1
-
-
0026115117
-
Microstructural design of toughened ceramics
-
P. F. Becher, "Microstructural Design of Toughened Ceramics," J. Am. Ceram. Soc., 74 [2] 255-69 (1991).
-
(1991)
J. Am. Ceram. Soc.
, vol.74
, Issue.2
, pp. 255-269
-
-
Becher, P.F.1
-
2
-
-
0029244597
-
Using microstructure to attack the brittle nature of silicon nitride ceramics
-
P. F. Becher, S.-L. Hwang, and C.-H. Hsueh, "Using Microstructure to Attack the Brittle Nature of Silicon Nitride Ceramics," MRS Bull., 20, 23-7 (1995).
-
(1995)
MRS Bull.
, vol.20
, pp. 23-27
-
-
Becher, P.F.1
Hwang, S.-L.2
Hsueh, C.-H.3
-
3
-
-
0027091113
-
Toughening mechanisms for ceramic materials
-
R. W. Steinbrech, "Toughening Mechanisms for Ceramic Materials," J. Eur. Ceram. Soc., 10, 131-42 (1992).
-
(1992)
J. Eur. Ceram. Soc.
, vol.10
, pp. 131-142
-
-
Steinbrech, R.W.1
-
4
-
-
0008447233
-
Flaw-insensitive ceramics
-
S. J. Bennison, N. P. Padture, J. L. Runyan, and B. R. Lawn, "Flaw-Insensitive Ceramics," Philos. Mag. Lett., 64 [4] 191-95 (1991).
-
(1991)
Philos. Mag. Lett.
, vol.64
, Issue.4
, pp. 191-195
-
-
Bennison, S.J.1
Padture, N.P.2
Runyan, J.L.3
Lawn, B.R.4
-
5
-
-
0001296081
-
Contact fatigue in silicon nitride
-
S. K. Lee and B. R. Lawn, "Contact Fatigue in Silicon Nitride," J. Am. Ceram. Soc, 82 [5] 1281-88 (1999).
-
(1999)
J. Am. Ceram. Soc
, vol.82
, Issue.5
, pp. 1281-1288
-
-
Lee, S.K.1
Lawn, B.R.2
-
6
-
-
0029251007
-
Relation between strength, microstructure, and grain-bridging characteristics in in situ reinforce silicon nitride
-
C. W. Li, S.-C. Lui, and J. Goldacker, "Relation Between Strength, Microstructure, and Grain-Bridging Characteristics in In Situ Reinforce Silicon Nitride," J. Am. Ceram. Soc, 78 [2] 449-59 (1995).
-
(1995)
J. Am. Ceram. Soc
, vol.78
, Issue.2
, pp. 449-459
-
-
Li, C.W.1
Lui, S.-C.2
Goldacker, J.3
-
7
-
-
0033750188
-
Silicon nitride and related materials
-
F. L. Riley, "Silicon Nitride and Related Materials," J. Am. Ceram. Soc, 83 [2] 245-65 (2000).
-
(2000)
J. Am. Ceram. Soc
, vol.83
, Issue.2
, pp. 245-265
-
-
Riley, F.L.1
-
8
-
-
0032207131
-
Microstructural design of silicon nitride with improved fracture toughness: I, effects of grain shape and size
-
P. F. Becher, E. Y. Sun, K. P. Plucknett, K. B. Alexander, C.-H. Hsueh, H.-T. Lin, S. B. Waters, C. G. Westmoreland, E. -S. Kang, K. Hirao, and M. E. Brito, "Microstructural Design of Silicon Nitride with Improved Fracture Toughness: I, Effects of Grain Shape and Size," J. Am. Ceram. Soc, 81 [11] 2821-30 (1998).
-
(1998)
J. Am. Ceram. Soc
, vol.81
, Issue.11
, pp. 2821-2830
-
-
Becher, P.F.1
Sun, E.Y.2
Plucknett, K.P.3
Alexander, K.B.4
Hsueh, C.-H.5
Lin, H.-T.6
Waters, S.B.7
Westmoreland, C.G.8
Kang, E.S.9
Hirao, K.10
Brito, M.E.11
-
9
-
-
0024612051
-
Effects of aspect ratios of ellipsoidal inclusions on elastic stress transfer of ceramic composites
-
C. H. Hsueh, "Effects of Aspect Ratios of Ellipsoidal Inclusions on Elastic Stress Transfer of Ceramic Composites,"J. Am. Ceram. Soc., 72 [2] 344-47 (1989).
-
(1989)
J. Am. Ceram. Soc.
, vol.72
, Issue.2
, pp. 344-347
-
-
Hsueh, C.H.1
-
10
-
-
0031124255
-
Stress transfer in a model composite containing a single embedded fiber
-
C. H. Hsueh, R. J. Young, X. Yang, and P. F. Becher, "Stress Transfer in a Model Composite Containing a Single Embedded Fiber," Acta Metall. Mater., 45 [4] 1469-76 (1997).
-
(1997)
Acta Metall. Mater.
, vol.45
, Issue.4
, pp. 1469-1476
-
-
Hsueh, C.H.1
Young, R.J.2
Yang, X.3
Becher, P.F.4
-
11
-
-
0028478884
-
Microstructural control of silicon nitride by seeding with rodlike β-silicon nitride particles
-
K. Hirao, T. Nagaoka, M. E. Brito, and S. Kanzaki, "Microstructural Control of Silicon Nitride by Seeding with Rodlike β-Silicon Nitride Particles," J. Am. Ceram. Soc., 77 [7] 1857-62 (1994).
-
(1994)
J. Am. Ceram. Soc.
, vol.77
, Issue.7
, pp. 1857-1862
-
-
Hirao, K.1
Nagaoka, T.2
Brito, M.E.3
Kanzaki, S.4
-
12
-
-
0029325006
-
Processing strategy for producing highly anisotropic silicon nitride
-
K. Hirao, M. Ohashi, M. E. Brito, and S. Kanzaki, "Processing strategy for producing highly anisotropic silicon nitride," J. Am. Ceram. Soc., 78 [6] 1687-90 (1995).
-
(1995)
J. Am. Ceram. Soc.
, vol.78
, Issue.6
, pp. 1687-1690
-
-
Hirao, K.1
Ohashi, M.2
Brito, M.E.3
Kanzaki, S.4
-
13
-
-
0000719475
-
Effect of microstructure on the erosion and impact damage of sintered silicon nitride
-
J. E. Ritter, S. R. Choi, K. Jakus, P. J. Whalen, and R. G. Rateick, "Effect of Microstructure on the Erosion and Impact Damage of Sintered Silicon Nitride," J. Mater. Sci., 26, 5543-46 (1991).
-
(1991)
J. Mater. Sci.
, vol.26
, pp. 5543-5546
-
-
Ritter, J.E.1
Choi, S.R.2
Jakus, K.3
Whalen, P.J.4
Rateick, R.G.5
-
14
-
-
0027575845
-
4
-
4," Wear, 162-164, 280-84 (1993).
-
(1993)
Wear
, vol.162-164
, pp. 280-284
-
-
Marrero, M.1
Routbort, J.2
Whalen, P.3
Li, C.-W.4
Karasek, K.R.5
-
15
-
-
0029676239
-
4
-
4," Tribol. Trans., 39, 374-79 (1996).
-
(1996)
Tribol. Trans.
, vol.39
, pp. 374-379
-
-
Karasek, K.R.1
Whalen, P.J.2
Rateick, R.G.3
Routbort, J.L.4
Hamilton, A.C.5
-
16
-
-
0027668312
-
4 single crystal particles
-
4 Single Crystal Particles," J. Ceram. Soc. Jpn., Int. Ed., 101 [9] 1051-53 (1993).
-
(1993)
J. Ceram. Soc. Jpn., Int. Ed.
, vol.101
, Issue.9
, pp. 1051-1053
-
-
Hirao, K.1
Tsuge, A.2
Brito, M.E.3
Kanzaki, S.4
-
18
-
-
0003893686
-
The determination of density porosity and water absorption
-
AS 1774.5
-
AS 1774.5, "The Determination of Density Porosity and Water Absorption," Stand. Assoc. Aust., 1-3 (1979).
-
(1979)
Stand. Assoc. Aust.
, pp. 1-3
-
-
-
19
-
-
84987335986
-
A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements
-
G. R. Anstis, P. Chantikul, B. R. Lawn, and D. B. Marshall, "A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: I, Direct Crack Measurements," J. Am. Ceram. Soc., 64 [9] 533-8 (1981).
-
(1981)
J. Am. Ceram. Soc.
, vol.64
, Issue.9
, pp. 533-538
-
-
Anstis, G.R.1
Chantikul, P.2
Lawn, B.R.3
Marshall, D.B.4
-
20
-
-
0033916591
-
Erosion of alumina ceramics by air- And water-suspended garnet particles
-
Y. Zhang, Y.-B. Cheng, and S. Lathabai, "Erosion of Alumina Ceramics by Air- and Water-Suspended Garnet Particles," Wear, 240, 40-51 (2000).
-
(2000)
Wear
, vol.240
, pp. 40-51
-
-
Zhang, Y.1
Cheng, Y.-B.2
Lathabai, S.3
-
21
-
-
1542538398
-
On the ductile behaviour of nominally brittle materials during erosive cutting
-
G. L. Sheldon and I. Finnie, "On the Ductile Behaviour of Nominally Brittle Materials During Erosive Cutting," Trans. ASME, 88B, 387-92 (1966).
-
(1966)
Trans. ASME
, vol.88 B
, pp. 387-392
-
-
Sheldon, G.L.1
Finnie, I.2
-
22
-
-
0017982146
-
Impact damage in brittle materials in the elastic-plastic response regime
-
A. G. Evans, M. E. Gulden, and M. Rosenblatt, "Impact Damage in Brittle Materials in the Elastic-Plastic Response Regime," Proc. R. Soc. London, Ser. A, 361, 343-65 (1978).
-
(1978)
Proc. R. Soc. London, Ser. A
, vol.361
, pp. 343-365
-
-
Evans, A.G.1
Gulden, M.E.2
Rosenblatt, M.3
-
23
-
-
0018305252
-
Strength degradation of glass impacted with sharp particles: I, annealed surfaces
-
S. M. Wiederhorn and B. R. Lawn, "Strength Degradation of Glass Impacted with Sharp Particles: I, Annealed Surfaces," J. Am. Ceram. Soc., 62 [1-2] 66-70 (1979).
-
(1979)
J. Am. Ceram. Soc.
, vol.62
, Issue.1-2
, pp. 66-70
-
-
Wiederhorn, S.M.1
Lawn, B.R.2
-
24
-
-
84985084859
-
R-curve behavior and strength for in-situ reinforced silicon nitrides with different microstructures
-
C. W. Li, D. J. Lee, and S. C. Lui, "R-curve Behavior and Strength for In-Situ Reinforced Silicon Nitrides with Different Microstructures," J. Am. Ceram. Soc., 75 [7] 1777-85 (1992).
-
(1992)
J. Am. Ceram. Soc.
, vol.75
, Issue.7
, pp. 1777-1785
-
-
Li, C.W.1
Lee, D.J.2
Lui, S.C.3
-
25
-
-
0029409604
-
Fracture resistance behaviour of highly anisotropic silicon nitride
-
T. Ohji, K. Hirao, and S. Kanzaki, "Fracture Resistance Behaviour of Highly Anisotropic Silicon Nitride," J. Am. Ceram. Soc., 78 [11] 3125-28 (1995).
-
(1995)
J. Am. Ceram. Soc.
, vol.78
, Issue.11
, pp. 3125-3128
-
-
Ohji, T.1
Hirao, K.2
Kanzaki, S.3
-
26
-
-
0035501832
-
Influence of microstructure on the erosive wear behaviour of Ca α-sialon materials
-
Y. Zhang, Y.-B. Cheng, and S. Lathabai, "Influence of Microstructure on the Erosive Wear Behaviour of Ca α-Sialon Materials," J. Eur. Ceram. Soc., 21, 2435-45 (2001).
-
(2001)
J. Eur. Ceram. Soc.
, vol.21
, pp. 2435-2445
-
-
Zhang, Y.1
Cheng, Y.-B.2
Lathabai, S.3
-
27
-
-
0026106843
-
R curve effects in solid particle erosion of ceramics
-
S. Srinivasan and R. O. Scattergood, "R curve Effects in Solid Particle Erosion of Ceramics," Wear, 142, 115-33 (1991).
-
(1991)
Wear
, vol.142
, pp. 115-133
-
-
Srinivasan, S.1
Scattergood, R.O.2
-
28
-
-
27644598009
-
-
Ph.D. Thesis, School of Physics and Materials Engineering, Monash University, Victoria, Australia
-
Y. Zhang "Erosion Behaviour of Engineering Ceramics"; Ph.D. Thesis, School of Physics and Materials Engineering, Monash University, Victoria, Australia, 2002.
-
(2002)
Erosion Behaviour of Engineering Ceramics
-
-
Zhang, Y.1
-
29
-
-
0035324374
-
R-curve behaviour of in situ toughened α-sialon ceramics
-
M. Zenotchkine, R. Shuba, J. S. Kim, and I. W. Chen, "R-curve Behaviour of In Situ Toughened α-Sialon Ceramics," J. Am. Ceram. Soc., 84 [4] 884-86 (2001).
-
(2001)
J. Am. Ceram. Soc.
, vol.84
, Issue.4
, pp. 884-886
-
-
Zenotchkine, M.1
Shuba, R.2
Kim, J.S.3
Chen, I.W.4
|