메뉴 건너뛰기




Volumn 256, Issue 23, 2010, Pages 7102-7110

Bioactive glass thin films deposited by magnetron sputtering technique: The role of working pressure

Author keywords

Bioglass thin films; Biomineralization; Carbonated hydroxyapatite; Magnetron sputtering; SBF

Indexed keywords

BIOACTIVE GLASS; BIOMINERALIZATION; COATINGS; HYDROXYAPATITE; MAGNETRON SPUTTERING; TEMPERATURE;

EID: 77955305506     PISSN: 01694332     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.apsusc.2010.05.035     Document Type: Article
Times cited : (36)

References (47)
  • 3
    • 66849129389 scopus 로고    scopus 로고
    • Evaluation of the interactions between collagen and the surface of a bioactive glass during in vitro test
    • R. Oréfice, L. Hench, and A. Brennan Evaluation of the interactions between collagen and the surface of a bioactive glass during in vitro test J. Biomed. Mater. Res-A 90 1 2009 114 120
    • (2009) J. Biomed. Mater. Res-A , vol.90 , Issue.1 , pp. 114-120
    • Oréfice, R.1    Hench, L.2    Brennan, A.3
  • 4
    • 67349179185 scopus 로고    scopus 로고
    • Differentiation of fetal osteoblasts and formation of mineralized bone nodules by 45S5 Bioglass® conditioned medium in the absence of osteogenic supplements
    • O. Tsigkou, J.R. Jones, J.M. Polak, and M.M. Stevens Differentiation of fetal osteoblasts and formation of mineralized bone nodules by 45S5 Bioglass® conditioned medium in the absence of osteogenic supplements Biomaterials 30 2009 3542 3550
    • (2009) Biomaterials , vol.30 , pp. 3542-3550
    • Tsigkou, O.1    Jones, J.R.2    Polak, J.M.3    Stevens, M.M.4
  • 6
    • 57949084889 scopus 로고    scopus 로고
    • Bioactive glass nanopowder and bioglass coating for biocompatibility improvement of metallic implant
    • M.H. Fathi, and A. Doostmohammadi Bioactive glass nanopowder and bioglass coating for biocompatibility improvement of metallic implant J. Mater. Process. Technol. 209 2009 1385 1391
    • (2009) J. Mater. Process. Technol. , vol.209 , pp. 1385-1391
    • Fathi, M.H.1    Doostmohammadi, A.2
  • 8
    • 45849127236 scopus 로고    scopus 로고
    • Bioactive borate glass coatings for titanium alloys
    • L. Peddi, R.K. Brow, and R.F. Brown Bioactive borate glass coatings for titanium alloys J. Mater. Sci. -Mater. Med. 19 2008 3145 3152
    • (2008) J. Mater. Sci. -Mater. Med. , vol.19 , pp. 3145-3152
    • Peddi, L.1    Brow, R.K.2    Brown, R.F.3
  • 10
    • 1542350252 scopus 로고    scopus 로고
    • The effect of bond coat on mechanical properties of plasma sprayed bioglass-titanium coatings
    • G. Goller The effect of bond coat on mechanical properties of plasma sprayed bioglass-titanium coatings Ceram. Int. 30 2004 351 355
    • (2004) Ceram. Int. , vol.30 , pp. 351-355
    • Goller, G.1
  • 14
    • 68649100124 scopus 로고    scopus 로고
    • Effect of annealing upon the structure and adhesion properties of sputtered bio-glass/titanium coatings
    • G.E. Stan, C.O. Morosanu, D.A. Marcov, I. Pasuk, F. Miculescu, and G. Reumont Effect of annealing upon the structure and adhesion properties of sputtered bio-glass/titanium coatings Appl. Surf. Sci. 255 2009 9132 9138
    • (2009) Appl. Surf. Sci. , vol.255 , pp. 9132-9138
    • Stan, G.E.1    Morosanu, C.O.2    Marcov, D.A.3    Pasuk, I.4    Miculescu, F.5    Reumont, G.6
  • 16
    • 0346753804 scopus 로고    scopus 로고
    • Surface potential change in bioactive titanium metal during the process of apatite formation in simulated body fluid
    • H.-M. Kim, T. Himeno, M. Kawashita, J.-H. Lee, T. Kokubo, and T. Nakamura Surface potential change in bioactive titanium metal during the process of apatite formation in simulated body fluid J. Biomed. Mater. Res.-A 67 4 2003 1305 1309
    • (2003) J. Biomed. Mater. Res.-A , vol.67 , Issue.4 , pp. 1305-1309
    • Kim, H.-M.1    Himeno, T.2    Kawashita, M.3    Lee, J.-H.4    Kokubo, T.5    Nakamura, T.6
  • 18
    • 71549170825 scopus 로고    scopus 로고
    • Tailoring the bioactivity of commercially pure titanium by grain refinement using groove pressing
    • A. Thirugnanam, T.S. Sampath Kumar, and U. Chakkingal Tailoring the bioactivity of commercially pure titanium by grain refinement using groove pressing Mater. Sci. Eng. C 30 2010 203 208
    • (2010) Mater. Sci. Eng. C , vol.30 , pp. 203-208
    • Thirugnanam, A.1    Sampath Kumar, T.S.2    Chakkingal, U.3
  • 19
    • 0025449531 scopus 로고
    • Solutions able to reproduce in vivo surface-structure change in bioactive glass-ceramic A-W
    • T. Kokubo, H. Kushitani, S. Sakka, T. Kitsugi, and T. Yamamuro Solutions able to reproduce in vivo surface-structure change in bioactive glass-ceramic A-W J. Biomed. Mater. Res. 24 1990 721 734
    • (1990) J. Biomed. Mater. Res. , vol.24 , pp. 721-734
    • Kokubo, T.1    Kushitani, H.2    Sakka, S.3    Kitsugi, T.4    Yamamuro, T.5
  • 20
    • 32144437418 scopus 로고    scopus 로고
    • How useful is SBF in predicting in vivo bone bioactivity?
    • T. Kokubo, and H. Takadama How useful is SBF in predicting in vivo bone bioactivity? Biomaterials 27 2006 2907 2915
    • (2006) Biomaterials , vol.27 , pp. 2907-2915
    • Kokubo, T.1    Takadama, H.2
  • 21
    • 0020940620 scopus 로고
    • Determination of the thickness and optical constants of amorphous silicon
    • R.J. Swanepoel Determination of the thickness and optical constants of amorphous silicon J. Phys. E. Sci. Instrum. 16 1983 1214 1222
    • (1983) J. Phys. E. Sci. Instrum. , vol.16 , pp. 1214-1222
    • Swanepoel, R.J.1
  • 22
    • 34247572519 scopus 로고    scopus 로고
    • One-dimensional analysis of the rate of plasma-assisted sputter deposition
    • A. Palmero, H. Rudolph, and H.P.M. Habraken One-dimensional analysis of the rate of plasma-assisted sputter deposition J. Appl. Phys. 101 2007 083307-083307-6
    • (2007) J. Appl. Phys. , vol.101
    • Palmero, A.1    Rudolph, H.2    Habraken, H.P.M.3
  • 23
    • 35548953580 scopus 로고    scopus 로고
    • On the ion and neutral atom bombardment of the growth surface in magnetron plasma sputter deposition
    • E.D. van Hattum, A. Palmero, W.M. Arnoldbik, H. Rudolph, and F.H.P.M. Habraken On the ion and neutral atom bombardment of the growth surface in magnetron plasma sputter deposition Appl. Phys. Lett. 91 2007 171501-171501-3
    • (2007) Appl. Phys. Lett. , vol.91
    • Van Hattum, E.D.1    Palmero, A.2    Arnoldbik, W.M.3    Rudolph, H.4    Habraken, F.H.P.M.5
  • 24
    • 77955305162 scopus 로고    scopus 로고
    • http://www.doitpoms.ac.uk/tlplib/ellingham-diagrams/ellingham.php
  • 25
    • 77955309876 scopus 로고    scopus 로고
    • http://www.doitpoms.ac.uk/tlplib/ellingham-diagrams/interactive.php
  • 28
    • 34250099141 scopus 로고
    • Stabilization of radiation centers on non-bridging oxygen atoms in vitreous silicon dioxide
    • O.N. Bilan, N.G. Cherenda, and D.M. Yudin Stabilization of radiation centers on non-bridging oxygen atoms in vitreous silicon dioxide J. Appl. Spectrosc. 45 6 1986 1319 1321
    • (1986) J. Appl. Spectrosc. , vol.45 , Issue.6 , pp. 1319-1321
    • Bilan, O.N.1    Cherenda, N.G.2    Yudin, D.M.3
  • 33
    • 14944358653 scopus 로고    scopus 로고
    • Preparation and comprehensive characterization of a calcium hydroxyapatite reference material
    • M. Markovic, B.O. Fowler, and M.S. Tung Preparation and comprehensive characterization of a calcium hydroxyapatite reference material J. Res. Natl. Inst. Stand. Technol. 109 2004 553 568
    • (2004) J. Res. Natl. Inst. Stand. Technol. , vol.109 , pp. 553-568
    • Markovic, M.1    Fowler, B.O.2    Tung, M.S.3
  • 37
    • 84865737490 scopus 로고
    • Bioceramics: From concept to clinic
    • L.L. Hench Bioceramics: from concept to clinic J. Am. Ceram. Soc. 74 1991 1487 1510
    • (1991) J. Am. Ceram. Soc. , vol.74 , pp. 1487-1510
    • Hench, L.L.1
  • 38
    • 48049117101 scopus 로고    scopus 로고
    • The role of the pressure in pulsed laser deposition of bioactive glass films
    • Y. Zhao, M. Song, C. Chen, and J. Liu The role of the pressure in pulsed laser deposition of bioactive glass films J. Non-Cryst. Solids 354 2008 4000 4004
    • (2008) J. Non-Cryst. Solids , vol.354 , pp. 4000-4004
    • Zhao, Y.1    Song, M.2    Chen, C.3    Liu, J.4
  • 39
    • 75949103646 scopus 로고    scopus 로고
    • Adherent functional graded hydroxylapatite coatings produced by sputtering deposition techniques
    • G.E. Stan Adherent functional graded hydroxylapatite coatings produced by sputtering deposition techniques J. Optoelectron. Adv. Mater. 11 2009 1132 1138
    • (2009) J. Optoelectron. Adv. Mater. , vol.11 , pp. 1132-1138
    • Stan, G.E.1
  • 40


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.