym. Sci. Pol. Chem.
, vol.33
, pp. 15
-
-
Sachinvala, N.D.1
Ju, R.F.2
Litt, M.H.3
Niemczura, W.P.4
-
25
-
-
84869165222
-
-
Phosphorus NMR,
-
Phosphorus NMR, http://chem.ch.huji.ac.il/nmr/techniques/1d/row3/p.html
-
-
-
-
26
-
-
76349090778
-
-
T. Ruman, K. Dlugopolska, A. Jurkiewicz, D. Kramarz, T. Fraczyk, A. Les, W. Rode, Lett. Org. Chem. 2009, 6, 642.
-
(2009)
Lett. Org. Chem.
, vol.6
, pp. 642
-
-
Ruman, T.1
Dlugopolska, K.2
Jurkiewicz, A.3
Kramarz, D.4
Fraczyk, T.5
Les, A.6
Rode, W.7
-
36
-
-
84964144442
-
-
G. C. Tesoro, S. B. Sello, J. J. Willard, Text. Res. J. 1969, 39, 180.
-
(1969)
Text. Res. J.
, vol.39
, pp. 180
-
-
Tesoro, G.C.1
Sello, S.B.2
Willard, J.J.3
-
39
-
-
42549164603
-
Chapter 10, Heat and Flame Protection
-
Eds: A. R. Horrocks, S. C. Anand), Woodhead Pub
-
P. Bajaj, Chapter 10, Heat and Flame Protection, In: Handbook of Technical Textiles, (Eds: A. R. Horrocks, S. C. Anand ), Woodhead Pub, 2000, 223.
-
(2000)
Handbook of Technical Textiles
, pp. 223
-
-
Bajaj, P.1
-
40
-
-
77953247838
-
-
Q. L. Li, X. L. Wang, D. Y. Wang, W. C. Xiong, G. H. Zhong, Y. Z. Wang, J. Appl. Polym. Sci. 2010, 117, 3066.
-
(2010)
J. Appl. Polym. Sci.
, vol.117
, pp. 3066
-
-
Li, Q.L.1
Wang, X.L.2
Wang, D.Y.3
Xiong, W.C.4
Zhong, G.H.5
Wang, Y.Z.6
-
42
-
-
84869159498
-
-
K. R. Ito, T. lodama, M. Tomizu, Y. Negoro, A. Orita, T. Osaki, N. Hosoki, T. Tanaka, T. Imanishi, S. Obika, Nucleic Acids Res., 2010, 1
-
(2010)
Nucleic Acids Res.
, pp. 1
-
-
Ito, K.R.1
Lodama, T.2
Tomizu, M.3
Negoro, Y.4
Orita, A.5
Osaki, T.6
Hosoki, N.7
Tanaka, T.8
Imanishi, T.9
Obika, S.10
-
43
-
-
0347992904
-
-
A. Mucha, J. Grembecka, T. Cierpicki, P. Kafarski, Eur. J. Org. Chem. 2003, 4797.
-
(2003)
Eur. J. Org. Chem.
, pp. 4797
-
-
Mucha, A.1
Grembecka, J.2
Cierpicki, T.3
Kafarski, P.4
-
45
-
-
67349207927
-
-
S. Gaan, P. Rupper, V. Salimova, M. Heuberger, S. Rabe, F. Vogel, Polym. Degrad. Stab. 2009, 94, 1125.
-
(2009)
Polym. Degrad. Stab.
, vol.94
, pp. 1125
-
-
Gaan, S.1
Rupper, P.2
Salimova, V.3
Heuberger, M.4
Rabe, S.5
Vogel, F.6
|