Toughening of laminated ZrB2-SiC ceramics with residual surface compression

Author keywords

C. Fracture; C. Toughness and toughening; D. Borides; Laminated structure

Indexed keywords

C. FRACTURE; C. TOUGHNESS AND TOUGHENING; COMPRESSIVE LAYERS; CRACK DEFLECTIONS; D. BORIDES; FRACTURE LOAD; GEOMETRICAL PARAMETERS; LAMINATED CERAMICS; LAMINATED STRUCTURE; RESIDUAL COMPRESSIVE STRESS; SIC CERAMICS; STACKING LAYERS; SURFACE COMPRESSION; TENSILE LAYER; THEORETICAL CALCULATIONS; THEORETICAL PREDICTION; TOUGHENING EFFECTS;

EID: 79960388545     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2011.05.024     Document Type: Article
Times cited : (51)

References (38)
  • 2
    • 0033323434 scopus 로고    scopus 로고
    • Mechanical, thermal, and oxidation properties of refractory hafnium and zirconium compounds
    • Opeka M.M., Talmy I.G., Wuchina E.J., Zaykoski J.A., Causey S.J. Mechanical, thermal, and oxidation properties of refractory hafnium and zirconium compounds. J Eur Ceram Soc 1999, 19:2405-2414.
    • (1999) J Eur Ceram Soc , vol.19 , pp. 2405-2414
    • Opeka, M.M.1    Talmy, I.G.2    Wuchina, E.J.3    Zaykoski, J.A.4    Causey, S.J.5
  • 4
    • 57849135454 scopus 로고    scopus 로고
    • Microstructure and properties of silicon carbide whisker reinforced zirconium diboride ultra-high temperature ceramics
    • Zhang X.H., Xu L., Han W.B., Weng L., Han J.C., Du S.Y. Microstructure and properties of silicon carbide whisker reinforced zirconium diboride ultra-high temperature ceramics. Solid State Sci 2009, 11:156-161.
    • (2009) Solid State Sci , vol.11 , pp. 156-161
    • Zhang, X.H.1    Xu, L.2    Han, W.B.3    Weng, L.4    Han, J.C.5    Du, S.Y.6
  • 11
    • 36848998806 scopus 로고    scopus 로고
    • 2-SiC composite fabricated by the spark plasma sintering-reactive synthesis (SPS-RS) method
    • 2-SiC composite fabricated by the spark plasma sintering-reactive synthesis (SPS-RS) method. J Am Ceram Soc 2007, 90(12):4040-4042.
    • (2007) J Am Ceram Soc , vol.90 , Issue.12 , pp. 4040-4042
    • Zhao, Y.1    Wang, L.J.2    Zhang, G.J.3    Jiang, W.4    Chen, L.D.5
  • 12
    • 33646708519 scopus 로고    scopus 로고
    • Pressureless densification of zirconium diboride with boron carbide additions
    • Zhang S.C., Hilmas G.E., Fahrenholtz W.G. Pressureless densification of zirconium diboride with boron carbide additions. J Am Ceram Soc 2006, 89:1544-1550.
    • (2006) J Am Ceram Soc , vol.89 , pp. 1544-1550
    • Zhang, S.C.1    Hilmas, G.E.2    Fahrenholtz, W.G.3
  • 16
    • 0031197453 scopus 로고    scopus 로고
    • Microstructure and high-temperature mechanical behavior of alumina/alumina-yttria-stabilized tetragonal zirconia multilayer composites
    • Jiménez-Melendo M., Clauss C., Domĺnguez-Rodrĺguez A., Sánchez-Herencia A.J., Moya J.S. Microstructure and high-temperature mechanical behavior of alumina/alumina-yttria-stabilized tetragonal zirconia multilayer composites. J Am Ceram Soc 1997, 80(8):2126-2130.
    • (1997) J Am Ceram Soc , vol.80 , Issue.8 , pp. 2126-2130
    • Jiménez-Melendo, M.1    Clauss, C.2    Domĺnguez-Rodrĺguez, A.3    Sánchez-Herencia, A.J.4    Moya, J.S.5
  • 17
    • 33747350290 scopus 로고    scopus 로고
    • Fabrication and residual stresses characterization of novel non-oxide multilayer ceramics
    • Sciti D., Nagliati M., Tochino S., Pezzotti G., Guicciardi S. Fabrication and residual stresses characterization of novel non-oxide multilayer ceramics. J Eur Ceram Soc 2006, 26:3415-3423.
    • (2006) J Eur Ceram Soc , vol.26 , pp. 3415-3423
    • Sciti, D.1    Nagliati, M.2    Tochino, S.3    Pezzotti, G.4    Guicciardi, S.5
  • 18
    • 0029753871 scopus 로고    scopus 로고
    • Toughing of layered ceramic composites with residual surface compression
    • Lakshminarayanan R., Shetty D.K., Cutler R.A. Toughing of layered ceramic composites with residual surface compression. J Am Ceram Soc 1996, 79(1):79-87.
    • (1996) J Am Ceram Soc , vol.79 , Issue.1 , pp. 79-87
    • Lakshminarayanan, R.1    Shetty, D.K.2    Cutler, R.A.3
  • 19
    • 33646841691 scopus 로고    scopus 로고
    • Laminated ceramic structures from oxide systems
    • Portu G., Micele L., Pezzotti G. Laminated ceramic structures from oxide systems. Composites: Part B 2006, 37:556-567.
    • (2006) Composites: Part B , vol.37 , pp. 556-567
    • Portu, G.1    Micele, L.2    Pezzotti, G.3
  • 20
    • 33751010735 scopus 로고    scopus 로고
    • Layered materials with high strength and flaw tolerance based on alumina and aluminium titanate
    • Bueno S., Baudĺn C. Layered materials with high strength and flaw tolerance based on alumina and aluminium titanate. J Eur Cer Soc 2007, 27:1455-1462.
    • (2007) J Eur Cer Soc , vol.27 , pp. 1455-1462
    • Bueno, S.1    Baudĺn, C.2
  • 21
    • 0033905282 scopus 로고    scopus 로고
    • Fracture behaviour of alumina/monazite multilayer laminates
    • Mawdsley J.R., Kovar D., Halloran J.W. Fracture behaviour of alumina/monazite multilayer laminates. J Am Ceram Soc 2000, 83(4):802-808.
    • (2000) J Am Ceram Soc , vol.83 , Issue.4 , pp. 802-808
    • Mawdsley, J.R.1    Kovar, D.2    Halloran, J.W.3
  • 22
    • 0034209713 scopus 로고    scopus 로고
    • Biomimetic structure design-a possible approach to change the brittleness of ceramics in nature
    • Wang C.A., Huang Y., Zan Q.F., Guo H., Cai S.Y. Biomimetic structure design-a possible approach to change the brittleness of ceramics in nature. Mater Sci Eng C 2000, 11:9-12.
    • (2000) Mater Sci Eng C , vol.11 , pp. 9-12
    • Wang, C.A.1    Huang, Y.2    Zan, Q.F.3    Guo, H.4    Cai, S.Y.5
  • 25
    • 79960413485 scopus 로고    scopus 로고
    • Design and production of ceramic laminates with high mechanical resistance and reliability
    • Sglavo V.M., Bertoldi M. Design and production of ceramic laminates with high mechanical resistance and reliability. Acta Mater 2006, 544:929-937.
    • (2006) Acta Mater , vol.544 , pp. 929-937
    • Sglavo, V.M.1    Bertoldi, M.2
  • 26
    • 33748974829 scopus 로고    scopus 로고
    • Residual stresses, strength and toughness of laminates with different layer thickness ratios
    • Bermejo R., Torres Y., Sanchez-Herencia A.J., Baudín C., Anglada M., Llanes L. Residual stresses, strength and toughness of laminates with different layer thickness ratios. Acta Mater 2006, 54:4745-4757.
    • (2006) Acta Mater , vol.54 , pp. 4745-4757
    • Bermejo, R.1    Torres, Y.2    Sanchez-Herencia, A.J.3    Baudín, C.4    Anglada, M.5    Llanes, L.6
  • 27
    • 35448972439 scopus 로고    scopus 로고
    • Potential of SiC multilayer ceramics for high temperature applications in oxidising environment
    • Pavese M., Fino P., Ortona A., Badini C. Potential of SiC multilayer ceramics for high temperature applications in oxidising environment. Ceram Int 2008, 34:197-203.
    • (2008) Ceram Int , vol.34 , pp. 197-203
    • Pavese, M.1    Fino, P.2    Ortona, A.3    Badini, C.4
  • 28
    • 27644560090 scopus 로고    scopus 로고
    • Tailored residual stresses in high reliability alumina-mullite ceramic laminates
    • Sglavo V.M., Paternoster M., Bertoldi M. Tailored residual stresses in high reliability alumina-mullite ceramic laminates. J Am Ceram Soc 2005, 88(10):2826-2832.
    • (2005) J Am Ceram Soc , vol.88 , Issue.10 , pp. 2826-2832
    • Sglavo, V.M.1    Paternoster, M.2    Bertoldi, M.3
  • 31
    • 0029376584 scopus 로고
    • Surface cracking in layers under biaxial residual compressive stress
    • Ho S., Hillman C., Lange F.F., Suo Z. Surface cracking in layers under biaxial residual compressive stress. J Am Ceram Soc 1995, 78(9):2353-2357.
    • (1995) J Am Ceram Soc , vol.78 , Issue.9 , pp. 2353-2357
    • Ho, S.1    Hillman, C.2    Lange, F.F.3    Suo, Z.4
  • 34
    • 0014852532 scopus 로고
    • A novel principle for the computation of stress intensity factors
    • Bueckner H.F. A novel principle for the computation of stress intensity factors. Z Angew Math Mech 1970, 50(9):529-546.
    • (1970) Z Angew Math Mech , vol.50 , Issue.9 , pp. 529-546
    • Bueckner, H.F.1
  • 35
    • 33847014988 scopus 로고
    • Influence of crack-surface interactions on stress intensity factor in ceramics
    • Fett T., Munz D. Influence of crack-surface interactions on stress intensity factor in ceramics. J Mater Sci Lett 1990, 9:1403-1406.
    • (1990) J Mater Sci Lett , vol.9 , pp. 1403-1406
    • Fett, T.1    Munz, D.2
  • 37
    • 79960421605 scopus 로고    scopus 로고
    • Ultra high temperature ceramics for hypersonic vehicle applications. Sandia report;. Sand 2006-2925.
    • Loehman R, Corral E, Dumm HP, Kotula P, Tandon R. Ultra high temperature ceramics for hypersonic vehicle applications. Sandia report; 2006. Sand 2006-2925.
    • (2006)
    • Loehman, R.1    Corral, E.2    Dumm, H.P.3    Kotula, P.4    Tandon, R.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.