메뉴 건너뛰기




Volumn 22, Issue 4, 2010, Pages 535-546

Spectroscopic study of the product of thermal transformation of chrysotile-asbestos containing materials (ACM)

Author keywords

Asbestos; Iron coordination; KRY AS; Spectroscopy; Thermal transformation

Indexed keywords

ACTIVATION ANALYSIS; ALUMINUM COMPOUNDS; CEMENTS; FOURIER TRANSFORM INFRARED SPECTROSCOPY; HEMATITE; IRON; IRON METALLOGRAPHY; LAND FILL; MAGNESIUM COMPOUNDS; MAGNETITE; MOLYBDENUM METALLOGRAPHY; NANOCRYSTALLINE MATERIALS; OLIVINE; OXIDATION; PACKAGING MATERIALS; PARAMAGNETISM; RAW MATERIALS; SERPENTINE; SILICATES; SPECTROSCOPIC ANALYSIS; SPECTROSCOPY;

EID: 77957693250     PISSN: 09351221     EISSN: None     Source Type: Journal    
DOI: 10.1127/0935-1221/2010/0022-2038     Document Type: Conference Paper
Times cited : (36)

References (43)
  • 1
    • 0002580976 scopus 로고
    • Infrared spectra, symmetry and structure relation of some carbonate minerals
    • Adler, H.H. & Kerr, P.F. (1963): Infrared spectra, symmetry and structure relation of some carbonate minerals. Am. Mineral., 48, 839-853.
    • (1963) Am. Mineral. , vol.48 , pp. 839-853
    • Adler, H.H.1    Kerr, P.F.2
  • 3
    • 0034850504 scopus 로고    scopus 로고
    • 3+ clusters in spinel-magnesioferrite solid solution crystals: A potential monitor for ordering in oxide spinels
    • 3+ clusters in spinel-magnesioferrite solid solution crystals: a potential monitor for ordering in oxide spinels. Phys. Chem. Minerals, 28, 435-444.
    • (2001) Phys. Chem. Minerals , vol.28 , pp. 435-444
    • Andreozzi, G.B.1    Hålenius, U.2    Skogby, H.3
  • 5
    • 0001117512 scopus 로고
    • A structural study of the thermal transformation of serpentine minerals to forsterite
    • Brindley, G.W. & Zussman, J. (1957): A structural study of the thermal transformation of serpentine minerals to forsterite. Am. Mineral., 42, 461-474.
    • (1957) Am. Mineral. , vol.42 , pp. 461-474
    • Brindley, G.W.1    Zussman, J.2
  • 6
    • 0020847269 scopus 로고
    • Coordination of iron in oxide glasses through high-resolution K-edge spectra: Information from the pre-edge
    • Calas, G., Petiau, J. (1983): Coordination of iron in oxide glasses through high-resolution K-edge spectra: information from the pre-edge. Solid State Commun., 48, 625-629.
    • (1983) Solid State Commun. , vol.48 , pp. 625-629
    • Calas, G.1    Petiau, J.2
  • 7
    • 0037980083 scopus 로고    scopus 로고
    • Kinetic study of the dehydroxylation of chrysotile asbestos with temperature by in situ XRPD
    • DOI 10.1007/s00269-003-0298-2
    • Cattaneo, A., Gualtieri, A.F., Artioli, G. (2003): Kinetic study of the dehydroxylation of chrysotile asbestos with temperature by in situ XEPD. Phys. Chem. Minerals, 30, 177-183. (Pubitemid 36669611)
    • (2003) Physics and Chemistry of Minerals , vol.30 , Issue.3 , pp. 177-183
    • Cattaneo, A.1    Gualtieri, A.F.2    Artioli, G.3
  • 8
    • 0001526418 scopus 로고    scopus 로고
    • Measurement of Fe oxidation state and coordination in geological glasses by synchrotron micro-XANES spectroscopy
    • San Francisco, CA
    • Delaney, J.S., Bajt, S., Newville, M., Sutton, S.R., Dyar, M.D. (1996): Measurement of Fe oxidation state and coordination in geological glasses by synchrotron micro-XANES spectroscopy. Amer. Geophys. Union 1996 Fall Meeting, San Francisco, CA, 77, 835-836.
    • (1996) Amer. Geophys. Union 1996 Fall Meeting , vol.77 , pp. 835-836
    • Delaney, J.S.1    Bajt, S.2    Newville, M.3    Sutton, S.R.4    Dyar, M.D.5
  • 9
    • 0346378462 scopus 로고
    • Etiology of lung cancer
    • Doll, R. (1955): Etiology of lung cancer. Adv. Cancer Res., 3, 1-50.
    • (1955) Adv. Cancer Res. , vol.3 , pp. 1-50
    • Doll, R.1
  • 10
    • 5044238466 scopus 로고    scopus 로고
    • The effect of redox state on the local structural environment of iron in silicate glasses: A combined XAFS spectroscopy, molecular dynamics, and bond valence study
    • Farges, F., Lefrere, Y., Rossano, S., Berthereau, A., Calas, G., Brown, G.E., Jr. (2004): The effect of redox state on the local structural environment of iron in silicate glasses: a combined XAFS spectroscopy, molecular dynamics, and bond valence study. J. Non-Cryst. Solids, 344, 176-188.
    • (2004) J. Non-Cryst. Solids , vol.344 , pp. 176-188
    • Farges, F.1    Lefrere, Y.2    Rossano, S.3    Berthereau, A.4    Calas, G.5    Brown Jr., G.E.6
  • 11
    • 0001044606 scopus 로고
    • The infrared spectra of minerals
    • London
    • Farmer, V.C. (1974): The infrared spectra of minerals. Mineralogical Society, London, 342-348.
    • (1974) Mineralogical Society , pp. 342-348
    • Farmer, V.C.1
  • 13
    • 0029588566 scopus 로고
    • Role of iron in the reactivity of mineral fibers
    • DOI 10.1016/0378-4274(95)03531-1
    • Fubini, B. & Mollo, L. (1995): Role of iron in the reactivity of mineral fibers. Toxicol Lett., 82, 951-960. (Pubitemid 26054775)
    • (1995) Toxicology Letters , vol.82-83 , pp. 951-960
    • Fubini, B.1    Mollo, L.2
  • 15
    • 0014879881 scopus 로고
    • Determination of chrysotile in airborne asbestos by an infra-red spectrometric technique
    • Gadsden, J.A., Parker, J., Smith, W.L. (1970): Determination of chrysotile in airborne asbestos by an infra-red spectrometric technique. Atmos. Environ., 4, 6, 667-670.
    • (1970) Atmos. Environ , vol.4 , Issue.6 , pp. 667-670
    • Gadsden, J.A.1    Parker, J.2    Smith, W.L.3
  • 16
    • 0035094818 scopus 로고    scopus 로고
    • High-resolution XANES spectra of iron in minerals and glasses: Structural information from the pre-edge region
    • DOI 10.1016/S0009-2541(00)00322-3, PII S0009254100003223
    • Galoisy, L., Calas, G., Arrio, M.A. (2001): High-resolution XANES spectra of iron in minerals and glasses: structural information from the pre-edge region. Chem. Geol., 174, 307-319. (Pubitemid 32258735)
    • (2001) Chemical Geology , vol.174 , Issue.1-3 , pp. 307-319
    • Galoisy, L.1    Calas, G.2    Arrio, M.A.3
  • 17
    • 0037115372 scopus 로고    scopus 로고
    • Iron local structure in tektites and impact glasses by extended X-ray absorption fine structure and high-resolution X-ray absorption near-edge structure spectroscopy
    • DOI 10.1016/S0016-7037(02)01030-X
    • Giuli, G., Pratesi, G., Cipriani, C., Paris, E. (2002): Iron local structure in tektites and impact glasses by extended X-ray absorption fine structure and high-resolution X-ray absorption near-edge structure spectroscopy. Geochim. Cosmochim. Acta, 66, 4347-4353. (Pubitemid 36029343)
    • (2002) Geochimica et Cosmochimica Acta , vol.66 , Issue.24 , pp. 4347-4353
    • Giuli, G.1    Pratesi, G.2    Cipriani, C.3    Paris, E.4
  • 18
    • 0033934010 scopus 로고    scopus 로고
    • Thermal decomposition of asbestos and recycling in traditional ceramics
    • Gualtieri, A.F. & Tartaglia, A. (2000): Thermal decomposition of asbestos and recycling in traditional ceramics. J. Eur. Ceram. Soc., 20, 9, 1409-1418.
    • (2000) J. Eur. Ceram. Soc. , vol.20 , Issue.9 , pp. 1409-1418
    • Gualtieri, A.F.1    Tartaglia, A.2
  • 19
    • 4043108748 scopus 로고    scopus 로고
    • The quantitative determination of the crystalline and amorphous content by the Rietveld method, application to glass ceramics with different absorbtion coefficients, in Diffraction Analysis of the Microstructure of Materials
    • E.J. Mithemeijer, P. Scardi, eds.
    • Gualtieri, A.F., Guagliardi, A., Iseppi, A. (2004): The quantitative determination of the crystalline and amorphous content by the Rietveld method, application to glass ceramics with different absorbtion coefficients, in "Diffraction Analysis of the Microstructure of Materials", E.J. Mithemeijer, P. Scardi, eds., Springer Series in Material Science, 68, 147-165.
    • (2004) Springer Series in Material Science , vol.68 , pp. 147-165
    • Gualtieri, A.F.1    Guagliardi, A.2    Iseppi, A.3
  • 20
    • 39849094035 scopus 로고    scopus 로고
    • The transformation sequence of cement-asbestos slates up to 1200 °C and safe recycling of the reaction product in stoneware tile mixtures
    • DOI 10.1016/j.jhazmat.2007.07.037, PII S0304389407010138
    • Gualtieri, A.F., Cavenati, C., Zanatto, I., Meloni, M., Elmi, G., Lassinantti Gualtieri, M. (2007): The transformation sequence of cement-asbestos slates up to 1200 °C and safe re cycling of the reaction product in stoneware tile mixture. J. Hazard. Mater., 152, 563-570. (Pubitemid 351318031)
    • (2008) Journal of Hazardous Materials , vol.152 , Issue.2 , pp. 563-570
    • Gualtieri, A.F.1    Cavenati, C.2    Zanatto, I.3    Meloni, M.4    Elmi, G.5    Gualtieri, M.L.6
  • 21
    • 0001439527 scopus 로고
    • Infrared and thermogravimetric studies of the thermal degradation of chrysotile asbestos fibers: Evidence for matrix effects
    • Jolicoeur, C. & Duchesne, D. (1981): Infrared and thermogravimetric studies of the thermal degradation of chrysotile asbestos fibers: evidence for matrix effects. Can. J. Chem., 59, 1521-1526.
    • (1981) Can. J. Chem. , vol.59 , pp. 1521-1526
    • Jolicoeur, C.1    Duchesne, D.2
  • 25
    • 1842731331 scopus 로고    scopus 로고
    • Materials recycling and industrial ecology
    • Linton, J.D. & Yeomans, J.S. (2004): Materials recycling and industrial ecology. Nat. Mater., 3, 4, 199-201.
    • (2004) Nat. Mater , vol.3 , Issue.4 , pp. 199-201
    • Linton, J.D.1    Yeomans, J.S.2
  • 27
    • 0037437309 scopus 로고    scopus 로고
    • FTIR techniques in clay mineral studies
    • Madejova, J. (2003): FTIR techniques in clay mineral studies. Vib. Spectrosc., 31, 1-10.
    • (2003) Vib. Spectrosc , vol.31 , pp. 1-10
    • Madejova, J.1
  • 28
    • 0346255922 scopus 로고
    • Histology of pulmonary asbestosis
    • Mc Donald, S. (1927): Histology of pulmonary asbestosis. Br. Med. J., 2, 1025-1026.
    • (1927) Br. Med. J. , vol.2 , pp. 1025-1026
    • Mc Donald, S.1
  • 30
    • 0030520353 scopus 로고    scopus 로고
    • X-ray Optics of a Dynamical Sagittal-Focusing Monochromator on the GILDA Beamline at the ESRF
    • DOI 10.1107/S0909049596004992
    • Pascarelli, S., Boscherini, F., D'Acapito, F., Hrdy, J., Meneghini, C., Mobilio, S. (1996): X-ray optics of a dynamical sagittal-focusing monochromator on the GILDA beamline at the ESRF. J. Synchrotron Radiat., 3, 147-155. (Pubitemid 126106642)
    • (1996) Journal of Synchrotron Radiation , vol.3 , Issue.4 , pp. 147-155
    • Pascarelli, S.1    Boscherini, F.2    D'Acapito, F.3    Hrdy, J.4    Meneghini, C.5    Mobilio, S.6
  • 32
    • 24944582891 scopus 로고    scopus 로고
    • The ancient glass production of the Medieval Val Gargassa glasshouse: Fe and Mn XANES study
    • DOI 10.1016/j.jnoncrysol.2005.06.046, PII S0022309305005211
    • Quartieri, S., Riccardi, M.P., Messiga, B., Boscherini, F. (2005): XANES study of the ancient glass production of the Medieval Val Gargassa glasshouse (Genova, Italy). J. Non-Cryst. Solids, 351, 3013-3022. (Pubitemid 41327268)
    • (2005) Journal of Non-Crystalline Solids , vol.351 , Issue.37-39 , pp. 3013-3022
    • Quartieri, S.1    Riccardi, M.P.2    Messiga, B.3    Boscherini, F.4
  • 33
    • 4444366235 scopus 로고    scopus 로고
    • Assessment of the use of Raman spectroscopy for the determination of amphibole asbestos
    • DOI 10.1180/0026461046830197
    • Rinaudo, C., Belluso, E., Gastaldi, E. (2004): Assessment of the use of Raman spectroscopy for the determination of amphibole asbestos. Mineral. Mag., 68, 455-465. (Pubitemid 39174674)
    • (2004) Mineralogical Magazine , vol.68 , Issue.3 , pp. 455-465
    • Rinaudo, C.1    Belluso, E.2    Gastaldi, D.3
  • 34
    • 0018688523 scopus 로고
    • Mortality of chrysotile asbestos workers at the Balangero Mine, Northern Italy
    • Rubino, G.F., Piolatto, G., Newhouse, M.L., Scansetti, G., Aresini, G.A. (1979): Mortality of chrysotile asbestos workers at the Balangero Mine, Northern Italy. Occup. Environ. Med., 36, 187-194. (Pubitemid 10221757)
    • (1979) British Journal of Industrial Medicine , vol.36 , Issue.3 , pp. 187-194
    • Rubino, G.F.1    Piolatto, G.2    Newhouse, M.L.3
  • 35
    • 77957712267 scopus 로고    scopus 로고
    • L'amianto: Dall'ambiente di lavoro all'ambiente di vita. Nuovi indicatori per futuri effetti, i Documenti 12
    • Pavia, IRCCS
    • Scansetti, G. (1997): L'amianto: dall'ambiente di lavoro all'ambiente di vita. Nuovi indicatori per futuri effetti, I Documenti 12, Fondazione Salvatore Maugeri, Pavia, IRCCS, 9-24.
    • (1997) Fondazione Salvatore Maugeri , pp. 9-24
    • Scansetti, G.1
  • 36
    • 0004806973 scopus 로고
    • Pulmonary asbestosis in South Africa
    • Simson, F.W. (1928): Pulmonary asbestosis in South Africa. Br. Med. J., 1, 885-887.
    • (1928) Br. Med. J. , vol.1 , pp. 885-887
    • Simson, F.W.1
  • 38
    • 0035073837 scopus 로고    scopus 로고
    • EXPGUI, a graphical user interface for GSAS
    • Toby, B.H. (2001): EXPGUI, a graphical user interface for GSAS. J. Appl Crystallogr., 34, 210-213.
    • (2001) J. Appl Crystallogr , vol.34 , pp. 210-213
    • Toby, B.H.1
  • 39
    • 0021055173 scopus 로고
    • X-ray K-edge absorption spectra of Fe minerals and model compounds: Near-edge structure
    • Waychunas, G.A., Apted, M.J., Brown, G.E., Jr (1983): X-ray K-edge absorption spectra of Fe minerals and model compounds: near-edge structure. Phys. Chem. Minerals, 10, 1-9.
    • (1983) Phys. Chem. Minerals , vol.10 , pp. 1-9
    • Waychunas, G.A.1    Apted, M.J.2    Brown Jr., G.E.3
  • 40
    • 10944246642 scopus 로고    scopus 로고
    • Determination of the iron oxidation state in basaltic glasses using XANES at the K-edge
    • DOI 10.1016/j.chemgeo.2004.08.034, PII S0009254104003328, 7th Silicate Melt Workshop
    • Wilke, M., Partzsch, G.M., Bernhardt, R., Lattard, D. (2004): Determination of the iron oxidation state in basaltic glasses using XANES at the K-edge. Chem. Geol., 213, 71-87. (Pubitemid 40014514)
    • (2004) Chemical Geology , vol.213 , Issue.1-3 , pp. 71-87
    • Wilke, M.1    Partzsch, G.M.2    Bernhardt, R.3    Lattard, D.4
  • 41
    • 33646193171 scopus 로고    scopus 로고
    • Structural environment of iron in hydrous aluminosilicate glass and meltevidence from X-ray absorption spectroscopy
    • Wilke, M., Schmidt, C., Farges, F., Malavergne, V., Gautron, L., Simionovici, A., Hahn, M., Petit, P.E. (2006): Structural environment of iron in hydrous aluminosilicate glass and meltevidence from X-ray absorption spectroscopy. Chem. Geol., 229, 144-161.
    • (2006) Chem. Geol. , vol.229 , pp. 144-161
    • Wilke, M.1    Schmidt, C.2    Farges, F.3    Malavergne, V.4    Gautron, L.5    Simionovici, A.6    Hahn, M.7    Petit, P.E.8
  • 42
    • 33846406077 scopus 로고    scopus 로고
    • Speciation of Fe in silicate glasses and melts by in-situ XANES spectroscopy
    • DOI 10.2138/am.2007.1976
    • Wilke, M., Farges, F., Partzsch, G.M., Schmidt, C., Behrens, H. (2007): Speciation of Fe in silicate glasses and melts by in-situ XANES spectroscopy. Am. Mineral, 92, 44-56. (Pubitemid 46139552)
    • (2007) American Mineralogist , vol.92 , Issue.1 , pp. 44-56
    • Wilke, M.1    Farges, F.2    Partzsch, G.M.3    Schmidt, C.4    Behrens, H.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.