The effect of AlBr3 additive on the thermal degradation of PMMA A study using TG-DTA-DTG, IR and PY-GC-MS techniques

Author keywords

Aluminum tribromide; Degradation mechanism; Flammability test; IR spectroscopy; PMMA; Py GC MS; Thermal degradation; Thermoanalytical study

Indexed keywords

DEGRADATION MECHANISM; IR SPECTROSCOPY; PMMA; PY-GC-MS; THERMAL DEGRADATION; THERMOANALYTICAL STUDY;

EID: 68349095080     PISSN: 13886150     EISSN: None     Source Type: Journal    
DOI: 10.1007/s10973-009-0063-y     Document Type: Article
Times cited : (17)

References (34)
  • 2
    • 3543068796 scopus 로고    scopus 로고
    • Multimonomer and cross-linked polymers formed by its copolymerization- thermal studies
    • H Szocik R Jantas 2004 Multimonomer and cross-linked polymers formed by its copolymerization-thermal studies J Therm Anal Calorim 76 1 307 12
    • (2004) J Therm Anal Calorim , vol.76 , Issue.1 , pp. 307-12
    • Szocik, H.1    Jantas, R.2
  • 4
    • 33846879165 scopus 로고    scopus 로고
    • Mechanical properties and morphology of epoxy/poly (vinyl acetate)/poly (4-vinyl phenol) brominated system
    • MG Prolongo C Arribas C Salom RM Masegosa 2007 Mechanical properties and morphology of epoxy/poly (vinyl acetate)/poly (4-vinyl phenol) brominated system J Therm Anal Calorim 87 1 33 40
    • (2007) J Therm Anal Calorim , vol.87 , Issue.1 , pp. 33-40
    • Prolongo, M.G.1    Arribas, C.2    Salom, C.3    Masegosa, R.M.4
  • 5
    • 33846889000 scopus 로고    scopus 로고
    • Epoxy/poly(4-vinylphenol) blends Cross linked by imidazole initiation
    • SG Prolongo MG Prolongo 2007 Epoxy/poly(4-vinylphenol) blends Cross linked by imidazole initiation J Therm Anal Calorim 87 1 259 68
    • (2007) J Therm Anal Calorim , vol.87 , Issue.1 , pp. 259-68
    • Prolongo, S.G.1    Prolongo, M.G.2
  • 6
    • 33846891795 scopus 로고    scopus 로고
    • Morphology and dynamic mechanical properties of epoxy/poly (styrene-co-allyl alcohol) blend-influence of hardener nature
    • SG Prolonga M Buron A Salazar A Urena J Rodriguez 2007 Morphology and dynamic mechanical properties of epoxy/poly (styrene-co-allyl alcohol) blend-influence of hardener nature J Therm Anal Calorim 87 1 269 76
    • (2007) J Therm Anal Calorim , vol.87 , Issue.1 , pp. 269-76
    • Prolonga, S.G.1    Buron, M.2    Salazar, A.3    Urena, A.4    Rodriguez, J.5
  • 7
    • 21144446568 scopus 로고    scopus 로고
    • Hoffman-Lauritzen, parameters for non-isothermal crystallization of poly (ethylene terephthalate) and poly(ethylenie, oxide) melts
    • S Vyazovkin J Stone N Sbirrazzuoli 2005 Hoffman-Lauritzen, parameters for non-isothermal crystallization of poly (ethylene terephthalate) and poly(ethylenie, oxide) melts J Therm Anal Calorim 80 1 177 80
    • (2005) J Therm Anal Calorim , vol.80 , Issue.1 , pp. 177-80
    • Vyazovkin, S.1    Stone, J.2    Sbirrazzuoli, N.3
  • 8
    • 0024774818 scopus 로고
    • Study of the mechanism of thermal degradation of poly (vinyl chloride)
    • H Zuoyun H Xingzhou S Gang 1989 Study of the mechanism of thermal degradation of poly (vinyl chloride) Polym Degrad Stab 24 127 35
    • (1989) Polym Degrad Stab , vol.24 , pp. 127-35
    • Zuoyun, H.1    Xingzhou, H.2    Gang, S.3
  • 9
    • 0026754895 scopus 로고
    • The effect of metal acetlyacetonates on the thermal degradation of poly (methyl methacrylate): Part II-manganese (III) acetylacetonate
    • IC McNeill JJ Liggat 1992 The effect of metal acetlyacetonates on the thermal degradation of poly (methyl methacrylate): part II-manganese (III) acetylacetonate Polym Degrad Stab 37 1 25 32
    • (1992) Polym Degrad Stab , vol.37 , Issue.1 , pp. 25-32
    • McNeill, I.C.1    Liggat, J.J.2
  • 10
    • 18144385116 scopus 로고    scopus 로고
    • UV-Laser-assisted degradation of poly (methyl methacrylate)
    • C Wochnowski MA Shams Eldin S Metev 2005 UV-Laser-assisted degradation of poly (methyl methacrylate) Polym Degrad Stab 89 2 252 64
    • (2005) Polym Degrad Stab , vol.89 , Issue.2 , pp. 252-64
    • Wochnowski, C.1    Shams Eldin, M.A.2    Metev, S.3
  • 11
    • 0039508163 scopus 로고
    • Degradation of polymer mixtures-III: Poly(vinyl chloride)/poly(methyl methacrylate) mixtures, studied by thermal volatilization analysis and other techniques. the nature of the reaction products and the mechanism of interaction of the polymers
    • IC McNeill D Neil 1970 Degradation of polymer mixtures-III: poly(vinyl chloride)/poly(methyl methacrylate) mixtures, studied by thermal volatilization analysis and other techniques. The nature of the reaction products and the mechanism of interaction of the polymers Eur Polym J 6 4 569 83
    • (1970) Eur Polym J , vol.6 , Issue.4 , pp. 569-83
    • McNeill, I.C.1    Neil, D.2
  • 12
    • 0346640379 scopus 로고    scopus 로고
    • Thermal degradation behavior of blends of phenyl methacrylate-styrene copolymers with aluminum isopropoxide
    • S Zulfiqar K Masud Q Ameer 2003 Thermal degradation behavior of blends of phenyl methacrylate-styrene copolymers with aluminum isopropoxide J Therm Anal Calorim 73 3 877 86
    • (2003) J Therm Anal Calorim , vol.73 , Issue.3 , pp. 877-86
    • Zulfiqar, S.1    Masud, K.2    Ameer, Q.3
  • 14
    • 0030673322 scopus 로고    scopus 로고
    • Study of phenolic resin/EVA blends by thermal analysis
    • CG Mothe MIB Tavares 1997 Study of phenolic resin/EVA blends by thermal analysis J Therm Anal 49 477 81
    • (1997) J Therm Anal , vol.49 , pp. 477-81
    • Mothe, C.G.1    Tavares, M.I.B.2
  • 17
    • 0346849806 scopus 로고    scopus 로고
    • TG/DTA/MS of poly(methyl methacrylate)-the effect of particle size
    • SM Dakka 2003 TG/DTA/MS OF poly(methyl methacrylate)-the effect of particle size J Therm Anal Calorim 74 1 729 34
    • (2003) J Therm Anal Calorim , vol.74 , Issue.1 , pp. 729-34
    • Dakka, S.M.1
  • 18
    • 1842459218 scopus 로고    scopus 로고
    • TG/MS of poly (methyl methacrylate)-the effect of heating rate on the rate of production of evolved gases
    • SM Dakka 2004 TG/MS of poly (methyl methacrylate)-the effect of heating rate on the rate of production of evolved gases J Therm Anal Calorim 75 3 765 72
    • (2004) J Therm Anal Calorim , vol.75 , Issue.3 , pp. 765-72
    • Dakka, S.M.1
  • 19
    • 0346640419 scopus 로고    scopus 로고
    • The role of the oxidative environment
    • SM Dakka 2003 The role of the oxidative environment J Therm Anal Calorim 73 1 17 24
    • (2003) J Therm Anal Calorim , vol.73 , Issue.1 , pp. 17-24
    • Dakka, S.M.1
  • 20
    • 33846857742 scopus 로고    scopus 로고
    • Effects of incorporation of modified silica nanoparticles on the mechanical and thermal properties of PMMA
    • S Etienne C Becher D Ruch B Grignard G Cartigny C Detrenbleur 2007 Effects of incorporation of modified silica nanoparticles on the mechanical and thermal properties of PMMA J Therm Anal Calorim 87 1 101 4
    • (2007) J Therm Anal Calorim , vol.87 , Issue.1 , pp. 101-4
    • Etienne, S.1    Becher, C.2    Ruch, D.3    Grignard, B.4    Cartigny, G.5    Detrenbleur, C.6
  • 21
    • 0037289477 scopus 로고    scopus 로고
    • Blend formation between homo and co-polymers at 289.15 K.PMMA.SAN bends
    • C Cardelli G Conti P Giann R Porta 2003 Blend formation between homo and co-polymers at 289.15 K.PMMA.SAN bends J Therm Anal Calorim 71 2 353 365
    • (2003) J Therm Anal Calorim , vol.71 , Issue.2 , pp. 353-365
    • Cardelli, C.1    Conti, G.2    Giann, P.3    Porta, R.4
  • 22
    • 0021294468 scopus 로고
    • The effect of zinc bromide on the thermal degradation of poly (methyl methacrylate) part-I, thermal analysis studies and general nature of the interaction
    • IC McNeill RC McGuiness 1984 The effect of zinc bromide on the thermal degradation of poly (methyl methacrylate) part-I, thermal analysis studies and general nature of the interaction Polym Degrad Stab 9 3 167 83
    • (1984) Polym Degrad Stab , vol.9 , Issue.3 , pp. 167-83
    • McNeill, I.C.1    McGuiness, R.C.2
  • 23
    • 0034502049 scopus 로고    scopus 로고
    • Thermal degradation of blends of allyl methacrylate-methyl methacrylate copolymers with aluminum ethoxide
    • S Zulfiqar K Masud 2000 Thermal degradation of blends of allyl methacrylate-methyl methacrylate copolymers with aluminum ethoxide Polym Degrad Stab 70 229 39
    • (2000) Polym Degrad Stab , vol.70 , pp. 229-39
    • Zulfiqar, S.1    Masud, K.2
  • 24
    • 0036437002 scopus 로고    scopus 로고
    • Thermal degradation of blends of phenyl methacrylate-styrene copolymers with aluminium ethoxide
    • references therein
    • S Zulfiqar K Masud Q Ameer 2002 Thermal degradation of blends of phenyl methacrylate-styrene copolymers with aluminium ethoxide Polym Degrad Stab 77 457 64 references therein
    • (2002) Polym Degrad Stab , vol.77 , pp. 457-64
    • Zulfiqar, S.1    Masud, K.2    Ameer, Q.3
  • 25
    • 6444237288 scopus 로고
    • A new analysis of thermogravimetric traces
    • HH Horowitz G Metzger 1963 A new analysis of thermogravimetric traces Anal Chem 35 1464 68
    • (1963) Anal Chem , vol.35 , pp. 1464-68
    • Horowitz, H.H.1    Metzger, G.2
  • 26
    • 0346154880 scopus 로고    scopus 로고
    • Flame retardant and mechanical properties of natural fibre-PP composite containing magnesium hydroxide
    • M Sain SH Park F Suhara S Law 2004 Flame retardant and mechanical properties of natural fibre-PP composite containing magnesium hydroxide Polym Degrad Stab 83 363 7
    • (2004) Polym Degrad Stab , vol.83 , pp. 363-7
    • Sain, M.1    Park, S.H.2    Suhara, F.3    Law, S.4
  • 27
    • 84981788911 scopus 로고
    • Thermal degradation of polymer mixtures. (I) Degradation of polystyrene- poly methyl methacrylate mixture and a comparison with the degradation of styrene-methyl methacrylate copolymers
    • N Grassie IC McNeill I Cooke 1968 Thermal degradation of polymer mixtures. (I) Degradation of polystyrene- poly methyl methacrylate mixture and a comparison with the degradation of styrene-methyl methacrylate copolymers J Appl Polym Sci 12 831 7
    • (1968) J Appl Polym Sci , vol.12 , pp. 831-7
    • Grassie, N.1    McNeill, I.C.2    Cooke, I.3
  • 28
    • 0023173574 scopus 로고
    • Catalytic degradation of polystyrene in the presence of aluminium chloride catalyst
    • H Nanbu Y Sakuma Y Ishihara T Takesue T Ikemura 1987 Catalytic degradation of polystyrene in the presence of aluminium chloride catalyst Polym Degrad Stab 19 1 61 76
    • (1987) Polym Degrad Stab , vol.19 , Issue.1 , pp. 61-76
    • Nanbu, H.1    Sakuma, Y.2    Ishihara, Y.3    Takesue, T.4    Ikemura, T.5
  • 29
    • 0026151978 scopus 로고
    • Thermal degradation of poly(methyl methacrylate): 4. Random side-group scission
    • LE Manring 1991 Thermal degradation of poly(methyl methacrylate): 4. Random side-group scission Macromolecules 24 11 3304 9
    • (1991) Macromolecules , vol.24 , Issue.11 , pp. 3304-9
    • Manring, L.E.1
  • 30
    • 0029713260 scopus 로고    scopus 로고
    • The effect of silicon and phosphorus on the degradation of PMMA
    • TC Chang YC Chen YS Chiu SY Ho 1996 The effect of silicon and phosphorus on the degradation of PMMA Polymer 37 14 2963 68
    • (1996) Polymer , vol.37 , Issue.14 , pp. 2963-68
    • Chang, T.C.1    Chen, Y.C.2    Chiu, Y.S.3    Ho, S.Y.4
  • 31
    • 0004152851 scopus 로고
    • Sadtler Research Laboratories, Philadelphia, PA 5
    • The Sadtler Standard Spectra, Sadtler Research Laboratories, Philadelphia, PA 5;1974.
    • (1974) The Sadtler Standard Spectra
  • 32
    • 1542790533 scopus 로고    scopus 로고
    • Thermal degradation and flammability characteristics of some polystyrenes and poly(methyl methacrylate)s chemically modified with silicon-containing groups
    • JR Ebdon BJ Hunt P Joseph 2004 Thermal degradation and flammability characteristics of some polystyrenes and poly(methyl methacrylate)s chemically modified with silicon-containing groups Polym Degrad Stab 83 1 181 5
    • (2004) Polym Degrad Stab , vol.83 , Issue.1 , pp. 181-5
    • Ebdon, J.R.1    Hunt, B.J.2    Joseph, P.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.