Volumn 58, Issue 4, 2010, Pages 306-309

A core fracture with all-ceramic crowns: A case report

Author keywords

[No Author keywords available]

Indexed keywords

ADULT; ARTICLE; DENTAL SURGERY; HUMAN; MALE; MANDIBLE; MOLAR TOOTH; TOOTH CROWN; TOOTH FRACTURE; TOOTH PROSTHESIS;

EID: 77957952807     PISSN: 03636771     EISSN: None     Source Type: Journal    
DOI: None     Document Type: Article
Times cited : (1)

References (22)
  • 1
    • 7444265287 scopus 로고    scopus 로고
    • In wfrofractjre strength of teeth restored with different all-ceramic crown systems
    • Potiket N, Chiche G, Finger IM. In wfrofractjre strength of teeth restored with different all-ceramic crown systems. J Prosthet Dent 2004; 92(51:491-495
    • (2004) J Prosthet Dent , vol.92 , Issue.51 , pp. 491-495
    • Potiket, N.1    Chiche, G.2    Finger, I.M.3
  • 2
    • 0029678682 scopus 로고    scopus 로고
    • Ceramics in dentistry: Historical roots and current perspectives
    • Kelly JR, Nishimura I, Campbell SD. Ceramics in dentistry: Historical roots and current perspectives. J Prosthet Dent 1996;75(1):18-32.
    • (1996) J Prosthet Dent , vol.75 , Issue.1 , pp. 18-32
    • Kelly, J.R.1    Nishimura, I.2    Campbell, S.D.3
  • 3
    • 0347510923 scopus 로고    scopus 로고
    • The confusing array of tooth-colored crowns
    • Christensen GJ. The confusing array of tooth-colored crowns. J Am Dent Assoc 2003; 134(9); 1253-1255.
    • (2003) J Am Dent Assoc , vol.134 , Issue.9 , pp. 1253-1255
    • Christensen, G.J.1
  • 4
    • 55249125701 scopus 로고    scopus 로고
    • Esthetic dentistry-2008
    • Christensen GJ, Esthetic dentistry-2008. Alpha Omegan 2008;101(2):69-70.
    • (2008) Alpha Omegan , vol.101 , Issue.2 , pp. 69-70
    • Christensen, G.J.1
  • 5
    • 1842732685 scopus 로고    scopus 로고
    • Strength, fracture toughness and microstructtire of a selection of all-ceramic materials. Part I. Pressable and alumina glass-infiltrated ceramics
    • Guazzato M, Albatry M, Ringer SP, Swain MV. Strength, fracture toughness and microstructtire of a selection of all-ceramic materials. Part I. Pressable and alumina glass-infiltrated ceramics. Dent Mater 2004;20(5):441-448.
    • (2004) Dent Mater , vol.20 , Issue.5 , pp. 441-448
    • Guazzato, M.1    Albatry, M.2    Ringer, S.P.3    Swain, M.V.4
  • 6
    • 1842783267 scopus 로고    scopus 로고
    • Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics
    • Guazzato M, Albakry M, Ringer SP, Swain MV. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II Zirconia-based dental ceramics. Dent Mater 2004;20(5):449-456.
    • (2004) Dent Mater , vol.20 , Issue.5 , pp. 449-456
    • Guazzato, M.1    Albakry, M.2    Ringer, S.P.3    Swain, M.V.4
  • 7
    • 29144487947 scopus 로고    scopus 로고
    • Load-to-fracture value of different all-ceramic crown systems
    • Synder MD, Hogg KD. Load-to-fracture value of different all-ceramic crown systems. J Contemp Dent Pract 2005;(6)4:54-63.
    • (2005) J Contemp Dent Pract , vol.6 , Issue.4 , pp. 54-63
    • Synder, M.D.1    Hogg, K.D.2
  • 8
    • 0038727300 scopus 로고    scopus 로고
    • An in vitro study of the compressive load at fracture of Procera AllCeram crowns with varying thickness of veneer porcelain
    • DOI 10.1067/mpr.2003.85
    • Webber 6, McDonald A, Knowles J. An in vitro study of the compressive load at fracture of Procera AllCeram crowns with varying thickness of veneer porcelain. J Prosthet Dent 2003,89(2): 154-160. (Pubitemid 37323913)
    • (2003) Journal of Prosthetic Dentistry , vol.89 , Issue.2 , pp. 154-160
    • Webber, B.1    McDonald, A.2    Knowles, J.3
  • 9
    • 0035654749 scopus 로고    scopus 로고
    • Influence of core buildup material on the fatigue strength of an all-ceramic crown
    • Azer SS, Drummond JL, Campbell SD, Moneim AE. Influence of core buildup material on the fatigue strength of an all-ceramic crown. J Prosthet Dent 2001;86(6):624-631.
    • (2001) J Prosthet Dent , vol.86 , Issue.6 , pp. 624-631
    • Azer, S.S.1    Drummond, J.L.2    Campbell, S.D.3    Moneim, A.E.4
  • 10
    • 0035220559 scopus 로고    scopus 로고
    • Evolution of dental ceramics in the twentieth century
    • McLean M Evolution of dental ceramics in the twentieth century. J Prosthet Dent 2001 ;85(1): 61-66. 11. LasCasas EB, deAlmeida AF, Cimini Junior CA, Gomes PdeT, Cornacchia TP, Saffar JM. Determination of tangential and normal components of oral forces. J Appl Oral Sd 2007; 15(1 ):70-76.
    • (2001) J Prosthet Dent , vol.85 , Issue.1 , pp. 61-66
    • McLean, M.1
  • 11
    • 3142781983 scopus 로고    scopus 로고
    • Swein MV.A review of critical issues of dental ceramics
    • Ironside JG, Swein MV.A review of critical issues of dental ceramics. J Aust Ceram Soc 1998; 34(2)78-91.
    • (1998) J Aust Ceram Soc , vol.34 , Issue.2 , pp. 78-91
    • Ironside, J.G.1
  • 12
    • 2942547986 scopus 로고    scopus 로고
    • Fracture resistance of three all-ceramic restorative systems for posterior applications
    • Pallis K, Griggs JA,Woody RD, Guillen GE, Miller AW. Fracture resistance of three all-ceramic restorative systems for posterior applications. J Prosthet Dent 2004;91(6):561-569.
    • (2004) J Prosthet Dent , vol.91 , Issue.6 , pp. 561-569
    • Pallis, K.1    Griggs, J.A.2    Woody, R.D.3    Guillen, G.E.4    Miller, A.W.5
  • 14
    • 33847045629 scopus 로고    scopus 로고
    • Dental ceramics and the molar crown testing ground
    • Thompson VP, Rekow DE. Dental ceramics and the molar crown testing ground. J Appl Oral Sd 2004; 12 (Spec lssue):26-36.
    • (2004) J Appl Oral Sd , vol.12 , Issue.SPEC ISSUE , pp. 26-36
    • Thompson, V.P.1    Rekow, D.E.2
  • 15
    • 33749072477 scopus 로고    scopus 로고
    • Effect of mechanical cycling on the flexural strength of densely sintered ceramics
    • Itinoche KM, Ozcan M, Bottino MA, Oyafuso D, Effect of mechanical cycling on the flexural strength of densely sintered ceramics. Dent Mater 2006;22(11):1029-1034.
    • (2006) Dent Mater , vol.22 , Issue.11 , pp. 1029-1034
    • Itinoche, K.M.1    Ozcan, M.2    Ma, B.3    Oyafuso, D.4
  • 16
    • 2942547986 scopus 로고    scopus 로고
    • Fracture resistance of three all-ceramic restorative systems for posterior applications
    • Pallis K, Griggs JA, Woody RD, Guillen GE, Miller AW. Fracture resistance of three all-ceramic restorative systems for posterior applications. J Prosthet Dent 2004,91(6):561-569.
    • (2004) J Prosthet Dent , vol.91 , Issue.6 , pp. 561-569
    • Pallis, K.1    Griggs, J.A.2    Woody, R.D.3    Guillen, G.E.4    Miller, A.W.5
  • 17
    • 32044472550 scopus 로고    scopus 로고
    • The influence of different core materials on the FEA-de-termined stress distribution in dental crowns
    • De lager N, de Kler M, van der Zel JM. The influence of different core materials on the FEA-de-termined stress distribution in dental crowns Dent Mater 2006;22(3):234-242.
    • (2006) Dent Mater , vol.22 , Issue.3 , pp. 234-242
    • De Lager, N.1    De Kler, M.2    Van Der Zel, J.M.3
  • 18
    • 34548590390 scopus 로고    scopus 로고
    • Fractographic ceramic failure analysis using the replica technique
    • Scherrer SS, Quinn JB, Qtiinn GD, Anselm Wis-kott HW. Fractographic ceramic failure analysis using the replica technique. Dent Mater 2007; 23(11):1397-1404.
    • (2007) Dent Mater , vol.23 , Issue.11 , pp. 1397-1404
    • Scherrer, S.S.1    Quinn, J.B.2    Qtiinn, G.D.3    Anselm Wiskott, H.W.4
  • 19
    • 38749102377 scopus 로고    scopus 로고
    • Evaluation of load at fracture of Procera AllCeram copings using different luting cements
    • Al-Makramani BM, RazakAA, Abu-Hassan Ml. Evaluation of load at fracture of Procera AllCeram copings using different luting cements. J Prosthodont 2008;17:120-124.
    • (2008) J Prosthodont , vol.17 , pp. 120-124
    • Al-Makramani, B.M.1    Razak, A.A.2    Abu-Hassan, M.I.3
  • 21
    • 16344363996 scopus 로고    scopus 로고
    • Influence of surface and heat treatments on the flexural strength of a glass-infiltrated alumina/ zirconia-reirtforced dental ceramic
    • Guazzato M,Albakry M, Quach L, Swain MV. influence of surface and heat treatments on the flexural strength of a glass-infiltrated alumina/ zirconia-reirtforced dental ceramic. Dent Mater 2005;21(5):454-463.
    • (2005) Dent Mater , vol.21 , Issue.5 , pp. 454-463
    • Guazzato, M.1    Albakry, M.2    Quach, L.3    Swain, M.V.4
  • 22
    • 25144475575 scopus 로고    scopus 로고
    • Frac-trographic analyses of three ceramic whole crown restoration failures
    • Quinn JB, Quinn GD, Kelly JR, Scherrer SS. Frac-trographic analyses of three ceramic whole crown restoration failures. Dent Mater 2005; 21(10):920-929.
    • (2005) Dent Mater , vol.21 , Issue.10 , pp. 920-929
    • Quinn, J.B.1    Quinn, G.D.2    Kelly, J.R.3    Scherrer, S.S.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.