Volumn 12, Issue 1, 2010, Pages 27-31

Effect of chlorhexidine application in a self-etching adhesive on the immediate resin-dentin bond strength

Author keywords

Bond degradation; Chlorhexidine; Matrix metalloproteinases; Microtensile bond test; Self etching adhesives

Indexed keywords

CHLORHEXIDINE; CLEARFIL SE BOND; DENTIN BONDING AGENT; RESIN; RESIN CEMENT; TOPICAL ANTIINFECTIVE AGENT;

EID: 77951218829     PISSN: 14615185     EISSN: 17579988     Source Type: Journal    
DOI: 10.3290/j.jad.a17543     Document Type: Article
Times cited : (38)

References (35)
  • 1
    • 0035343992 scopus 로고    scopus 로고
    • Mode of failure in the dentin-adhesive resin-resin composite bonded joint as determined by strength-based (µTBS) and fracture-based (CNSB) mechanical testing
    • Armstrong SR, Keller JC, Boyer DB. Mode of failure in the dentin-adhesive resin-resin composite bonded joint as determined by strength-based (µTBS) and fracture-based (CNSB) mechanical testing. Dent Mater 2001; 17: 201-210.
    • (2001) Dent Mater , vol.17 , pp. 201-210
    • Armstrong, S.R.1    Keller, J.C.2    Boyer, D.B.3
  • 2
    • 0035350653 scopus 로고    scopus 로고
    • The influence of water storage and Cfactor on the dentin-resin composite microtensile bond strength and debond pathway utilizing a filled and unfilled adhesive resin
    • Armstrong SR, Keller JC, Boyer DB. The influence of water storage and Cfactor on the dentin-resin composite microtensile bond strength and debond pathway utilizing a filled and unfilled adhesive resin. Dent Mater 2001;17: 268-276.
    • (2001) Dent Mater , vol.17 , pp. 268-276
    • Armstrong, S.R.1    Keller, J.C.2    Boyer, D.B.3
  • 3
    • 12344299287 scopus 로고    scopus 로고
    • Resin-dentin interfacial ultrastructure and microtensile dentin bond strength after five-year water storage
    • Armstrong SR, Vargas MA, Chung I, Pashley DH, Campbell JA, Laffoon JE, Qian F. Resin-dentin interfacial ultrastructure and microtensile dentin bond strength after five-year water storage. Oper Dent 2004;29: 705-712.
    • (2004) Oper Dent , vol.29 , pp. 705-712
    • Armstrong, S.R.1    Vargas, M.A.2    Chung, I.3    Pashley, D.H.4    Campbell, J.A.5    Laffoon, J.E.6    Qian, F.7
  • 4
    • 0042809966 scopus 로고    scopus 로고
    • Microtensile bond strength of a total-etch 3-step, total-etch 2-step, self-etch 2-step, and a self-etch 1- step dentin bonding system through 15-month water storage
    • Armstrong SR, Vargas MA, Fang Q, Laffoon JE. Microtensile bond strength of a total-etch 3-step, total-etch 2-step, self-etch 2-step, and a self-etch 1- step dentin bonding system through 15-month water storage. J Adhes Dent 2003;5: 47-56.
    • (2003) J Adhes Dent , vol.5 , pp. 47-56
    • Armstrong, S.R.1    Vargas, M.A.2    Fang, Q.3    Laffoon, J.E.4
  • 5
    • 14644444542 scopus 로고    scopus 로고
    • Matrix metalloproteinases inhibition impairs the processing, formation and mineralization of dental tissues during mouse molar development
    • Bourd-Boittin K, Fridman R, Fanchon S, Septier D, Goldberg M, Menashi S. Matrix metalloproteinases inhibition impairs the processing, formation and mineralization of dental tissues during mouse molar development. Exp Cell Res 2005;304: 493-505.
    • (2005) Exp Cell Res , vol.304 , pp. 493-505
    • Bourd-Boittin, K.1    Fridman, R.2    Fanchon, S.3    Septier, D.4    Goldberg, M.5    Menashi, S.6
  • 7
    • 0030225111 scopus 로고    scopus 로고
    • Dentin bond durability after three years using a dentin bonding agent with and without priming
    • Burrow MF, Satoh M, Tagami J. Dentin bond durability after three years using a dentin bonding agent with and without priming. Dent Mater 1996;12: 302-307.
    • (1996) Dent Mater , vol.12 , pp. 302-307
    • Burrow, M.F.1    Satoh, M.2    Tagami, J.3
  • 13
    • 0034281213 scopus 로고    scopus 로고
    • The effect of caries detector dyes and a cavity cleansing agent on composite resin bonding to enamel and dentin
    • el-Housseiny AA, Jamjoum H. The effect of caries detector dyes and a cavity cleansing agent on composite resin bonding to enamel and dentin. J Clin Pediatr Dent 2000;25: 57-63.
    • (2000) J Clin Pediatr Dent , vol.25 , pp. 57-63
    • El-Housseiny, A.A.1    Jamjoum, H.2
  • 14
    • 0032911382 scopus 로고    scopus 로고
    • Inhibition of the activities of matrix metalloproteinases 2, 8, and 9 by chlorhexidine
    • Gendron R, Grenier D, Sorsa T, Mayrand D. Inhibition of the activities of matrix metalloproteinases 2, 8, and 9 by chlorhexidine. Clin Diagn Lab Immunol 1999;6: 437-439.
    • (1999) Clin Diagn Lab Immunol , vol.6 , pp. 437-439
    • Gendron, R.1    Grenier, D.2    Sorsa, T.3    Mayrand, D.4
  • 15
    • 0029286296 scopus 로고
    • Effect of long-term water storage on dentin bonding
    • Gwinnett AJ, Yu S. Effect of long-term water storage on dentin bonding. Am J Dent 1995;8: 109-111.
    • (1995) Am J Dent , vol.8 , pp. 109-111
    • Gwinnett, A.J.1    Yu, S.2
  • 16
    • 0038122968 scopus 로고    scopus 로고
    • In vitro degradation of resin-dentin bonds analyzed by microtensile bond test, scanning and transmission electron microscopy
    • Hashimoto M, Ohno H, Sano H, Kaga M, Oguchi H. In vitro degradation of resin-dentin bonds analyzed by microtensile bond test, scanning and transmission electron microscopy. Biomaterials 2003;24: 3795-3803.
    • (2003) Biomaterials , vol.24 , pp. 3795-3803
    • Hashimoto, M.1    Ohno, H.2    Sano, H.3    Kaga, M.4    Oguchi, H.5
  • 19
    • 33645364093 scopus 로고    scopus 로고
    • Chlorhexidine arrests subclinical breakdown of dentin hybrid layers in vivo
    • Hebling J, Pashley DH, Tjäderhane L, Tay FR. Chlorhexidine arrests subclinical breakdown of dentin hybrid layers in vivo. J Dent Res 2005;84: 741-746.
    • (2005) J Dent Res , vol.84 , pp. 741-746
    • Hebling, J.1    Pashley, D.H.2    Tjäderhane, L.3    Tay, F.R.4
  • 20
    • 0034783857 scopus 로고    scopus 로고
    • Me-ta-analytical review of factors involved in dentin adherence
    • Leloup G, D’Hoore W, Bouter D, Degrange M, Vreven J. Me-ta-analytical review of factors involved in dentin adherence. J Dent Res 2001;80: 1605-1614.
    • (2001) J Dent Res , vol.80 , pp. 1605-1614
    • Leloup, G.1    D’Hoore, W.2    Bouter, D.3    Degrange, M.4    Vreven, J.5
  • 27
    • 0028418126 scopus 로고
    • Effects of chlorhexidine on dentin surfaces and shear bond strengths
    • Perdigão J, Denehy GE, Swift EJ Jr. Effects of chlorhexidine on dentin surfaces and shear bond strengths. Am J Dent 1994;7: 81-84.
    • (1994) Am J Dent , vol.7 , pp. 81-84
    • Perdigão, J.1    Denehy, G.E.2    Swift, E.J.3
  • 28
    • 0035511953 scopus 로고    scopus 로고
    • Effect of preliminary treatment of the dentin surface on the shear bond strength of resin composite to dentin
    • Pilo R, Cardash HS, Oz-Ari B, Ben-Amar A. Effect of preliminary treatment of the dentin surface on the shear bond strength of resin composite to dentin. Oper Dent 2001;26: 569-575.
    • (2001) Oper Dent , vol.26 , pp. 569-575
    • Pilo, R.1    Cardash, H.S.2    Oz-Ari, B.3    Ben-Amar, A.4
  • 29
    • 0028476472 scopus 로고
    • Relationship between surface area for adhesion and tensile bond strength: Evaluation of a micro-tensile bond test
    • Sano H, Shono T, Sonoda H, Takatsu T, Ciucchi B, Carvalho R, Pashley DH. Relationship between surface area for adhesion and tensile bond strength: evaluation of a micro-tensile bond test. Dent Mater 1994;10: 236-240.
    • (1994) Dent Mater , vol.10 , pp. 236-240
    • Sano, H.1    Shono, T.2    Sonoda, H.3    Takatsu, T.4    Ciucchi, B.5    Carvalho, R.6    Pashley, D.H.7
  • 30
    • 0346787868 scopus 로고    scopus 로고
    • In vitro effect of cavity disinfectants on the bond strength of dentin bonding systems
    • Say EC, Koray F, Tarim B, Soyman M, Gulmez T. In vitro effect of cavity disinfectants on the bond strength of dentin bonding systems. Quintessence Int 2004;35: 56-60.
    • (2004) Quintessence Int , vol.35 , pp. 56-60
    • Say, E.C.1    Koray, F.2    Tarim, B.3    Soyman, M.4    Gulmez, T.5
  • 31
    • 0036719793 scopus 로고    scopus 로고
    • The localization of matrix metalloproteinase-20 (MMP-20, enamelysin) in mature human teeth
    • Sulkala M, Larmas M, Sorsa T, Salo T, Tjäderhane L. The localization of matrix metalloproteinase-20 (MMP-20, enamelysin) in mature human teeth. J Dent Res 2002;81: 603-608.
    • (2002) J Dent Res , vol.81 , pp. 603-608
    • Sulkala, M.1    Larmas, M.2    Sorsa, T.3    Salo, T.4    Tjäderhane, L.5
  • 34
    • 0032223705 scopus 로고    scopus 로고
    • The activation and function of host matrix metalloproteinases in dentin matrix breakdown in caries lesions
    • Tjäderhane L, Larjava H, Sorsa T, Uittol VJ, Larmas M, Salol T. The activation and function of host matrix metalloproteinases in dentin matrix breakdown in caries lesions. J Dent Res 1998;77: 1622-1629.
    • (1998) J Dent Res , vol.77 , pp. 1622-1629
    • Tjäderhane, L.1    Larjava, H.2    Sorsa, T.3    Uittol, V.J.4    Larmas, M.5    Salol, T.6


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.