High temperature piezoelectric BiScO 3-PbTiO 3 synthesized by mechanochemical methods

Author keywords

Electroceramics; Mechanosynthesis; Perovskites; Piezoelectricity; Temperature dependence

Indexed keywords

ELECTROCERAMICS; HIGH CURIE TEMPERATURE; HIGH SENSITIVITY; HIGH TEMPERATURE; HIGH TEMPERATURE ACTUATION; MECHANOCHEMICAL EFFECTS; MECHANOCHEMICAL METHOD; MECHANOSYNTHESIS; MODEL SYSTEM; MORPHOTROPIC PHASE BOUNDARIES; NANOCRYSTALLINES; PEROVSKITE SOLID SOLUTIONS; PIEZOELECTRIC COEFFICIENT; PIEZOELECTRIC PROPERTY; PIEZOELECTRIC RESPONSE; ROOM TEMPERATURE; SYSTEMATIC STUDY; TEMPERATURE DEPENDENCE; TOLERANCE FACTOR;

EID: 83455177982     PISSN: 13596454     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.actamat.2011.10.050     Document Type: Article