메뉴 건너뛰기




Volumn 54, Issue 4, 2008, Pages 289-293

Durability of isocyanate resin adhesives for wood V: Changes of color and chemical structure in photodegradation

Author keywords

Color; Durability; Isocyanate adhesives; P MDI; Photodegradation

Indexed keywords

CHEMICAL BONDS; COLOR; COLORIMETRY; FOURIER TRANSFORMS; INFRARED SPECTROSCOPY; IRRADIATION; OPTICAL PROPERTIES; PHOTODEGRADATION; QUANTUM CHEMISTRY; STRUCTURE (COMPOSITION); SULFATE MINERALS; WOOD;

EID: 50049119334     PISSN: 14350211     EISSN: None     Source Type: Journal    
DOI: 10.1007/s10086-008-0948-6     Document Type: Article
Times cited : (14)

References (21)
  • 1
    • 0142129887 scopus 로고    scopus 로고
    • Durability of isocyanate resin adhesives for wood I: Thermal properties of isocyanate resin cured with water
    • K. Umemura A. Takahashi S. Kawai 1998 Durability of isocyanate resin adhesives for wood I: thermal properties of isocyanate resin cured with water J Wood Sci 44 204 210
    • (1998) J Wood Sci , vol.44 , pp. 204-210
    • Umemura, K.1    Takahashi, A.2    Kawai, S.3
  • 2
    • 0033344984 scopus 로고    scopus 로고
    • Durability of isocyanate resin adhesives for wood II: Effect of the addition of several polyols on the thermal properties
    • K. Umemura A. Takahashi S. Kawai 1999 Durability of isocyanate resin adhesives for wood II: effect of the addition of several polyols on the thermal properties J Appl Polym Sci 74 1807 1814
    • (1999) J Appl Polym Sci , vol.74 , pp. 1807-1814
    • Umemura, K.1    Takahashi, A.2    Kawai, S.3
  • 3
    • 0142071559 scopus 로고    scopus 로고
    • Effect of polyol on thermo-oxidative degradation of isocyanate resin for wood adhesives
    • K. Umemura S. Kawai 2002 Effect of polyol on thermo-oxidative degradation of isocyanate resin for wood adhesives J Wood Sci 48 25 31
    • (2002) J Wood Sci , vol.48 , pp. 25-31
    • Umemura, K.1    Kawai, S.2
  • 4
    • 0142134907 scopus 로고    scopus 로고
    • Durability of isocyanate resin adhesives for wood III: Degradation under constant dry heating
    • K. Umemura S. Kawai 2002 Durability of isocyanate resin adhesives for wood III: degradation under constant dry heating J Wood Sci 48 380 386
    • (2002) J Wood Sci , vol.48 , pp. 380-386
    • Umemura, K.1    Kawai, S.2
  • 5
    • 0142134903 scopus 로고    scopus 로고
    • Durability of isocyanate resin adhesives for wood IV: Degradation under constant steam heating
    • K. Umemura A. Takahashi S. Kawai 2002 Durability of isocyanate resin adhesives for wood IV: degradation under constant steam heating J Wood Sci 48 387 393
    • (2002) J Wood Sci , vol.48 , pp. 387-393
    • Umemura, K.1    Takahashi, A.2    Kawai, S.3
  • 6
    • 0025839393 scopus 로고
    • Photostability of polyetherurethaneureas
    • B.P. Thapliyal R. Chandra 1991 Photostability of polyetherurethaneureas Polym Int 24 7 13
    • (1991) Polym Int , vol.24 , pp. 7-13
    • Thapliyal, B.P.1    Chandra, R.2
  • 7
    • 26844514380 scopus 로고    scopus 로고
    • Photolysis of methylene 4,4′-diphenyldiisocyanate-based polyurethane ureas and polyureas
    • C.E. Hoyle H. Shah K. Moussa 1996 Photolysis of methylene 4,4′-diphenyldiisocyanate-based polyurethane ureas and polyureas Polym Durability 249 91 111
    • (1996) Polym Durability , vol.249 , pp. 91-111
    • Hoyle, C.E.1    Shah, H.2    Moussa, K.3
  • 8
    • 0027151692 scopus 로고
    • Photodegradation of MDI based polyurethane/urea elastomers
    • H. Shah C.E. Hoyle 1993 Photodegradation of MDI based polyurethane/urea elastomers Polym Mater Sci Eng 68 74 75
    • (1993) Polym Mater Sci Eng , vol.68 , pp. 74-75
    • Shah, H.1    Hoyle, C.E.2
  • 9
    • 0030168350 scopus 로고    scopus 로고
    • The effect of different molecular weight of soft segments in polyurethanes on photooxidative stability
    • E.G. Bajsic V. Rek A. Sendijarevic V. Sendijarevic K.C. Frish 1996 The effect of different molecular weight of soft segments in polyurethanes on photooxidative stability Polym Degrad Stab 52 223 233
    • (1996) Polym Degrad Stab , vol.52 , pp. 223-233
    • Bajsic, E.G.1    Rek, V.2    Sendijarevic, A.3    Sendijarevic, V.4    Frish, K.C.5
  • 10
    • 0032028577 scopus 로고    scopus 로고
    • Infrared analysis of the photochemical behavior of segmented polyurethanes
    • C. Wilhelm A. Rivaton J.L. Gardette 1998 Infrared analysis of the photochemical behavior of segmented polyurethanes Polymer 39 1223 1232
    • (1998) Polymer , vol.39 , pp. 1223-1232
    • Wilhelm, C.1    Rivaton, A.2    Gardette, J.L.3
  • 11
    • 0032640570 scopus 로고    scopus 로고
    • Deterioration of novel polyesterurethane elastomers in outdoor exposure
    • M. Furukawa K. Wakiyama 1999 Deterioration of novel polyesterurethane elastomers in outdoor exposure Polym Degrad Stab 65 15 24
    • (1999) Polym Degrad Stab , vol.65 , pp. 15-24
    • Furukawa, M.1    Wakiyama, K.2
  • 12
    • 0031211170 scopus 로고    scopus 로고
    • Infrared analysis of the photochemical behavior of segmented polyurethanes: 1 aliphatic poly(ester-urethane)
    • C. Wilhelm J.-L. Gardette 1997 Infrared analysis of the photochemical behavior of segmented polyurethanes: 1 aliphatic poly(ester-urethane) Polymer 38 4019 4031
    • (1997) Polymer , vol.38 , pp. 4019-4031
    • Wilhelm, C.1    Gardette, J.-L.2
  • 13
    • 33748312240 scopus 로고    scopus 로고
    • Influence of wood extractives on the photo-discoloration of wood surfaces exposed to artificial weathering
    • P. Nzokou D.P. Kamdem 2006 Influence of wood extractives on the photo-discoloration of wood surfaces exposed to artificial weathering Color Res Appl 31 425 434
    • (2006) Color Res Appl , vol.31 , pp. 425-434
    • Nzokou, P.1    Kamdem, D.P.2
  • 14
    • 0001275723 scopus 로고
    • Weathering characteristics of hardwood surfaces
    • D.-S. Hon S.C. Clemson W.C. Feist 1986 Weathering characteristics of hardwood surfaces Wood Sci Technol 20 169 183
    • (1986) Wood Sci Technol , vol.20 , pp. 169-183
    • Hon, D.-S.1    Clemson, S.C.2    Feist, W.C.3
  • 15
    • 1442307669 scopus 로고    scopus 로고
    • A spectrocolorimetric study on the effect of ultraviolet irradiation of four tropical hardwoods
    • T.C.M. Pastore K.O. Santos J.C. Rubim 2004 A spectrocolorimetric study on the effect of ultraviolet irradiation of four tropical hardwoods Bioresource Technol 93 37 42
    • (2004) Bioresource Technol , vol.93 , pp. 37-42
    • Pastore, T.C.M.1    Santos, K.O.2    Rubim, J.C.3
  • 17
    • 26944496034 scopus 로고    scopus 로고
    • Light source dependence of the photodegradation of wood
    • L. Tolvaj K. Mitsui 2005 Light source dependence of the photodegradation of wood J Wood Sci 51 468 473
    • (2005) J Wood Sci , vol.51 , pp. 468-473
    • Tolvaj, L.1    Mitsui, K.2
  • 18
    • 0034859231 scopus 로고    scopus 로고
    • Photo-oxidation studies on polyurethane coating: Effect of additives on yellowing of polyurethane
    • R.P. Singh N.S. Tomer S.V. Bhadraiah 2001 Photo-oxidation studies on polyurethane coating: effect of additives on yellowing of polyurethane Polym Degrad Stab 73 443 446
    • (2001) Polym Degrad Stab , vol.73 , pp. 443-446
    • Singh, R.P.1    Tomer, N.S.2    Bhadraiah, S.V.3
  • 19
    • 0032592151 scopus 로고    scopus 로고
    • Spectroscopic and electrochemical properties of poly(2,5-dimethyl aniline) films
    • A.A. Athawale B.A. Deore M.V. Kulkarni 1999 Spectroscopic and electrochemical properties of poly(2,5-dimethyl aniline) films Mater Chem Phys 60 262 267
    • (1999) Mater Chem Phys , vol.60 , pp. 262-267
    • Athawale, A.A.1    Deore, B.A.2    Kulkarni, M.V.3
  • 20
    • 0012541075 scopus 로고
    • Structural determination of a semiconductive tetramer of aniline by IR, UV-visible, ESR, XPS and mass spectroscopy techniques
    • S.N. Hari 1991 Structural determination of a semiconductive tetramer of aniline by IR, UV-visible, ESR, XPS and mass spectroscopy techniques J Mater Sci 26 1683 1690
    • (1991) J Mater Sci , vol.26 , pp. 1683-1690
    • Hari, S.N.1
  • 21
    • 9344254189 scopus 로고    scopus 로고
    • Investigation of the electropolymerization of aniline by the in situ techniques of attenuated total reflection (ATR) and external reflection (IRRAS)
    • Z. Angela D. Lothar 1997 Investigation of the electropolymerization of aniline by the in situ techniques of attenuated total reflection (ATR) and external reflection (IRRAS) J Mol Struct 410-411 165 171
    • (1997) J Mol Struct , vol.410-411 , pp. 165-171
    • Angela, Z.1    Lothar, D.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.