Volumn 83, Issue 4, 2000, Pages 802-808

Fracture behavior of alumina/monazite multilayer laminates

Author keywords

[No Author keywords available]

Indexed keywords

ALUMINA; CERAMIC COATINGS; CERAMIC MATRIX COMPOSITES; COMPOSITE MICROMECHANICS; CRACK INITIATION; DELAMINATION; FRACTURE TOUGHNESS; FRICTION; MATHEMATICAL MODELS; MONAZITE; MULTILAYERS; STRESS ANALYSIS;

EID: 0033905282     PISSN: 00027820     EISSN: None     Source Type: Journal    
DOI: 10.1111/j.1151-2916.2000.tb01278.x     Document Type: Article
Times cited : (39)

References (28)
  • 2
    • 0022060228 scopus 로고
    • Failure mechanisms in ceramic-fiber/ceramic-matrix composites
    • D. B. Marshall and A. G. Evans, "Failure Mechanisms in Ceramic-Fiber/Ceramic-Matrix Composites," J. Am. Ceram. Soc., 68 [5] 225-31 (1985).
    • (1985) J. Am. Ceram. Soc. , vol.68 , Issue.5 , pp. 225-231
    • Marshall, D.B.1    Evans, A.G.2
  • 4
    • 0027576037 scopus 로고
    • Functional interfaces for oxide/oxide composites
    • P. E. D. Morgan and D. B. Marshall, "Functional Interfaces for Oxide/Oxide Composites," Mater. Sci. Eng. A, A162, 15-25 (1993).
    • (1993) Mater. Sci. Eng. A , vol.A162 , pp. 15-25
    • Morgan, P.E.D.1    Marshall, D.B.2
  • 5
    • 0002215665 scopus 로고
    • Solid state reactions between rare earth orthophosphates and oxide
    • Y. Hikichi, K. Hukuo, and J. Shiokawa, "Solid State Reactions between Rare Earth Orthophosphates and Oxide," Bull. Chem. Soc. Jpn., 53, 1455-56 (1980).
    • (1980) Bull. Chem. Soc. Jpn. , vol.53 , pp. 1455-1456
    • Hikichi, Y.1    Hukuo, K.2    Shiokawa, J.3
  • 7
    • 0029324743 scopus 로고
    • Ceramic composites of monazite and alumina
    • P. E. D. Morgan and D. B. Marshall, "Ceramic Composites of Monazite and Alumina," J. Am. Ceram. Soc., 78 [6] 1553-63 (1995).
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.6 , pp. 1553-1563
    • Morgan, P.E.D.1    Marshall, D.B.2
  • 9
    • 0000669132 scopus 로고
    • Dispersants for nonaqueous tape casting
    • Edited by J. B. Blum and W. R. Cannon. American Ceramic Society, Westerville, OH
    • W. R. Cannon, J. R. Morris, and K. R. Mikeska, "Dispersants for Nonaqueous Tape Casting": pp. 161-74 in Advances in Ceramics, Vol. 19, Multilayer Ceramic Devices. Edited by J. B. Blum and W. R. Cannon. American Ceramic Society, Westerville, OH, 1986.
    • (1986) Advances in Ceramics, Vol. 19, Multilayer Ceramic Devices , vol.19 , pp. 161-174
    • Cannon, W.R.1    Morris, J.R.2    Mikeska, K.R.3
  • 11
    • 0024621114 scopus 로고
    • A test specimen for determining the fracture resistance of bimaterial interfaces
    • P. G. Charalambides, J. Lund, A. G. Evans, and R. M. McMeeking, "A Test Specimen for Determining the Fracture Resistance of Bimaterial Interfaces," J. Appl. Mech., 56, 77-82 (1989).
    • (1989) J. Appl. Mech. , vol.56 , pp. 77-82
    • Charalambides, P.G.1    Lund, J.2    Evans, A.G.3    McMeeking, R.M.4
  • 12
    • 0024301167 scopus 로고
    • Sandwich test specimen for measuring interface crack toughness
    • Z. Suo and J. W. Hutchinson, "Sandwich Test Specimen for Measuring Interface Crack Toughness," Mater. Sci. Eng. A, A107, 135-43 (1989).
    • (1989) Mater. Sci. Eng. A , vol.A107 , pp. 135-143
    • Suo, Z.1    Hutchinson, J.W.2
  • 14
    • 0031098081 scopus 로고    scopus 로고
    • Simple method for measuring frictional sliding resistance and energy dissipation in layered ceramics
    • D. Kovar and M. D. Thouless, "Simple Method for Measuring Frictional Sliding Resistance and Energy Dissipation in Layered Ceramics." J. Am. Ceram. Soc., 80 [3] 673-79 (1997).
    • (1997) J. Am. Ceram. Soc. , vol.80 , Issue.3 , pp. 673-679
    • Kovar, D.1    Thouless, M.D.2
  • 15
    • 0029326911 scopus 로고
    • High-temperature stability of monazite-alumina composites
    • P. E. D. Morgan, D. B. Marshall, and R. M. Housley, "High-Temperature Stability of Monazite Alumina Composites," Mater. Sci. Eng. A, A195, 215-22 (1995).
    • (1995) Mater. Sci. Eng. A , vol.A195 , pp. 215-222
    • Morgan, P.E.D.1    Marshall, D.B.2    Housley, R.M.3
  • 16
    • 0008515543 scopus 로고    scopus 로고
    • Standard test method for water absorption, bulk density, apparent porosity, and apparent specific gravity of fired whiteware products
    • ASTM Standard C373-72, American Society for Testing and Materials, Philadelphia, PA (now in West Conshohocken, PA)
    • "Standard Test Method for Water Absorption, Bulk Density, Apparent Porosity, and Apparent Specific Gravity of Fired Whiteware Products," ASTM Standard C373-72, 1982 Annual Book of ASTM Standards, American Society for Testing and Materials, Philadelphia, PA (now in West Conshohocken, PA).
    • 1982 Annual Book of ASTM Standards
  • 17
    • 0025491091 scopus 로고
    • Models of fiber debonding and pullout in brittle composites with friction
    • J. W. Hutchinson and H. M. Jensen, "Models of Fiber Debonding and Pullout in Brittle Composites with Friction." Mech. Mater., 9, 119-63 (1990).
    • (1990) Mech. Mater. , vol.9 , pp. 119-163
    • Hutchinson, J.W.1    Jensen, H.M.2
  • 18
    • 0008514718 scopus 로고
    • Ceramics, friction, and chemistry
    • T. E. Fischer and W. M. Mullins, "Ceramics, Friction, and Chemistry," CHEMTECH, 27-31 (1993).
    • (1993) CHEMTECH , pp. 27-31
    • Fischer, T.E.1    Mullins, W.M.2
  • 19
    • 0028468742 scopus 로고
    • The friction and wear of ceramic/ceramic and ceramic/metal combinations in sliding contact
    • H. E. Sliney and C. Dellacorte, "The Friction and Wear of Ceramic/Ceramic and Ceramic/Metal Combinations in Sliding Contact," Lubr. Eng., 50 [7] 571-76 (1994).
    • (1994) Lubr. Eng. , vol.50 , Issue.7 , pp. 571-576
    • Sliney, H.E.1    Dellacorte, C.2
  • 20
    • 0027560399 scopus 로고
    • Fracture behaviour of ceramic laminates in bending - II. Comparison of model predictions with experimental data
    • A. J. Phillipps, W. J. Clegg, and T. W. Clyne, "Fracture Behaviour of Ceramic Laminates in Bending - II. Comparison of Model Predictions with Experimental Data," Acta Metall. Mater., 41 [3] 819-27 (1993).
    • (1993) Acta Metall. Mater. , vol.41 , Issue.3 , pp. 819-827
    • Phillipps, A.J.1    Clegg, W.J.2    Clyne, T.W.3
  • 21
    • 0028483304 scopus 로고
    • The failure of layered ceramics in bending and tension
    • A. J. Phillipps, W. J. Clegg, and T. W. Clyne, "The Failure of Layered Ceramics in Bending and Tension," Composites (Guildford, UK), 25 [7] 524-33 (1994).
    • (1994) Composites (Guildford, UK) , vol.25 , Issue.7 , pp. 524-533
    • Phillipps, A.J.1    Clegg, W.J.2    Clyne, T.W.3
  • 22
    • 0023983975 scopus 로고
    • Effects pull-out on the mechanical properties of ceramic-matrix composites
    • M. D. Thouless and A. G. Evans, "Effects Pull-Out on the Mechanical Properties of Ceramic-Matrix Composites," Acta Metall., 36 [3] 517-22 (1988).
    • (1988) Acta Metall. , vol.36 , Issue.3 , pp. 517-522
    • Thouless, M.D.1    Evans, A.G.2
  • 23
    • 0024884622 scopus 로고
    • Crack deflection at an interface between dissimilar elastic materials
    • M.-Y. He and J. W. Hutchinson, "Crack Deflection at an Interface Between Dissimilar Elastic Materials," Int. J. Solids Struct., 25 [9] 1053-67 (1989).
    • (1989) Int. J. Solids Struct. , vol.25 , Issue.9 , pp. 1053-1067
    • He, M.-Y.1    Hutchinson, J.W.2
  • 24
    • 0028730620 scopus 로고
    • Crack deflection at an interface between dissimilar elastic materials: Role of residual stresses
    • H. Y. He, A. G. Evans, and J. W. Hutchinson, "Crack Deflection at an Interface Between Dissimilar Elastic Materials: Role of Residual Stresses," Int. J. Solids Struct., 31 [24] 3443-55 (1994).
    • (1994) Int. J. Solids Struct. , vol.31 , Issue.24 , pp. 3443-3455
    • He, H.Y.1    Evans, A.G.2    Hutchinson, J.W.3
  • 25
    • 84985156402 scopus 로고
    • Kinking of a crack out of an interface: Role of in-plane stress
    • M.-Y. He, A. Bartlett, and A. G. Evans, "Kinking of a Crack Out of an Interface: Role of In-Plane Stress," J. Am. Ceram. Soc., 74 [4] 767-71 (1991).
    • (1991) J. Am. Ceram. Soc. , vol.74 , Issue.4 , pp. 767-771
    • He, M.-Y.1    Bartlett, A.2    Evans, A.G.3
  • 26
    • 0032046413 scopus 로고    scopus 로고
    • Crack deflection and propagation in layered silicon nitride/boron nitride ceramics
    • D. Kovar, M. D. Thouless, and J. W. Halloran, "Crack Deflection and Propagation in Layered Silicon Nitride/Boron Nitride Ceramics," J. Am. Ceram. Soc., 81 [4] 1004-12 (1998).
    • (1998) J. Am. Ceram. Soc. , vol.81 , Issue.4 , pp. 1004-1012
    • Kovar, D.1    Thouless, M.D.2    Halloran, J.W.3
  • 27
    • 0027641266 scopus 로고
    • Cracking and stress redistribution in ceramic layered composites
    • K. S. Chan. M.-Y. He, and J. W. Hutchinson, "Cracking and Stress Redistribution in Ceramic Layered Composites," Mater. Sci. Eng. A, A167, 57-64 (1993).
    • (1993) Mater. Sci. Eng. A , vol.A167 , pp. 57-64
    • Chan, K.S.1    He, M.-Y.2    Hutchinson, J.W.3
  • 28
    • 0001126960 scopus 로고    scopus 로고
    • Control of interfacial properties through fiber coatings: Monazite coatings in oxide - Oxide composites
    • D.-H. Kuo, W. M. Kriven, and T. J. Mackin, "Control of Interfacial Properties through Fiber Coatings: Monazite Coatings in Oxide - Oxide Composites," J. Am. Ceram. Soc., 89 [12] 2987-96 (1997).
    • (1997) J. Am. Ceram. Soc. , vol.89 , Issue.12 , pp. 2987-2996
    • Kuo, D.-H.1    Kriven, W.M.2    Mackin, T.J.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.