메뉴 건너뛰기




Volumn 31, Issue 1-2, 2011, Pages 199-215

Oxidation behavior of hot pressed ZrB2-SiC and HfB2-SiC composites

Author keywords

B. Composites; C. Hardness; C. Residual stress; D. Borides; Oxidation

Indexed keywords

AIR COOLING; B. COMPOSITES; C. HARDNESS; C. RESIDUAL STRESS; CYCLIC OXIDATION; CYCLIC OXIDATION BEHAVIOR; D. BORIDES; ISOTHERMAL OXIDATIONS; MASS GAIN; MASS INCREASE; NONISOTHERMAL; OXIDATION BEHAVIORS; OXIDE SCALE; PHASE TRANSFORMATION; STABLE OXIDES; THERMAL RESIDUAL STRESS; THERMOGRAVIMETRIC ANALYZERS;

EID: 78049478704     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2010.08.018     Document Type: Article
Times cited : (81)

References (46)
  • 1
    • 84975353152 scopus 로고
    • The oxidation kinetics of zirconium diboride and zirconium carbide at high temperatures
    • Kuriakose A.K., Margrave J.L. The oxidation kinetics of zirconium diboride and zirconium carbide at high temperatures. J. Electrochem. Soc. 1964, 111:827-831.
    • (1964) J. Electrochem. Soc. , vol.111 , pp. 827-831
    • Kuriakose, A.K.1    Margrave, J.L.2
  • 4
    • 0033323434 scopus 로고    scopus 로고
    • Mechanical, thermal, and oxidation properties of refractory hafnium and zirconium compounds
    • Opeka M.M., Talmy I.G., Wuchina E.J., Zaykoski J.A., Causey S.J. Mechanical, thermal, and oxidation properties of refractory hafnium and zirconium compounds. J. Eur. Ceram. Soc. 1999, 19:2405-2414.
    • (1999) J. Eur. Ceram. Soc. , vol.19 , pp. 2405-2414
    • Opeka, M.M.1    Talmy, I.G.2    Wuchina, E.J.3    Zaykoski, J.A.4    Causey, S.J.5
  • 9
    • 34248399787 scopus 로고
    • Sintering
    • NTIS Report AD 428006, Federal Scientific and Technical Information, Springfield, VA, L. Kauffman, E.V. Clougherty (Eds.)
    • Coble R.L., Hobbs H.A. Sintering. Investigation of Boride Compounds for very high Temperature Applications 1973, 82-100. NTIS Report AD 428006, Federal Scientific and Technical Information, Springfield, VA. L. Kauffman, E.V. Clougherty (Eds.).
    • (1973) Investigation of Boride Compounds for very high Temperature Applications , pp. 82-100
    • Coble, R.L.1    Hobbs, H.A.2
  • 10
    • 4544347679 scopus 로고    scopus 로고
    • High speed propulsion: performance advantage of advanced materials
    • Jackson T.A., Eklund D.R., Fink A.J. High speed propulsion: performance advantage of advanced materials. J. Mater. Sci. 2004, 39:5905-5913.
    • (2004) J. Mater. Sci. , vol.39 , pp. 5905-5913
    • Jackson, T.A.1    Eklund, D.R.2    Fink, A.J.3
  • 11
    • 4544353663 scopus 로고    scopus 로고
    • The hypersonic environment: required operating conditions and design challenges
    • Vanwie D.M., Drewary D.G., King D.E., Hudson C.M. The hypersonic environment: required operating conditions and design challenges. J. Mater. Sci. 2004, 39:5915-5924.
    • (2004) J. Mater. Sci. , vol.39 , pp. 5915-5924
    • Vanwie, D.M.1    Drewary, D.G.2    King, D.E.3    Hudson, C.M.4
  • 12
    • 12844278742 scopus 로고    scopus 로고
    • Ultrahigh-temperature ceramics for hypersonic vehicle applications
    • Loehman R.E. Ultrahigh-temperature ceramics for hypersonic vehicle applications. Ind. Heat. 2004.
    • (2004) Ind. Heat.
    • Loehman, R.E.1
  • 13
    • 4544366215 scopus 로고    scopus 로고
    • 2-based ultra-high temperature ceramics: effect of Ta additions
    • 2-based ultra-high temperature ceramics: effect of Ta additions. J. Mater. Sci. 2004, 39:5969-5977.
    • (2004) J. Mater. Sci. , vol.39 , pp. 5969-5977
    • Opila, E.1    Levine, S.2    Lorincz, J.3
  • 16
    • 33748936677 scopus 로고    scopus 로고
    • Oxidation of zirconium diboride-silicon carbide at 1500°C a low partial pressure of oxygen
    • Rezaie A.R., Fahrenholtz W.G., Hilmas G.E. Oxidation of zirconium diboride-silicon carbide at 1500°C a low partial pressure of oxygen. J. Am. Ceram. Soc. 2006, 89(10):3240-3245.
    • (2006) J. Am. Ceram. Soc. , vol.89 , Issue.10 , pp. 3240-3245
    • Rezaie, A.R.1    Fahrenholtz, W.G.2    Hilmas, G.E.3
  • 17
    • 33846372666 scopus 로고    scopus 로고
    • Evolution of structure during the oxidation of zirconium diboride-silicon carbide in air up to 1500°C
    • Rezaie A., Fahrenholtz W.G., Hilmas G.E. Evolution of structure during the oxidation of zirconium diboride-silicon carbide in air up to 1500°C. J. Eur. Ceram. Soc. 2007, 27:2495-2501.
    • (2007) J. Eur. Ceram. Soc. , vol.27 , pp. 2495-2501
    • Rezaie, A.1    Fahrenholtz, W.G.2    Hilmas, G.E.3
  • 18
    • 4544330453 scopus 로고    scopus 로고
    • Oxidation-based materials selection for 2000°C+hypersonic aerosurfaces: theoretical considerations and historical experience
    • Opeka M.M., Talmy I.G., Zaykoski J.A. Oxidation-based materials selection for 2000°C+hypersonic aerosurfaces: theoretical considerations and historical experience. J. Mater. Sci. 2004, 39:5887-5904.
    • (2004) J. Mater. Sci. , vol.39 , pp. 5887-5904
    • Opeka, M.M.1    Talmy, I.G.2    Zaykoski, J.A.3
  • 24
    • 58849138332 scopus 로고    scopus 로고
    • Mechanical, thermal, and oxidation behaviour of zirconium diboride based ultra-high temperature ceramic composites
    • Mitra R., Upender S., Mallik M., Chakraborty S., Ray K.K. Mechanical, thermal, and oxidation behaviour of zirconium diboride based ultra-high temperature ceramic composites. Key Eng. Mater. 2009, 395:55-68.
    • (2009) Key Eng. Mater. , vol.395 , pp. 55-68
    • Mitra, R.1    Upender, S.2    Mallik, M.3    Chakraborty, S.4    Ray, K.K.5
  • 26
    • 0021375644 scopus 로고
    • Boron analysis and mapping with a windowless energy dispersive detector
    • C2:185-C2:188
    • Sandborg A.O., Whitehead M.E. Boron analysis and mapping with a windowless energy dispersive detector. J. Phys. Colloques 1984, 45. C2:185-C2:188.
    • (1984) J. Phys. Colloques , vol.45
    • Sandborg, A.O.1    Whitehead, M.E.2
  • 27
    • 0036606849 scopus 로고    scopus 로고
    • Oxidation behavior of extruded Mo5Si3Bx-MoSi2-MoB intermetallics from 600-1600°C
    • Thom A.J., Summers E., Mufit A. Oxidation behavior of extruded Mo5Si3Bx-MoSi2-MoB intermetallics from 600-1600°C. Intermetallics 2002, 10:555-570.
    • (2002) Intermetallics , vol.10 , pp. 555-570
    • Thom, A.J.1    Summers, E.2    Mufit, A.3
  • 28
    • 0003427458 scopus 로고
    • Addison Wesley Publishing Company, Inc., New York, NY
    • Cullity B.D. Elements of X-ray Diffraction 1978, Addison Wesley Publishing Company, Inc., New York, NY, p. 447-78.
    • (1978) Elements of X-ray Diffraction , pp. 447-478
    • Cullity, B.D.1
  • 29
    • 0033875475 scopus 로고    scopus 로고
    • High temperature stress measurements during the oxidation of NiAl
    • Schumann E., Sarioglu C., Blachere J.R., Pettit F.S., Meier G.H. High temperature stress measurements during the oxidation of NiAl. Oxid. Met. 2000, 53(3-4):259-272.
    • (2000) Oxid. Met. , vol.53 , Issue.3-4 , pp. 259-272
    • Schumann, E.1    Sarioglu, C.2    Blachere, J.R.3    Pettit, F.S.4    Meier, G.H.5
  • 30
    • 78049463318 scopus 로고    scopus 로고
    • Oxidation behaviour of Mo-Si-B and Mo-Si-B-Al alloys
    • Paswan S., Mitra R., Roy S.K. Oxidation behaviour of Mo-Si-B and Mo-Si-B-Al alloys. Metall. Mater. Trans. A 2009, 40:2644-2658.
    • (2009) Metall. Mater. Trans. A , vol.40 , pp. 2644-2658
    • Paswan, S.1    Mitra, R.2    Roy, S.K.3
  • 31
    • 66249093919 scopus 로고
    • The gaseous oxides of the platinum metals
    • Alcock C.B. The gaseous oxides of the platinum metals. Platinum Met. Rev. 1961, 5(4):134-139.
    • (1961) Platinum Met. Rev. , vol.5 , Issue.4 , pp. 134-139
    • Alcock, C.B.1
  • 32
    • 35848953179 scopus 로고    scopus 로고
    • J. Phy. Chem. Ref. Data, Monograph 9, American Institute for Physics, Woodbury, NY
    • Chase M.W. NIST-JANAF Thermochemical Tables 1998, J. Phy. Chem. Ref. Data, Monograph 9, American Institute for Physics, Woodbury, NY. Fourth edition.
    • (1998) NIST-JANAF Thermochemical Tables
    • Chase, M.W.1
  • 33
    • 33846188476 scopus 로고    scopus 로고
    • 2-SiC oxidation: formation of a SiC-depleted region
    • 2-SiC oxidation: formation of a SiC-depleted region. J. Am. Ceram. Soc. 2007, 90(1):143-148.
    • (2007) J. Am. Ceram. Soc. , vol.90 , Issue.1 , pp. 143-148
    • Fahrenholtz, W.G.1
  • 34
    • 0015082862 scopus 로고
    • Active to passive transition in the oxidation of SiC
    • Antill J.E., Warburton J.B. Active to passive transition in the oxidation of SiC. Corros. Sci. 1971, 11:337-342.
    • (1971) Corros. Sci. , vol.11 , pp. 337-342
    • Antill, J.E.1    Warburton, J.B.2
  • 35
    • 0031249110 scopus 로고    scopus 로고
    • High-temperature oxidation of silicon carbide and silicon nitride
    • Narushima T., Goto T., Hirai T., Iguchi Y. High-temperature oxidation of silicon carbide and silicon nitride. Mater. Trans. JIM 1997, 38(10):821-835.
    • (1997) Mater. Trans. JIM , vol.38 , Issue.10 , pp. 821-835
    • Narushima, T.1    Goto, T.2    Hirai, T.3    Iguchi, Y.4
  • 37
    • 37849185381 scopus 로고    scopus 로고
    • Effect of particle size on oxidation of silicon carbide powders
    • Quanli J., Haijun Z., Suping L., Xiaolin J. Effect of particle size on oxidation of silicon carbide powders. Ceram. Int. 2007, 33(2):309-313.
    • (2007) Ceram. Int. , vol.33 , Issue.2 , pp. 309-313
    • Quanli, J.1    Haijun, Z.2    Suping, L.3    Xiaolin, J.4
  • 38
    • 33847095847 scopus 로고    scopus 로고
    • 2-SiC composites for protection of carbon-based materials
    • 2-SiC composites for protection of carbon-based materials. Acta Astronaut. 2007, 60:858-864.
    • (2007) Acta Astronaut. , vol.60 , pp. 858-864
    • Lespade, P.1    Richet, N.2    Goursat, P.3
  • 39
    • 0033907979 scopus 로고    scopus 로고
    • Alloy design strategies for promoting protective oxide-scale formation
    • Brady M.P., Gleeson B., Wright I.G. Alloy design strategies for promoting protective oxide-scale formation. JOM 2000, 52:16-21.
    • (2000) JOM , vol.52 , pp. 16-21
    • Brady, M.P.1    Gleeson, B.2    Wright, I.G.3
  • 40
    • 34347231928 scopus 로고    scopus 로고
    • Oxidation behavior of the Mo-Si-B and Mo-Si-B-Al alloys in the temperature range of 700-1300°C
    • Paswan S., Mitra R., Roy S.K. Oxidation behavior of the Mo-Si-B and Mo-Si-B-Al alloys in the temperature range of 700-1300°C. Intermetallics 2007, 15:1217-1227.
    • (2007) Intermetallics , vol.15 , pp. 1217-1227
    • Paswan, S.1    Mitra, R.2    Roy, S.K.3
  • 42
    • 0037425408 scopus 로고    scopus 로고
    • Stress distributions in growing oxide films
    • Krishnamurty R., Srolovitz D.J. Stress distributions in growing oxide films. Acta Mater. 2003, 51(8):2171-2190.
    • (2003) Acta Mater. , vol.51 , Issue.8 , pp. 2171-2190
    • Krishnamurty, R.1    Srolovitz, D.J.2
  • 44
    • 0018529273 scopus 로고
    • Transformation toughening in partially stabilized zirconia (PSZ)
    • Porter D.L., Evans A.G., Heuer A.H. Transformation toughening in partially stabilized zirconia (PSZ). Acta Metall. 1979, 27:1649-1654.
    • (1979) Acta Metall. , vol.27 , pp. 1649-1654
    • Porter, D.L.1    Evans, A.G.2    Heuer, A.H.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.