Volumn 31, Issue 5, 2011, Pages 877-882

Effect of MoSi2 content on the lubricated sliding-wear resistance of ZrC-MoSi2 composites

Author keywords

Contact mechanical properties; Sliding wear; Tribology; ZrC

Indexed keywords

CONTACT-MECHANICAL PROPERTIES; ELECTRICAL CONTACTS; GRAIN PULLOUT; MECHANISTIC MODELS; MILD WEAR; ROOM TEMPERATURE; SINTERING ADDITIVES; SLIDING WEAR; SPEED-UPS; TRIBOLOGICAL APPLICATIONS; WEAR RESISTANT; ZRC;

EID: 78751567957     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2010.11.017     Document Type: Article
Times cited : (25)

References (23)
  • 1
    • 76049100313 scopus 로고    scopus 로고
    • UHTCs: ultra-high temperature ceramic materials for extreme environment applications
    • WINTER
    • Wuchina E., Opila E., Opeka M., Fahrenholtz W., Talmy I. UHTCs: ultra-high temperature ceramic materials for extreme environment applications. Electrochem Soc Interface 2007, (Winter):30-36.
    • (2007) Electrochem Soc Interface , pp. 30-36
    • Wuchina, E.1    Opila, E.2    Opeka, M.3    Fahrenholtz, W.4    Talmy, I.5
  • 2
    • 0001426016 scopus 로고
    • Engineering properties of carbides
    • ASM International, Materials Park, OH
    • Shaffer P.T.B. Engineering properties of carbides. Ceramics and glasses: engineered materials handbook 1991, vol. 4:804-811. ASM International, Materials Park, OH.
    • (1991) Ceramics and glasses: engineered materials handbook , vol.4 , pp. 804-811
    • Shaffer, P.T.B.1
  • 3
    • 33846372666 scopus 로고    scopus 로고
    • Evolution of structure during the oxidation of zirconium diboride-silicon carbide in air up to 1500°C
    • Rezaie A., Fahrenholtz W.G., Hilmas G.E. Evolution of structure during the oxidation of zirconium diboride-silicon carbide in air up to 1500°C. J Eur Ceram Soc 2007, 27(6):2495-2501.
    • (2007) J Eur Ceram Soc , vol.27 , Issue.6 , pp. 2495-2501
    • Rezaie, A.1    Fahrenholtz, W.G.2    Hilmas, G.E.3
  • 4
    • 0003749418 scopus 로고
    • Cambridge University Press, Cambridge, UK
    • Lawn B.R. Fracture of brittle solids 1993, Cambridge University Press, Cambridge, UK. 2nd ed.
    • (1993) Fracture of brittle solids
    • Lawn, B.R.1
  • 5
    • 84987335986 scopus 로고
    • A critical evaluation of indentation techniques for measuring fracture toughness: I. Direct crack measurements
    • Anstis G.R., Chantikul P., Marshall D.B., Lawn B.R. A critical evaluation of indentation techniques for measuring fracture toughness: I. Direct crack measurements. J Am Ceram Soc 1981, 64(9):533-538.
    • (1981) J Am Ceram Soc , vol.64 , Issue.9 , pp. 533-538
    • Anstis, G.R.1    Chantikul, P.2    Marshall, D.B.3    Lawn, B.R.4
  • 6
    • 53349103178 scopus 로고    scopus 로고
    • Microstructure and mechanical characterization of ZrC-Mo cermets produced by hot isostatic pressing
    • Landwehr S.E., Hilmas G.E., Fahrenholtz W.G., Talmy I.G., DiPietro S.G. Microstructure and mechanical characterization of ZrC-Mo cermets produced by hot isostatic pressing. Mater Sci Eng A 2008, 497(1-2):79-86.
    • (2008) Mater Sci Eng A , vol.497 , Issue.1-2 , pp. 79-86
    • Landwehr, S.E.1    Hilmas, G.E.2    Fahrenholtz, W.G.3    Talmy, I.G.4    DiPietro, S.G.5
  • 9
    • 33845945316 scopus 로고
    • The deformation and ageing of mild steel. 3. Discussion of results
    • Hall E.O. The deformation and ageing of mild steel. 3. Discussion of results. Proc Phys Soc London Sect B 1951, 64(381):747-753.
    • (1951) Proc Phys Soc London Sect B , vol.64 , Issue.381 , pp. 747-753
    • Hall, E.O.1
  • 10
    • 0002228943 scopus 로고
    • The cleavage strength of polycrystals
    • Petch N.J. The cleavage strength of polycrystals. J Iron Steel Inst London 1953, 174(1):25-28.
    • (1953) J Iron Steel Inst London , vol.174 , Issue.1 , pp. 25-28
    • Petch, N.J.1
  • 11
    • 0027663584 scopus 로고
    • Model for toughness curves in two-phase ceramics: I. Basic fracture mechanics
    • Lawn B.R., Padture N.P., Braun L.M., Bennison S.J. Model for toughness curves in two-phase ceramics: I. Basic fracture mechanics. J Am Ceram Soc 1993, 76(9):2235-2240.
    • (1993) J Am Ceram Soc , vol.76 , Issue.9 , pp. 2235-2240
    • Lawn, B.R.1    Padture, N.P.2    Braun, L.M.3    Bennison, S.J.4
  • 12
    • 0027658716 scopus 로고
    • Model for toughness curves in two-phase ceramics: II. Microstructural variables
    • Padture N.P., Runyan J.L., Bennison S.J., Braun L.M., Lawn B.R. Model for toughness curves in two-phase ceramics: II. Microstructural variables. J Am Ceram Soc 1993, 76(9):2241-2247.
    • (1993) J Am Ceram Soc , vol.76 , Issue.9 , pp. 2241-2247
    • Padture, N.P.1    Runyan, J.L.2    Bennison, S.J.3    Braun, L.M.4    Lawn, B.R.5
  • 14
    • 33846351913 scopus 로고
    • Grain-size and R curve effects in the abrasive wear of alumina
    • Cho S.-J., Hockey B.J., Lawn B.R., Bennison S.J. Grain-size and R curve effects in the abrasive wear of alumina. J Am Ceram Soc 1989, 72(7):1249-1252.
    • (1989) J Am Ceram Soc , vol.72 , Issue.7 , pp. 1249-1252
    • Cho, S.-J.1    Hockey, B.J.2    Lawn, B.R.3    Bennison, S.J.4
  • 15
    • 44049121717 scopus 로고
    • The transition from mild to severe wear in alumina during sliding
    • Cho S.-J., Moon H., Hockey B.J., Hsu S.M. The transition from mild to severe wear in alumina during sliding. Acta Metall Mater 1992, 40(1):185-192.
    • (1992) Acta Metall Mater , vol.40 , Issue.1 , pp. 185-192
    • Cho, S.-J.1    Moon, H.2    Hockey, B.J.3    Hsu, S.M.4
  • 16
    • 0029289227 scopus 로고
    • Wear and wear transition mechanism in silicon carbide ceramics during sliding
    • Cho S.-J., Um C.-D., Kim S.-S. Wear and wear transition mechanism in silicon carbide ceramics during sliding. J Am Ceram Soc 1995, 78(4):1076-1078.
    • (1995) J Am Ceram Soc , vol.78 , Issue.4 , pp. 1076-1078
    • Cho, S.-J.1    Um, C.-D.2    Kim, S.-S.3
  • 17
    • 0002023796 scopus 로고    scopus 로고
    • Wear and wear transition mechanisms of ceramics
    • Wang Y., Hsu S.M. Wear and wear transition mechanisms of ceramics. Wear 1996, 195(1-2):112-122.
    • (1996) Wear , vol.195 , Issue.1-2 , pp. 112-122
    • Wang, Y.1    Hsu, S.M.2
  • 18
    • 0030146805 scopus 로고    scopus 로고
    • Wear and wear transition in silicon carbide ceramics during sliding
    • Cho S.-J., Um C.-D., Kim S.-S. Wear and wear transition in silicon carbide ceramics during sliding. J Am Ceram Soc 1996, 79(5):1247-1251.
    • (1996) J Am Ceram Soc , vol.79 , Issue.5 , pp. 1247-1251
    • Cho, S.-J.1    Um, C.-D.2    Kim, S.-S.3
  • 20
    • 10044250907 scopus 로고    scopus 로고
    • Wear-resistant ultra-fine-grained ceramics
    • Wang X., Padture N.P., Tanaka H., Ortiz A.L. Wear-resistant ultra-fine-grained ceramics. Acta Mater 2005, 53(2):271-277.
    • (2005) Acta Mater , vol.53 , Issue.2 , pp. 271-277
    • Wang, X.1    Padture, N.P.2    Tanaka, H.3    Ortiz, A.L.4
  • 21
    • 27644523198 scopus 로고    scopus 로고
    • Effect of microstructure on sliding-wear properties of liquid-phase-sintered α-SiC
    • Borrero-López O., Ortiz A.L., Guiberteau F., Padture N.P. Effect of microstructure on sliding-wear properties of liquid-phase-sintered α-SiC. J Am Ceram Soc 2005, 88(8):2159-2163.
    • (2005) J Am Ceram Soc , vol.88 , Issue.8 , pp. 2159-2163
    • Borrero-López, O.1    Ortiz, A.L.2    Guiberteau, F.3    Padture, N.P.4
  • 22
    • 34248582292 scopus 로고    scopus 로고
    • Microstructural design of sliding-wear-resistant liquid-phase-sintered sic: an overview
    • Borrero-López O., Ortiz A.L., Guiberteau F., Padture N.P. Microstructural design of sliding-wear-resistant liquid-phase-sintered sic: an overview. J Eur Ceram Soc 2007, 27(11):3351-3357.
    • (2007) J Eur Ceram Soc , vol.27 , Issue.11 , pp. 3351-3357
    • Borrero-López, O.1    Ortiz, A.L.2    Guiberteau, F.3    Padture, N.P.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.