Volumn 35, Issue 7, 2009, Pages 2767-2774

Oxidation behavior of silicon carbide based biomorphic ceramics prepared by chemical vapor infiltration and reaction technique

Author keywords

Biomorphic ceramics; D. SiC; Oxidation resistance; SiC Si3N4

Indexed keywords

BEFORE AND AFTER; BIOMORPHIC CERAMICS; BIOMORPHIC SIC; CHEMICAL VAPOR INFILTRATION AND REACTIONS; COARSE GRAINS; COMPOSITE CERAMIC; D. SIC; FINE GRAIN STRUCTURE; FINE GRAINS; OXIDATION BEHAVIORS; SEM/EDX; SIC-SI3N4; THERMAL GRAVIMETRIC ANALYSIS;

EID: 67649635630     PISSN: 02728842     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.ceramint.2009.03.025     Document Type: Article
Times cited : (17)

References (14)
  • 3
    • 0027282886 scopus 로고
    • Corrosion of silicon-based ceramics in combustion environment
    • Jacobson N.S. Corrosion of silicon-based ceramics in combustion environment. J. Am. Ceram. Soc. 76 (1993) 3-28
    • (1993) J. Am. Ceram. Soc. , vol.76 , pp. 3-28
    • Jacobson, N.S.1
  • 4
    • 0026152727 scopus 로고
    • Oxidation resistance coating of TiC-SiC system on C/C composite by chemical vapor deposition
    • Kawai C., and Igarashi T. Oxidation resistance coating of TiC-SiC system on C/C composite by chemical vapor deposition. Ceram. Soc. Jpn. 5 (1991) 390-394
    • (1991) Ceram. Soc. Jpn. , vol.5 , pp. 390-394
    • Kawai, C.1    Igarashi, T.2
  • 5
    • 13444305497 scopus 로고    scopus 로고
    • Application of the chemical vapor infiltration and reaction (CVI-R) technique for the preparation of highly porous biomorphic SiC ceramics derived from paper
    • Streitwieser D.A., Popovska N., Gehard H., and Emig G. Application of the chemical vapor infiltration and reaction (CVI-R) technique for the preparation of highly porous biomorphic SiC ceramics derived from paper. J. Eur. Ceram. Soc. 6 (2005) 817-828
    • (2005) J. Eur. Ceram. Soc. , vol.6 , pp. 817-828
    • Streitwieser, D.A.1    Popovska, N.2    Gehard, H.3    Emig, G.4
  • 8
    • 0032050590 scopus 로고    scopus 로고
    • Oxidation behavior of chemically-vapor-deposited silicon carbide and silicon nitride from 1200 °C to 1600 °C
    • Fox D.S. Oxidation behavior of chemically-vapor-deposited silicon carbide and silicon nitride from 1200 °C to 1600 °C. J. Am. Ceram. Soc. 4 (1998) 945-950
    • (1998) J. Am. Ceram. Soc. , vol.4 , pp. 945-950
    • Fox, D.S.1
  • 9
    • 0036833025 scopus 로고    scopus 로고
    • High temperature oxidation of multilayered SiC processed by tape casting and sintering
    • Badini C., Fino P., Ortona A., and Amelio C. High temperature oxidation of multilayered SiC processed by tape casting and sintering. J. Eur. Ceram. Soc. 22 (2002) 2071-2079
    • (2002) J. Eur. Ceram. Soc. , vol.22 , pp. 2071-2079
    • Badini, C.1    Fino, P.2    Ortona, A.3    Amelio, C.4
  • 10
    • 2542471748 scopus 로고    scopus 로고
    • Influence of the preparation temperature on the phase, microstructure and anti-oxidation property of a SiC coating for C/C composites
    • Huang J., Li H., Zeng X., Xiong X., and Fu Y. Influence of the preparation temperature on the phase, microstructure and anti-oxidation property of a SiC coating for C/C composites. Carbon 42 (2004) 1517-1521
    • (2004) Carbon , vol.42 , pp. 1517-1521
    • Huang, J.1    Li, H.2    Zeng, X.3    Xiong, X.4    Fu, Y.5
  • 11
    • 0035882010 scopus 로고    scopus 로고
    • A high-temperature oxidation resistance coationg, for graphite, prepared by atmopheric pressure chemical vapor deposition
    • Bahlawane N. A high-temperature oxidation resistance coationg, for graphite, prepared by atmopheric pressure chemical vapor deposition. Thin Solid Films 394 (2001) 297-302
    • (2001) Thin Solid Films , vol.394 , pp. 297-302
    • Bahlawane, N.1
  • 12
    • 0032675032 scopus 로고    scopus 로고
    • 4 + SiC)/C layer for the oxidation protection of carbon-carbon composites
    • 4 + SiC)/C layer for the oxidation protection of carbon-carbon composites. Carbon 37 (1999) 1417-1423
    • (1999) Carbon , vol.37 , pp. 1417-1423
    • Zhu, Y.C.1    Ohtani, S.2    Sato, Y.3    Iwamoto, N.4
  • 13
    • 0042062272 scopus 로고    scopus 로고
    • Multilayer coating with self-sealing properties for carbon-carbon composites
    • Smeacetto F., Ferraris M., and Salvo M. Multilayer coating with self-sealing properties for carbon-carbon composites. Carbon 41 (2003) 2105-2111
    • (2003) Carbon , vol.41 , pp. 2105-2111
    • Smeacetto, F.1    Ferraris, M.2    Salvo, M.3
  • 14
    • 0025559851 scopus 로고
    • High temperature oxidation protection coatings for monolithic or composite ceramics
    • Desmaison J. High temperature oxidation protection coatings for monolithic or composite ceramics. Werkstoff und Korrosion 41 (1990) 749-750
    • (1990) Werkstoff und Korrosion , vol.41 , pp. 749-750
    • Desmaison, J.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.