Volumn 27, Issue 3, 2008, Pages 392-402

Fracture analysis of annealed PVDF films

Author keywords

Annealing; Film; Fracture; PVDF

Indexed keywords

ANNEALING; CAVITATION; DIFFERENTIAL SCANNING CALORIMETRY; FLUORINE CONTAINING POLYMERS; MECHANICAL TESTING; MICROMECHANICS; PHASE TRANSITIONS;

EID: 41749115923     PISSN: 01429418     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.polymertesting.2008.01.006     Document Type: Article
Times cited : (30)

References (33)
  • 1
    • 0004729421 scopus 로고
    • Poly(vinylidene fluoride)
    • Kraschwitz J.I., and Howe-Grant M. (Eds), Wiley, New York
    • Dohany J.E. Poly(vinylidene fluoride). In: Kraschwitz J.I., and Howe-Grant M. (Eds). KIRK-OTHMER Encyclopedia of Chemical Technology vol. 11 (1994), Wiley, New York
    • (1994) KIRK-OTHMER Encyclopedia of Chemical Technology , vol.11
    • Dohany, J.E.1
  • 2
    • 23944468509 scopus 로고    scopus 로고
    • On the strain-induced crystalline phase changes in semi-crystalline polymers: mechanisms and incidence on the mechanical properties
    • Seguela R. On the strain-induced crystalline phase changes in semi-crystalline polymers: mechanisms and incidence on the mechanical properties. J. Macromol. Sci. Rev. C 45 (2005) 263-287
    • (2005) J. Macromol. Sci. Rev. C , vol.45 , pp. 263-287
    • Seguela, R.1
  • 3
    • 0024016509 scopus 로고
    • Deformation of semicrystalline polymers via crystal-crystal phase transition
    • Saraf R.F., and Porter R.S. Deformation of semicrystalline polymers via crystal-crystal phase transition. J. Polym. Sci. Phys. B 26 (1988) 1049-1057
    • (1988) J. Polym. Sci. Phys. B , vol.26 , pp. 1049-1057
    • Saraf, R.F.1    Porter, R.S.2
  • 4
    • 0024641242 scopus 로고
    • Deformation and transformation mechanisms of poly(vinylidene fluoride) (PVF2)
    • Hsu T.-C., and Geil P.H. Deformation and transformation mechanisms of poly(vinylidene fluoride) (PVF2). J. Mater. Sci. 24 (1989) 1219-1232
    • (1989) J. Mater. Sci. , vol.24 , pp. 1219-1232
    • Hsu, T.-C.1    Geil, P.H.2
  • 5
    • 0011398361 scopus 로고
    • On the α→β transition by deformation of highly oriented poly(vinylidene fluoride)
    • Yang D.C., and Thomas E.L. On the α→β transition by deformation of highly oriented poly(vinylidene fluoride). J. Mater. Sci. Lett. 3 (1984) 929-936
    • (1984) J. Mater. Sci. Lett. , vol.3 , pp. 929-936
    • Yang, D.C.1    Thomas, E.L.2
  • 6
    • 0019242329 scopus 로고
    • II-I crystal transformation of poly(vinylidene fluoride) under tensile and compressional stresses
    • Matsushige K., Nagata K., Imada S., and Takemura T. II-I crystal transformation of poly(vinylidene fluoride) under tensile and compressional stresses. Polymer 21 (1980) 1391-1397
    • (1980) Polymer , vol.21 , pp. 1391-1397
    • Matsushige, K.1    Nagata, K.2    Imada, S.3    Takemura, T.4
  • 7
    • 0343193254 scopus 로고    scopus 로고
    • Cavitation in strained polyvinylidene fluoride: mechanical and X-ray experimental studies
    • Castagnet S., Girault S., Gacougnolle J.L., and Dang P. Cavitation in strained polyvinylidene fluoride: mechanical and X-ray experimental studies. Polymer 41 (2000) 7523-7530
    • (2000) Polymer , vol.41 , pp. 7523-7530
    • Castagnet, S.1    Girault, S.2    Gacougnolle, J.L.3    Dang, P.4
  • 8
    • 0142089087 scopus 로고    scopus 로고
    • Role of the entangled amorphous network in tensile deformation of semicrystalline polymers
    • Men Y., Rieger J., and Strobl G. Role of the entangled amorphous network in tensile deformation of semicrystalline polymers. Phys. Rev. Lett. 91 (2003) 955021-955024
    • (2003) Phys. Rev. Lett. , vol.91 , pp. 955021-955024
    • Men, Y.1    Rieger, J.2    Strobl, G.3
  • 9
    • 22944466657 scopus 로고    scopus 로고
    • Structural changes during plastic deformation at crack tips in PVDF films: a scanning X-ray scattering study
    • Maier G.A., Wallner G.M., Lang R.W., and Fratzl P. Structural changes during plastic deformation at crack tips in PVDF films: a scanning X-ray scattering study. Macromolecules 38 (2005) 6099-6105
    • (2005) Macromolecules , vol.38 , pp. 6099-6105
    • Maier, G.A.1    Wallner, G.M.2    Lang, R.W.3    Fratzl, P.4
  • 10
    • 34248393578 scopus 로고    scopus 로고
    • Fracture of poly(vinylidene fluoride): a combined synchrotron and laboratory in-situ X-ray scattering study
    • Maier G.A., Keckes J., Wallner G.M., Lang R.W., Armenitsch H., and Fratzl P. Fracture of poly(vinylidene fluoride): a combined synchrotron and laboratory in-situ X-ray scattering study. J. Appl. Crystallogr. 40 (2007) s564-s567
    • (2007) J. Appl. Crystallogr. , vol.40
    • Maier, G.A.1    Keckes, J.2    Wallner, G.M.3    Lang, R.W.4    Armenitsch, H.5    Fratzl, P.6
  • 11
    • 0031102306 scopus 로고    scopus 로고
    • Fracture toughness evaluation of ductile polymeric films
    • Hashemi S.J. Fracture toughness evaluation of ductile polymeric films. J. Mater. Sci. 32 (1997) 1563-1573
    • (1997) J. Mater. Sci. , vol.32 , pp. 1563-1573
    • Hashemi, S.J.1
  • 12
    • 0030230795 scopus 로고    scopus 로고
    • The essential fracture work concept for toughness measurement of ductile polymers
    • Wu J., and Mai Y.W. The essential fracture work concept for toughness measurement of ductile polymers. Polym. Eng. Sci. 36 (1996) 2275-2288
    • (1996) Polym. Eng. Sci. , vol.36 , pp. 2275-2288
    • Wu, J.1    Mai, Y.W.2
  • 13
    • 0031238385 scopus 로고    scopus 로고
    • Thickness dependence of work of fracture parameters of an amorphous copolyester
    • Karger-Kocsis J., Czigany T., and Moskala E.J. Thickness dependence of work of fracture parameters of an amorphous copolyester. Polymer 38 (1997) 4587-4593
    • (1997) Polymer , vol.38 , pp. 4587-4593
    • Karger-Kocsis, J.1    Czigany, T.2    Moskala, E.J.3
  • 14
    • 0033310790 scopus 로고    scopus 로고
    • Factors affecting work of fracture of uPVC film
    • Arkhireyeva A., Hashemi S., and O′Brien M. Factors affecting work of fracture of uPVC film. J. Mater. Sci. 34 (1999) 5961-5974
    • (1999) J. Mater. Sci. , vol.34 , pp. 5961-5974
    • Arkhireyeva, A.1    Hashemi, S.2    OBrien, M.3
  • 15
    • 0000368803 scopus 로고    scopus 로고
    • On the essential work of fracture method: energy partitioning of the fracture process in iPP films
    • Ferrer-Balas D., Maspoch M.L., Martinez A.B., and Santana O.O. On the essential work of fracture method: energy partitioning of the fracture process in iPP films. Polym. Bull. 42 (1999) 101-108
    • (1999) Polym. Bull. , vol.42 , pp. 101-108
    • Ferrer-Balas, D.1    Maspoch, M.L.2    Martinez, A.B.3    Santana, O.O.4
  • 16
    • 0034487609 scopus 로고    scopus 로고
    • Effect of strain rate on the fracture toughness of some ductile polymers using the essential work of fracture (EWF) approach
    • Ching E.C.Y., Poon W.K.Y., Li R.K.Y., and Mai Y.W. Effect of strain rate on the fracture toughness of some ductile polymers using the essential work of fracture (EWF) approach. Polym. Eng. Sci. 40 (2000) 2558-2568
    • (2000) Polym. Eng. Sci. , vol.40 , pp. 2558-2568
    • Ching, E.C.Y.1    Poon, W.K.Y.2    Li, R.K.Y.3    Mai, Y.W.4
  • 17
    • 0030736321 scopus 로고    scopus 로고
    • Hybrid effects on mechanical properties of polyoxymethylene
    • Hashemi S., Elmes P., and Sandford S. Hybrid effects on mechanical properties of polyoxymethylene. Polym. Eng. Sci. 37 (1997) 45-58
    • (1997) Polym. Eng. Sci. , vol.37 , pp. 45-58
    • Hashemi, S.1    Elmes, P.2    Sandford, S.3
  • 18
    • 0041379171 scopus 로고    scopus 로고
    • Work of fracture of high impact polystyrene (HIPS) film under plane stress conditions
    • Hashemi S. Work of fracture of high impact polystyrene (HIPS) film under plane stress conditions. J. Mater. Sci. 38 (2003) 3055-3062
    • (2003) J. Mater. Sci. , vol.38 , pp. 3055-3062
    • Hashemi, S.1
  • 19
    • 0025383435 scopus 로고
    • Plane-strain essential work of fracture as a measure of the fracture toughness of ductile polymers
    • Saleemi A.S., and Nairn J.A. Plane-strain essential work of fracture as a measure of the fracture toughness of ductile polymers. Polym. Eng. Sci. 30 (1990) 211-218
    • (1990) Polym. Eng. Sci. , vol.30 , pp. 211-218
    • Saleemi, A.S.1    Nairn, J.A.2
  • 20
    • 0343627987 scopus 로고    scopus 로고
    • Relationship between morphology and mechanical properties of polypropylene/ethene-co-butene binary blends with various butene contents
    • Mouzakis D.E., Mäder D., Mülhaupt R., and Kager-Kocsis J. Relationship between morphology and mechanical properties of polypropylene/ethene-co-butene binary blends with various butene contents. J. Mater. Sci. 35 (2000) 1219-1230
    • (2000) J. Mater. Sci. , vol.35 , pp. 1219-1230
    • Mouzakis, D.E.1    Mäder, D.2    Mülhaupt, R.3    Kager-Kocsis, J.4
  • 21
    • 0037474734 scopus 로고    scopus 로고
    • Radiation induced embrittlement of PTFE
    • Fayolle B., Audouin L., and Verdu J. Radiation induced embrittlement of PTFE. Polymer 44 (2003) 2773-2780
    • (2003) Polymer , vol.44 , pp. 2773-2780
    • Fayolle, B.1    Audouin, L.2    Verdu, J.3
  • 22
    • 4043140773 scopus 로고    scopus 로고
    • Polyolefin nanocomposites: essential work of fracture analysis
    • Bureau M.N., Perrin-Sarazin F., and Ton-That M.T. Polyolefin nanocomposites: essential work of fracture analysis. Polym. Eng. Sci. 44 (2004) 1142-1151
    • (2004) Polym. Eng. Sci. , vol.44 , pp. 1142-1151
    • Bureau, M.N.1    Perrin-Sarazin, F.2    Ton-That, M.T.3
  • 23
    • 0031599028 scopus 로고    scopus 로고
    • Using essential work of fracture method for studying physical aging in thin ductile, polymeric films
    • Liu C.H., and Nairn J.A. Using essential work of fracture method for studying physical aging in thin ductile, polymeric films. Polym. Eng. Sci. 38 (1998) 186-193
    • (1998) Polym. Eng. Sci. , vol.38 , pp. 186-193
    • Liu, C.H.1    Nairn, J.A.2
  • 24
    • 0034138573 scopus 로고    scopus 로고
    • Influence of annealing on the microstructural tensile and fracture properties of polypropylene films
    • Ferrer-Balas D., Maspoch M.L., Martinez A.B., and Santana O.O. Influence of annealing on the microstructural tensile and fracture properties of polypropylene films. Polymer 42 (2004) 1697-1705
    • (2004) Polymer , vol.42 , pp. 1697-1705
    • Ferrer-Balas, D.1    Maspoch, M.L.2    Martinez, A.B.3    Santana, O.O.4
  • 25
    • 0042882323 scopus 로고    scopus 로고
    • Plane stress fracture toughness of physically aged plasticized PETG as assessed by the essential work of fracture (EWF) method
    • Karger-Kocsis J., Barany T., and Moskala E.J. Plane stress fracture toughness of physically aged plasticized PETG as assessed by the essential work of fracture (EWF) method. Polymer 44 (2003) 5691-5699
    • (2003) Polymer , vol.44 , pp. 5691-5699
    • Karger-Kocsis, J.1    Barany, T.2    Moskala, E.J.3
  • 26
    • 33846012230 scopus 로고    scopus 로고
    • Influence of annealing on the fracture behaviour of 200 μm thick α-PVDF films
    • Wallner G.M., Major Z., Maier G., and Lang R.W. Influence of annealing on the fracture behaviour of 200 μm thick α-PVDF films. Adv. Eng. Mater. 8 (2006) 1140-1145
    • (2006) Adv. Eng. Mater. , vol.8 , pp. 1140-1145
    • Wallner, G.M.1    Major, Z.2    Maier, G.3    Lang, R.W.4
  • 27
    • 41749119735 scopus 로고    scopus 로고
    • E. Clutton, Testing protocol for essential work of fracture, ESIS-TC4, 1997.
    • E. Clutton, Testing protocol for essential work of fracture, ESIS-TC4, 1997.
  • 28
    • 0343826837 scopus 로고    scopus 로고
    • Essential work of fracture on PET films: influence of the thickness and the orientation
    • Maspoch M.L., Henault V., Ferrer-Balas D., Velasco J.I., and Santana O.O. Essential work of fracture on PET films: influence of the thickness and the orientation. Polym. Test. 19 (2000) 559-568
    • (2000) Polym. Test. , vol.19 , pp. 559-568
    • Maspoch, M.L.1    Henault, V.2    Ferrer-Balas, D.3    Velasco, J.I.4    Santana, O.O.5
  • 29
    • 0003372790 scopus 로고
    • Crystal melting
    • Academic Press, New York
    • Wunderlich B. Crystal melting. Macromolecular Physics vol. 3 (1980), Academic Press, New York
    • (1980) Macromolecular Physics , vol.3
    • Wunderlich, B.1
  • 30
    • 0038825112 scopus 로고    scopus 로고
    • Influence of annealing and chain defects on the melting behaviour of poly(vinylidene fluoride)
    • Marega C., and Marigo A. Influence of annealing and chain defects on the melting behaviour of poly(vinylidene fluoride). Eur. Polym. J. 38 (2003) 1713-1720
    • (2003) Eur. Polym. J. , vol.38 , pp. 1713-1720
    • Marega, C.1    Marigo, A.2
  • 31
    • 0033750932 scopus 로고    scopus 로고
    • Influence of structural and topological constraints on the crystallization and melting behavior of polymers. 2. Poly(arylene ether ether ketone)
    • Marand H., Alizadeh A., Farmer R., Desai R., and Velikov V. Influence of structural and topological constraints on the crystallization and melting behavior of polymers. 2. Poly(arylene ether ether ketone). Macromolecules 33 (2000) 3392-3403
    • (2000) Macromolecules , vol.33 , pp. 3392-3403
    • Marand, H.1    Alizadeh, A.2    Farmer, R.3    Desai, R.4    Velikov, V.5
  • 32
    • 0842328669 scopus 로고    scopus 로고
    • Structural evolution of PVDF during storage or annealing
    • Neidhöfer M., Beaume F., Ibos L., Bernes A., and Lacabanne C. Structural evolution of PVDF during storage or annealing. Polymer 45 (2004) 1679-1688
    • (2004) Polymer , vol.45 , pp. 1679-1688
    • Neidhöfer, M.1    Beaume, F.2    Ibos, L.3    Bernes, A.4    Lacabanne, C.5
  • 33
    • 27144449674 scopus 로고    scopus 로고
    • Damage and fracture of polyvinylidene fluoride (PVDF) at 20 °C: experiments and modelling
    • Challier M., Besson J., Laiarinandrasana L., and Piques R. Damage and fracture of polyvinylidene fluoride (PVDF) at 20 °C: experiments and modelling. Eng. Fract. Mech. 73 (2006) 79-90
    • (2006) Eng. Fract. Mech. , vol.73 , pp. 79-90
    • Challier, M.1    Besson, J.2    Laiarinandrasana, L.3    Piques, R.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.