2
-
-
0025106024
-
Galvanic corrosion of lead solder in copper pipework
-
Gregory R. Galvanic corrosion of lead solder in copper pipework. Water Environ. J. 1990, 4:112-118.
-
(1990)
Water Environ. J.
, vol.4
, pp. 112-118
-
-
Gregory, R.1
-
3
-
-
0032678525
-
Desktop guidance for mitigating Pb and Cu corrosion by-products
-
Edwards M., Jacobs S., Dodrill D. Desktop guidance for mitigating Pb and Cu corrosion by-products. J. Am. Water Works Assoc. 1999, 91:66-77.
-
(1999)
J. Am. Water Works Assoc.
, vol.91
, pp. 66-77
-
-
Edwards, M.1
Jacobs, S.2
Dodrill, D.3
-
4
-
-
79960278067
-
-
Role of chloride, sulfate, and alkalinity on galvanic lead corrosion, Corrosion, accepted for publication.
-
C.K. Nguyen, B.N. Clark, K.R. Stone, M.A. Edwards, Role of chloride, sulfate, and alkalinity on galvanic lead corrosion, Corrosion (2011), accepted for publication.
-
(2011)
-
-
Nguyen, C.K.1
Clark, B.N.2
Stone, K.R.3
Edwards, M.A.4
-
5
-
-
34547401015
-
Chloride-to-sulfate mass ratio and lead leaching to water
-
Edwards M., Triantafyllidou S. Chloride-to-sulfate mass ratio and lead leaching to water. J. Am. Water Works Assoc. 2007, 99:96-109.
-
(2007)
J. Am. Water Works Assoc.
, vol.99
, pp. 96-109
-
-
Edwards, M.1
Triantafyllidou, S.2
-
6
-
-
64349117395
-
Elevated blood lead in young children due to lead-contaminated drinking water: Washington, DC, 2001-2004
-
Edwards M., Triantafyllidou S., Best D. Elevated blood lead in young children due to lead-contaminated drinking water: Washington, DC, 2001-2004. Environ. Sci. Technol. 2009, 43:1618-1623.
-
(2009)
Environ. Sci. Technol.
, vol.43
, pp. 1618-1623
-
-
Edwards, M.1
Triantafyllidou, S.2
Best, D.3
-
7
-
-
65549102908
-
Mapping out lead's legacy
-
Renner R. Mapping out lead's legacy. Environ. Sci. Technol. 2009, 43:1655-1658.
-
(2009)
Environ. Sci. Technol.
, vol.43
, pp. 1655-1658
-
-
Renner, R.1
-
8
-
-
33847061841
-
Lead in water linked to coagulant
-
Renner R. Lead in water linked to coagulant. Environ. Sci. Technol. 2006, 40:5164-5168.
-
(2006)
Environ. Sci. Technol.
, vol.40
, pp. 5164-5168
-
-
Renner, R.1
-
9
-
-
77956556553
-
Corrosive microenvironments at lead solder surfaces arising from galvanic corrosion with copper pipe
-
Nguyen C.K., Stone K.R., Dudi A., Edwards M.A. Corrosive microenvironments at lead solder surfaces arising from galvanic corrosion with copper pipe. Environ. Sci. Technol. 2010, 44:7076-7081.
-
(2010)
Environ. Sci. Technol.
, vol.44
, pp. 7076-7081
-
-
Nguyen, C.K.1
Stone, K.R.2
Dudi, A.3
Edwards, M.A.4
-
10
-
-
24344453282
-
-
Department of Civil and Environmental Engineering, Virginia Tech, Blacksburg, VA
-
Dudi A. Reconsidering Lead Corrosion in Drinking Water: Product Testing, Direct Chloramines Attack and Galvanic Corrosion 2004, Department of Civil and Environmental Engineering, Virginia Tech, Blacksburg, VA.
-
(2004)
Reconsidering Lead Corrosion in Drinking Water: Product Testing, Direct Chloramines Attack and Galvanic Corrosion
-
-
Dudi, A.1
-
11
-
-
0002892192
-
Corrosion control on the basis of utility experience
-
Dodrill D.M., Edwards M. Corrosion control on the basis of utility experience. J. Am. Water Works Assoc. 1995, 87:74-85.
-
(1995)
J. Am. Water Works Assoc.
, vol.87
, pp. 74-85
-
-
Dodrill, D.M.1
Edwards, M.2
-
12
-
-
0030615596
-
Lead corrosion control from lead, copper-lead solder, and brass coupons in drinking water employing free and combined chlorine
-
Lin N.H., Torrents A., Davis A.P., Zeinali M., Taylor F.A. Lead corrosion control from lead, copper-lead solder, and brass coupons in drinking water employing free and combined chlorine. J. Environ. Sci. Health A 1997, 32:865-884.
-
(1997)
J. Environ. Sci. Health A
, vol.32
, pp. 865-884
-
-
Lin, N.H.1
Torrents, A.2
Davis, A.P.3
Zeinali, M.4
Taylor, F.A.5
-
13
-
-
0024698702
-
Understanding corrosion control strategies for lead
-
Schock M.R. Understanding corrosion control strategies for lead. J. Am. Water Works Assoc. 1989, 81:88-100.
-
(1989)
J. Am. Water Works Assoc.
, vol.81
, pp. 88-100
-
-
Schock, M.R.1
-
14
-
-
0015628301
-
Corrosion-resistant lead-indium and lead-tin alloys: surface studies by photo-electron spectroscopy (ESCA)
-
Bird R.J. Corrosion-resistant lead-indium and lead-tin alloys: surface studies by photo-electron spectroscopy (ESCA). Metal Sci. 1973, 7:109-113.
-
(1973)
Metal Sci.
, vol.7
, pp. 109-113
-
-
Bird, R.J.1
-
15
-
-
0019080036
-
AES study of tin-lead alloys: effects of ion sputtering and oxidation on surface composition and structure
-
Frankenthal R.P., Siconolfi D.J. AES study of tin-lead alloys: effects of ion sputtering and oxidation on surface composition and structure. J. Vac. Sci. Technol. 1980, 17:1315-1319.
-
(1980)
J. Vac. Sci. Technol.
, vol.17
, pp. 1315-1319
-
-
Frankenthal, R.P.1
Siconolfi, D.J.2
-
17
-
-
0005812205
-
-
National Risk Management Research Laboratory, Office of Research and Development, Cincinnati, OH
-
Lytle D., Schock M. Stagnation Time, Composition, pH and Orthophosphate Effects on Metal Leaching from Brass 1996, National Risk Management Research Laboratory, Office of Research and Development, Cincinnati, OH.
-
(1996)
Stagnation Time, Composition, pH and Orthophosphate Effects on Metal Leaching from Brass
-
-
Lytle, D.1
Schock, M.2
-
18
-
-
0026376579
-
Control of lead corrosion by chemical treatment
-
Boffardi B.P., Sherbondy A.M. Control of lead corrosion by chemical treatment. Corrosion 1991, 47:966-975.
-
(1991)
Corrosion
, vol.47
, pp. 966-975
-
-
Boffardi, B.P.1
Sherbondy, A.M.2
-
21
-
-
0026080350
-
Electrochemical behaviour of tin in bicarbonate solution at pH 8
-
Drogowska M., Ménard H., Brossard L. Electrochemical behaviour of tin in bicarbonate solution at pH 8. J. Appl. Electrochem. 1991, 21:84-90.
-
(1991)
J. Appl. Electrochem.
, vol.21
, pp. 84-90
-
-
Drogowska, M.1
Ménard, H.2
Brossard, L.3
-
22
-
-
25744461374
-
The divalency of tin ions formed during anodic dissolution and the behavior of the tin anode
-
Straumanis M.E., Dutta M. The divalency of tin ions formed during anodic dissolution and the behavior of the tin anode. Inorgan. Chem. 1966, 5:992-995.
-
(1966)
Inorgan. Chem.
, vol.5
, pp. 992-995
-
-
Straumanis, M.E.1
Dutta, M.2
-
24
-
-
49849119165
-
Behaviour of tin as metal-metal phosphate electrode and mechanism of promotion and inhibition of its corrosion by phosphate ions
-
Awad S.A., Kassab A. Behaviour of tin as metal-metal phosphate electrode and mechanism of promotion and inhibition of its corrosion by phosphate ions. J. Electroanal. Chem. 1969, 20:203-212.
-
(1969)
J. Electroanal. Chem.
, vol.20
, pp. 203-212
-
-
Awad, S.A.1
Kassab, A.2
-
25
-
-
0034536873
-
Formation equilibria of tin(II) orthophosphate complexes
-
Ciavatta L., Iuliano M. Formation equilibria of tin(II) orthophosphate complexes. Polyhedron 2000, 19:2403-2407.
-
(2000)
Polyhedron
, vol.19
, pp. 2403-2407
-
-
Ciavatta, L.1
Iuliano, M.2
-
26
-
-
0034771021
-
A critical review of thermodynamic data for inorganic tin species
-
Séby F., Potin-Gautier M., Giffaut E., Donard O.F.X. A critical review of thermodynamic data for inorganic tin species. Geochim. Cosmochim. Acta 2001, 65:3041-3053.
-
(2001)
Geochim. Cosmochim. Acta
, vol.65
, pp. 3041-3053
-
-
Séby, F.1
Potin-Gautier, M.2
Giffaut, E.3
Donard, O.F.X.4
-
27
-
-
0018310179
-
Anodic behaviour of tin in neutral phosphate solution
-
Do Duc H., Tissot P. Anodic behaviour of tin in neutral phosphate solution. Corros. Sci. 1979, 19:179-190.
-
(1979)
Corros. Sci.
, vol.19
, pp. 179-190
-
-
Do Duc, H.1
Tissot, P.2
-
28
-
-
0018297660
-
Rotating disc and ring disc electrode studies of tin in neutral phosphate solution
-
Do Duc H., Tissot P. Rotating disc and ring disc electrode studies of tin in neutral phosphate solution. Corros. Sci. 1979, 19:191-197.
-
(1979)
Corros. Sci.
, vol.19
, pp. 191-197
-
-
Do Duc, H.1
Tissot, P.2
-
29
-
-
0036138681
-
Potentiodynamic behaviour of tin in different buffer solutions
-
Alvarez P.E., Ribotta S.B., Folquer M.E., Gervasi C.A., Vilche J.R. Potentiodynamic behaviour of tin in different buffer solutions. Corros. Sci. 2002, 44:49-65.
-
(2002)
Corros. Sci.
, vol.44
, pp. 49-65
-
-
Alvarez, P.E.1
Ribotta, S.B.2
Folquer, M.E.3
Gervasi, C.A.4
Vilche, J.R.5
-
30
-
-
79951809593
-
Chloride-to-sulfate mass ratio: practical studies in lead solder galvanic corrosion
-
Nguyen C.K., Stone K.R., Edwards M.A. Chloride-to-sulfate mass ratio: practical studies in lead solder galvanic corrosion. J. Am. Water Works Assoc. 2011, 103:81-92.
-
(2011)
J. Am. Water Works Assoc.
, vol.103
, pp. 81-92
-
-
Nguyen, C.K.1
Stone, K.R.2
Edwards, M.A.3
-
31
-
-
0003425384
-
-
American Public Health Association (APHA), APHA, American Water Works Association, and Water Environment Federation, Washington, DC
-
Standard Methods for the Examination of Water and Wastewater 1998, American Public Health Association (APHA), APHA, American Water Works Association, and Water Environment Federation, Washington, DC. 20th ed.
-
(1998)
Standard Methods for the Examination of Water and Wastewater
-
-
-
32
-
-
79951809364
-
-
ASTM Standard G71-81, Standard Guide for Conducting and Evaluating Galvanic Corrosion Tests in Electrolytes, ASTM International, West Conshohocken, PA,
-
ASTM Standard G71-81, Standard Guide for Conducting and Evaluating Galvanic Corrosion Tests in Electrolytes, ASTM International, West Conshohocken, PA, 2009.
-
(2009)
-
-
-
33
-
-
69049106365
-
Generation of tin(II) oxide crystals on lead-free solder joints in deionized water
-
Chang H., Chen H., Li M., Wang L., Fu Y. Generation of tin(II) oxide crystals on lead-free solder joints in deionized water. J. Electron. Mater. 2009, 38:2170-2178.
-
(2009)
J. Electron. Mater.
, vol.38
, pp. 2170-2178
-
-
Chang, H.1
Chen, H.2
Li, M.3
Wang, L.4
Fu, Y.5
-
34
-
-
79951809097
-
-
Water Research Foundation and U.S. Environmental Protection Agency, Denver, CO
-
Nguyen C.K., Stone K.R., Clark B., Gagnon G., Knowles A., Edwards M.A. Impact of Chloride:Sulfate Mass Ratio Changes on Lead Leaching in Potable Water 2010, Water Research Foundation and U.S. Environmental Protection Agency, Denver, CO.
-
(2010)
Impact of Chloride:Sulfate Mass Ratio Changes on Lead Leaching in Potable Water
-
-
Nguyen, C.K.1
Stone, K.R.2
Clark, B.3
Gagnon, G.4
Knowles, A.5
Edwards, M.A.6
|