Volumn 17, Issue 2, 2004, Pages 142-149

Strength, reliability, and mode of fracture of bilayered porcelain/core ceramics

Author keywords

[No Author keywords available]

Indexed keywords

ANALYSIS OF VARIANCE; ARTICLE; CERAMIC PROSTHESIS; COMPARATIVE STUDY; DATA ANALYSIS; EVALUATION; RELIABILITY; SCANNING ELECTRON MICROSCOPY; STATISTICAL ANALYSIS; STRENGTH; STRESS; TENSILE STRENGTH; TENSION; TOOTH FRACTURE; TOOTH PROSTHESIS;

EID: 1842850520     PISSN: 08932174     EISSN: None     Source Type: Journal    
DOI: None     Document Type: Article
Times cited : (69)

References (23)
  • 1
    • 0035348103 scopus 로고    scopus 로고
    • Flexural strength of Cerec 2 machined and jointed In-Ceram Alumina and In-Ceram Zirconia bars
    • Apholt W, Bindl A, Lüthy H, Mörmann WH. Flexural strength of Cerec 2 machined and jointed In-Ceram Alumina and In-Ceram Zirconia bars. Dent Mater 2001;17:260-267.
    • (2001) Dent Mater , vol.17 , pp. 260-267
    • Apholt, W.1    Bindl, A.2    Lüthy, H.3    Mörmann, W.H.4
  • 2
    • 0036518474 scopus 로고    scopus 로고
    • Flexural strength of In-Ceram Alumina and In-Ceram Zirconia core materials
    • Chong KH, Chai J, Takahashi Y, Wozniak WT. Flexural strength of In-Ceram Alumina and In-Ceram Zirconia core materials. Int J Prosthodont 2002;15:183-188.
    • (2002) Int J Prosthodont , vol.15 , pp. 183-188
    • Chong, K.H.1    Chai, J.2    Takahashi, Y.3    Wozniak, W.T.4
  • 3
    • 0036636830 scopus 로고    scopus 로고
    • The mechanical properties of In-Ceram Alumina and In-Ceram Zirconia
    • Guazzato M, Albakry M, Swain MV, Ironside JV. The mechanical properties of In-Ceram Alumina and In-Ceram Zirconia. Int J Prosthodont 2002;15:339-346.
    • (2002) Int J Prosthodont , vol.15 , pp. 339-346
    • Guazzato, M.1    Albakry, M.2    Swain, M.V.3    Ironside, J.V.4
  • 4
    • 1842732685 scopus 로고    scopus 로고
    • Strength, fracture toughness and microstructure of a selection of all-ceramic materials: Part I, pressable and alumina glass-infiltrated
    • forthcoming
    • Guazzato M, Albakry M, Swain MV, Ringer PS. Strength, fracture toughness and microstructure of a selection of all-ceramic materials: Part I, pressable and alumina glass-infiltrated. Dent Mater (forthcoming).
    • Dent Mater
    • Guazzato, M.1    Albakry, M.2    Swain, M.V.3    Ringer, P.S.4
  • 5
    • 0035512807 scopus 로고    scopus 로고
    • Use of contact testing in the characterization and design of all-ceramic crownlike layer structures: A review
    • Lawn BR, Deng Y, Thompson VP. Use of contact testing in the characterization and design of all-ceramic crownlike layer structures: A review. J Prosthet Dent 2001;86:495-510.
    • (2001) J Prosthet Dent , vol.86 , pp. 495-510
    • Lawn, B.R.1    Deng, Y.2    Thompson, V.P.3
  • 6
    • 0029318343 scopus 로고
    • Failure of all-ceramic fixed partial dentures in vitro and in vivo: Analysis and modeling
    • Kelly JR, Tesk JA, Sorensen JA. Failure of all-ceramic fixed partial dentures in vitro and in vivo: analysis and modeling. J Dent Res 1995;74:1253-1258.
    • (1995) J Dent Res , vol.74 , pp. 1253-1258
    • Kelly, J.R.1    Tesk, J.A.2    Sorensen, J.A.3
  • 9
    • 0032018019 scopus 로고    scopus 로고
    • Evaluation of mechanical properties of dental ceramic core materials in combination with porcelain
    • Zeng K, Odén A, Rowcliffe D. Evaluation of mechanical properties of dental ceramic core materials in combination with porcelain. Int J Prosthodont 1998;11:183-189.
    • (1998) Int J Prosthodont , vol.11 , pp. 183-189
    • Zeng, K.1    Odén, A.2    Rowcliffe, D.3
  • 10
    • 0034230609 scopus 로고    scopus 로고
    • Influence of relative layer height and testing method on the failure mode and origin in a bilayered dental ceramic composite
    • Thompson GA. Influence of relative layer height and testing method on the failure mode and origin in a bilayered dental ceramic composite. Dent Mater 2000;16:235-243.
    • (2000) Dent Mater , vol.16 , pp. 235-243
    • Thompson, G.A.1
  • 11
    • 0034441675 scopus 로고    scopus 로고
    • Crack initiation modes in bilayered alumina/porcelain disks as a function of core/veneer thickness ratio and supporting substrate stiffness
    • Wakabayashi N, Anusavice KJ. Crack initiation modes in bilayered alumina/porcelain disks as a function of core/veneer thickness ratio and supporting substrate stiffness. J Dent Res 2000;79:1398-1404.
    • (2000) J Dent Res , vol.79 , pp. 1398-1404
    • Wakabayashi, N.1    Anusavice, K.J.2
  • 12
    • 0035653377 scopus 로고    scopus 로고
    • Validation of finite element analysis in dental ceramics research
    • Lang LA, Wang RF, Kang B, White SN. Validation of finite element analysis in dental ceramics research. J Prosthet Dent 2001;86:650-654.
    • (2001) J Prosthet Dent , vol.86 , pp. 650-654
    • Lang, L.A.1    Wang, R.F.2    Kang, B.3    White, S.N.4
  • 14
    • 0036634261 scopus 로고    scopus 로고
    • Finite element analysis studies of an all-ceramic crown on a first premolar tooth
    • Proos KA, Swain MV, Ironside JV, Steven G. Finite element analysis studies of an all-ceramic crown on a first premolar tooth. Int J Prosthodont 2002;15:404-412.
    • (2002) Int J Prosthodont , vol.15 , pp. 404-412
    • Proos, K.A.1    Swain, M.V.2    Ironside, J.V.3    Steven, G.4
  • 15
    • 0026891764 scopus 로고
    • Tensile stress in glass-ceramic crowns: Effect of flaws and cement voids
    • Anusavice KJ, Hojjatie B. Tensile stress in glass-ceramic crowns: Effect of flaws and cement voids. Int J Prosthodont 1992;5:351-358.
    • (1992) Int J Prosthodont , vol.5 , pp. 351-358
    • Anusavice, K.J.1    Hojjatie, B.2
  • 16
    • 1942508734 scopus 로고
    • ASTM Designation D4065-82. Standard test method for dynamic Young's modulus, shear modulus, and Poisson's ratio for advanced ceramics by impulse excitation of vibration
    • Philadelphia: ASTM
    • American Society for Testing and Materials. ASTM Designation D4065-82. Standard test method for dynamic Young's modulus, shear modulus, and Poisson's ratio for advanced ceramics by impulse excitation of vibration. In: Annual Book of ASTM Standards 15.02. Philadelphia: ASTM, 1994.
    • (1994) Annual Book of ASTM Standards 15.02
  • 17
    • 1842867407 scopus 로고    scopus 로고
    • Sydney: G+D Computing
    • G+D Computing. Using Strand7. Sydney: G+D Computing, 1999:1-220.
    • (1999) Using Strand7 , pp. 1-220
  • 19
    • 0018057730 scopus 로고
    • Fractographic analysis of ceramics
    • Strauss BM, Cullen WH (eds). Philadelphia: ASTM
    • Mecholsky JJ, Freiman SW, Rice RW. Fractographic analysis of ceramics. In: Strauss BM, Cullen WH (eds). Fractography in Failure Analysis. Philadelphia: ASTM, 1978:363-379.
    • (1978) Fractography in Failure Analysis , pp. 363-379
    • Mecholsky, J.J.1    Freiman, S.W.2    Rice, R.W.3
  • 20
    • 0025492382 scopus 로고
    • Fracture surface analysis of dental ceramics: Clinically failed restorations
    • Kelly JR, Giordano R, Pober R, Cima MJ. Fracture surface analysis of dental ceramics: Clinically failed restorations. Int J Prosthodont 1990;3:430-440.
    • (1990) Int J Prosthodont , vol.3 , pp. 430-440
    • Kelly, J.R.1    Giordano, R.2    Pober, R.3    Cima, M.J.4
  • 21
    • 0033228179 scopus 로고    scopus 로고
    • The influence of clinically induced variability on the bi-axial fracture strength of aluminous core porcelain discs
    • Fleming GJP, Shelton RM, Marquis PM. The influence of clinically induced variability on the bi-axial fracture strength of aluminous core porcelain discs. J Dent 1999;27:587-594.
    • (1999) J Dent , vol.27 , pp. 587-594
    • Fleming, G.J.P.1    Shelton, R.M.2    Marquis, P.M.3
  • 23
    • 0025617576 scopus 로고
    • Influence of test method on failure stress of brittle dental materials
    • Ban S, Anusavice KJ. Influence of test method on failure stress of brittle dental materials. J Dent Res 1990;69:1791-1799.
    • (1990) J Dent Res , vol.69 , pp. 1791-1799
    • Ban, S.1    Anusavice, K.J.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.