Characterization of corrosion phenomena of Zr-Ti-Cu-Al-Ni metallic glass by SEM and TEM

Author keywords

Corrosion; Metallic glass; SEM; TEM

Indexed keywords

CORRODED SURFACE; CORROSION PHENOMENA; CORROSION PITS; CORROSION PITTING; CORROSION PROCESS; CU-AL-NI; DEEP PIT; DUAL ROLE; GALVANIC CELLS; OPEN CIRCUIT CONDITIONS; SEM; SEM AND TEM; TEM;

EID: 77955426395     PISSN: 10445803     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.matchar.2010.06.013     Document Type: Article
Times cited : (38)

References (37)
  • 2
    • 27744436121 scopus 로고    scopus 로고
    • Metallic glasses as structural materials
    • M.F. Ashby, and A.L. Greer Metallic glasses as structural materials Scr Mater 54 2006 321 326
    • (2006) Scr Mater , vol.54 , pp. 321-326
    • Ashby, M.F.1    Greer, A.L.2
  • 3
    • 0031141898 scopus 로고    scopus 로고
    • Effect of oxygen impurity on crystallization of an undercooled bulk glass forming Zr-Ti-Cu-Ni-Al alloy
    • X.H. Lin, W.L. Johnson, and W.K. Rhim Effect of oxygen impurity on crystallization of an undercooled bulk glass forming Zr-Ti-Cu-Ni-Al alloy Mater Trans JIM 38 1997 473 477
    • (1997) Mater Trans JIM , vol.38 , pp. 473-477
    • Lin, X.H.1    Johnson, W.L.2    Rhim, W.K.3
  • 4
    • 0031212226 scopus 로고    scopus 로고
    • Bulk glass formation in the Zr-Ti-Al-Cu-Ni system
    • L.Q. Xing, and P. Ochin Bulk glass formation in the Zr-Ti-Al-Cu-Ni system J Mater Sci Lett 16 1997 1277 1280
    • (1997) J Mater Sci Lett , vol.16 , pp. 1277-1280
    • Xing, L.Q.1    Ochin, P.2
  • 5
    • 0035906681 scopus 로고    scopus 로고
    • Influence of decomposition on the thermal stability of undercooled Zr-Ti-Cu-Ni-Al alloys
    • A.A. Kündig, J.F. Löffler, W.L. Johnson, P.J. Uggowitzer, and P. Thiyagarajan Influence of decomposition on the thermal stability of undercooled Zr-Ti-Cu-Ni-Al alloys Scr Mater 44 2001 1269 1273
    • (2001) Scr Mater , vol.44 , pp. 1269-1273
    • Kündig, A.A.1    Löffler, J.F.2    Johnson, W.L.3    Uggowitzer, P.J.4    Thiyagarajan, P.5
  • 6
  • 7
    • 33947264672 scopus 로고    scopus 로고
    • Corrosion and related mechanical properties of bulk metallic glasses
    • J.R. Scully, A. Gebert, and J.H. Payer Corrosion and related mechanical properties of bulk metallic glasses J Mater Res 22 2007 302 313
    • (2007) J Mater Res , vol.22 , pp. 302-313
    • Scully, J.R.1    Gebert, A.2    Payer, J.H.3
  • 9
    • 0023119574 scopus 로고
    • The electrochemical properties of metallic glasses
    • M.D. Archer, C.C. Corke, and B.H. Harji The electrochemical properties of metallic glasses Electrochim Acta 32 1987 13 26
    • (1987) Electrochim Acta , vol.32 , pp. 13-26
    • Archer, M.D.1    Corke, C.C.2    Harji, B.H.3
  • 10
    • 77955421799 scopus 로고    scopus 로고
    • Metastable alloys
    • K. Hashimoto Metastable alloys E. Winston Revie, Uhlig's Corrosion Handbook 2nd ed 2000 John Wiley & Sons, Inc. 929 939
    • (2000) Uhlig's Corrosion Handbook , pp. 929-939
    • Hashimoto, K.1
  • 11
    • 38649116988 scopus 로고    scopus 로고
    • Corrosion of amorphous metals
    • J.R. Scully, and A. Lucente Corrosion of amorphous metals S.D. Cramer, B. Covino Jr ASM Handbook vol. 13B 2005 American Society for Metals Metals Park, OH 476 489
    • (2005) ASM Handbook , vol.13 , pp. 476-489
    • Scully, J.R.1    Lucente, A.2
  • 12
    • 0036849416 scopus 로고    scopus 로고
    • Corrosion behaviour of Zr-based bulk glass-forming alloys containing Nb or Ti
    • V.R. Raju, U. Kühn, U. Wolff, F. Schneider, J. Eckert, and R. Reiche Corrosion behaviour of Zr-based bulk glass-forming alloys containing Nb or Ti Mater Lett 57 2002 173 177
    • (2002) Mater Lett , vol.57 , pp. 173-177
    • Raju, V.R.1    Kühn, U.2    Wolff, U.3    Schneider, F.4    Eckert, J.5    Reiche, R.6
  • 13
    • 0036857515 scopus 로고    scopus 로고
    • Localized corrosion behavior of a Zr-based bulk metallic glass relative to its crystalline state
    • W.H. Peter, R.A. Buchanan, C.T. Liu, P.K. Liaw, M.L. Morrison, and J.A. Horton Localized corrosion behavior of a Zr-based bulk metallic glass relative to its crystalline state Intermetallics 10 2002 1157 1162
    • (2002) Intermetallics , vol.10 , pp. 1157-1162
    • Peter, W.H.1    Buchanan, R.A.2    Liu, C.T.3    Liaw, P.K.4    Morrison, M.L.5    Horton, J.A.6
  • 15
    • 64849106104 scopus 로고    scopus 로고
    • Effect of structural defects, surface irregularities, and quenched-in defects on corrosion of Zr-based metallic glasses
    • B. Vishwanadh, G.J. Abraham, Neogy S. Jagannath, R.S. Dutta, and G.K. Dey Effect of structural defects, surface irregularities, and quenched-in defects on corrosion of Zr-based metallic glasses Metall. Mater Trans 40A 2009 1131 1141
    • (2009) Metall. Mater Trans , vol.40 , pp. 1131-1141
    • Vishwanadh, B.1    Abraham, G.J.2    Jagannath, N.S.3    Dutta, R.S.4    Dey, G.K.5
  • 17
    • 70449625328 scopus 로고    scopus 로고
    • Corrosion of a Zr-based bulk metallic glass with different surface finishing states
    • A. Gebert, P.F. Gostin, U. Kühn, and L. Schultz Corrosion of a Zr-based bulk metallic glass with different surface finishing states ECS Transactions 2008 doi:10.1149/1.3091901
    • (2008) ECS Transactions
    • Gebert, A.1    Gostin, P.F.2    Kühn, U.3    Schultz, L.4
  • 18
    • 77049105109 scopus 로고    scopus 로고
    • Eckert J. Effect of shot-peening on the corrosion resistance of a Zr-based BMG
    • A. Gebert, A. Concustell, A.L. Greer, and L. Schultz Eckert J. Effect of shot-peening on the corrosion resistance of a Zr-based BMG Scripta Mater 2010 doi:10.1016/j.scriptamat.2010.01.004.
    • (2010) Scripta Mater
    • Gebert, A.1    Concustell, A.2    Greer, A.L.3    Schultz, L.4
  • 20
    • 0035906783 scopus 로고    scopus 로고
    • Environmental properties of Zr-based metallic glasses and nanocrystalline alloys
    • U. Köster, D. Zander, Rüdiger A. Triwikantoro, and L. Jastrow Environmental properties of Zr-based metallic glasses and nanocrystalline alloys Scr Mater 44 2001 1649 1654
    • (2001) Scr Mater , vol.44 , pp. 1649-1654
    • Köster, U.1    Zander, D.2    Triwikantoro, R.A.3    Jastrow, L.4
  • 21
    • 2942750522 scopus 로고    scopus 로고
    • Corrosion resistance of Zr-based bulk amorphous alloys containing Pd
    • F.X. Qin, H.F. Zhang, Y.F. Deng, B.Z. Ding, and Z.Q. Hu Corrosion resistance of Zr-based bulk amorphous alloys containing Pd J Alloys Compd 375 2004 318 323
    • (2004) J Alloys Compd , vol.375 , pp. 318-323
    • Qin, F.X.1    Zhang, H.F.2    Deng, Y.F.3    Ding, B.Z.4    Hu, Z.Q.5
  • 24
    • 45449087711 scopus 로고    scopus 로고
    • Pitting corrosion of Cu-Zr metallic glasses in hydrochloric acid solutions
    • H.B. Lu, L.C. Zhang, A. Gebert, and L. Schultz Pitting corrosion of Cu-Zr metallic glasses in hydrochloric acid solutions J Alloys Compd 462 2008 60 67
    • (2008) J Alloys Compd , vol.462 , pp. 60-67
    • Lu, H.B.1    Zhang, L.C.2    Gebert, A.3    Schultz, L.4
  • 25
  • 26
    • 67650590964 scopus 로고    scopus 로고
    • Devitrification of Fe-based amorphous metal SAM 1651 and the effect of heat-treatment on corrosion behavior
    • H.M. Ha, J.R. Miller, and J.H. Payer Devitrification of Fe-based amorphous metal SAM 1651 and the effect of heat-treatment on corrosion behavior J Electrochem Soc 156 2009 C246 C252
    • (2009) J Electrochem Soc , vol.156
    • Ha, H.M.1    Miller, J.R.2    Payer, J.H.3
  • 27
    • 71349087494 scopus 로고    scopus 로고
    • Effect of hydrofluoric acid treatment on the crystallisation behaviour of Zr-Ti-Cu-Al-Ni metallic glass
    • J. Paillier, and A. Gebert Effect of hydrofluoric acid treatment on the crystallisation behaviour of Zr-Ti-Cu-Al-Ni metallic glass Thermochim Acta 497 2010 85 95
    • (2010) Thermochim Acta , vol.497 , pp. 85-95
    • Paillier, J.1    Gebert, A.2
  • 28
    • 22644431660 scopus 로고    scopus 로고
    • Artifacts induced in metallic glasses during TEM sample preparation
    • B.B. Sun, Y.B. Wang, J. Wen, H. Yang, M.L. Sui, and J.Q. Wang Artifacts induced in metallic glasses during TEM sample preparation Scr Mater 53 2005 805 809
    • (2005) Scr Mater , vol.53 , pp. 805-809
    • Sun, B.B.1    Wang, Y.B.2    Wen, J.3    Yang, H.4    Sui, M.L.5    Wang, J.Q.6
  • 31
    • 0037131883 scopus 로고    scopus 로고
    • Effect of surface pretreatment on the electrochemical activity of a glass-forming Zr-Ti-Al-Cu-Ni alloy
    • U. Wolff, A. Gebert, J. Eckert, and L. Schultz Effect of surface pretreatment on the electrochemical activity of a glass-forming Zr-Ti-Al-Cu-Ni alloy J Alloys Compd 346 2002 222 229
    • (2002) J Alloys Compd , vol.346 , pp. 222-229
    • Wolff, U.1    Gebert, A.2    Eckert, J.3    Schultz, L.4
  • 32
    • 69149093493 scopus 로고    scopus 로고
    • Online hyphenation of potentiostat to a microflow-capillary FI-ICP-MS for simultaneous in situ electrochemical, time and element resolved characterization of local corrosion processes
    • N. Homazava, T. Suter, P. Schmutz, S. Toggweiler, A. Grimberg, and U. Krähenbühl Online hyphenation of potentiostat to a microflow-capillary FI-ICP-MS for simultaneous in situ electrochemical, time and element resolved characterization of local corrosion processes J Anal At Spectrom 24 2009 1161 1169
    • (2009) J Anal at Spectrom , vol.24 , pp. 1161-1169
    • Homazava, N.1    Suter, T.2    Schmutz, P.3    Toggweiler, S.4    Grimberg, A.5    Krähenbühl, U.6
  • 33
    • 0026945022 scopus 로고
    • Metallic impurities segregation at the interface between Si wafer and liquid during wet cleaning
    • T. Ohmi, T. Imaoka, I. Sugiyama, and T. Kezuka Metallic impurities segregation at the interface between Si wafer and liquid during wet cleaning J Electrochem Soc 139 1992 3317 3335 (Pubitemid 23597607)
    • (1992) Journal of the Electrochemical Society , vol.139 , Issue.11 , pp. 3317-3335
    • Ohmi, T.1    Imaoka, T.2    Sugiyama, I.3    Kezuka, T.4
  • 34
    • 58749106955 scopus 로고    scopus 로고
    • Formation of rosette-like nanopatterns by selective corrosion of metallic glass
    • J. Yu, W. Zhang, A. Inoue, T. Sakurai, H. Kimura, and M. Chen Formation of rosette-like nanopatterns by selective corrosion of metallic glass Jpn J Appl Phys 47 2008 8678 8680
    • (2008) Jpn J Appl Phys , vol.47 , pp. 8678-8680
    • Yu, J.1    Zhang, W.2    Inoue, A.3    Sakurai, T.4    Kimura, H.5    Chen, M.6
  • 35
    • 24644467739 scopus 로고    scopus 로고
    • Characterization of oxide layers on amorphous Zr-based alloys by Auger electron spectroscopy with sputter depth profiling
    • S. Baunack, Mudali U. Kamachi, and A. Gebert Characterization of oxide layers on amorphous Zr-based alloys by Auger electron spectroscopy with sputter depth profiling Appl Surf Sci 252 2005 162 166
    • (2005) Appl Surf Sci , vol.252 , pp. 162-166
    • Baunack, S.1    Kamachi, M.U.2    Gebert, A.3
  • 36
    • 0034226760 scopus 로고    scopus 로고
    • Copper deposition during the corrosion of aluminum alloy 2024 in sodium chloride solutions
    • H.M. Obispo, L.E. Murr, R.M. Arrowood, and E.A. Trillo Copper deposition during the corrosion of aluminum alloy 2024 in sodium chloride solutions J Mater Sci 35 2000 3479 3495
    • (2000) J Mater Sci , vol.35 , pp. 3479-3495
    • Obispo, H.M.1    Murr, L.E.2    Arrowood, R.M.3    Trillo, E.A.4
  • 37
    • 50249179088 scopus 로고    scopus 로고
    • Element-specific in situ corrosion behavior of Zr-Cu-Ni-Al-Nb bulk metallic glass in acidic media studied using a novel microcapillary flow injection inductively coupled plasma mass spectrometry technique
    • N. Homazava, A. Shabko, D. Logvinovich, U. Krähenbühl, and A. Ulrich Element-specific in situ corrosion behavior of Zr-Cu-Ni-Al-Nb bulk metallic glass in acidic media studied using a novel microcapillary flow injection inductively coupled plasma mass spectrometry technique Intermetallics 16 2008 1066 1072
    • (2008) Intermetallics , vol.16 , pp. 1066-1072
    • Homazava, N.1    Shabko, A.2    Logvinovich, D.3    Krähenbühl, U.4    Ulrich, A.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.