1
-
-
44049121717
-
The Transition from Mild to Severe Wear in Alumina during Sliding
-
1
-
S.-J. Cho, H. Moon, B. J. Hockey, and S. M. Hsu, "The Transition from Mild to Severe Wear in Alumina during Sliding," Acta Metall. Mater., 40 [1] 185-92 (1992).
-
(1992)
Acta Metall. Mater.
, vol.40
, pp. 185-192
-
-
Cho, S.-J.1
Moon, H.2
Hockey, B.J.3
Hsu, S.M.4
-
2
-
-
33846351913
-
Grain-Size and R-Curve Effects in the Abrasive Wear of Alumina
-
7
-
S.-J. Cho, B. J. Hockey, B. R. Lawn, and S. J. Bennison, "Grain-Size and R-Curve Effects in the Abrasive Wear of Alumina," J. Am. Ceram. Soc., 72 [7] 1249-52 (1989).
-
(1989)
J. Am. Ceram. Soc.
, vol.72
, pp. 1249-1252
-
-
Cho, S.-J.1
Hockey, B.J.2
Lawn, B.R.3
Bennison, S.J.4
-
3
-
-
0029289227
-
Wear and Wear Transition Mechanism in SiC during Sliding
-
4
-
S.-J. Cho, C. D. Um, and S. S. Kim, "Wear and Wear Transition Mechanism in SiC during Sliding," J. Am. Ceram. Soc., 78 [4] 1076-78 (1995).
-
(1995)
J. Am. Ceram. Soc.
, vol.78
, pp. 1076-1078
-
-
Cho, S.-J.1
Um, C.D.2
Kim, S.S.3
-
4
-
-
0024764313
-
Quantitative Wear Maps as a Visualization of Wear Mechanism Transitions in Ceramics Materials
-
S. M. Hsu, Y. S. Wang, and R. G. Munro, "Quantitative Wear Maps as a Visualization of Wear Mechanism Transitions in Ceramics Materials," Wear, 134, 1-11 (1989).
-
(1989)
Wear
, vol.134
, pp. 1-11
-
-
Hsu, S.M.1
Wang, Y.S.2
Munro, R.G.3
-
5
-
-
0027886431
-
Hot Isostatic Pressing of α-Silicon Carbide Ceramics
-
J. She, J. Guo, and D. Jiang, "Hot Isostatic Pressing of α-Silicon Carbide Ceramics," Ceram. Int., 19, 347-51 (1993).
-
(1993)
Ceram. Int.
, vol.19
, pp. 347-351
-
-
She, J.1
Guo, J.2
Jiang, D.3
-
6
-
-
0027694118
-
Microstructure and Properties of Self-Reinforced Silicon Nitride
-
11
-
A. J. Pyzik and D. R. Beaman, "Microstructure and Properties of Self-Reinforced Silicon Nitride," J. Am. Ceram. Soc., 76 [11] 2737-44 (1993).
-
(1993)
J. Am. Ceram. Soc.
, vol.76
, pp. 2737-2744
-
-
Pyzik, A.J.1
Beaman, D.R.2
-
7
-
-
0028382729
-
In situ-Toughened Silicon Carbide
-
2
-
N. P. Padture, "In situ-Toughened Silicon Carbide," J. Am. Ceram. Soc., 77 [2] 519-23 (1994).
-
(1994)
J. Am. Ceram. Soc.
, vol.77
, pp. 519-523
-
-
Padture, N.P.1
-
8
-
-
0028529919
-
Toughness Properties of a Silicon Carbide with an in situ Induced Heterogeneous Grain Structure
-
10
-
N. P. Padture and B. R. Lawn, "Toughness Properties of a Silicon Carbide with an in situ Induced Heterogeneous Grain Structure," J. Am. Ceram. Soc., 77 [10] 2518-22 (1994).
-
(1994)
J. Am. Ceram. Soc.
, vol.77
, pp. 2518-2522
-
-
Padture, N.P.1
Lawn, B.R.2
-
9
-
-
0025401705
-
Whisker Toughening: A Comparison between Aluminum Oxide and Silicon Nitride Toughened with Silicon Carbide
-
3
-
G. H. Campbell, M. Rühle, B. J. Dalgleish, and A. G. Evans, "Whisker Toughening: A Comparison between Aluminum Oxide and Silicon Nitride Toughened with Silicon Carbide," J. Am. Ceram. Soc., 73 [3] 521-30 (1990).
-
(1990)
J. Am. Ceram. Soc.
, vol.73
, pp. 521-530
-
-
Campbell, G.H.1
Rühle, M.2
Dalgleish, B.J.3
Evans, A.G.4
-
10
-
-
0027658716
-
Model for Toughness Curves in Two-Phase Ceramics: II, Microstructural Variables
-
9
-
B. R. Lawn, N. P. Padture, L. M. Braun, and S. J. Bennison, "Model for Toughness Curves in Two-Phase Ceramics: II, Microstructural Variables," J. Am. Ceram. Soc., 76 [9] 2241-47 (1993).
-
(1993)
J. Am. Ceram. Soc.
, vol.76
, pp. 2241-2247
-
-
Lawn, B.R.1
Padture, N.P.2
Braun, L.M.3
Bennison, S.J.4
|