Volumn 41, Issue 11-12, 2009, Pages 1085-1093

EDM machinability and frictional behavior of ZrO2-WC composites

Author keywords

Dry reciprocative friction; Nanocrystalline; Surface integrity; Wire EDM; ZrO2 WC composite

Indexed keywords

DEIONIZED WATER; ELECTRIC DIPOLE MOMENTS; ELECTRIC DISCHARGE MACHINING; ELECTRIC DISCHARGES; FRICTION; MICROMACHINING; NANOCRYSTALLINE MATERIALS; SURFACES; WIRE; ZIRCONIUM; ZIRCONIUM ALLOYS;

EID: 63749083672     PISSN: 02683768     EISSN: 14333015     Source Type: Journal    
DOI: 10.1007/s00170-008-1551-0     Document Type: Article
Times cited : (27)

References (33)
  • 1
    • 0033873591 scopus 로고    scopus 로고
    • Transformation toughening in zirconia-containing ceramics
    • RHJ Hannink PM Kelly BC Muddle 2000 Transformation toughening in zirconia-containing ceramics J Am Ceram Soc 83 3 461 487
    • (2000) J Am Ceram Soc , vol.83 , Issue.3 , pp. 461-487
    • Hannink, R.H.J.1    Kelly, P.M.2    Muddle, B.C.3
  • 2
    • 0036962147 scopus 로고    scopus 로고
    • Phase transitions in zirconium dioxide and related materials for high performance engineering ceramics
    • doi:10.1023/A:1021099308957
    • MH Bocanegra-Bernal SD De La Torre 2002 Phase transitions in zirconium dioxide and related materials for high performance engineering ceramics J Mater Sci 37 23 4947 4971 doi:10.1023/A:1021099308957
    • (2002) J Mater Sci , vol.37 , Issue.23 , pp. 4947-4971
    • Bocanegra-Bernal, M.H.1    De La Torre, S.D.2
  • 3
    • 0037308603 scopus 로고    scopus 로고
    • Alumina ceramics with partially stabilized zirconia for cutting tools
    • DOI 10.1016/S0924-0136(02)00232-7
    • B Smuk M Szutkowska J Walter 2003 Alumina ceramics with partially stabilized zirconia for cutting tools J Mater Process Tech 133 1-2 195 198 DOI 10.1016/S0924-0136(02)00232-7
    • (2003) J Mater Process Tech , vol.133 , Issue.12 , pp. 195-198
    • Smuk, B.1    Szutkowska, M.2    Walter, J.3
  • 5
    • 0027837466 scopus 로고
    • Machining performance of phase transformation toughened alumina and partially stabilized zirconia composite cutting tools
    • DOI 10.1016/0955-2219(93)90079-7
    • T Sornakumar R Krishnamurthy CV Gokularathnam 1993 Machining performance of phase transformation toughened alumina and partially stabilized zirconia composite cutting tools J Europ Ceram Soc 12 6 455 460 DOI 10.1016/0955-2219(93) 90079-7
    • (1993) J Europ Ceram Soc , vol.12 , Issue.6 , pp. 455-460
    • Sornakumar, T.1    Krishnamurthy, R.2    Gokularathnam, C.V.3
  • 6
    • 0032002537 scopus 로고    scopus 로고
    • The effect of wear on the tetragonal-to-monoclinic transformation and the residual stress distribution in zirconia-toughened alumina cutting tools
    • DOI 10.1016/S0043-1648(97)00208-1
    • V Sergo V Lughi G Pezzotti E Lucchini S Meriani N Muraki G Katagiri T Nishida 1998 The effect of wear on the tetragonal-to-monoclinic transformation and the residual stress distribution in zirconia-toughened alumina cutting tools Wear 214 2 264 270 DOI 10.1016/S0043-1648(97)00208-1
    • (1998) Wear , vol.214 , Issue.2 , pp. 264-270
    • Sergo, V.1    Lughi, V.2    Pezzotti, G.3    Lucchini, E.4    Meriani, S.5    Muraki, N.6    Katagiri, G.7    Nishida, T.8
  • 8
    • 0036566936 scopus 로고    scopus 로고
    • Bioceramics in joint replacement: State-of-the-art and future options
    • G Willmann 2002 Bioceramics in joint replacement: State-of-the-art and future options CFI Ceram Forum Int 79 5 E27 E31
    • (2002) CFI Ceram Forum Int , vol.79 , Issue.5
    • Willmann, G.1
  • 9
    • 0031467964 scopus 로고    scopus 로고
    • Standardization of zirconia ceramics for total hip replacements
    • G Willmann 1997 Standardization of zirconia ceramics for total hip replacements Biomed Tech 42 12 342 346
    • (1997) Biomed Tech , vol.42 , Issue.12 , pp. 342-346
    • Willmann, G.1
  • 12
    • 0037257544 scopus 로고    scopus 로고
    • Wear properties of zirconia/alumina combination for joint prostheses
    • DOI 10.1016/S0043-1648(02)00296-X
    • Y Morita K Nakata K Ikeuchi 2003 Wear properties of zirconia/alumina combination for joint prostheses Wear 254 147 153 DOI 10.1016/S0043-1648(02) 00296-X
    • (2003) Wear , vol.254 , pp. 147-153
    • Morita, Y.1    Nakata, K.2    Ikeuchi, K.3
  • 13
    • 0028374821 scopus 로고
    • Study on the honing of zirconia ceramics by diamond abrasive sticks
    • DOI 10.1016/0924-0136(94)90061-2
    • J-D Kim Y-B Lee Se-H Park 1994 Study on the honing of zirconia ceramics by diamond abrasive sticks J Mater Process Tech 41 2 201 212 DOI 10.1016/0924-0136(94)90061-2
    • (1994) J Mater Process Tech , vol.41 , Issue.2 , pp. 201-212
    • Kim, J.-D.1    Lee, Y.-B.2    Se-H, P.3
  • 18
    • 0032123747 scopus 로고    scopus 로고
    • Zirconia matrix-tungsten carbide particulate composites manufactured by hot-pressing technique
    • DOI 10.1016/S0167-577X(98)00010-X
    • Z Pedzich K Haberko J Piekarczyk M Faryna L Litynska 1998 Zirconia matrix-tungsten carbide particulate composites manufactured by hot-pressing technique Mater Lett 36 70 75 DOI 10.1016/S0167-577X(98)00010-X
    • (1998) Mater Lett , vol.36 , pp. 70-75
    • Pedzich, Z.1    Haberko, K.2    Piekarczyk, J.3    Faryna, M.4    Litynska, L.5
  • 19
    • 4243715480 scopus 로고    scopus 로고
    • Toughening mechanisms in the TZP- WC particulate composites
    • Z Pedzich K Haberko 1997 Toughening mechanisms in the TZP- WC particulate composites Key Eng Mater 136 3 2076 2079
    • (1997) Key Eng Mater , vol.136 , Issue.3 , pp. 2076-2079
    • Pedzich, Z.1    Haberko, K.2
  • 20
    • 7444246802 scopus 로고    scopus 로고
    • Hard, tough and strong ZrO2-WC composites from nanosized powders
    • DOI 10.1016/j.jeurceramsoc.2004.01.015
    • G Anné S Put K Vanmeensel D Jiang J Vleugels O Van der Biest 2005 Hard, tough and strong ZrO2-WC composites from nanosized powders J Europ Ceram Soc 25 55 63 DOI 10.1016/j.jeurceramsoc.2004.01.015
    • (2005) J Europ Ceram Soc , vol.25 , pp. 55-63
    • Anné, G.1    Put, S.2    Vanmeensel, K.3    Jiang, D.4    Vleugels, J.5    Van Der Biest, O.6
  • 21
    • 33750977254 scopus 로고    scopus 로고
    • 2-WC nanocomposites with superior properties
    • DOI 10.1016/j.jeurceramsoc.2006.05.028
    • 2-WC nanocomposites with superior properties J Europ Ceram Soc 27 1247 1251 DOI 10.1016/j.jeurceramsoc.2006.05.028
    • (2007) J Europ Ceram Soc , vol.27 , pp. 1247-1251
    • Jiang, D.1    Van Der Biest, O.2    Vleugels, J.3
  • 24
    • 2942521110 scopus 로고    scopus 로고
    • Investigation of material removal mechanisms in EDM of composite ceramic materials
    • DOI 10.1016/j.jmatprotec.2004.02.013
    • B Lauwers J-P Kruth W Liu W Eeraerts B Schacht P Bleys 2004 Investigation of material removal mechanisms in EDM of composite ceramic materials J Mater Process Tech 146 1-3 347 352 DOI 10.1016/j.jmatprotec.2004.02.013
    • (2004) J Mater Process Tech , vol.146 , Issue.13 , pp. 347-352
    • Lauwers, B.1    Kruth, J.-P.2    Liu, W.3    Eeraerts, W.4    Schacht, B.5    Bleys, P.6
  • 25
    • 2942519445 scopus 로고    scopus 로고
    • Machining of low electrical conductive materials by wire electrical discharge machining (WEDM)
    • DOI 10.1016/j.jmatprotec.2003.11.055
    • J Kozak KP Rajurkar N Chandarana 2004 Machining of low electrical conductive materials by wire electrical discharge machining (WEDM) J Mater Process Tech 149/1-3 266 271 DOI 10.1016/j.jmatprotec.2003.11.055
    • (2004) J Mater Process Tech , pp. 266-271
    • Kozak, J.1    Rajurkar, K.P.2    Chandarana, N.3
  • 26
    • 58149368795 scopus 로고
    • EDM-future steps towards the machining of ceramics
    • W Konig DF Dauw G Levy U Panten 1988 EDM-future steps towards the machining of ceramics Annals of the CIRP 37 2 623 631
    • (1988) Annals of the CIRP , vol.37 , Issue.2 , pp. 623-631
    • Konig, W.1    Dauw, D.F.2    Levy, G.3    Panten, U.4
  • 27
    • 0022025341 scopus 로고
    • Wire electro-chemical discharge machining of glasses and ceramics
    • H Tsuchiya T Inoue M Miyazaki 1985 Wire electro-chemical discharge machining of glasses and ceramics Bull Jpn Soc Precis Eng 19 1 73 74
    • (1985) Bull Jpn Soc Precis Eng , vol.19 , Issue.1 , pp. 73-74
    • Tsuchiya, H.1    Inoue, T.2    Miyazaki, M.3
  • 28
    • 0030785147 scopus 로고    scopus 로고
    • Processing of advanced ceramics using the wire-cut EDM process
    • DOI 10.1016/S0924-0136(96)02735-5
    • YK Lok TC Lee 1997 Processing of advanced ceramics using the wire-cut EDM process J Mater Process Tech 63 1-3 839 843 DOI 10.1016/S0924-0136(96)02735-5
    • (1997) J Mater Process Tech , vol.63 , Issue.13 , pp. 839-843
    • Lok, Y.K.1    Lee, T.C.2
  • 29
    • 0035217505 scopus 로고    scopus 로고
    • Development of optimum electrodischarge machining technology for advanced ceramics
    • DOI 10.1007/PL00003958
    • JA Sanchez I Cabanes LN Lopez de Lacalle A Lamikiz 2001 Development of optimum electrodischarge machining technology for advanced ceramics Int J Adv Manuf Tech 18 12 897 905 DOI 10.1007/PL00003958
    • (2001) Int J Adv Manuf Tech , vol.18 , Issue.12 , pp. 897-905
    • Sanchez, J.A.1    Cabanes, I.2    Lopez De Lacalle, L.N.3    Lamikiz, A.4
  • 30
    • 2942511558 scopus 로고    scopus 로고
    • Machining phenomena in WEDM of insulating ceramics
    • DOI 10.1016/j.jmatprotec.2003.12.027
    • T Tani Y Fukuzawa N Mohri N Saito M Okada 2004 Machining phenomena in WEDM of insulating ceramics J Mater Process Tech 149 1-3 124 128 DOI 10.1016/j.jmatprotec.2003.12.027
    • (2004) J Mater Process Tech , vol.149 , Issue.13 , pp. 124-128
    • Tani, T.1    Fukuzawa, Y.2    Mohri, N.3    Saito, N.4    Okada, M.5
  • 33
    • 0027100436 scopus 로고
    • Investigation on the optimum carbide content and machining condition for wire EDM of zirconia ceramics
    • DOI 10.1016/S0007-8506(07)61192-5
    • T Matsuo E Oshima 1992 Investigation on the optimum carbide content and machining condition for wire EDM of zirconia ceramics CIRP Annals Manufacturing Technology 41 1 231 234 DOI 10.1016/S0007-8506(07)61192-5
    • (1992) CIRP Annals Manufacturing Technology , vol.41 , Issue.1 , pp. 231-234
    • Matsuo, T.1    Oshima, E.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.