Use of pre-oxidation to improve reactive wetting of high manganese alloyed steel during hot-dip galvanizing

Author keywords

High Mn alloyed steel; Hot dip galvanizing; Pre oxidation; Reactive Zn wetting; Selective oxidation; TWIP steel

Indexed keywords

ALLOYED STEELS; HOT-DIP GALVANIZING; PRE-OXIDATION; REACTIVE ZN WETTING; SELECTIVE OXIDATION; TWIP STEEL;

EID: 80052381727     PISSN: 02578972     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.surfcoat.2011.07.088     Document Type: Article
Times cited : (54)

References (46)
  • 11
    • 80052367947 scopus 로고    scopus 로고
    • Ph.D. Thesis, RWTH Aachen.
    • R. Leuschner, Ph.D. Thesis, RWTH Aachen, 2007.
    • (2007)
    • Leuschner, R.1
  • 20
    • 80052363349 scopus 로고    scopus 로고
    • Patent Application WO 0 2008 022 980 A3.
    • M. Meurer, R. Leuschner, H. Hofmann, Patent Application WO 0 2008 022 980 A3, 2008.
    • (2008)
    • Meurer, M.1    Leuschner, R.2    Hofmann, H.3
  • 24
    • 80052369226 scopus 로고    scopus 로고
    • Ph.D. Thesis, RWTH Aachen.
    • M. Norden, Ph.D. Thesis, RWTH Aachen, 2010.
    • (2010)
    • Norden, M.1
  • 33
    • 80052382012 scopus 로고    scopus 로고
    • Ph.D. Thesis, Freie Universität Berlin.
    • Y. Joseph, Ph.D. Thesis, Freie Universität Berlin, 2001.
    • (2001)
    • Joseph, Y.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.