Volumn 54, Issue 11, 2011, Pages 3109-3118

TiO2 nanoparticles' effects on properties of concrete using ground granulated blast furnace slag as binder

Author keywords

compressive strength; concrete; ground granulated blast furnace slag; pore structure

Indexed keywords

BLAST FURNACES; CALCIUM SILICATE; COMPRESSIVE STRENGTH; CONCRETES; HYDRATED LIME; NANOPARTICLES; OXIDE MINERALS; PARTICLE SIZE; PORE STRUCTURE; PORTLAND CEMENT; SLAGS; STRUCTURAL PROPERTIES; TITANIUM DIOXIDE;

EID: 81955160868     PISSN: 16747321     EISSN: 18691900     Source Type: Journal    
DOI: 10.1007/s11431-011-4421-1     Document Type: Article
Times cited : (42)

References (61)
  • 1
    • 0034213814 scopus 로고    scopus 로고
    • High performance cementing materials from industrial slags - A review
    • DOI 10.1016/S0921-3449(99)00060-9, PII S0921344999000609
    • C. Shi J. Qian 2000 High performance cementing materials from industrial slags: A review Resour Conserv Recycl 29 195 207 10.1016/S0921-3449(99)00060-9 (Pubitemid 30320847)
    • (2000) Resources, Conservation and Recycling , vol.29 , Issue.3 , pp. 195-207
    • Shi, C.1    Qian, J.2
  • 2
    • 49549137272 scopus 로고
    • The economic and environmental benefits of increased use of pfa and granulated slag
    • 10.1016/0301-4207(75)90030-6
    • M. A. Smith 1975 The economic and environmental benefits of increased use of pfa and granulated slag Resour Policy 1 3 154 170 10.1016/0301-4207(75) 90030-6
    • (1975) Resour Policy , vol.1 , Issue.3 , pp. 154-170
    • Smith, M.A.1
  • 4
    • 0028752116 scopus 로고
    • The effects of different cementing materials and curing on concrete scaling
    • 10.1520/CCA10291J
    • I. Afrani C. Rogers 1994 The effects of different cementing materials and curing on concrete scaling Cement Concrete Aggregates 16 132 139 10.1520/CCA10291J
    • (1994) Cement Concrete Aggregates , vol.16 , pp. 132-139
    • Afrani, I.1    Rogers, C.2
  • 5
    • 0342738768 scopus 로고
    • Properties of fresh and hardened concrete incorporating ground granulated blast furnace slag
    • V. M. Malhotra (eds). Minister of Supply and Services Canada
    • Malhotra V M. Properties of fresh and hardened concrete incorporating ground granulated blast furnace slag. In: Malhotra V M, ed. Supplementary Cementing Materials for Concrete. Canada: Minister of Supply and Services, 1987. 291-336
    • (1987) Supplementary Cementing Materials for Concrete , pp. 291-336
    • Malhotra, V.M.1
  • 6
    • 0343173188 scopus 로고
    • Some properties of alkali-activated slag cements
    • Isozaki K. Some properties of alkali-activated slag cements. CAJ Rev, 1986: 120-123
    • (1986) CAJ Rev , pp. 120-123
    • Isozaki, K.1
  • 8
    • 0026005365 scopus 로고
    • Hydration of alkali-slag cements at 150°C
    • 10.1016/0008-8846(91)90035-G
    • C. Shi X. Wu M. Tang 1991 Hydration of alkali-slag cements at 150°C Cem Concr Res 21 91 100 10.1016/0008-8846(91)90035-G
    • (1991) Cem Concr Res , vol.21 , pp. 91-100
    • Shi, C.1    Wu, X.2    Tang, M.3
  • 10
    • 0343760462 scopus 로고
    • Immobilization of radioactive wastes with Portland and alkali-slag cement pastes
    • C. Shi X. Shen X. Wu, et al. 1994 Immobilization of radioactive wastes with Portland and alkali-slag cement pastes Cemento 91 2 97 108
    • (1994) Cemento , vol.91 , Issue.2 , pp. 97-108
    • Shi, C.1    Shen, X.2    Wu, X.3
  • 12
    • 0035510888 scopus 로고    scopus 로고
    • Effect of fire and cooling mode on the properties of slag mortars
    • DOI 10.1016/S0008-8846(01)00561-0, PII S0008884601005610
    • M. M. Sohaib S. A. Ahmed M. M. Balaha 2001 Effect of fire and cooling mode on the properties of slag mortars Cem Concr Res 31 11 1533 1538 10.1016/S0008-8846(01)00561-0 (Pubitemid 33149309)
    • (2001) Cement and Concrete Research , vol.31 , Issue.11 , pp. 1533-1538
    • Shoaib, M.M.1    Ahmed, S.A.2    Balaha, M.M.3
  • 13
    • 0028257268 scopus 로고
    • Use of supplementary cementing materials to increase the resistance to chloride ion penetration of concretes cured at elevated temperatures
    • R. J. Detwiler C. A. Fapohunda J. Natale 1994 Use of supplementary cementing materials to increase the resistance to chloride ion penetration of concretes cured at elevated temperatures ACI Mater J 91 1 63 66
    • (1994) ACI Mater J , vol.91 , Issue.1 , pp. 63-66
    • Detwiler, R.J.1    Fapohunda, C.A.2    Natale, J.3
  • 14
    • 0038034121 scopus 로고    scopus 로고
    • The effect of pozzolans and slag on the expansion of mortars cured at elevated temperature: Part i expansive behaviour
    • 10.1016/S0008-8846(02)01066-9
    • T. Ramlochan P. Zacarias M. D. A. Thomas, et al. 2003 The effect of pozzolans and slag on the expansion of mortars cured at elevated temperature: Part I expansive behaviour Cem Concr Res 33 6 807 814 10.1016/S0008-8846(02) 01066-9
    • (2003) Cem Concr Res , vol.33 , Issue.6 , pp. 807-814
    • Ramlochan, T.1    Zacarias, P.2    Thomas, M.D.A.3
  • 15
    • 0036766955 scopus 로고    scopus 로고
    • Durability of ternary blend concretes with silica fume and blast furnace slag: Laboratory and outdoor exposure site studies
    • R. F. Bleszynski R. D. Hooton M. D. A. Thomas, et al. 2002 Durability of ternary blend concretes with silica fume and blast furnace slag: Laboratory and outdoor exposure site studies ACI Mater J 99 5 499 508
    • (2002) ACI Mater J , vol.99 , Issue.5 , pp. 499-508
    • Bleszynski, R.F.1    Hooton, R.D.2    Thomas, M.D.A.3
  • 16
    • 33845390846 scopus 로고    scopus 로고
    • 2 addition on properties of hardened cement paste as compared with silica fume
    • DOI 10.1016/j.conbuildmat.2005.09.001, PII S0950061805002837, Fracture, Acoustic Emission and NDE in Concrete (KIFA-4)
    • 2 addition on properties of hardened cement paste as compared with silica fume Constr Build Mat 21 539 545 10.1016/j.conbuildmat.2005.09.001 (Pubitemid 44895433)
    • (2007) Construction and Building Materials , vol.21 , Issue.3 , pp. 539-545
    • Qing, Y.1    Zenan, Z.2    Deyu, K.3    Rongshen, C.4
  • 18
    • 78049527171 scopus 로고    scopus 로고
    • 2 nanoparticles
    • 10.1007/BF02823370
    • 2 nanoparticles KSCE J 11 1 37 42 10.1007/BF02823370
    • (2007) KSCE J , vol.11 , Issue.1 , pp. 37-42
    • Jo, B.W.1    Kim, C.H.2    Lim, J.H.3
  • 22
    • 33645150832 scopus 로고    scopus 로고
    • Effect of nanosilica on characteriza tion of Portland cement composite
    • 10.1016/j.cemconres.2005.11.006
    • J. Y. Shih T. P. Chang T. C. Hsiao 2006 Effect of nanosilica on characteriza tion of Portland cement composite Cem Con Res 36 697 706 10.1016/j.cemconres.2005.11.006
    • (2006) Cem Con Res , vol.36 , pp. 697-706
    • Shih, J.Y.1    Chang, T.P.2    Hsiao, T.C.3
  • 23
    • 33847788101 scopus 로고    scopus 로고
    • Improvement of initial mechanical strength by nanoalumina in belite cements
    • DOI 10.1016/j.matlet.2006.07.150, PII S0167577X06009694
    • I. Campillo A. Guerrero J. S. Dolado, et al. 2007 Improvement of initial mechanical strength by nanoalumina in belite cements Mater Lett 61 1889 1892 10.1016/j.matlet.2006.07.150 (Pubitemid 46389530)
    • (2007) Materials Letters , vol.61 , Issue.8-9 , pp. 1889-1892
    • Campillo, I.1    Guerrero, A.2    Dolado, J.S.3    Porro, A.4    Ibanez, J.A.5    Goni, S.6
  • 24
    • 27844577681 scopus 로고    scopus 로고
    • Investigations on the preparation and mechanical properties of the nano-alumina reinforced cement composite
    • DOI 10.1016/j.matlet.2005.08.061, PII S0167577X05008463
    • Z. Li H. Wang S. He, et al. 2006 Investigations on the preparation and mechanical properties of the nano-alumina reinforced cement composite Mater Lett 60 356 359 10.1016/j.matlet.2005.08.061 (Pubitemid 41654581)
    • (2006) Materials Letters , vol.60 , Issue.3 , pp. 356-359
    • Li, Z.1    Wang, H.2    He, S.3    Lu, Y.4    Wang, M.5
  • 25
    • 1542475838 scopus 로고    scopus 로고
    • A study on mechanical and pressure-sensitive properties of cement mortar with nanophase materials
    • 10.1016/j.cemconres.2003.08.025
    • H. Li H. Xiao J. Ou 2004 A study on mechanical and pressure-sensitive properties of cement mortar with nanophase materials Cem Con Res 34 435 438 10.1016/j.cemconres.2003.08.025
    • (2004) Cem Con Res , vol.34 , pp. 435-438
    • Li, H.1    Xiao, H.2    Ou, J.3
  • 26
    • 0036501942 scopus 로고    scopus 로고
    • Characterization and properties of portland cement composites incorporating zinc-iron oxide nanoparticles
    • DOI 10.1023/A:1014304131987
    • L. M. Flores-Velez O. Dominguez 2002 Characterization and properties of Portland cement composites incorporating zinc-iron oxide nanoparticles J Mater Sci 37 983 988 10.1023/A:1014304131987 (Pubitemid 34269082)
    • (2002) Journal of Materials Science , vol.37 , Issue.5 , pp. 983-988
    • Flores-Velez, L.Ma.1    Dominguez, O.2
  • 27
    • 77957664111 scopus 로고    scopus 로고
    • 2 nanoparticles
    • 10.1016/j.msea.2010.08.095
    • 2 nanoparticles Mater Sci Eng A 527 7663 7672 10.1016/j.msea.2010.08.095
    • (2010) Mater Sci Eng A , vol.527 , pp. 7663-7672
    • Nazari, A.1    Riahi, S.2
  • 28
    • 80051593245 scopus 로고    scopus 로고
    • 2 nanoparticles on flexural damage of self-compacting concrete
    • doi: 10.1177/1056789510385262
    • 2 nanoparticles on flexural damage of self-compacting concrete. Int J Damage Mech, 2010, doi: 10.1177/1056789510385262
    • (2010) Int J Damage Mech
    • Nazari, A.1    Riahi, S.2
  • 29
    • 78049529122 scopus 로고    scopus 로고
    • 2 nanoparticles on water permeability and thermal and mechanical properties of high strength self-compacting concrete
    • 10.1016/j.msea.2010.09.074
    • 2 nanoparticles on water permeability and thermal and mechanical properties of high strength self-compacting concrete Mater Sci Eng A 528 2 756 763 10.1016/j.msea.2010.09. 074
    • (2010) Mater Sci Eng A , vol.528 , Issue.2 , pp. 756-763
    • Nazari, A.1    Riahi, S.2
  • 30
    • 79955816719 scopus 로고    scopus 로고
    • 2 nanoparticles
    • doi: 10.1617/s11527-010-9664-y
    • 2 nanoparticles. Mater Struct, 2010, doi: 10.1617/s11527-010-9664-y
    • (2010) Mater Struct
    • Nazari, A.1
  • 31
    • 78651419158 scopus 로고    scopus 로고
    • The effects of zinc dioxide nanoparticles on flexural strength of self-compacting concrete
    • 10.1016/j.compositesb.2010.09.001
    • A. Nazari S. Riahi 2011 The effects of zinc dioxide nanoparticles on flexural strength of self-compacting concrete Compos Part B-Eng 42 2 167 175 10.1016/j.compositesb.2010.09.001
    • (2011) Compos Part B-Eng , vol.42 , Issue.2 , pp. 167-175
    • Nazari, A.1    Riahi, S.2
  • 32
    • 84867246296 scopus 로고    scopus 로고
    • 2 nanoparticles on split tensile strength of self-compacting concrete
    • doi: 10.1080/17458080.2010.524669
    • 2 nanoparticles on split tensile strength of self-compacting concrete. J Exp Nanosc, 2010, doi: 10.1080/17458080.2010.524669
    • (2010) J Exp Nanosc
    • Nazari, A.1    Riahi, S.2
  • 33
    • 79953655921 scopus 로고    scopus 로고
    • 2 nanoparticle blended cementitious composite
    • doi: 10.1177/0021998310376118
    • 2 nanoparticle blended cementitious composite. J Compos Mater, 2010, doi: 10.1177/0021998310376118
    • (2010) J Compos Mater
    • Nazari, A.1    Riahi, S.2
  • 34
    • 79955025467 scopus 로고    scopus 로고
    • 3 nanoparticles on water permeability, workability, and setting time of concrete
    • doi: 10.1177/0021998310377945
    • 3 nanoparticles on water permeability, workability, and setting time of concrete. J Compos Mater, 2010, doi: 10.1177/0021998310377945
    • (2010) J Compos Mater
    • Nazari, A.1    Riahi, S.2
  • 35
    • 79957584407 scopus 로고    scopus 로고
    • 3 nanoparticles binary blended concrete
    • doi: 10.1177/0021998310378907
    • 3 nanoparticles binary blended concrete. J Compos Mater, 2010, doi: 10.1177/0021998310378907
    • (2010) J Compos Mater
    • Nazari, A.1    Riahi, S.2
  • 36
    • 79955112331 scopus 로고    scopus 로고
    • 3 nanoparticles binary blended concrete
    • doi: 10.1177/0021998310378909
    • 3 nanoparticles binary blended concrete. J Compos Mater, 2010, doi: 10.1177/0021998310378909
    • (2010) J Compos Mater
    • Nazari, A.1    Riahi, S.2
  • 37
    • 79957585028 scopus 로고    scopus 로고
    • 2 nanoparticles on properties of binary blended concrete
    • doi: 10.1177/0021998310378910
    • 2 nanoparticles on properties of binary blended concrete. J Compos Mater, 2010, doi: 10.1177/0021998310378910
    • (2010) J Compos Mater
    • Nazari, A.1    Riahi, S.2
  • 38
    • 79954993424 scopus 로고    scopus 로고
    • Optimization mechanical properties of Cr2O3 nanoparticle binary blended cementitious composite
    • doi: 10.1177/0021998310377944
    • Nazari A, Riahi S. Optimization mechanical properties of Cr2O3 nanoparticle binary blended cementitious composite. J Compos Mater, 2010, doi: 10.1177/0021998310377944
    • (2010) J Compos Mater
    • Nazari, A.1    Riahi, S.2
  • 39
    • 33947251789 scopus 로고    scopus 로고
    • Flexural fatigue performance of concrete containing nano-particles for pavement
    • DOI 10.1016/j.ijfatigue.2006.10.004, PII S0142112306002994
    • H. Li M. H. Zhang J. P. Ou 2007 Flexural fatigue performance of concrete containing nano-nanoparticles for pavement Int J Fatigue 29 1292 1301 10.1016/j.ijfatigue.2006.10.004 (Pubitemid 46435717)
    • (2007) International Journal of Fatigue , vol.29 , Issue.7 , pp. 1292-1301
    • Li, H.1    Zhang, M.-h.2    Ou, J.-p.3
  • 40
    • 33646756595 scopus 로고    scopus 로고
    • Abrasion resistance of concrete containing nano-particles for pavement
    • DOI 10.1016/j.wear.2005.08.006, PII S0043164805004308
    • H. Li M. H. Zhang J. P. Ou 2006 Abrasion resistance of concrete containing nano-nanoparticles for pavement Wear 260 1262 1266 10.1016/j.wear.2005.08.006 (Pubitemid 43765990)
    • (2006) Wear , vol.260 , Issue.11-12 , pp. 1262-1266
    • Li, H.1    Zhang, M.-h.2    Ou, J.-p.3
  • 42
    • 0004077698 scopus 로고    scopus 로고
    • ASTM C150, Standard Specification for Portland Cement. ASTM Philadelphia, PA
    • ASTM C150, Standard Specification for Portland Cement, Annual Book of ASTM Standards. Philadelphia, PA: ASTM, 2001
    • (2001) Annual Book of ASTM Standards
  • 44
    • 0033102546 scopus 로고    scopus 로고
    • Mercury intrusion porosimetry and image analysis of cement-based materials
    • DOI 10.1006/jcis.1998.5986
    • A. B. Abell K. L. Willis D. A. Lange 1999 Mercury intrusion porosimetry and image nalysis of cement-based materials J Colloid Interface Sci 211 39 44 10.1006/jcis.1998.5986 (Pubitemid 29394455)
    • (1999) Journal of Colloid and Interface Science , vol.211 , Issue.1 , pp. 39-44
    • Abell, A.B.1    Willis, K.L.2    Lange, D.A.3
  • 45
    • 0036722027 scopus 로고    scopus 로고
    • Development of technique for observing pores in hardened cement paste
    • DOI 10.1016/S0008-8846(02)00806-2, PII S0008884602008062
    • K. Tanaka K. Kurumisawa 2002 Development of technique for observing pores in hardened cement paste Cem Con Res 32 1435 1441 10.1016/S0008-8846(02)00806-2 (Pubitemid 34802439)
    • (2002) Cement and Concrete Research , vol.32 , Issue.9 , pp. 1435-1441
    • Tanaka, K.1    Kurumisawa, K.2
  • 46
    • 77957688086 scopus 로고    scopus 로고
    • Influencia de los superplastificantes en la microestructura de la pasta hidratada y en el comportamiento diferido de los morteros de cemento
    • J. Roncero R. Gettu 2002 Influencia de los superplastificantes en la microestructura de la pasta hidratada y en el comportamiento diferido de los morteros de cemento Cemento Hormigón 832 12 28
    • (2002) Cemento Hormigón , vol.832 , pp. 12-28
    • Roncero, J.1    Gettu, R.2
  • 51
    • 31044437327 scopus 로고    scopus 로고
    • The influence of fillers on the properties of self-compacting concrete in fresh and hardened state
    • RILEM Publications S.A.R.L.; Reykjavik
    • Heirman G, Vandewalle L. The influence of fillers on the properties of self-compacting concrete in fresh and hardened state. Proceedings of the 3rd International RILEM Symposium on Self-Compacting Concrete. RILEM Publications S.A.R.L.; Reykjavik, 2003. 606-618
    • (2003) Proceedings of the 3rd International RILEM Symposium on Self-Compacting Concrete , pp. 606-618
    • Heirman, G.1    Vandewalle, L.2
  • 52
    • 33845668450 scopus 로고    scopus 로고
    • Influence of limestone powder used as filler in SCC on hydration and microstructure of cement pastes
    • DOI 10.1016/j.cemconcomp.2006.09.003, PII S0958946506001685
    • G. Ye X. Xiu G. De Schutter, et al. 2007 Influence of limestone powder as filler in SCC on hydration and microstructure of cement pastes Cem Con Compos 29 2 94 102 10.1016/j.cemconcomp.2006.09.003 (Pubitemid 44960814)
    • (2007) Cement and Concrete Composites , vol.29 , Issue.2 , pp. 94-102
    • Ye, G.1    Liu, X.2    De Schutter, G.3    Poppe, A.-M.4    Taerwe, L.5
  • 53
    • 0029308636 scopus 로고
    • Effect of cement type on chloride binding and corrosion of steel in concrete
    • 10.1016/0008-8846(95)00080-V
    • C. Arya Y. Xu 1995 Effect of cement type on chloride binding and corrosion of steel in concrete Cem Concr Res 25 4 893 902 10.1016/0008-8846(95) 00080-V
    • (1995) Cem Concr Res , vol.25 , Issue.4 , pp. 893-902
    • Arya, C.1    Xu, Y.2
  • 54
    • 33644894187 scopus 로고    scopus 로고
    • Durability of marine concrete structures-field investigations and modeling
    • R. B. Polder de Rooij 2005 Durability of marine concrete structures-field investigations and modeling Heron 50 3 133 153
    • (2005) Heron , vol.50 , Issue.3 , pp. 133-153
    • Polder, R.B.1    De Rooij2
  • 55
    • 0033928641 scopus 로고    scopus 로고
    • Corrosion inhibition in concrete arising from its acid neutralisation capacity
    • DOI 10.1016/S0010-938X(00)00008-1, PII S0010938X00000081
    • G. K. Glass B. Reddy N. R. Buenfeld 2000 Corrosion inhibition in concrete arising from its acid neutralization capacity Corros Sci 42 1587 1598 10.1016/S0010-938X(00)00008-1 (Pubitemid 30480621)
    • (2000) Corrosion Science , vol.42 , Issue.9 , pp. 1587-1598
    • Glass, G.K.1    Reddy, B.2    Buenfeld, N.R.3
  • 56
    • 0036778764 scopus 로고    scopus 로고
    • Monitoring electrical resistance of concretes containing alternative cementitious materials to assess their resistance to chloride penetration
    • DOI 10.1016/S0958-9465(01)00075-0, PII S0958946501000750
    • P. A. M. Basheer P. R. V. Gilleece A. E. Long, et al. 2002 Monitoring electrical resistance of concretes containing alternative cementitious materials to assess their resistance to chloride penetration Cem Concr Compos 24 437 449 10.1016/S0958-9465(01)00075-0 (Pubitemid 34802155)
    • (2002) Cement and Concrete Composites , vol.24 , Issue.5 , pp. 437-449
    • Basheer, P.A.M.1    Gilleece, P.R.V.2    Long, A.E.3    Mc Carter, W.J.4
  • 57
    • 19344372366 scopus 로고    scopus 로고
    • Polycarboxylate superplasticiser admixtures: Effect on hydration, microstructure and rheological behaviour in cement pastes
    • DOI 10.1680/adcr.17.2.77.65044
    • F. Puertas H. Santos M. Palacios, et al. 2005 Polycarboxylate superplasticiser admixtures: Effect on hydration, microstructure and rheological behavior Adv Cem Res 17 2 77 89 10.1680/adcr.2005.17.2.77 (Pubitemid 40718153)
    • (2005) Advances in Cement Research , vol.17 , Issue.2 , pp. 77-89
    • Puertas, F.1    Santos, H.2    Palacios, M.3    Martinez-Ramirez, S.4
  • 59
    • 0345058229 scopus 로고
    • Miscibility of special elements in tricalcium silicate and alite and the hydration properties of C3S solid solutions
    • Tokyo
    • Kondo R, Yoshida K. Miscibility of special elements in tricalcium silicate and alite and the hydration properties of C3S solid solutions. 5th Int Symp on the Chem of Cement, Tokyo, I-262. 1968
    • (1968) 5th Int Symp on the Chem of Cement
    • Kondo, R.1    Yoshida, K.2
  • 60
    • 0345058237 scopus 로고
    • Addition of titanium dioxide to Portland cement clinkers
    • Teoreanu I, Muntean M, Balusoiu H. Addition of titanium dioxide to Portland cement clinkers. Il Cemento, 1987. 497-404
    • (1987) Il Cemento , pp. 497-404
    • Teoreanu, I.1    Muntean, M.2    Balusoiu, H.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.