Volumn , Issue , 2006, Pages 536-559

Silicon nitride and silicon carbide-based ceramics

Author keywords

[No Author keywords available]

Indexed keywords


EID: 72449149917     PISSN: None     EISSN: None     Source Type: Book    
DOI: 10.1533/9781845691066     Document Type: Chapter
Times cited : (2)

References (39)
  • 1
    • 84987335986 scopus 로고
    • 'A critical evaluation of indentation techniques for measuring fracture toughness: I, Direct crack measurements'
    • Anstis, G.R., et al. (1981), 'A critical evaluation of indentation techniques for measuring fracture toughness: I, Direct crack measurements', J. Am. Ceram. Soc., 64(9), 533-8.
    • (1981) J. Am. Ceram. Soc. , vol.64 , Issue.9 , pp. 533-538
    • Anstis, G.R.1
  • 2
    • 0003893686 scopus 로고
    • 'The determination of density, porosity and water absorption'
    • AS 1774.5
    • AS 1774.5 (1979), 'The determination of density, porosity and water absorption', Standards Association of Australia, 1-3.
    • (1979) Standards Association of Australia , pp. 1-3
  • 3
    • 0027188897 scopus 로고
    • 'The influence of microstructure on the mechanical behaviour of silicon nitride ceramics'
    • Chen I-W, MRS, Pittsburgh, PA
    • Becher, P.F. et al. (1993), 'The influence of microstructure on the mechanical behaviour of silicon nitride ceramics', in Chen I-W, Silicon Nitride - Scientific and Technological Advances, MRS Symposium Proceedings, 287, MRS, Pittsburgh, PA, p. 147.
    • (1993) Silicon Nitride - Scientific and Technological Advances, MRS Symposium Proceedings , vol.287 , pp. 147
    • Becher, P.F.1
  • 4
    • 0001935647 scopus 로고
    • 'Microstructural contribution to the fracture resistance of silicon nitride ceramics'
    • Hoffmann M. J. and Petzow G., Dordrecht, Kluwer Academic
    • Becher, P.F. et al. (1994), 'Microstructural contribution to the fracture resistance of silicon nitride ceramics', in Hoffmann M. J. and Petzow G., Tailoring of Mechanical Properties of Si3N4 Ceramics, NATO ASI Series, Series E: Applied Science, 276, Dordrecht, Kluwer Academic, 87-100.
    • (1994) Tailoring of Mechanical Properties of Si3N4 Ceramics, NATO ASI Series, Series E: Applied Science , vol.276 , pp. 87-100
    • Becher, P.F.1
  • 5
    • 0032207131 scopus 로고    scopus 로고
    • 'Microstructural design of silicon nitride with improved fracture toughness: I, Effects of grain shape and size'
    • Becher, P.F. et al. (1998), 'Microstructural design of silicon nitride with improved fracture toughness: I, Effects of grain shape and size', J. Am. Ceram. Soc., 81(11), 2821-30.
    • (1998) J. Am. Ceram. Soc. , vol.81 , Issue.11 , pp. 2821-2830
    • Becher, P.F.1
  • 6
    • 0024751958 scopus 로고
    • 'Role of interfacial grain-bridging sliding friction in crack-resistance and strength properties of non-transforming ceramics'
    • Bennison, S.J. and Lawn, B.R. (1989), 'Role of interfacial grain-bridging sliding friction in crack-resistance and strength properties of non-transforming ceramics', Acta Metall. Mater., 37(10), 2659-71.
    • (1989) Acta Metall. Mater. , vol.37 , Issue.10 , pp. 2659-2671
    • Bennison, S.J.1    Lawn, B.R.2
  • 7
    • 33751500834 scopus 로고
    • 'α-Sialon ceramics: a review'
    • Cao, G.Z. and Metselaar, R. (1991), 'α-Sialon ceramics: a review', Chem. Mater., 3, 242-52.
    • (1991) Chem. Mater. , vol.3 , pp. 242-252
    • Cao, G.Z.1    Metselaar, R.2
  • 8
    • 0033337384 scopus 로고    scopus 로고
    • 'Model for fatigue crack growth in grain-bridging ceramics'
    • Chen, I.-W. and Engineer, M. (1999), 'Model for fatigue crack growth in grain-bridging ceramics', J. Am. Ceram. Soc., 82(12), 3549-60.
    • (1999) J. Am. Ceram. Soc. , vol.82 , Issue.12 , pp. 3549-3560
    • Chen, I.-W.1    Engineer, M.2
  • 9
    • 0030671549 scopus 로고    scopus 로고
    • 'A tough SiAlON ceramic based on α-Si3N4 with a whisker-like microstructure'
    • Chen, I.-W. and Rosenflanz, A. (1997), 'A tough SiAlON ceramic based on α-Si3N4 with a whisker-like microstructure', Nature, 389, 701-4.
    • (1997) Nature , vol.389 , pp. 701-704
    • Chen, I.-W.1    Rosenflanz, A.2
  • 10
    • 0032208008 scopus 로고    scopus 로고
    • 'Microstructural design of silicon nitride with improved fracture toughness: II, Effects of yttria and alumina additives'
    • Ellen, Y.S. et al. (1998), 'Microstructural design of silicon nitride with improved fracture toughness: II, Effects of yttria and alumina additives', J. Am. Ceram. Soc., 81(11), 2831-40.
    • (1998) J. Am. Ceram. Soc. , vol.81 , Issue.11 , pp. 2831-2840
    • Ellen, Y.S.1
  • 11
    • 0017982146 scopus 로고
    • 'Impact damage in brittle materials in the elastic-plastic response regime'
    • Evans, A.G. et al. (1978), 'Impact damage in brittle materials in the elastic-plastic response regime', Proc. R. Soc. London, Ser. A, 361, 343-65.
    • (1978) Proc. R. Soc. London, Ser. A , vol.361 , pp. 343-365
    • Evans, A.G.1
  • 12
    • 0023327964 scopus 로고
    • 'Crack-interface grain bridging as a fracture resistance mechanism in ceramics'
    • Fairbanks, C.J. et al. (1987), 'Crack-interface grain bridging as a fracture resistance mechanism in ceramics', J. Am. Ceram. Soc., 70, 279-94.
    • (1987) J. Am. Ceram. Soc. , vol.70 , pp. 279-294
    • Fairbanks, C.J.1
  • 13
    • 36849158053 scopus 로고
    • 'α-Sialon ceramics'
    • Hampshire, S. et al. (1978), 'α-Sialon ceramics', Nature, 274, 880-2.
    • (1978) Nature , vol.274 , pp. 880-882
    • Hampshire, S.1
  • 14
    • 0029325006 scopus 로고
    • 'Processing strategy for producing highly anisotropic silicon nitride'
    • Hirao, K. et al. (1995), 'Processing strategy for producing highly anisotropic silicon nitride', J. Am. Ceram. Soc., 78(6), 1687-90.
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.6 , pp. 1687-1690
    • Hirao, K.1
  • 15
    • 0001859143 scopus 로고
    • 'Analysis of microstructural development and mechanical properties of Si3N4 ceramics'
    • Hoffmann, M. J. and Petzow, G., Dordrecht, Kluwer Academic
    • Hoffmann, M.J. (1994), 'Analysis of microstructural development and mechanical properties of Si3N4 ceramics', in Hoffmann, M. J. and Petzow, G., Tailoring of Mechanical Properties of Si3N4 ceramics, NATO ASI Series, Series E: Applied Science, 276, Dordrecht, Kluwer Academic, 59-71.
    • (1994) Tailoring of Mechanical Properties of Si3N4 ceramics, NATO ASI Series, Series E: Applied Science , vol.276 , pp. 59-71
    • Hoffmann, M.J.1
  • 16
    • 85047673403 scopus 로고
    • 'Review -sialons and related nitrogen ceramics'
    • Jack, K.H. (1976), 'Review -sialons and related nitrogen ceramics', J. Mater. Sci., 11, 1135-58.
    • (1976) J. Mater. Sci. , vol.11 , pp. 1135-1158
    • Jack, K.H.1
  • 17
    • 0342415933 scopus 로고
    • 'In situ measurements of bridged crack interfaces in the scanning electron microscope'
    • Kelly, J.F. et al. (1991), 'In situ measurements of bridged crack interfaces in the scanning electron microscope', J. Am. Ceram. Soc., 74, 3154-7.
    • (1991) J. Am. Ceram. Soc. , vol.74 , pp. 3154-3157
    • Kelly, J.F.1
  • 18
    • 0034228465 scopus 로고    scopus 로고
    • 'Microstructure control of in-situ-toughened α-sialon ceramics'
    • Kim, J. et al. (2000), 'Microstructure control of in-situ-toughened α-sialon ceramics', J. Am. Ceram. Soc. 83(7), 1819-21.
    • (2000) J. Am. Ceram. Soc. , vol.83 , Issue.7 , pp. 1819-1821
    • Kim, J.1
  • 19
    • 0032631387 scopus 로고    scopus 로고
    • 'Microstructure and fracture toughness of Si3N4 ceramics: combined roles of grain morphology and secondary phase chemistry'
    • Kleebe, H.-J. et al. (1999), 'Microstructure and fracture toughness of Si3N4 ceramics: combined roles of grain morphology and secondary phase chemistry', J. Am. Ceram. Soc., 82(7), 1857-67.
    • (1999) J. Am. Ceram. Soc. , vol.82 , Issue.7 , pp. 1857-1867
    • Kleebe, H.-J.1
  • 20
    • 0015671407 scopus 로고
    • 'Relation between strength, fracture energy, and microstructure of hot-pressed silicon nitride'
    • Lange, F.F. (1973), 'Relation between strength, fracture energy, and microstructure of hot-pressed silicon nitride', J. Am. Ceram. Soc., 56(10), 518-22.
    • (1973) J. Am. Ceram. Soc. , vol.56 , Issue.10 , pp. 518-522
    • Lange, F.F.1
  • 23
    • 0027575845 scopus 로고
    • 'Solid-particle erosion of in situ reinforced Si3N4'
    • Marrero, M. et al. (1993), 'Solid-particle erosion of in situ reinforced Si3N4', Wear, 162-164, 280-4.
    • (1993) Wear , vol.162-164 , pp. 280-284
    • Marrero, M.1
  • 24
    • 0029409604 scopus 로고
    • 'Fracture resistance behaviour of highly anisotropic silicon nitride'
    • Ohji, T. et al. (1995), 'Fracture resistance behaviour of highly anisotropic silicon nitride', J. Am. Ceram. Soc., 78(11), 3125-28.
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.11 , pp. 3125-3128
    • Ohji, T.1
  • 25
    • 0028529919 scopus 로고
    • 'Toughness properties of a silicon carbide with an in situ induced heterogeneous grain structure'
    • Padture, N.P. and Lawn, B.R. (1994), 'Toughness properties of a silicon carbide with an in situ induced heterogeneous grain structure', J. Am. Ceram. Soc., 77(10), 2518-22.
    • (1994) J. Am. Ceram. Soc. , vol.77 , Issue.10 , pp. 2518-2522
    • Padture, N.P.1    Lawn, B.R.2
  • 26
    • 0018996430 scopus 로고
    • 'The erosion of reaction-bonded SiC'
    • Routbort, J.L. et al. (1980), 'The erosion of reaction-bonded SiC', Wear, 59, 363-75.
    • (1980) Wear , vol.59 , pp. 363-375
    • Routbort, J.L.1
  • 27
    • 1542538398 scopus 로고
    • 'On the ductile behaviour of nominally brittle materials during erosive cutting'
    • Sheldon, G.L. and Finnie, I. (1966), 'On the ductile behaviour of nominally brittle materials during erosive cutting', Trans. ASME, 88B, 387-92.
    • (1966) Trans. ASME , vol.88 B , pp. 387-392
    • Sheldon, G.L.1    Finnie, I.2
  • 28
    • 0019930357 scopus 로고
    • 'Coal slurry erosion of reaction-bonded SiC'
    • Shetty, D.K. et al. (1982), 'Coal slurry erosion of reaction-bonded SiC', Wear, 79, 275-9.
    • (1982) Wear , vol.79 , pp. 275-279
    • Shetty, D.K.1
  • 29
    • 0031126842 scopus 로고
    • 'The effect of plume divergence on the spatial distribution and magnitude of wear in gas-blast erosion'
    • Shipway, P.H. (1997), 'The effect of plume divergence on the spatial distribution and magnitude of wear in gas-blast erosion', Wear, 205, 169-77.
    • (1982) Wear , vol.205 , pp. 169-177
    • Shipway, P.H.1
  • 30
    • 0026106843 scopus 로고
    • 'R curve effects in solid particle erosion of ceramics'
    • Srinivasan, S., and Scattergood, R.O. (1991), 'R curve effects in solid particle erosion of ceramics', Wear, 142, 115-33.
    • (1991) Wear , vol.142 , pp. 115-133
    • Srinivasan, S.1    Scattergood, R.O.2
  • 31
    • 0004076431 scopus 로고
    • Weinheim, VCH
    • Swain, M. (1994), Structure and Properties of Ceramics, Weinheim, VCH. van Tendeloo, G. et al. (1983), 'Characterization of AlN ceramics containing long-period polytypes', J. Mater. Sci., 18, 525-32.
    • (1994) Structure and Properties of Ceramics
    • Swain, M.1
  • 32
    • 0020704724 scopus 로고
    • 'Characterization of AlN ceramics containing long-period polytypes'
    • Wiederhorn, S.M. and Lawn, B.R. (1979), 'Strength degradation of glass impacted with sharp particles: I, Annealed surfaces', J. Am. Ceram. Soc., 62(1-2), 66-70.
    • (1983) J. Mater. Sci. , vol.18 , pp. 525-532
    • Van Tendeloo, G.1
  • 33
    • 0018305252 scopus 로고
    • 'Strength degradation of glass impacted with sharp particles: I, Annealed surfaces'
    • Wood, C.A. and Cheng, Y.-B. (2000), 'Phase relationships and microstructures of Ca and Al-rich α-sialon ceramics', J. Eur. Ceram. Soc., 20, 357-66.
    • (1979) J. Am. Ceram. Soc. , vol.62 , Issue.1-2 , pp. 66-70
    • Wiederhorn, S.M.1    Lawn, B.R.2
  • 34
    • 0034159399 scopus 로고    scopus 로고
    • 'Phase relationships and microstructures of Ca and Al-rich α-sialon ceramics'
    • Zhang, Y. et al. (2000), 'Erosion of alumina ceramics by air- and water-suspended garnet particles', Wear, 240, 40-51.
    • (2000) J. Eur. Ceram. Soc. , vol.20 , pp. 357-366
    • Wood, C.A.1    Cheng, Y.-B.2
  • 35
    • 0033916591 scopus 로고    scopus 로고
    • 'Erosion of alumina ceramics by air- and water-suspended garnet particles'
    • Zhang, Y. et al. (2001), 'Influence of microstructure on the erosive wear behaviour of Ca α-sialon materials', J. Eur. Ceram. Soc., 21(13), 2435-45.
    • (2000) Wear , vol.240 , pp. 40-51
    • Zhang, Y.1
  • 36
    • 0035501832 scopus 로고    scopus 로고
    • 'Influence of microstructure on the erosive wear behaviour of Ca α-sialon materials'
    • Zhang, Y. and Cheng, Y.-B. (2003), 'Microstructural design of Ca α-sialon ceramics: effects of starting compositions and processing conditions', J. Euro. Ceram. Soc., 23 (9), 1531-41.
    • (2001) J. Eur. Ceram. Soc. , vol.21 , Issue.13 , pp. 2435-2445
    • Zhang, Y.1
  • 37
    • 0037411708 scopus 로고    scopus 로고
    • 'Microstructural design of Ca α-sialon ceramics: effects of starting compositions and processing conditions'
    • Zhang, Y. et al. (2005), 'Erosion response of highly anisotropic silicon nitride', J. Am. Ceram. Soc., 88(1), 114-20.
    • (2003) J. Euro. Ceram. Soc. , vol.23 , Issue.9 , pp. 1531-1541
    • Zhang, Y.1    Cheng, Y.-B.2
  • 38
    • 27644482450 scopus 로고    scopus 로고
    • 'Erosion response of highly anisotropic silicon nitride'
    • Zhao, H. et al. (1997), 'Elongated α-sialon grains in pressureless sintered sialon ceramics', J. Eur. Ceram. Soc., 18, 1053-7.
    • (2005) J. Am. Ceram. Soc. , vol.88 , Issue.1 , pp. 114-120
    • Zhang, Y.1
  • 39
    • 84882897610 scopus 로고    scopus 로고


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.