Unidirectional carbon fibre reinforced poly (vinylidene fluoride): Impact of atmospheric plasma on composite performance

Author keywords

A. Carbon fibre; E. Powder processing; PVDF; PVDF composites

Indexed keywords

ATMOSPHERIC PLASMAS; CARBON FIBRES; CRITICAL ENERGY RELEASE RATE; ESSENTIAL WORK OF FRACTURE; FIBRE VOLUME FRACTION; FLEXURAL STRENGTH; IN-LINE; MODE II; POLY(VINYLIDENE FLUORIDE); POWDER PROCESSING; PVDF; PVDF COMPOSITES; SHORT BEAMS;

EID: 79952534862     PISSN: 1359835X     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.compositesa.2011.01.001     Document Type: Article
Times cited : (16)

References (56)
  • 2
    • 0024899737 scopus 로고
    • The interface in carbon fibre composites
    • M.R. Piggott The interface in carbon fibre composites Carbon 27 1989 662 757
    • (1989) Carbon , vol.27 , pp. 662-757
    • Piggott, M.R.1
  • 3
    • 27644491663 scopus 로고    scopus 로고
    • Offshore composites: Transition barriers to an enabling technology
    • DOI 10.1016/j.compscitech.2005.05.019, PII S0266353805001922
    • O. Ochoa, and M. Salama Offshore composites: transition barriers to an enabling technology Compos Sci Technol 65 15-16 2005 2588 2596 (Pubitemid 41574409)
    • (2005) Composites Science and Technology , vol.65 , Issue.SPEC. ISS. 15-16 , pp. 2588-2596
    • Ochoa, O.O.1    Salama, M.M.2
  • 7
    • 0042979876 scopus 로고    scopus 로고
    • Polyacrylonitrile (PAN)-based carbon fibers
    • Amsterdam: Elsevier Science
    • Shindo A. Polyacrylonitrile (PAN)-based carbon fibers. In: Comprehensive composite materials. Amsterdam: Elsevier Science; 2000.
    • (2000) Comprehensive Composite Materials
    • Shindo, A.1
  • 9
    • 0042830708 scopus 로고    scopus 로고
    • Interface and impregnation relevant tests for continuous glass fibre-polypropylene composites
    • P. Nygard, and C.G. Gustafson Interface and impregnation relevant tests for continuous glass fibre-polypropylene composites Compos Part A - Appl Sci Manuf 34 10 2003 995 1006
    • (2003) Compos Part A - Appl Sci Manuf , vol.34 , Issue.10 , pp. 995-1006
    • Nygard, P.1    Gustafson, C.G.2
  • 10
    • 19944368832 scopus 로고    scopus 로고
    • Influence of KOH solution on the tensile strength and chemical stability of carbon fiber-reinforced epoxy resin composites
    • DOI 10.1002/app.21634
    • A.A. Wazzan, A. Al-Turaif, and M.A. Daous Influence of KOH solution on the tensile strength and chemical stability of carbon fiber-reinforced epoxy resin composites J Appl Polym Sci 96 5 2005 1682 1690 (Pubitemid 40751459)
    • (2005) Journal of Applied Polymer Science , vol.96 , Issue.5 , pp. 1682-1690
    • Wazzan, A.A.1    Al-Turaif, H.A.2    Daous, M.A.3
  • 11
    • 0242692413 scopus 로고    scopus 로고
    • Autoclave forming of thermoplastic composite parts
    • I. Fernandez, F. Blas, and A. Frovel Autoclave forming of thermoplastic composite parts J Mater Process Technol 143 2003 266 269
    • (2003) J Mater Process Technol , vol.143 , pp. 266-269
    • Fernandez, I.1    Blas, F.2    Frovel, A.3
  • 12
    • 33751580323 scopus 로고    scopus 로고
    • Effect of hot water immersion on the performance of carbon reinforced unidirectional poly(ether ether ketone) (PEEK) composites: Stress rupture under end-loaded bending
    • DOI 10.1016/j.compositesa.2006.03.004, PII S1359835X06001278
    • A. Bismarck, M. Hofmeier, and G. Dörner Effect of hot water immersion on the performance of carbon reinforced unidirectional poly(ether ether ketone) (PEEK) composites: stress rupture under end-loaded bending Compos Part A - Appl Sci Manuf 38 2 2007 407 426 (Pubitemid 44842015)
    • (2007) Composites Part A: Applied Science and Manufacturing , vol.38 , Issue.2 , pp. 407-426
    • Bismarck, A.1    Hofmeier, M.2    Dorner, G.3
  • 14
    • 6444242613 scopus 로고    scopus 로고
    • Influence of processing conditions on bending property of continuous carbon fiber reinforced PEEK composites
    • DOI 10.1016/j.compscitech.2004.05.014, PII S026635380400140X
    • K. Fujihara, Z.M. Huang, S. Ramakrishna, and H. Hamada Influence of processing conditions on bending property of continuous carbon fiber reinforced PEEK composites Compos Sci Technol 64 16 2004 2525 2534 (Pubitemid 39407994)
    • (2004) Composites Science and Technology , vol.64 , Issue.16 , pp. 2525-2534
    • Fujihara, K.1    Huang, Z.-M.2    Ramakrishna, S.3    Hamada, H.4
  • 15
    • 0022737523 scopus 로고
    • Polyetheretherketone (PEEK)-processing-structure and properties studies for a matrix in high-performance composites
    • J.C. Seferis Polyetheretherketone (PEEK)-processing-structure and properties studies for a matrix in high-performance composites Polym Compos 7 3 1986 158 169
    • (1986) Polym Compos , vol.7 , Issue.3 , pp. 158-169
    • Seferis, J.C.1
  • 16
    • 0034883146 scopus 로고    scopus 로고
    • Blends and composites based on fluoropolymers
    • DOI 10.1002/1521-3900(200106)170:1<149::AID-MASY149>3.0.CO;2-J
    • J.G. Drobny Blends and composites based on fluoropolymers Macromol Symp 170 2001 149 156 (Pubitemid 32777304)
    • (2001) Macromolecular Symposia , vol.170 , pp. 149-156
    • Drobny, J.G.1
  • 18
    • 33947613153 scopus 로고    scopus 로고
    • Fluoropolymers in automotive applications
    • DOI 10.1002/pat.807
    • J.G. Drobny Fluoropolymers in automotive applications Polym Adv Technol 18 2 2007 117 121 (Pubitemid 46487340)
    • (2007) Polymers for Advanced Technologies , vol.18 , Issue.2 , pp. 117-121
    • Drobny, J.G.1
  • 19
    • 80052076670 scopus 로고    scopus 로고
    • Unplasticized copolymer tested for high temperature flexible lines
    • M. Hallberg Unplasticized copolymer tested for high temperature flexible lines Offshore 1999 1 4
    • (1999) Offshore , pp. 1-4
    • Hallberg, M.1
  • 20
    • 0028196316 scopus 로고
    • Fluorination of carbon-fibers by halogen fluorides
    • M. Zayat, D. Davidov, and H. Selig Fluorination of carbon-fibers by halogen fluorides Carbon 32 3 1994 485 491
    • (1994) Carbon , vol.32 , Issue.3 , pp. 485-491
    • Zayat, M.1    Davidov, D.2    Selig, H.3
  • 22
    • 0028484920 scopus 로고
    • Surface, interphase and composite property relations in fibre-reinforced polymers
    • E. Mäder, K. Grundke, H.J. Jacobasch, and G. Wachinger Surface, interphase and composite property relations in fibre-reinforced polymers Composites 25 7 1994 739 744
    • (1994) Composites , vol.25 , Issue.7 , pp. 739-744
    • Mäder, E.1    Grundke, K.2    Jacobasch, H.J.3    Wachinger, G.4
  • 24
    • 33748967925 scopus 로고    scopus 로고
    • Tactical planning of offshore petroleum production
    • DOI 10.1016/j.ejor.2005.06.060, PII S0377221705006363
    • N.L. Ulstein, B. Nygreen, and J.R. Sagli Tactical planning of offshore petroleum production Eur J Oper Res 176 1 2007 550 564 (Pubitemid 44442716)
    • (2007) European Journal of Operational Research , vol.176 , Issue.1 , pp. 550-564
    • Ulstein, N.L.1    Nygreen, B.2    Sagli, J.R.3
  • 26
    • 0347590920 scopus 로고    scopus 로고
    • Adhesion and friction behavior between fluorinated carbon fibers and poly (vinylidene fluoride)
    • A. Bismarck, and E. Schulz Adhesion and friction behavior between fluorinated carbon fibers and poly (vinylidene fluoride) J Mater Sci 38 24 2003 4965 4972
    • (2003) J Mater Sci , vol.38 , Issue.24 , pp. 4965-4972
    • Bismarck, A.1    Schulz, E.2
  • 27
    • 34548057304 scopus 로고    scopus 로고
    • Fluorinated carbon fibres and their suitability as reinforcement for fluoropolymers
    • DOI 10.1016/j.compscitech.2007.02.012, PII S0266353807000826
    • K.K.C. Ho, G. Kalinka, M.Q. Tran, N.V. Polyakova, and A. Bismarck Fluorinated carbon fibres and their suitability as reinforcement for fluoropolymers Compos Sci Technol 67 2007 2699 2706 (Pubitemid 47289216)
    • (2007) Composites Science and Technology , vol.67 , Issue.13 , pp. 2699-2706
    • Ho, K.K.C.1    Kalinka, G.2    Tran, M.Q.3    Polyakova, N.V.4    Bismarck, A.5
  • 28
    • 42249109987 scopus 로고    scopus 로고
    • Carbon fibre reinforced poly(vinylidene fluoride): Impact of matrix modification on fibre/polymer adhesion
    • M.Q. Tran, K.K.C. Ho, G. Kalinka, M.S.P. Shaffer, and A. Bismarck Carbon fibre reinforced poly(vinylidene fluoride): impact of matrix modification on fibre/polymer adhesion Compos Sci Technol 68 7-8 2008 1766 1776
    • (2008) Compos Sci Technol , vol.68 , Issue.78 , pp. 1766-1776
    • Tran, M.Q.1    Ho, K.K.C.2    Kalinka, G.3    Shaffer, M.S.P.4    Bismarck, A.5
  • 29
    • 33846517449 scopus 로고    scopus 로고
    • Fluorination of carbon fibres in atmospheric plasma
    • DOI 10.1016/j.carbon.2006.11.015, PII S0008622306005793
    • K.K.C. Ho, A.F. Lee, and A. Bismarck Fluorination of carbon fibres in atmospheric plasma Carbon 45 4 2007 775 784 (Pubitemid 46161433)
    • (2007) Carbon , vol.45 , Issue.4 , pp. 775-784
    • Ho, K.K.C.1    Lee, A.F.2    Bismarck, A.3
  • 30
    • 34547160249 scopus 로고    scopus 로고
    • Interfacial behavior between atmospheric-plasma-fluorinated carbon fibers and poly(vinylidene fluoride)
    • DOI 10.1016/j.jcis.2007.04.076, PII S0021979707005619
    • K.K.C. Ho, S. Lamoriniere, G. Kalinka, E. Schulz, and A. Bismarck Interfacial behavior between atmospheric-plasma-fluorinated carbon fibers and poly(vinylidene fluoride) J Colloid Interface Sci 313 2 2007 476 484 (Pubitemid 47126484)
    • (2007) Journal of Colloid and Interface Science , vol.313 , Issue.2 , pp. 476-484
    • Ho, K.K.C.1    Lamoriniere, S.2    Kalinka, G.3    Schulz, E.4    Bismarck, A.5
  • 32
    • 5244304624 scopus 로고    scopus 로고
    • Aqueous powder slurry manufacture of continuous fiber reinforced polyethylene composite
    • L.G. Tang, L. Li, X.S. Yi, and Z.R. Pan Aqueous powder slurry manufacture of continuous fiber reinforced polyethylene composite Polym Compos 18 2 1997 223 231 (Pubitemid 127602184)
    • (1997) Polymer Composites , vol.18 , Issue.2 , pp. 223-231
    • Tang, L.1    Li, L.2    Yi, X.3    Pan, Z.4
  • 33
    • 0042785641 scopus 로고    scopus 로고
    • Processing technologies for continuous fibre reinforced thermoplastics with novel polymer blends
    • DOI 10.1016/S0266-3538(03)00107-6
    • P. Mitschang, M. Blinzler, and A. Woginger Processing technologies for continuous fibre reinforced thermoplastics with novel polymer blends Compos Sci Technol 63 14 2003 2099 2110 (Pubitemid 37106184)
    • (2003) Composites Science and Technology , vol.63 , Issue.14 , pp. 2099-2110
    • Mitschang, P.1    Blinzler, M.2    Woginger, A.3
  • 34
    • 0027668582 scopus 로고
    • Manufacture of high performance fibre-reinforced thermoplastics by aqueous powder impregnation
    • A.M. Vodermayer, J.C. Kaerger, and G. Hinrichsen Manufacture of high performance fibre-reinforced thermoplastics by aqueous powder impregnation Compos Manuf 4 3 1993 123 132
    • (1993) Compos Manuf , vol.4 , Issue.3 , pp. 123-132
    • Vodermayer, A.M.1    Kaerger, J.C.2    Hinrichsen, G.3
  • 38
    • 79952533034 scopus 로고    scopus 로고
    • Wet impregnation as route to unidirectional carbon fibre reinforced thermoplastic composites manufacturing
    • doi:10.1179/1743289810Y.0000000022
    • Ho KKC, Shamsuddin SR, Riaz, S, Lamorinere S, Tran MQ, Javaid A, et al. Wet impregnation as route to unidirectional carbon fibre reinforced thermoplastic composites manufacturing. Plast Rubber Compos (2011). doi:10.1179/1743289810Y.0000000022.
    • (2011) Plast Rubber Compos
    • Ho, K.K.C.1    Shamsuddin, S.R.2    Riaz, S.3    Lamorinere, S.4    Tran, M.Q.5    Javaid, A.6
  • 40
    • 77955636068 scopus 로고    scopus 로고
    • Impact of in-line atmospheric plasma fluorination of carbon fibers on the performance of unidirectional, carbon fiber-reinforced polyvinylidene fluoride
    • S.R. Shamsuddin, K.K.C. Ho, S. Lamoriniere, A.F. Lee, and A. Bismarck Impact of in-line atmospheric plasma fluorination of carbon fibers on the performance of unidirectional, carbon fiber-reinforced polyvinylidene fluoride Adv Polym Technol 29 2 2010 86 97
    • (2010) Adv Polym Technol , vol.29 , Issue.2 , pp. 86-97
    • Shamsuddin, S.R.1    Ho, K.K.C.2    Lamoriniere, S.3    Lee, A.F.4    Bismarck, A.5
  • 45
    • 0001441436 scopus 로고
    • Rupture of rubber. I. Characteristic energy for tearing
    • R.S. Rivlin, and A.G. Thomas Rupture of rubber. I. Characteristic energy for tearing J Polym Sci 10 3 1953 291 318
    • (1953) J Polym Sci , vol.10 , Issue.3 , pp. 291-318
    • Rivlin, R.S.1    Thomas, A.G.2
  • 46
    • 0000971828 scopus 로고
    • Tear properties of vulcanizates containing carbon black
    • H.W. Greensmith Tear properties of vulcanizates containing carbon black J Polym Sci 21 98 1956 175 187
    • (1956) J Polym Sci , vol.21 , Issue.98 , pp. 175-187
    • Greensmith, H.W.1
  • 47
    • 39049128024 scopus 로고    scopus 로고
    • Fracture strength and adhesive strength of hydroxyapatite-filled polycaprolactone
    • DOI 10.1007/s10856-007-3016-7
    • S.C. Wong, and A. Baji Fracture strength and adhesive strength of hydroxyapatite-filled polycaprolactone J Mater Sci- Mater Med 19 2 2008 929 936 (Pubitemid 351244018)
    • (2008) Journal of Materials Science: Materials in Medicine , vol.19 , Issue.2 , pp. 929-936
    • Wong, S.-C.1    Baji, A.2
  • 48
    • 0032143206 scopus 로고    scopus 로고
    • Deformation rate dependence of the essential and non-essential work of fracture parameters in an amorphous copolyester
    • PII S0032386198000299
    • J. Karger-Kocsis, T. Czigany, and E.J. Moskala Deformation rate dependence of the essential and non-essential work of fracture parameters in an amorphous copolyester Polymer 39 17 1998 3939 3944 (Pubitemid 128369797)
    • (1998) Polymer , vol.39 , Issue.17 , pp. 3939-3944
    • Karger-Kocsis, J.1    Czigany, T.2    Moskala, E.J.3
  • 49
    • 0018058123 scopus 로고
    • Some observations on the tearing of ductile materials
    • DOI 10.1016/0013-7944(78)90042-5
    • D.P. Isherwood, and J.G. Williams Some observations on tearing of ductile materials Eng Fract Mech 10 4 1978 887 895 (Pubitemid 9390476)
    • (1978) Engineering Fracture Mechanics , vol.10 , Issue.4 , pp. 887-895
    • Isherwood, D.P.1    Williams, J.G.2
  • 51
    • 0028992508 scopus 로고
    • Interlaminar fracture-toughness of CFRP influenced by fibre surface-treatment. 1. Experimental results
    • H. Albertsen, J. Ivens, P. Peters, M. Wevers, and I. Verpoest Interlaminar fracture-toughness of CFRP influenced by fibre surface-treatment. 1. Experimental results Compos Sci Technol 54 2 1995 133 145
    • (1995) Compos Sci Technol , vol.54 , Issue.2 , pp. 133-145
    • Albertsen, H.1    Ivens, J.2    Peters, P.3    Wevers, M.4    Verpoest, I.5
  • 52
    • 0024903602 scopus 로고
    • Study of the delamination resistance of IM6/PEEK composites
    • DOI 10.1016/0266-3538(89)90085-7
    • P. Davies, W. Cantwell, C. Moulin, and H.H. Kausch A study of the delamination resistance of IM6/PEEK composites Compos Sci Technol 36 2 1989 153 166 (Pubitemid 20610108)
    • (1989) Composites Science and Technology , vol.36 , Issue.2 , pp. 153-166
    • Davies, P.1    Cantwell, W.2    Moulin, C.3    Kausch, H.H.4
  • 54
    • 0027693819 scopus 로고
    • Plane-stress fracture of polycarbonate films
    • S. Hashemi Plane-stress fracture of polycarbonate films J Mater Sci 28 22 1993 6178 6184
    • (1993) J Mater Sci , vol.28 , Issue.22 , pp. 6178-6184
    • Hashemi, S.1
  • 55
    • 77957578098 scopus 로고    scopus 로고
    • Application of the essential work of fracture (EWF) concept for polymers, related blends and composites: A review
    • T. Bárány, T. Czigány, and J. Karger-Kocsis Application of the essential work of fracture (EWF) concept for polymers, related blends and composites: a review Progress Polym Sci 35 10 2010 1257 1287
    • (2010) Progress Polym Sci , vol.35 , Issue.10 , pp. 1257-1287
    • Bárány, T.1    Czigány, T.2    Karger-Kocsis, J.3
  • 56
    • 41749115923 scopus 로고    scopus 로고
    • Fracture analysis of annealed PVDF films
    • G.M. Wallner, Z. Major, G.A. Maier, and R.W. Lang Fracture analysis of annealed PVDF films Polym Test 27 3 2008 392 402
    • (2008) Polym Test , vol.27 , Issue.3 , pp. 392-402
    • Wallner, G.M.1    Major, Z.2    Maier, G.A.3    Lang, R.W.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.