Volumn 30, Issue 3, 2003, Pages 177-183

Kinetic study of the dehydroxylation of chrysotile asbestos with temperature by in situ XRPD

Author keywords

Activation energy; Asbestos; Chrysotile; In situ powder diffraction; Reactions kinetics

Indexed keywords

ACTIVATION ENERGY; DIFFUSION; NUCLEATION; REACTION KINETICS; SYNCHROTRONS; X RAY DIFFRACTION ANALYSIS;

EID: 0037980083     PISSN: 03421791     EISSN: None     Source Type: Journal    
DOI: 10.1007/s00269-003-0298-2     Document Type: Article
Times cited : (90)

References (32)
  • 1
    • 84975954347 scopus 로고
    • An environmental chamber for powder diffractometers and for temperatures up to 1200 °C under various atmospheres and vacuum
    • Anselmi-Tamburini U, Campari G, Gigna P, Spinolo G (1993) An environmental chamber for powder diffractometers and for temperatures up to 1200 °C under various atmospheres and vacuum. Powder Diff 8: 210-213
    • (1993) Powder Diff , vol.8 , pp. 210-213
    • Anselmi-Tamburini, U.1    Campari, G.2    Gigna, P.3    Spinolo, G.4
  • 2
    • 0005945130 scopus 로고
    • The dehydration of chrysotile in air and under hydrothermal conditions
    • Ball MC, Taylor HFW (1963) The dehydration of chrysotile in air and under hydrothermal conditions. Min Mag 33: 467-482
    • (1963) Min Mag , vol.33 , pp. 467-482
    • Ball, M.C.1    Taylor, H.F.W.2
  • 4
    • 0029502897 scopus 로고
    • Kinetic study of the kaolinite-mullite reaction sequence. Part I: Kaolinite dehydroxylation
    • Belotto M, Gualtieri AF, Artioli G, Clark SM (1995) Kinetic study of the kaolinite-mullite reaction sequence. Part I: kaolinite dehydroxylation. Phys Chem Miner 22: 207-214
    • (1995) Phys Chem Miner , vol.22 , pp. 207-214
    • Belotto, M.1    Gualtieri, A.F.2    Artioli, G.3    Clark, S.M.4
  • 5
    • 85051227605 scopus 로고
    • Quantitative phase analysis using the Rietveld-RIR method
    • Bish DL, Howard SA (1988) Quantitative phase analysis using the Rietveld-RIR method. J Appl Crystallogy 21: 86-91
    • (1988) J Appl Crystallogy , vol.21 , pp. 86-91
    • Bish, D.L.1    Howard, S.A.2
  • 7
    • 0001117512 scopus 로고
    • A structural study of the thermal transformation of serpentine minerals to forsterite
    • Brindley GW, Zussman J (1957) A structural study of the thermal transformation of serpentine minerals to forsterite. Am Mineral 42: 461-474
    • (1957) Am Mineral , vol.42 , pp. 461-474
    • Brindley, G.W.1    Zussman, J.2
  • 8
    • 0000346735 scopus 로고
    • Mechanism of formation of forsterite and enstatite from serpentine
    • Brindley GW, Hayami R (1965) Mechanism of formation of forsterite and enstatite from serpentine. Min Mag 35: 189-195
    • (1965) Min Mag , vol.35 , pp. 189-195
    • Brindley, G.W.1    Hayami, R.2
  • 9
    • 85061141292 scopus 로고
    • Diffusion in silicate melts
    • Stebbins JF, McMillan PF, Dingwell DB (eds) Reviews in mineralogy, Mineralogical Society of America, Washington, DC
    • Chakraboty S (1995) Diffusion in silicate melts. In: Structure, dynamics and properties of silicate melts. In: Stebbins JF, McMillan PF, Dingwell DB (eds) Reviews in mineralogy, vol. 32. Mineralogical Society of America, Washington, DC
    • (1995) Structure, Dynamics and Properties of Silicate Melts , vol.32
    • Chakraboty, S.1
  • 10
    • 0038000093 scopus 로고    scopus 로고
    • A newly developed high temperature chamber for in situ X-ray diffraction: Setup and calibration procedures
    • Dapiaggi M, Artioli G, Petras L (2002) A newly developed high temperature chamber for in situ X-ray diffraction: setup and calibration procedures. Rigaku J 19: 35-41
    • (2002) Rigaku J , vol.19 , pp. 35-41
    • Dapiaggi, M.1    Artioli, G.2    Petras, L.3
  • 12
    • 0000695099 scopus 로고    scopus 로고
    • Chemical aspects of the toxicity of inhaled mineral dusts
    • Fubini B, Otero Areán C (1999) Chemical aspects of the toxicity of inhaled mineral dusts. Chem Soc Rev 28: 373-381
    • (1999) Chem Soc Rev , vol.28 , pp. 373-381
    • Fubini, B.1    Otero Areán, C.2
  • 13
    • 0033934010 scopus 로고    scopus 로고
    • Thermal decomposition of asbestos and recycling in traditional ceramics
    • Gualtieri AF, Tartaglia A (2000) Thermal decomposition of asbestos and recycling in traditional ceramics. J Eur Ceram Soc 20: 1409-1418
    • (2000) J Eur Ceram Soc , vol.20 , pp. 1409-1418
    • Gualtieri, A.F.1    Tartaglia, A.2
  • 14
    • 0029541297 scopus 로고
    • Kinetic study of the kaolinite-mullite reaction sequence. Part II: Mullite formation
    • Gualtieri A, Bellotto M, Artioli G, Clark SM (1995) Kinetic study of the kaolinite-mullite reaction sequence. Part II: mullite formation. Phys Chem Miner 22: 215-222
    • (1995) Phys Chem Miner , vol.22 , pp. 215-222
    • Gualtieri, A.1    Bellotto, M.2    Artioli, G.3    Clark, S.M.4
  • 15
    • 0030772475 scopus 로고
    • Kinetics of formation of zeolite Na-A [LTA] from natural kaolinites
    • Gualtieri AF, Norby P, Artioli G, Hanson J (1977) Kinetics of formation of zeolite Na-A [LTA] from natural kaolinites. Phys Chem Minerals 24: 191-199
    • (1977) Phys Chem Minerals , vol.24 , pp. 191-199
    • Gualtieri, A.F.1    Norby, P.2    Artioli, G.3    Hanson, J.4
  • 16
    • 0002100591 scopus 로고
    • Expanded use of the Rietveld method in the studies of phase abundance in multiphase mixtures
    • Hill RJ (1991) Expanded use of the Rietveld method in the studies of phase abundance in multiphase mixtures. Powder Diff 6: 74-77.
    • (1991) Powder Diff , vol.6 , pp. 74-77
    • Hill, R.J.1
  • 17
    • 0026494692 scopus 로고
    • Biological effects of inhaled minerals
    • Guthrie GD (1992) Biological effects of inhaled minerals. Am Mineral 77: 225-243
    • (1992) Am Mineral , vol.77 , pp. 225-243
    • Guthrie, G.D.1
  • 21
    • 0038338037 scopus 로고
    • The thermal decomposition of chrysotile
    • Martin CJ (1977) The thermal decomposition of chrysotile. Miner Mag 35: 189-195
    • (1977) Miner Mag , vol.35 , pp. 189-195
    • Martin, C.J.1
  • 24
    • 0038109319 scopus 로고
    • New data on the composition and identification of chlorites
    • Nelson B, Roy R (1954) New data on the composition and identification of chlorites. Clays and Clay Minerals 2: 335-348
    • (1954) Clays and Clay Minerals , vol.2 , pp. 335-348
    • Nelson, B.1    Roy, R.2
  • 25
    • 1842783147 scopus 로고    scopus 로고
    • Synchrotron powder diffraction using the imaging plates - Crystal structure determination and Rietveld refinement
    • Norby P (1997) Synchrotron powder diffraction using the imaging plates - crystal structure determination and Rietveld refinement. J Appl Crystallogr 30: 21-30
    • (1997) J Appl Crystallogr , vol.30 , pp. 21-30
    • Norby, P.1
  • 27
    • 0019653998 scopus 로고
    • Grinding of chrysotile in hydrocarbons, alcohol and water
    • Papirer E, Roland P (1981) Grinding of chrysotile in hydrocarbons, alcohol and water. Clays Clay Miner 29: 161-170
    • (1981) Clays Clay Miner , vol.29 , pp. 161-170
    • Papirer, E.1    Roland, P.2
  • 28
    • 0002211129 scopus 로고
    • A profile refinement method for nuclear and magnetic structures
    • Rietveld HM (1969) A profile refinement method for nuclear and magnetic structures. J Appl Crystallogr 2: 65-71
    • (1969) J Appl Crystallogr , vol.2 , pp. 65-71
    • Rietveld, H.M.1
  • 29
    • 0024748843 scopus 로고
    • Effects of dry grinding and leaching on the crystal structure of chrysotile
    • Suquet H (1989) Effects of dry grinding and leaching on the crystal structure of chrysotile. Clays Clay Miner 37: 439-445
    • (1989) Clays Clay Miner , vol.37 , pp. 439-445
    • Suquet, H.1
  • 30
    • 84927522518 scopus 로고
    • Recommended values for the thermal expansivity of silicon from 0 to 1000 K
    • Swenson CA (1983) Recommended values for the thermal expansivity of silicon from 0 to 1000 K. J Phys Chem 12 (2): 179-181
    • (1983) J Phys Chem , vol.12 , Issue.2 , pp. 179-181
    • Swenson, C.A.1
  • 31
    • 0001829132 scopus 로고
    • Mineralogy of amphiboles and 1:1 layer silicates
    • Guthrie GD Jr, Mossman BT (eds) Mineralogical Society of America, Washington, DC
    • Veblen DR, Wylie AG (1993) Mineralogy of amphiboles and 1:1 layer silicates. In: Guthrie GD Jr, Mossman BT (eds) Health effects of mineral dusts, Mineralogical Society of America, vol 28. Washington, DC, pp 139-181
    • (1993) Health Effects of Mineral Dusts , vol.28 , pp. 139-181
    • Veblen, D.R.1    Wylie, A.G.2
  • 32
    • 0002818863 scopus 로고
    • Serpentine minerals: Structures and petrology
    • Bailey SW (ed) Mineralogical Society of America, Washington, DC
    • Wicks FJ, O'Hanley DS (1988) Serpentine minerals: structures and petrology, In: Bailey SW (ed) Hydrous phillosilicates. Mineralogical Society of America, vol. 19, Washington, DC, pp 91-188
    • (1988) Hydrous Phillosilicates , vol.19 , pp. 91-188
    • Wicks, F.J.1    O'Hanley, D.S.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.