메뉴 건너뛰기




Volumn 51, Issue 12, 2009, Pages 2932-2941

Mechanisms of long-term anaerobic corrosion of iron archaeological artefacts in seawater

Author keywords

A. Archaeological artefacts; A. Steel; C. Marine corrosion; C. Rust; C. Sulphate reducing bacteria

Indexed keywords

A. ARCHAEOLOGICAL ARTEFACTS; ANAEROBIC CORROSION; ARCHAEOLOGICAL ARTEFACTS; CORROSION PRODUCTS; ENVIRONMENTAL CONDITIONS; HYDROXYCHLORIDE; MACKINAWITE; MARINE CORROSION; MICRO-SCALES; NANOCRYSTALLINES; SULPHATE REDUCING BACTERIA; THERMODYNAMIC MODELLING;

EID: 72149084124     PISSN: 0010938X     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.corsci.2009.08.022     Document Type: Article
Times cited : (71)

References (49)
  • 1
    • 0012641736 scopus 로고    scopus 로고
    • The corrosion of excavated archaeological iron with details on weeping and akaganeite
    • Selwyn L.S., Sirois P.J., and Argyropoulos V. The corrosion of excavated archaeological iron with details on weeping and akaganeite. Studies in Conservation 44 (1999) 217-232
    • (1999) Studies in Conservation , vol.44 , pp. 217-232
    • Selwyn, L.S.1    Sirois, P.J.2    Argyropoulos, V.3
  • 2
    • 84975005401 scopus 로고
    • Post-excavation changes in iron antiquities
    • Turgoose S. Post-excavation changes in iron antiquities. Studies in Conservation 27 (1982) 97-101
    • (1982) Studies in Conservation , vol.27 , pp. 97-101
    • Turgoose, S.1
  • 3
    • 72149096560 scopus 로고    scopus 로고
    • L. Selwyn, Overview of archaeological iron: the corrosion problem, key factors affecting treatment, and gaps in current knowledge, in: Metal 2004: 2004; National Museum of Australia, Canberra: National Museum of Australia, 2004, pp. 294-306.
    • L. Selwyn, Overview of archaeological iron: the corrosion problem, key factors affecting treatment, and gaps in current knowledge, in: Metal 2004: 2004; National Museum of Australia, Canberra: National Museum of Australia, 2004, pp. 294-306.
  • 4
    • 84974883702 scopus 로고
    • Thermal decomposition of FeOCl and marine cast iron corrosion products
    • North N.A., and Pearson C. Thermal decomposition of FeOCl and marine cast iron corrosion products. Studies in Conservation 22 (1977) 146-157
    • (1977) Studies in Conservation , vol.22 , pp. 146-157
    • North, N.A.1    Pearson, C.2
  • 7
    • 0037374676 scopus 로고    scopus 로고
    • Formation of the Fe(II)-Fe(III) hydroxysulfate green rust during marine corrosion of steel
    • Refait P., Memet J.B., Bon C., Sabot R., and Genin J.-M.R. Formation of the Fe(II)-Fe(III) hydroxysulfate green rust during marine corrosion of steel. Corrosion Science 45 (2003) 833-845
    • (2003) Corrosion Science , vol.45 , pp. 833-845
    • Refait, P.1    Memet, J.B.2    Bon, C.3    Sabot, R.4    Genin, J.-M.R.5
  • 8
    • 33751507661 scopus 로고    scopus 로고
    • On the formation of β-FeOOH (Akaganeite) in chloride-containing environments
    • Refait P., and Rémazeilles C. On the formation of β-FeOOH (Akaganeite) in chloride-containing environments. Corrosion Science 49 (2007) 844-857
    • (2007) Corrosion Science , vol.49 , pp. 844-857
    • Refait, P.1    Rémazeilles, C.2
  • 9
    • 85167821286 scopus 로고
    • Seawater corrosivity around the world: results from three years of testing
    • Baloun C.H. (Ed), American Society for Testing and Materials, Philadelphia
    • Kirk W.W., and Pikul S.J. Seawater corrosivity around the world: results from three years of testing. In: Baloun C.H. (Ed). Corrosion in Natural Waters vol. 2 (1990), American Society for Testing and Materials, Philadelphia 2-36
    • (1990) Corrosion in Natural Waters , vol.2 , pp. 2-36
    • Kirk, W.W.1    Pikul, S.J.2
  • 10
    • 0022546712 scopus 로고
    • Development of high strength low alloy steels for marine applications, part 1: results of long term exposure tests on commercially available and experimental steels
    • Blekkenhorst F., Ferrari G.M., Wekken C.J.V.D., and Ijsseling F.P. Development of high strength low alloy steels for marine applications, part 1: results of long term exposure tests on commercially available and experimental steels. British Corrosion Journal 21 (1986) 163-176
    • (1986) British Corrosion Journal , vol.21 , pp. 163-176
    • Blekkenhorst, F.1    Ferrari, G.M.2    Wekken, C.J.V.D.3    Ijsseling, F.P.4
  • 11
    • 33847606953 scopus 로고    scopus 로고
    • The changing topography of corroding mild steel surfaces in seawater
    • Jeffrey R., and Melchers R.E. The changing topography of corroding mild steel surfaces in seawater. Corrosion Science 49 (2007) 2270-2288
    • (2007) Corrosion Science , vol.49 , pp. 2270-2288
    • Jeffrey, R.1    Melchers, R.E.2
  • 12
    • 0031096640 scopus 로고    scopus 로고
    • Seawater corrosivity around the world: results from five years of testing
    • Kain R.M., and Young W.T. (Eds), American Society for Testing and Materials, Philadelphia
    • Phull B.S., Pikul S.J., and Kain R.M. Seawater corrosivity around the world: results from five years of testing. In: Kain R.M., and Young W.T. (Eds). Corrosion Testing in Natural Waters vol. 2 (1997), American Society for Testing and Materials, Philadelphia 34-73
    • (1997) Corrosion Testing in Natural Waters , vol.2 , pp. 34-73
    • Phull, B.S.1    Pikul, S.J.2    Kain, R.M.3
  • 13
    • 5044247408 scopus 로고    scopus 로고
    • Pitting corrosion of mild steel in marine immersion environment, part 1: maximum pit depth
    • Melchers R.E. Pitting corrosion of mild steel in marine immersion environment, part 1: maximum pit depth. Corrosion (NACE) 60 (2004) 824-836
    • (2004) Corrosion (NACE) , vol.60 , pp. 824-836
    • Melchers, R.E.1
  • 14
    • 0002937778 scopus 로고
    • The role of sulphate-reducing and sulphur-oxidizing bacteria in the localized corrosion of iron-based alloys - a review
    • Cragnolino G., and Tuovinen O.H. The role of sulphate-reducing and sulphur-oxidizing bacteria in the localized corrosion of iron-based alloys - a review. International Biodeterioration 20 (1984) 9-26
    • (1984) International Biodeterioration , vol.20 , pp. 9-26
    • Cragnolino, G.1    Tuovinen, O.H.2
  • 15
    • 0012000060 scopus 로고
    • Biocorrosion: The action of sulphate reducing bacteria
    • Kluwer Academic Publishers, Dordrecht ed
    • W.A. Hamilton, Biocorrosion: the action of sulphate reducing bacteria, in: Biochemistry of microbial Degradation. Kluwer Academic Publishers, Dordrecht ed, 1994, pp. 555-570.
    • (1994) Biochemistry of microbial Degradation , pp. 555-570
    • Hamilton, W.A.1
  • 16
    • 0029132531 scopus 로고
    • Role of sulfate-reducing bacterie in corrosion of mild steels: a review
    • Lee W., Lewandowski Z., Nielsen P.H., and Hamilton W.A. Role of sulfate-reducing bacterie in corrosion of mild steels: a review. Biofouling 8 (1995) 165-194
    • (1995) Biofouling , vol.8 , pp. 165-194
    • Lee, W.1    Lewandowski, Z.2    Nielsen, P.H.3    Hamilton, W.A.4
  • 17
    • 0037374979 scopus 로고    scopus 로고
    • Bacteriological influence in the development of iron sulphide species in marine immersion environments
    • Jeffrey R., and Melchers R.E. Bacteriological influence in the development of iron sulphide species in marine immersion environments. Corrosion Science 45 (2003) 693-714
    • (2003) Corrosion Science , vol.45 , pp. 693-714
    • Jeffrey, R.1    Melchers, R.E.2
  • 18
    • 40949151029 scopus 로고    scopus 로고
    • Formation of the Fe(II-III) hydroxysulphate green rust during marine corrosion of steel associated to molecular detection of dissimilatory sulphite-reductase
    • Pineau S., Sabot R., Quillet L., Jeannin M., Caplat C., Dupont-Morral I., and Refait P. Formation of the Fe(II-III) hydroxysulphate green rust during marine corrosion of steel associated to molecular detection of dissimilatory sulphite-reductase. Corrosion Science 50 (2008) 1099-1111
    • (2008) Corrosion Science , vol.50 , pp. 1099-1111
    • Pineau, S.1    Sabot, R.2    Quillet, L.3    Jeannin, M.4    Caplat, C.5    Dupont-Morral, I.6    Refait, P.7
  • 19
    • 0037648521 scopus 로고    scopus 로고
    • Modelling of marine immersion corrosion for mild and low alloy steels - Part 1: phenomenological model
    • Melchers R.E. Modelling of marine immersion corrosion for mild and low alloy steels - Part 1: phenomenological model. Corrosion (NACE) 59 (2003) 319-334
    • (2003) Corrosion (NACE) , vol.59 , pp. 319-334
    • Melchers, R.E.1
  • 20
    • 33744790872 scopus 로고    scopus 로고
    • Models for the anaerobic phases of marine immersion corrosion
    • Melchers R.E., and Wells T. Models for the anaerobic phases of marine immersion corrosion. Corrosion Science 48 (2006) 1791-1811
    • (2006) Corrosion Science , vol.48 , pp. 1791-1811
    • Melchers, R.E.1    Wells, T.2
  • 21
    • 10044274161 scopus 로고    scopus 로고
    • Corrosion of iron archaeological artefacts in soil: characterisation of the corrosion system
    • Neff D., Dillmann P., Bellot-Gurlet L., and Béranger G. Corrosion of iron archaeological artefacts in soil: characterisation of the corrosion system. Corrosion Science 47 (2005) 515-535
    • (2005) Corrosion Science , vol.47 , pp. 515-535
    • Neff, D.1    Dillmann, P.2    Bellot-Gurlet, L.3    Béranger, G.4
  • 22
    • 33748967803 scopus 로고    scopus 로고
    • Corrosion of iron archaeological artefacts in soil: Estimation of the average corrosion rates involving analytical techniques and thermodynamic calculations
    • Neff D., Dillmann P., Decostes M., and Beranger G. Corrosion of iron archaeological artefacts in soil: Estimation of the average corrosion rates involving analytical techniques and thermodynamic calculations. Corrosion Science 48 (2006) 2947-2970
    • (2006) Corrosion Science , vol.48 , pp. 2947-2970
    • Neff, D.1    Dillmann, P.2    Decostes, M.3    Beranger, G.4
  • 23
    • 34147197527 scopus 로고    scopus 로고
    • Buried iron archaeological artefacts: corrosion mechanisms related to the presence of Cl-containing phases
    • Réguer S., Dillmann P., and Mirambet F. Buried iron archaeological artefacts: corrosion mechanisms related to the presence of Cl-containing phases. Corrosion Science 49 (2007) 2726-2744
    • (2007) Corrosion Science , vol.49 , pp. 2726-2744
    • Réguer, S.1    Dillmann, P.2    Mirambet, F.3
  • 24
    • 51249124452 scopus 로고    scopus 로고
    • Long-term corrosion behaviour of low-carbon steel in anoxic environment: characterisation of archaeological artefacts
    • Saheb M., Neff D., Dillmann P., Matthiesen H., and Foy E. Long-term corrosion behaviour of low-carbon steel in anoxic environment: characterisation of archaeological artefacts. Journal of Nuclear Materials 379 1-3 (2008) 118-123
    • (2008) Journal of Nuclear Materials , vol.379 , Issue.1-3 , pp. 118-123
    • Saheb, M.1    Neff, D.2    Dillmann, P.3    Matthiesen, H.4    Foy, E.5
  • 26
    • 51549108088 scopus 로고    scopus 로고
    • Corrosion behaviour of reinforced concrete: Laboratory experiments and archaeological analogues for long-term predictive modelling
    • L'hostis V., Foct F., and Dillmann P. Corrosion behaviour of reinforced concrete: Laboratory experiments and archaeological analogues for long-term predictive modelling. Journal of Nuclear Materials 379 (2008) 124-132
    • (2008) Journal of Nuclear Materials , vol.379 , pp. 124-132
    • L'hostis, V.1    Foct, F.2    Dillmann, P.3
  • 29
    • 72149086059 scopus 로고    scopus 로고
    • L. Long, Au Large des Saintes Maries de la Mer, Bilan scientifique du Département des Recherches Archéologiques Subaquatiques et Sous Marines (DRASSM) 2002. In.; 2003, pp. 51-57.
    • L. Long, Au Large des Saintes Maries de la Mer, Bilan scientifique du Département des Recherches Archéologiques Subaquatiques et Sous Marines (DRASSM) 2002. In.; 2003, pp. 51-57.
  • 30
    • 72149103839 scopus 로고    scopus 로고
    • Réseaux de production et standards de commercialisation du fer antique en méditerranée: les demi-produits des épaves romaines des Saintes-Maries-de-la-Mer (Bouches-du-Rhône, France)
    • Pagès G., Long L., Fluzin P., and Dillmann P. Réseaux de production et standards de commercialisation du fer antique en méditerranée: les demi-produits des épaves romaines des Saintes-Maries-de-la-Mer (Bouches-du-Rhône, France). Revue archéologique de Narbonnaise 41 (2008) 261-283
    • (2008) Revue archéologique de Narbonnaise , vol.41 , pp. 261-283
    • Pagès, G.1    Long, L.2    Fluzin, P.3    Dillmann, P.4
  • 31
    • 10044251755 scopus 로고    scopus 로고
    • Characterisation of iron archaeological analogues using micro diffraction under synchrotron radiation. Application to the study of long term corrosion behaviour of low alloy steels
    • Dillmann P., Neff D., Mazaudier F., Hoerle S., Chevallier P., and Beranger G. Characterisation of iron archaeological analogues using micro diffraction under synchrotron radiation. Application to the study of long term corrosion behaviour of low alloy steels. Journal of Physics IV France 12 (2002) 393-408
    • (2002) Journal of Physics IV France , vol.12 , pp. 393-408
    • Dillmann, P.1    Neff, D.2    Mazaudier, F.3    Hoerle, S.4    Chevallier, P.5    Beranger, G.6
  • 33
    • 4043153484 scopus 로고    scopus 로고
    • Structural characterization of corrosion products on archaeological iron. An integrated analytical approach to establish corrosion forms
    • Neff D., Reguer S., Bellot-Gurlet L., Dillmann P., and Bertholon R. Structural characterization of corrosion products on archaeological iron. An integrated analytical approach to establish corrosion forms. Journal of Raman Spectroscopy 35 (2004) 739-745
    • (2004) Journal of Raman Spectroscopy , vol.35 , pp. 739-745
    • Neff, D.1    Reguer, S.2    Bellot-Gurlet, L.3    Dillmann, P.4    Bertholon, R.5
  • 34
    • 34247128624 scopus 로고    scopus 로고
    • Deterioration of iron archaeological artefacts: μRaman investigation on chlorinated phases
    • Réguer S., Neff D., Bello-Gurlet L., and Dillmann P. Deterioration of iron archaeological artefacts: μRaman investigation on chlorinated phases. Journal of Raman Spectroscopy 38 (2007) 389-397
    • (2007) Journal of Raman Spectroscopy , vol.38 , pp. 389-397
    • Réguer, S.1    Neff, D.2    Bello-Gurlet, L.3    Dillmann, P.4
  • 35
    • 39749185505 scopus 로고    scopus 로고
    • Formation, fast oxidation and thermodynamic data of Fe(II) hydroxychlorides
    • Rémazeilles C., and Refait P. Formation, fast oxidation and thermodynamic data of Fe(II) hydroxychlorides. Corrosion Science 50 (2008) 856-864
    • (2008) Corrosion Science , vol.50 , pp. 856-864
    • Rémazeilles, C.1    Refait, P.2
  • 36
    • 54149114297 scopus 로고    scopus 로고
    • Characterisation of mackinawite by Raman spectroscopy: effects of crystallisation. Drying and oxidation
    • Bourdoiseau J.A., Jeannin M., Sabot R., Rémazeilles C., and Refait P. Characterisation of mackinawite by Raman spectroscopy: effects of crystallisation. Drying and oxidation. Corrosion Science 50 (2008) 3247-3255
    • (2008) Corrosion Science , vol.50 , pp. 3247-3255
    • Bourdoiseau, J.A.1    Jeannin, M.2    Sabot, R.3    Rémazeilles, C.4    Refait, P.5
  • 37
    • 0035365476 scopus 로고    scopus 로고
    • Characterization of ancient Indian iron and entrapped slag inclusions using electron, photon and nuclear microprobes
    • Dillmann P., and Balasubramaniam R. Characterization of ancient Indian iron and entrapped slag inclusions using electron, photon and nuclear microprobes. Bulletin of Materials Science 24 3 (2001) 317-322
    • (2001) Bulletin of Materials Science , vol.24 , Issue.3 , pp. 317-322
    • Dillmann, P.1    Balasubramaniam, R.2
  • 38
    • 34548757175 scopus 로고    scopus 로고
    • Slag inclusion analyses for studying ferrous alloys employed in French medieval buildings: supply of materials and diffusion of smelting processes
    • Dillmann P., and L'héritier M. Slag inclusion analyses for studying ferrous alloys employed in French medieval buildings: supply of materials and diffusion of smelting processes. Journal of Archaeological Science 34 11 (2007) 1810-1823
    • (2007) Journal of Archaeological Science , vol.34 , Issue.11 , pp. 1810-1823
    • Dillmann, P.1    L'héritier, M.2
  • 39
    • 0042918987 scopus 로고    scopus 로고
    • On the akaganeite crystal structure, phase transformations and possible role in post-excavational corrosion of iron artifacts
    • Stahl K., Nielsen K., Jiang J., Lebech B., Hanson J.C., Norby P., and Lanshot J.V. On the akaganeite crystal structure, phase transformations and possible role in post-excavational corrosion of iron artifacts. Corrosion Science 45 (2003) 2563-2575
    • (2003) Corrosion Science , vol.45 , pp. 2563-2575
    • Stahl, K.1    Nielsen, K.2    Jiang, J.3    Lebech, B.4    Hanson, J.C.5    Norby, P.6    Lanshot, J.V.7
  • 40
    • 0032409669 scopus 로고    scopus 로고
    • Energetics of stable and metastable low-temperature iron oxides and oxyhydroxides
    • Laberty C., and Navrotsky A. Energetics of stable and metastable low-temperature iron oxides and oxyhydroxides. Geochimica Cosmochimica Acta 62 (1998) 2905-2913
    • (1998) Geochimica Cosmochimica Acta , vol.62 , pp. 2905-2913
    • Laberty, C.1    Navrotsky, A.2
  • 43
    • 27344454785 scopus 로고    scopus 로고
    • Corrosion des surconteneurs de déchets, cas d'un surconteneur en acier faiblement allié
    • Bataillon C., Musy C., and Roy M. Corrosion des surconteneurs de déchets, cas d'un surconteneur en acier faiblement allié. Journal of Physics IV France 11 (2001) 267-274
    • (2001) Journal of Physics IV France , vol.11 , pp. 267-274
    • Bataillon, C.1    Musy, C.2    Roy, M.3
  • 44
    • 60349106658 scopus 로고    scopus 로고
    • Characterization of long-term corrosion of rebars embedded in concretes sampled on French historical buildings aged from 50 to 80 years
    • L'hostis V., Neff D., Bellot-Gurlet L., and Dillmann P. Characterization of long-term corrosion of rebars embedded in concretes sampled on French historical buildings aged from 50 to 80 years. Materials and Corrosion 60 2 (2009) 93-98
    • (2009) Materials and Corrosion , vol.60 , Issue.2 , pp. 93-98
    • L'hostis, V.1    Neff, D.2    Bellot-Gurlet, L.3    Dillmann, P.4
  • 46
    • 0026489377 scopus 로고
    • On the influence of carbonate in mineral dissolution: II The solubility of FeCO3(s) at 25 C and 1 atm total pressure
    • Bruno J., Wersin P., and Stumm W. On the influence of carbonate in mineral dissolution: II The solubility of FeCO3(s) at 25 C and 1 atm total pressure. Geochimica Cosmochimica Acta 26 (1992) 1149-1155
    • (1992) Geochimica Cosmochimica Acta , vol.26 , pp. 1149-1155
    • Bruno, J.1    Wersin, P.2    Stumm, W.3
  • 47
    • 0033030615 scopus 로고    scopus 로고
    • Soluble iron sulphide species in natural waters: Reappraisal of their stoichiometry and stability constants
    • Davison W., Phillips N., and Tabner B.J. Soluble iron sulphide species in natural waters: Reappraisal of their stoichiometry and stability constants. Aquatic Science 61 (1999) 23-43
    • (1999) Aquatic Science , vol.61 , pp. 23-43
    • Davison, W.1    Phillips, N.2    Tabner, B.J.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.