Volumn 26, Issue 23, 2010, Pages 18293-18299

Maximization of loading and stability of ssDNA: Iron oxide nanoparticle complexes formed through electrostatic interaction

Author keywords

[No Author keywords available]

Indexed keywords

BIO-CONJUGATION; ELECTROSTATIC COMPLEXES; ELECTROSTATIC INTERACTIONS; FLUORESCENCE QUENCHING; GAINING MOMENTUM; HIGH LOADINGS; IN-VITRO; INORGANIC NANOPARTICLE; IRON OXIDE NANOPARTICLE; LOADING LEVEL; OPTIMAL CONDITIONS; POSITIVELY CHARGED; PRACTICAL USE; SURFACE COATINGS; THERAPEUTIC TOOLS;

EID: 78650249331     PISSN: 07437463     EISSN: 15205827     Source Type: Journal    
DOI: 10.1021/la103237e     Document Type: Article
Times cited : (17)

References (41)
  • 9
    • 78650243118 scopus 로고    scopus 로고
    • Hannon, G. J. Nature 2002, 404, 293-296
    • (2002) Nature , vol.404 , pp. 293-296
    • Hannon, G.J.1
  • 37
    • 0030848621 scopus 로고    scopus 로고
    • Decher, G. Science 1997, 29, 1232-1237
    • (1997) Science , vol.29 , pp. 1232-1237
    • Decher, G.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.