2
-
-
2942686013
-
Perspectives in stabilisation of polyolefins
-
Al-Malaika S (2004) Perspectives in stabilisation of polyolefins. Adv Polym Sci 169:121-150
-
(2004)
Adv Polym Sci
, vol.169
, pp. 121-150
-
-
Al-Malaika, S.1
-
5
-
-
0141447819
-
The effect of degree of crosslinking on the fatigue crack initiation and propagation resistance of orthopedic-grade polyethylene
-
Baker DA, Bellare A, Pruitt L (2003) The effect of degree of crosslinking on the fatigue crack initiation and propagation resistance of orthopedic-grade polyethylene. J Biomed Mater Res 66A:146-154
-
(2003)
J Biomed Mater Res
, vol.66 A
, pp. 146-154
-
-
Baker, D.A.1
Bellare, A.2
Pruitt, L.3
-
6
-
-
26444509444
-
Cracking and impingement in ultra-high-molecular-weight polyethylene acetabular liners
-
DOI 10.1016/j.arth.2005.05.001, PII S0883540305002664
-
Birman M, Noble P, Conditt M, Li S, Mathis K (2005) Cracking and impingement in ultra-high molecular weight polyethylene acetabular liners. J Arthroplasty 20(7):87-92 (Pubitemid 41425791)
-
(2005)
Journal of Arthroplasty
, vol.20
, Issue.SUPPL. 3
, pp. 87-92
-
-
Birman, M.V.1
Noble, P.C.2
Conditt, M.A.3
Li, S.4
Mathis, K.B.5
-
7
-
-
58649122701
-
The epidemiology of revision total hip arthroplasty in the United States
-
Bozic K, Kurtz S, Lau E, Ong K, Vail T, Berry D (2009) The epidemiology of revision total hip arthroplasty in the United States. J Bone Joint Surg 91:128-133
-
(2009)
J Bone Joint Surg
, vol.91
, pp. 128-133
-
-
Bozic, K.1
Kurtz, S.2
Lau, E.3
Ong, K.4
Vail, T.5
Berry, D.6
-
8
-
-
36549013121
-
Stabilisation of ultra-high molecular weight polyethylene with Vitamin e
-
DOI 10.1016/j.polymdegradstab.2007.02.023, PII S0141391007002443, MoDeSt 2006
-
Bracco P, Brunella V, Zanetti M, Luda MP, Costa L (2007) Stabilisation of ultra-high molecular weight polyethylene with vitamin E. Polym Degrad Stab 92:2155-2162 (Pubitemid 350180039)
-
(2007)
Polymer Degradation and Stability
, vol.92
, Issue.12
, pp. 2155-2162
-
-
Bracco, P.1
Brunella, V.2
Zanetti, M.3
Luda, M.P.4
Costa, L.5
-
9
-
-
0020074850
-
Autoxidation of biological molecules. 1. The antioxidant activity of vitamin e and related chain-breaking phenolic antioxidants in vitro
-
DOI 10.1021/ja00411a035
-
Burton G, Ingold K (1981) Autoxidation of biological molecules. 1. The antioxidant activity of vitamin E and related chain-breaking phenolic antioxidants in vitro. J Am Chem Soc 103:6472-6477 (Pubitemid 12145820)
-
(1982)
Journal of the American Chemical Society
, vol.103
, Issue.21
, pp. 6472-6477
-
-
Burton, G.W.1
Ingold, K.U.2
-
10
-
-
0025315455
-
Vitamin E: Antioxidant activity, biokinetics, and bioavailability
-
Burton GW, Traber MG (1990) Vitamin E: Antioxidant activity, biokinetics, and bioavailability. Annu Rev Nutr 10:357-382
-
(1990)
Annu Rev Nutr
, vol.10
, pp. 357-382
-
-
Burton, G.W.1
Traber, M.G.2
-
11
-
-
0025522515
-
On the structures and yields of the first peroxyl radicals in g-irradiated polyolefins
-
Carlsson D, Chmela S, Lacoste J (1990) On the structures and yields of the first peroxyl radicals in g-irradiated polyolefins. Macromolecules 23:4934-4938
-
(1990)
Macromolecules
, vol.23
, pp. 4934-4938
-
-
Carlsson, D.1
Chmela, S.2
Lacoste, J.3
-
12
-
-
0041137490
-
Direct observations of macroperoxyl radical propagation and termination by electron spin resonance and infrared spectroscopies
-
Carlsson D, Dobbin C, Wiles D (1985) Direct observations of macroperoxyl radical propagation and termination by electron spin resonance and infrared spectroscopies. Macromolecules 18:2092-2094
-
(1985)
Macromolecules
, vol.18
, pp. 2092-2094
-
-
Carlsson, D.1
Dobbin, C.2
Wiles, D.3
-
13
-
-
0023206723
-
POLYOLEFIN OXIDATION: QUANTIFICATION of ALCOHOL and HYDROPEROXIDE PRODUCTS by NITRIC OXIDE REACTIONS
-
DOI 10.1016/0141-3910(87)90090-5
-
Carlsson DJ, Brousseau R, Zhang C, Wiles DM (1987) Polyolefin oxidation: quantification of alcohol and hydroperoxide products by nitric oxide reactions. Polym Degrad Stab 17:303-318 (Pubitemid 17600291)
-
(1987)
Polymer Degradation and Stability
, vol.17
, Issue.4
, pp. 303-318
-
-
Carlsson, D.J.1
Brousseau, R.2
Zhang, C.3
Wiles, D.M.4
-
14
-
-
0030468193
-
Overview of polyethylene as a bearing material: Comparison of sterilization methods
-
Collier J, Sutula L, Currier B, John H, Wooding R, Williams I, Farber K, Mayor M (1996) Overview of polyethylene as a bearing material: Comparison of sterilization methods. Clin Orthop 333:76-86
-
(1996)
Clin Orthop
, vol.333
, pp. 76-86
-
-
Collier, J.1
Sutula, L.2
Currier, B.3
John, H.4
Wooding, R.5
Williams, I.6
Farber, K.7
Mayor, M.8
-
15
-
-
37749040927
-
Physicochemical and mechanical properties of UHMWPE: 45 years' experience
-
Costa L, Bracco P, Brach del Prever E (2007) Physicochemical and mechanical properties of UHMWPE: 45 years' experience. Interact Surg 2(3-4):169-173
-
(2007)
Interact Surg
, vol.2
, Issue.3-4
, pp. 169-173
-
-
Costa, L.1
Bracco, P.2
Brach Del Prever, E.3
-
16
-
-
0031084281
-
Ultra-high molecular weight polyethylene: I. Mechano-oxidative degradation
-
Costa L, Luda MP, Trossarelli L (1997) Ultra-high molecular weight polyethylene: I. Mechano-oxidative degradation. Polym Degrad Stab 55:329-338
-
(1997)
Polym Degrad Stab
, vol.55
, pp. 329-338
-
-
Costa, L.1
Luda, M.P.2
Trossarelli, L.3
-
17
-
-
0031245597
-
Ultra high molecular weight polyethylene-II. Thermal-and photo-oxidation
-
Costa L, Luda MP, Trossarelli L (1997) Ultra high molecular weight polyethylene-II. Thermal-and photo-oxidation. Polym Degrad Stab 58:41-54
-
(1997)
Polym Degrad Stab
, vol.58
, pp. 41-54
-
-
Costa, L.1
Luda, M.P.2
Trossarelli, L.3
-
18
-
-
0032143159
-
In vivo UHMWPE biodegradation of retrieved prosthesis
-
Costa L, Luda MP, Trossarelli L, Brach del Prever EM, Crova M, Gallinaro P (1998) In vivo UHMWPE biodegradation of retrieved prosthesis. Biomaterials 19:1371-1385
-
(1998)
Biomaterials
, vol.19
, pp. 1371-1385
-
-
Costa, L.1
Luda, M.P.2
Trossarelli, L.3
Brach Del Prever, E.M.4
Crova, M.5
Gallinaro, P.6
-
19
-
-
0032052643
-
Oxidation in orthopaedic UHMWPE sterilized by gamma-radiation and ethylene oxide
-
DOI 10.1016/S0142-9612(97)00160-9, PII S0142961297001609
-
Costa L, Luda MP, Trossarelli L, Brach del Prever EM, Crova M, Gallinaro P (1998) Oxidation in orthopaedic UHMWPE sterilized by gamma radiation and ethylene oxide. Biomaterials 19:659-668 (Pubitemid 28276615)
-
(1998)
Biomaterials
, vol.19
, Issue.7-9
, pp. 659-668
-
-
Costa, L.1
Luda, M.P.2
Trossarelli, L.3
Brach, D.P.E.M.4
Crova, M.5
Gallinaro, P.6
-
20
-
-
9644257169
-
Large versus small femoral heads in metal-on-metal total hip arthroplasty
-
DOI 10.1016/j.arth.2004.09.006, PII S0883540304004917
-
Cuckler J, Moore K, Lombardi A Jr, McPherson E, Emerson R (2004) Large versus small femoral heads in metal-on-metal total hip arthroplasty. J Arthroplast 19(8 suppl 3):41-44 (Pubitemid 39575826)
-
(2004)
Journal of Arthroplasty
, vol.19
, Issue.8 SUPPL.
, pp. 41-44
-
-
Cuckler, J.M.1
Moore, K.D.2
Lombardi Jr., A.V.3
McPherson, E.4
Emerson, R.5
-
21
-
-
35448982702
-
Evaluation of oxidation and fatigue damage of retrieved Crossfire polyethylene acetabular cups
-
Currier BH, Currier JH, Mayor MB, Lyford K, Collier JP, Van Citters DW (2007) Evaluation of oxidation and fatigue damage of retrieved Crossfire polyethylene acetabular cups. J Bone Joint Surg 89A:2023-2029
-
(2007)
J Bone Joint Surg
, vol.89 A
, pp. 2023-2029
-
-
Currier, B.H.1
Currier, J.H.2
Mayor, M.B.3
Lyford, K.4
Collier, J.P.5
Van Citters, D.W.6
-
22
-
-
38749105452
-
5-Year experience of highly cross-linked polyethylene in cemented and uncemented sockets: Two randomized studies using radiostereometric analysis
-
DOI 10.1080/17453670710014518, PII 790014144
-
Digas G, Karrholm J, Thanner J, Herberts P (2007) 5-year experience of highly crosslinked polyethylene in cemented and uncemented sockets: Two randomized studies using radiostereo-metric analysis. Acta Orthop 78(6):746-754 (Pubitemid 351185595)
-
(2007)
Acta Orthopaedica
, vol.78
, Issue.6
, pp. 746-754
-
-
Digas, G.1
Karrholm, J.2
Thanner, J.3
Herberts, P.4
-
24
-
-
0026657363
-
The role of lipid peroxidation and antioxidants in oxidative modification of LDL
-
Esterbauer H, Gebicki J, Puhl H, Jurgens G (1992) The role of lipid peroxidation and antioxidants in oxidative modification of LDL. Free Radic Biol Med 13:341-390
-
(1992)
Free Radic Biol Med
, vol.13
, pp. 341-390
-
-
Esterbauer, H.1
Gebicki, J.2
Puhl, H.3
Jurgens, G.4
-
26
-
-
77949894544
-
Risk factors for accelerated polyethylene wear and osteolysis in ABG I total hip arthroplasty
-
Gallo J, Havranek V, Zapletalova J (2010) Risk factors for accelerated polyethylene wear and osteolysis in ABG I total hip arthroplasty. Int Orthop 34:19-26
-
(2010)
Int Orthop
, vol.34
, pp. 19-26
-
-
Gallo, J.1
Havranek, V.2
Zapletalova, J.3
-
27
-
-
1842473877
-
Recurrent Dislocation after Revision Total Hip Replacement with a Large Prosthetic Femoral Head: A Case Report
-
Halley D, Glassman A, Crowninshield R (2004) Recurrent dislocation after revision total hip replacement with a large prosthetic femoral head. J Bone Joint Surg 86A(4):827-830 (Pubitemid 38436730)
-
(2004)
Journal of Bone and Joint Surgery - Series A
, vol.86
, Issue.4
, pp. 827-830
-
-
Halley, D.1
Glassman, A.2
Crowninshield, R.D.3
-
28
-
-
54449100155
-
Highly crosslinked polyethylene is safe fro use in total knee arthroplasty
-
Hodrick J, Severson E, McAlister D, Dahl B, Hofmann A (2008) Highly crosslinked polyethylene is safe fro use in total knee arthroplasty. Clin Orthop Relat Res 466:2806-2812
-
(2008)
Clin Orthop Relat Res
, vol.466
, pp. 2806-2812
-
-
Hodrick, J.1
Severson, E.2
McAlister, D.3
Dahl, B.4
Hofmann, A.5
-
29
-
-
0034856352
-
A study of long-lived free radicals in gamma-irradiated medical grade polyethylene
-
DOI 10.1016/S0969-806X(01)00431-5, PII S0969806X01004315
-
Jahan MS, King MC, Haggard WO, Sevo KL, Parr JE (2001) A study of long-lived free radicals in gamma-irradiated medical grade polyethlene. Radiat Phys Chem 62:141-144 (Pubitemid 32823283)
-
(2001)
Radiation Physics and Chemistry
, vol.62
, Issue.1
, pp. 141-144
-
-
Jahan, M.S.1
King, M.C.2
Haggard, W.O.3
Sevo, K.L.4
Parr, J.E.5
-
30
-
-
78649461489
-
In vivo biological response to vitamin e and vitamin e-doped polyethylene
-
in press
-
Jarrett B, Cofske J, Rosenberg A, Oral E, Muratoglu O, Malchau H (2010) In vivo biological response to vitamin E and vitamin E-doped polyethylene. J Bone Joint Surg 92(13) (in press)
-
(2010)
J Bone Joint Surg
, vol.92
, Issue.13
-
-
Jarrett, B.1
Cofske, J.2
Rosenberg, A.3
Oral, E.4
Muratoglu, O.5
Malchau, H.6
-
31
-
-
0030015296
-
The chemistry and antioxidant properties of tocopherols and tocotrienols
-
Kamal-Eldin A, Appelqvist L (1996) The chemistry and antioxidant properties of tocopherols and tocotrienols. Lipids 31(7):671-701 (Pubitemid 26240763)
-
(1996)
Lipids
, vol.31
, Issue.7
, pp. 671-701
-
-
Kamal-Eldin, A.1
Appelqvist, L.-A.2
-
32
-
-
0002687797
-
Radiation induced oxidation of plastics
-
Singh A, Silverman J (eds) Munich, Carl Hanser Verlag
-
Kashiwabara H, Seguchi T (1992) Radiation induced oxidation of plastics. In Singh A, Silverman J (eds) Radiation processing of polymers. Munich, Carl Hanser Verlag, pp 221-254
-
(1992)
Radiation Processing of Polymers
, pp. 221-254
-
-
Kashiwabara, H.1
Seguchi, T.2
-
33
-
-
0026007741
-
Free radicals and crosslinking in irradiated polyethylene
-
Kashiwabara H, Shimada S, Hori Y (1991) Free radicals and crosslinking in irradiated polyethylene. Radiat Phys Chem 37 (1):43-46
-
(1991)
Radiat Phys Chem
, vol.37
, Issue.1
, pp. 43-46
-
-
Kashiwabara, H.1
Shimada, S.2
Hori, Y.3
-
35
-
-
77953123950
-
Mechanical properties, oxidation and clinical performance of retrieved highly crosslinked Crossfire liners after intermediate-term implantation
-
Kurtz S, Austin M, Azzam K, Sharkey P, MacDonald D, Medel F, Hozack W (2010) Mechanical properties, oxidation and clinical performance of retrieved highly crosslinked Crossfire liners after intermediate-term implantation. J Arthroplasty 25(4):614-625
-
(2010)
J Arthroplasty
, vol.25
, Issue.4
, pp. 614-625
-
-
Kurtz, S.1
Austin, M.2
Azzam, K.3
Sharkey, P.4
MacDonald, D.5
Medel, F.6
Hozack, W.7
-
36
-
-
67650500345
-
Trace concentrations of vitamin e protect radiation crosslinked UHMWPE from oxidative degradation
-
Kurtz S, Dumbleton J, Siskey R, Wang A, Manley M (2008) Trace concentrations of vitamin E protect radiation crosslinked UHMWPE from oxidative degradation. J Biomed Mater Res 90A:549-563
-
(2008)
J Biomed Mater Res
, vol.90 A
, pp. 549-563
-
-
Kurtz, S.1
Dumbleton, J.2
Siskey, R.3
Wang, A.4
Manley, M.5
-
37
-
-
0141924490
-
Degradation of mechanical properties of UHMWPE acetabular liners following long-term implantation
-
DOI 10.1016/S0883-5403(03)00292-4
-
Kurtz S, Hozack WJ, Marcolongo M, Turner J, Rimnac CM, Edidin A (2003) Degradation of mechanical properties of UHMWPE acetabular liners following long-term implantation. J Arthroplast 18(7 Supp 1):68-78 (Pubitemid 37259669)
-
(2003)
Journal of Arthroplasty
, vol.18
, Issue.7 SUPPL. 1
, pp. 68-78
-
-
Kurtz, S.M.1
Hozack, W.2
Marcolongo, M.3
Turner, J.4
Rimnac, C.5
Edidin, A.6
-
38
-
-
0032073035
-
Peroxy radical formation from plasma-induced surface radicals of polyethylene as studied by electron spin resonance
-
Kuzuya M, Kondo S, Sugito M, Yamashiro T (1998) Peroxy radical formation from plasma-induced surface free radicals of polyethylene as studied by electron spin resonance. Macromolecules 31:3230-3234 (Pubitemid 128575513)
-
(1998)
Macromolecules
, vol.31
, Issue.10
, pp. 3230-3234
-
-
Kuzuya, M.1
Kondo, S.-I.2
Sugito, M.3
Yamashiro, T.4
-
39
-
-
77349119374
-
Use of vitamin e to protect cross-linked UHMWPE from oxidation
-
Lerf R, Zurbrugg D, Delfosse D (2010) Use of vitamin E to protect cross-linked UHMWPE from oxidation. Biomaterials 31:3643-3648
-
(2010)
Biomaterials
, vol.31
, pp. 3643-3648
-
-
Lerf, R.1
Zurbrugg, D.2
Delfosse, D.3
-
41
-
-
0035584282
-
Post-gamma-irradiation reactions in vitamin e stabilised and unstabilised HDPE
-
DOI 10.1016/S0168-583X(01)00944-2, PII S0168583X01009442
-
Mallegol J, Carlsson D, Deschenes L (2001) Post-gamma irradiation reactions in vitamin E stabilized and unstabilised HDPE. Nucl Instrum Meth Phys Res B 185:283-293 (Pubitemid 33142322)
-
(2001)
Nuclear Instruments and Methods in Physics Research, Section B: Beam Interactions with Materials and Atoms
, vol.185
, Issue.1-4
, pp. 283-293
-
-
Mallegol, J.1
Carlsson, D.J.2
Deschenes, L.3
-
42
-
-
26844448524
-
In vivo comparative wear study of traditional and highly cross-linked polyethylene in total hip arthroplasty
-
Manning DW, Chiang PP, Martell JM, Galante JO, Harris WH (2005) In vivo comparative wear study of traditional and highly cross-linked polyethylene in total hip arthroplasty. J Arthroplasty 20(7):880-886
-
(2005)
J Arthroplasty
, vol.20
, Issue.7
, pp. 880-886
-
-
Manning, D.W.1
Chiang, P.P.2
Martell, J.M.3
Galante, J.O.4
Harris, W.H.5
-
43
-
-
0141993638
-
Clinical performance of a highly cross-linked polyethylene at two years in total hip arthroplasty: A randomized prospective trial
-
Martell JM, Verner JJ, Incavo SJ (2003) Clinical performance of a highly cross-linked polyethylene at two years in total hip arthroplasty: a randomized prospective trial. J Arthroplasty 18(7 Suppl 1):9
-
(2003)
J Arthroplasty
, vol.18
, Issue.7 SUPPL. 1
, pp. 9
-
-
Martell, J.M.1
Verner, J.J.2
Incavo, S.J.3
-
44
-
-
0032927112
-
Development of an extremely wear-resistant ultra high molecular weight polyethylene for total hip replacements
-
DOI 10.1002/jor.1100170203
-
McKellop H, Shen F-W, Lu B, Campbell P, Salovey R (1999) Development of an extremely wear resistant ultra-high molecular weight polyethylene for total hip replacements. J Orthop Res 17 (2):157-167 (Pubitemid 29190487)
-
(1999)
Journal of Orthopaedic Research
, vol.17
, Issue.2
, pp. 157-167
-
-
McKellop, H.1
Shen, F.-W.2
Lu, B.3
Campbell, P.4
Salovey, R.5
-
45
-
-
67449088227
-
A systematic review of radiological outcomes of highly crosslinked polyethylene versus conventional polyethylene in total hip arthroplasty
-
Mu Z, Tian J, Wu T, Yang J, Pei F (2009) A systematic review of radiological outcomes of highly crosslinked polyethylene versus conventional polyethylene in total hip arthroplasty. Int Orthop 33:599-604
-
(2009)
Int Orthop
, vol.33
, pp. 599-604
-
-
Mu, Z.1
Tian, J.2
Wu, T.3
Yang, J.4
Pei, F.5
-
46
-
-
0035117295
-
A novel method of crosslinking UHMWPE to improve wear, reduce oxidation and retain mechanical properties
-
Muratoglu OK, Bragdon CR, O'Connor DO, Jasty M, Harris WH (2001) A novel method of crosslinking UHMWPE to improve wear, reduce oxidation and retain mechanical properties. J Arthroplasty 16(2):149-160
-
(2001)
J Arthroplasty
, vol.16
, Issue.2
, pp. 149-160
-
-
Muratoglu, O.K.1
Bragdon, C.R.2
O'Connor, D.O.3
Jasty, M.4
Harris, W.H.5
-
47
-
-
0033178826
-
Unified wear model for highly crosslinked ultra-high molecular weight polyethylenes (UHMWPE)
-
DOI 10.1016/S0142-9612(99)00039-3, PII S0142961299000393
-
Muratoglu OK, Bragdon CR, O'Connor DO, Jasty M, Harris WH, Gul R, McGarry F (1999) Unified wear model for highly crosslinked ultra-high molecular weight polyethylenes (UHMWPE). Biomaterials 20(16):1463-1470 (Pubitemid 29348488)
-
(1999)
Biomaterials
, vol.20
, Issue.16
, pp. 1463-1470
-
-
Muratoglu, O.K.1
Bragdon, C.R.2
O'Connor, D.O.3
Jasty, M.4
Harris, W.H.5
Rizwan, G.6
McGarry, F.7
-
48
-
-
0035217940
-
Larger diameter femoral heads used in conjunction with a highly cross-linked ultra-high molecular weight polyethylene: A new concept
-
DOI 10.1054/arth.2001.28376
-
Muratoglu OK, Bragdon CR, O'Connor DO, Perinchief RS, Estok DM, Jasty M, Harris WH (2001) Larger diameter femoral heads used in conjunction with a highly cross-linked ultra-high molecular weight polyethylene: A new concept. J Arthroplasty 16(8 Suppl):24-30 (Pubitemid 33151043)
-
(2001)
Journal of Arthroplasty
, vol.16
, Issue.8 SUPPL. 1
, pp. 24-30
-
-
Muratoglu, O.K.1
Bragdon, C.R.2
O'Connor, D.3
Perinchief, R.S.4
Estok II, D.M.5
Jasty, M.6
Harris, W.H.7
-
49
-
-
0344308259
-
Effect of Radiation, Heat, and Aging on in Vitro Wear Resistance of Polyethylene
-
Muratoglu OK, Merrill EW, Bragdon CR, O'Connor DO, Hoeffel D, Burroughs B, Jasty M, Harris WH (2003) Effect of radiation, heat, and aging on in vitro wear resistance of polyethylene. Clin Orthop Relat Res 417:253-262 (Pubitemid 37504959)
-
(2003)
Clinical Orthopaedics and Related Research
, Issue.417
, pp. 253-262
-
-
Muratoglu, O.K.1
Merrill, E.W.2
Bragdon, C.R.3
O'Connor, D.4
Hoeffel, D.5
Burroughs, B.6
Jasty, M.7
Harris, W.H.8
-
50
-
-
33745009957
-
Wear Resistance and Mechanical Properties of Highly Cross-linked, Ultrahigh-Molecular Weight Polyethylene Doped with Vitamin e
-
DOI 10.1016/j.arth.2005.07.009, PII S0883540305004055
-
Oral E, Christensen S, Malhi A, Wannomae K, Muratoglu O (2006) Wear resistance and mechanical properties of highly crosslinked UHMWPE doped with vitamin E. J Arthroplasty 21 (4):580-591 (Pubitemid 43866398)
-
(2006)
Journal of Arthroplasty
, vol.21
, Issue.4
, pp. 580-591
-
-
Oral, E.1
Christensen, S.D.2
Malhi, A.S.3
Wannomae, K.K.4
Muratoglu, O.K.5
-
51
-
-
46149091039
-
The effects of high dose irradiation on the cross-linking of vitamin E-blended UHMWPE
-
Oral E, Godleski Beckos C, Malhi A, Muratoglu O (2008) The effects of high dose irradiation on the cross-linking of vitamin E-blended UHMWPE. Biomaterials 29:3557-3560
-
(2008)
Biomaterials
, vol.29
, pp. 3557-3560
-
-
Oral, E.1
Godleski Beckos, C.2
Malhi, A.3
Muratoglu, O.4
-
52
-
-
22544437873
-
Characterization of irradiated blends of alpha-tocopherol and UHMWPE
-
DOI 10.1016/j.biomaterials.2005.04.026, PII S0142961205003017
-
Oral E, Greenbaum ES, Malhi AS, Harris WH, Muratoglu OK (2005) Characterization of irradiated blends of alpha-tocopherol and UHMWPE. Biomaterials 26(33):6657-6663 (Pubitemid 41021758)
-
(2005)
Biomaterials
, vol.26
, Issue.33
, pp. 6657-6663
-
-
Oral, E.1
Greenbaum, E.S.2
Malhi, A.S.3
Harris, W.H.4
Muratoglu, O.K.5
-
53
-
-
26944432688
-
Mechanisms of decrease in fatigue crack propagation resistance in irradiated and melted UHMWPE
-
DOI 10.1016/j.biomaterials.2005.06.025, PII S0142961205005971
-
Oral E, Malhi A, Muratoglu O (2006) Mechanisms of decrease in fatigue crack propagation resistance in irradiated and melted UHMWPE. Biomaterials 27:917-925 (Pubitemid 41484124)
-
(2006)
Biomaterials
, vol.27
, Issue.6
, pp. 917-925
-
-
Oral, E.1
Malhi, A.S.2
Muratoglu, O.K.3
-
54
-
-
33746813263
-
The effect of alpha-tocopherol on the oxidation and free radical decay in irradiated UHMWPE
-
DOI 10.1016/j.biomaterials.2006.07.017, PII S0142961206006429
-
Oral E, Rowell S, Muratoglu O (2006) The effect of alpha-tocopherol on the oxidation and free radical decay in irradiated UHMWPE. Biomaterials 27:5580-5587 (Pubitemid 44176152)
-
(2006)
Biomaterials
, vol.27
, Issue.32
, pp. 5580-5587
-
-
Oral, E.1
Rowell, S.L.2
Muratoglu, O.K.3
-
55
-
-
2342495274
-
a-Tocopherol-doped irradiated UHMWPE for high fatigue resistance and low wear
-
DOI 10.1016/j.biomaterials.2003.12.048, PII S0142961203012201
-
Oral E, Wannomae KK, Hawkins NE, Harris WH, Muratoglu OK (2004) a-Tocopherol doped irradiated UHMWPE for high fatigue resistance and low wear. Biomaterials 25(24):5515-5522 (Pubitemid 38610190)
-
(2004)
Biomaterials
, vol.25
, Issue.24
, pp. 5515-5522
-
-
Oral, E.1
Wannomae, K.K.2
Hawkins, N.3
Harris, W.H.4
Muratoglu, O.K.5
-
56
-
-
34948901872
-
Diffusion of vitamin e in ultra-high molecular weight polyethylene
-
DOI 10.1016/j.biomaterials.2007.08.025, PII S0142961207006734
-
Oral E, Wannomae KK, Rowell SL, Muratoglu OK (2007) Diffusion of vitamin E in ultra-high molecular weight polyethylene. Biomaterials 28(35):5225-5237 (Pubitemid 47532197)
-
(2007)
Biomaterials
, vol.28
, Issue.35
, pp. 5225-5237
-
-
Oral, E.1
Wannomae, K.K.2
Rowell, S.L.3
Muratoglu, O.K.4
-
57
-
-
85166583471
-
Vitamin E: The antioxidant harvesting center of membranes and lipoproteins
-
Packer L, Fuchs J (eds) Marcel Dekker, Inc., New York
-
Packer L, Kagan VE (1993) Vitamin E: The antioxidant harvesting center of membranes and lipoproteins. In Packer L, Fuchs J (eds) Vitamin E in health and disease. Marcel Dekker, Inc., New York, pp 179-192
-
(1993)
Vitamin e in Health and Disease
, pp. 179-192
-
-
Packer, L.1
Kagan, V.E.2
-
58
-
-
0036799941
-
Studies on the effect of electron beam radiation on the molecular structure of ultra-high molecular weight polyethylene under the influence of alpha-tocopherol with respect to its application in medical implants
-
DOI 10.1023/A:1019892004830
-
Parth M, Aust N, Lederer K (2002) Studies on the effect of electron beam radiation on the molecular structure of ultra-high molecular weight polyethylene under the influence of alphatocopherol with respect to its application in medical implants. J Mater Sci Mater Med 13(10):917-921 (Pubitemid 35176956)
-
(2002)
Journal of Materials Science: Materials in Medicine
, vol.13
, Issue.10
, pp. 917-921
-
-
Parth, M.1
Aust, N.2
Lederer, K.3
-
59
-
-
0001738320
-
Gamma sterilization of UHMWPE articular implants: An analysis of the oxidation problem
-
DOI 10.1016/0142-9612(95)00349-5
-
Premnath V, Harris W, Jasty M, Merrill E (1996) Gamma sterilization of UHMWPE articular implants: an analysis of the oxidation problem. Ultra high molecular weight poly ethylene. Biomaterials 17:1741-1753 (Pubitemid 26355416)
-
(1996)
Biomaterials
, vol.17
, Issue.18
, pp. 1741-1753
-
-
Premnath, V.1
Harris, W.H.2
Jasty, M.3
Merrill, E.W.4
-
60
-
-
36049034416
-
Photochemical oxidation reactions of synthetic polymers
-
Kinell P, Ranby B (eds) Almqvist-Wiksell Forlag AB, Stockholm
-
Rabek J, Ranby B (1973) Photochemical oxidation reactions of synthetic polymers. In Kinell P, Ranby B (eds) ESR applications to polymer research. Almqvist-Wiksell Forlag AB, Stockholm
-
(1973)
ESR Applications to Polymer Research
-
-
Rabek, J.1
Ranby, B.2
-
62
-
-
0242526067
-
The induction of MMP-9 release from granulocytes by vitamin e in UHMWPE
-
Reno F, Bracco P, Lombardi F, Boccafoschi F, Costa L, Cannas M (2004) The induction of MMP-9 release from granulocytes by vitamin E in UHMWPE. Biomaterials 25(6):1001
-
(2004)
Biomaterials
, vol.25
, Issue.6
, pp. 1001
-
-
Reno, F.1
Bracco, P.2
Lombardi, F.3
Boccafoschi, F.4
Costa, L.5
Cannas, M.6
-
63
-
-
27644448756
-
Effect of cross-linking on the microstructure and mechanical properties of ultra-high molecular weight polyethylene
-
DOI 10.1097/01.blo.0000185310.59202.e5
-
Ries M, Pruitt L (2005) Effect of crosslinking on the microstructure and mechanical properties of ultra-high molecular weight polyethylene. Clin Orthop Relat Res 440:149-156 (Pubitemid 41579208)
-
(2005)
Clinical Orthopaedics and Related Research
, Issue.440
, pp. 149-156
-
-
Ries, M.D.1
Pruitt, L.2
-
64
-
-
38849153584
-
Very low wear of non-remelted highly cross-linked polyethylene cups: An RSA study lasting up to 6 years
-
DOI 10.1080/17453670710014509, PII 790014143
-
Rohrl S, Li M, Nilsson K, Nivbrant B (2007) Very low wear of non-remelted highly crosslinked polyethylene cups: An RSA study lasting up to 6 years. Acta Orthop 78(6):739-745 (Pubitemid 351192903)
-
(2007)
Acta Orthopaedica
, vol.78
, Issue.6
, pp. 739-745
-
-
Rohrl, S.M.1
Li, M.G.2
Nilsson, K.-G.3
Nivbrant, B.4
-
65
-
-
79955930069
-
Comparison of the oxidative stability of vitamin E-stabilized UHMWPE by blending and diffusion
-
in press
-
Rowell S, Oral E, Muratoglu O (2010) Comparison of the oxidative stability of vitamin E-stabilized UHMWPE by blending and diffusion. J Orthop Res (in press)
-
(2010)
J Orthop Res
-
-
Rowell, S.1
Oral, E.2
Muratoglu, O.3
-
66
-
-
0002393094
-
Antioxidants: Chain breaking mechanisms
-
Scott G (ed) Elsevier Science Publishers B.V.
-
Scott G (1993) Antioxidants: Chain breaking mechanisms. In Scott G (ed) Atmospheric oxidation and antioxidants. Elsevier Science Publishers B.V., pp 121-160
-
(1993)
Atmospheric Oxidation and Antioxidants
, pp. 121-160
-
-
Scott, G.1
-
67
-
-
85166566854
-
Analysis and distribution of vitamin e in vegetable oils and foods
-
Packer L, Fuchs J (eds) Marcel Dekker, Inc., New York
-
Sheppard AJ, Pennington JA, Weihrauch JL (1993) Analysis and distribution of vitamin E in vegetable oils and foods. In Packer L, Fuchs J (eds) Vitamin E in health and disease. Marcel Dekker, Inc., New York, pp 9-31
-
(1993)
Vitamin e in Health and Disease
, pp. 9-31
-
-
Sheppard, A.J.1
Pennington, J.A.2
Weihrauch, J.L.3
-
68
-
-
0033029624
-
Relationship of acetabular wear to osteolysis and loosening in total hip arthroplasty
-
Sochart DH (1999) Relationship of acetabular wear to osteolysis and loosening in total hip arthroplasty. Clin Orthop Relat Res 363:135-150
-
(1999)
Clin Orthop Relat Res
, vol.363
, pp. 135-150
-
-
Sochart, D.H.1
-
69
-
-
33645395712
-
Behavior of Hylamer polyethylene in hip arthroplasty: Comparison of two gamma sterilization techniques
-
Stea S, Antonietti B, Baruffaldi F, Visentin M, Bordini B, Sudanese A, Toni A (2006) Behavior of Hylamer polyethylene in hip arthroplasty: comparison of two gamma sterilization techniques. Int Orthop 30(1):35-38
-
(2006)
Int Orthop
, vol.30
, Issue.1
, pp. 35-38
-
-
Stea, S.1
Antonietti, B.2
Baruffaldi, F.3
Visentin, M.4
Bordini, B.5
Sudanese, A.6
Toni, A.7
-
70
-
-
35349019671
-
Rim cracking of the cross-linked longevity polyethylene acetabular liner after total hip arthroplasty
-
DOI 10.2106/JBJS.F.00758
-
Tower SS, Currier JH, Currier BH, Lyford KA, Van Citters DW, Mayor MB (2007) Rim cracking of the cross-linked longevity polyethylene acetabular liner after total hip arthroplasty. J Bone Joint Surg Am 89(10):2212-2217 (Pubitemid 47606168)
-
(2007)
Journal of Bone and Joint Surgery - Series A
, vol.89
, Issue.10
, pp. 2212-2217
-
-
Tower, S.S.1
Currier, J.H.2
Currier, B.H.3
Lyford, K.A.4
Van Citters, D.W.5
Mayor, M.B.6
-
71
-
-
84990111672
-
Polyolefine oxidation
-
Tudos F, Iring M (1988) Polyolefine oxidation. Acta Polym 39 (1/2):19-26
-
(1988)
Acta Polym
, vol.39
, Issue.1-2
, pp. 19-26
-
-
Tudos, F.1
Iring, M.2
-
72
-
-
33749235115
-
In vivo oxidation of retrieved crosslinked UHMWPE acetabular components with residual free radicals
-
Wannomae K, Bhattacharyya S, Freiberg A, Estok D, Harris W, Muratoglu O (2006) In vivo oxidation of retrieved crosslinked UHMWPE acetabular components with residual free radicals. J Arthroplasty 21(7):1005-1011
-
(2006)
J Arthroplasty
, vol.21
, Issue.7
, pp. 1005-1011
-
-
Wannomae, K.1
Bhattacharyya, S.2
Freiberg, A.3
Estok, D.4
Harris, W.5
Muratoglu, O.6
-
73
-
-
0036305013
-
Tests of biocompatibility of a-tocopherol with respect to the use as a stabilizer in ultrahigh molecular weight polyethylene for articulating surfaces in joint endoprostheses
-
Wolf C, Lederer K, Muller U (2002) Tests of biocompatibility of a-tocopherol with respect to the use as a stabilizer in ultrahigh molecular weight polyethylene for articulating surfaces in joint endoprostheses. J Mater Sci Mater Med 13:701-703
-
(2002)
J Mater Sci Mater Med
, vol.13
, pp. 701-703
-
-
Wolf, C.1
Lederer, K.2
Muller, U.3
-
74
-
-
33845428344
-
Stabilisation of crosslinked ultra-high molecular weight polyethylene (UHMW-PE)-acetabular components with alpha-tocopherol
-
DOI 10.1007/s10856-006-0607-7, Selected Papers from the 10th International Conference on Polymers in Medicine and Surgery, Cambridge UK, 2004
-
Wolf C, Maninger J, Lederer K, Fruhwirth-Smounig H, Gamse T, Marr R (2006) Stabilisation of crosslinked ultra-high molecular weight polyethylene (UHMW-PE)-acetabular components with alpha-tocopherol. J Mater Sci Mater Med 17:1323-1331 (Pubitemid 44900632)
-
(2006)
Journal of Materials Science: Materials in Medicine
, vol.17
, Issue.12
, pp. 1323-1331
-
-
Wolf, C.1
Maninger, J.2
Lederer, K.3
Fruhwirth-Smounig, H.4
Gamse, T.5
Marr, R.6
-
75
-
-
11044235590
-
Degradation diagnosis of ultrahigh-molecular weight polyethylene with terahertz-time-domain spectroscopy
-
DOI 10.1063/1.1827332, 3
-
Yamamoto K, Yamaguchi M, Tani M, Hangyo M, Teramura S, Isu T, Tomita N (2004) Degradation diagnosis of UHMWPE with terahertz-time-domain spectroscopy. Appl Phys Lett 85(22):5194-5196 (Pubitemid 40043527)
-
(2004)
Applied Physics Letters
, vol.85
, Issue.22
, pp. 5194-5196
-
-
Yamamoto, K.1
Yamaguchi, M.2
Tani, M.3
Hangyo, M.4
Teramura, S.5
Isu, T.6
Tomita, N.7
|