Volumn 27, Issue 12, 2007, Pages 3573-3588

Corrosion of Si3N4-ceramics in aqueous solutions. Part 2. Corrosion mechanisms in acids as a function of concentration, temperature and composition

Author keywords

Aqueous corrosion; Microstructure; Silicon nitride

Indexed keywords

CERAMIC MATERIALS; CORROSION; CORROSION RATE; CORROSION RESISTANCE; GRAIN BOUNDARIES; MORPHOLOGY; PASSIVATION; SULFURIC ACID; THERMAL EFFECTS;

EID: 34248564832     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2006.05.082     Document Type: Article
Times cited : (31)

References (29)
  • 3
    • 0037379198 scopus 로고    scopus 로고
    • Kinetic study of the corrosion of silicon nitride materials in acids
    • Schilm J., Herrmann M., and Michael G. Kinetic study of the corrosion of silicon nitride materials in acids. J. Eur. Ceram. Soc. 23 (2003) 577-584
    • (2003) J. Eur. Ceram. Soc. , vol.23 , pp. 577-584
    • Schilm, J.1    Herrmann, M.2    Michael, G.3
  • 4
    • 0037378349 scopus 로고    scopus 로고
    • Corrosion of silicon nitride materials in acidic and basic solutions and under hydrothermal conditions
    • Herrmann M., Schilm J., Michael G., Meinhardt J., and Flegler R. Corrosion of silicon nitride materials in acidic and basic solutions and under hydrothermal conditions. J. Eur. Ceram. Soc. 23 (2003) 585-594
    • (2003) J. Eur. Ceram. Soc. , vol.23 , pp. 585-594
    • Herrmann, M.1    Schilm, J.2    Michael, G.3    Meinhardt, J.4    Flegler, R.5
  • 5
    • 34248532956 scopus 로고    scopus 로고
    • J. Schilm, Korrosionsverhalten von Siliciumnitridkeramiken in Säuren, PhD Thesis, Fraunhofer IKTS Dresden and TU Bergakademie Freiberg, 2004.
  • 6
    • 0037377707 scopus 로고    scopus 로고
    • Corrosion of silicon nitride in aqueous acidic solutions: penetration monitoring
    • Seipel B., and Nickel K.G. Corrosion of silicon nitride in aqueous acidic solutions: penetration monitoring. J. Eur. Ceram. Soc. 23 (2003) 594-602
    • (2003) J. Eur. Ceram. Soc. , vol.23 , pp. 594-602
    • Seipel, B.1    Nickel, K.G.2
  • 7
    • 33748711292 scopus 로고    scopus 로고
    • Corrosion of YSiAlON-glasses in acidic and caustic media
    • Schilm J., Herrmann M., and Michael G. Corrosion of YSiAlON-glasses in acidic and caustic media. Sil. Ind. Special Issue 69 (2004) 317-324
    • (2004) Sil. Ind. Special Issue , vol.69 , pp. 317-324
    • Schilm, J.1    Herrmann, M.2    Michael, G.3
  • 8
    • 34248541636 scopus 로고    scopus 로고
    • B. Seipel, Korrosion von Siliciumnitrid und Zirkonoxidverstärktem Aluminiumoxid in Wässerigen Lösungen unter Durchflussbedingungen, PhD Thesis, University of Tübingen, 2003.
  • 9
    • 0035149370 scopus 로고    scopus 로고
    • Hydrothermal corrosion of nitride and carbide of silicon
    • Somiya S. Hydrothermal corrosion of nitride and carbide of silicon. Mater. Chem. Phys. 67 (2001) 157-163
    • (2001) Mater. Chem. Phys. , vol.67 , pp. 157-163
    • Somiya, S.1
  • 10
    • 34248510406 scopus 로고    scopus 로고
    • M. Fütting, TEM characterizations accomplished by the Fraunhofer IWM in Halle by order of the Fraunhofer IKTS in Dresden, 2003.
  • 11
    • 0038607112 scopus 로고    scopus 로고
    • M. Herrmann, J. Schilm. and G. Michael, Corrosion behaviour of different technical ceramics in acids, basic solutions and under hydrothermal condition, cfi, 80 (2003) 4, E27-E34.
  • 12
    • 0032154536 scopus 로고    scopus 로고
    • An inhomogeneous grain boundary composition in silicon nitride
    • Bando Y., Mitomo M., and Kurashima K.J. An inhomogeneous grain boundary composition in silicon nitride. Mater. Synth. Process. 6 (1998) 359
    • (1998) Mater. Synth. Process. , vol.6 , pp. 359
    • Bando, Y.1    Mitomo, M.2    Kurashima, K.J.3
  • 13
    • 1942455803 scopus 로고    scopus 로고
    • Observation of rare earth segregation in silicon nitride ceramics at subnanometer dimensions
    • Shibata N., Pennycook S.J., Gosnell T.R., Painter G.S., Shelton W.A., and Becher P. Observation of rare earth segregation in silicon nitride ceramics at subnanometer dimensions. Nature 428 (2004) 730-733
    • (2004) Nature , vol.428 , pp. 730-733
    • Shibata, N.1    Pennycook, S.J.2    Gosnell, T.R.3    Painter, G.S.4    Shelton, W.A.5    Becher, P.6
  • 14
    • 34248536877 scopus 로고    scopus 로고
    • R. Satet, Einfluss der Grenzflächeneigenschaften auf die Gefügeausbildung und das mechanische Verhalten von Siliciumnitrid-Keramiken, PhD Thesis, IKM University of Karlsruhe, 2003.
  • 15
    • 1342333910 scopus 로고    scopus 로고
    • Leaching behaviour of silicon nitride materials in sulphuric acid containing KF
    • Schilm J., Herrmann M., and Michael G. Leaching behaviour of silicon nitride materials in sulphuric acid containing KF. J. Eur. Ceram. Soc. 24 (2004)
    • (2004) J. Eur. Ceram. Soc. , vol.24
    • Schilm, J.1    Herrmann, M.2    Michael, G.3
  • 17
    • 0342922192 scopus 로고
    • Analysis of bulk amorphous oxynitride structures using the network theory of glasses
    • Risbud S.H. Analysis of bulk amorphous oxynitride structures using the network theory of glasses. Phys. Chem. Glasses 22 6 (1981) 168-170
    • (1981) Phys. Chem. Glasses , vol.22 , Issue.6 , pp. 168-170
    • Risbud, S.H.1
  • 18
    • 0030168929 scopus 로고    scopus 로고
    • Yttrium SiAlON glasses: structure and mechanical properties-elasticity and viscosity
    • Lemercier H., Rouxel T., Fargeot D., Besson J.-L., and Piriou B. Yttrium SiAlON glasses: structure and mechanical properties-elasticity and viscosity. J. Non-Cryst. Solids 201 (1996) 128-145
    • (1996) J. Non-Cryst. Solids , vol.201 , pp. 128-145
    • Lemercier, H.1    Rouxel, T.2    Fargeot, D.3    Besson, J.-L.4    Piriou, B.5
  • 19
    • 34248521248 scopus 로고    scopus 로고
    • R.K. Iler, Chemistry of Silica (Russian Translation), Mir, Mockwa, 1982. 286 ff, 320.
  • 20
    • 0742271799 scopus 로고    scopus 로고
    • Protection of silicon nitride ceramics against corrosion in acidic aqueous solutions by enforced internal passivation
    • Seipel B., and Nickel K.G. Protection of silicon nitride ceramics against corrosion in acidic aqueous solutions by enforced internal passivation. Ceram. Int. 30 2 (2004) 267-271
    • (2004) Ceram. Int. , vol.30 , Issue.2 , pp. 267-271
    • Seipel, B.1    Nickel, K.G.2
  • 21
    • 34248510405 scopus 로고    scopus 로고
    • 4-Werkstoffen, Abschlussbericht zum AiF-Vorhaben 12130 BR (2002).
  • 22
    • 0029172089 scopus 로고
    • Numerical solutions for mixed control of powder reactions for spherical, cylindrical or planar particles
    • Frade J.R., and Cable M. Numerical solutions for mixed control of powder reactions for spherical, cylindrical or planar particles. J. Am. Ceram. Soc. 78 (1995) 90-96
    • (1995) J. Am. Ceram. Soc. , vol.78 , pp. 90-96
    • Frade, J.R.1    Cable, M.2
  • 23
    • 0031144022 scopus 로고    scopus 로고
    • Theoretical solutions for mixed control of solid state reactions
    • Frade J.R., and Cable M. Theoretical solutions for mixed control of solid state reactions. J. Mater. Sci. 32 (1997) 2727-2733
    • (1997) J. Mater. Sci. , vol.32 , pp. 2727-2733
    • Frade, J.R.1    Cable, M.2
  • 24
    • 0032125403 scopus 로고    scopus 로고
    • Corrosion of silicon nitride ceramics in aqueous HCl and HF solutions at 27-80 °C
    • Sharkawy S.W., and El-Aslabi A.M. Corrosion of silicon nitride ceramics in aqueous HCl and HF solutions at 27-80 °C. Corr. Sci. 40 7 (1998) 1119-1129
    • (1998) Corr. Sci. , vol.40 , Issue.7 , pp. 1119-1129
    • Sharkawy, S.W.1    El-Aslabi, A.M.2
  • 25
    • 0012569136 scopus 로고
    • Corrosion of silicon nitride ceramics in HF and HCl solutions
    • Shimada M., and Sato T. Corrosion of silicon nitride ceramics in HF and HCl solutions. Ceram. Trans. Symp. 10 (1989) 355-364
    • (1989) Ceram. Trans. Symp. , vol.10 , pp. 355-364
    • Shimada, M.1    Sato, T.2
  • 26
    • 0343796965 scopus 로고
    • Corrosion behaviour of silicon nitride ceramics in caustic alkaline solutions at high temperatures
    • Sato T., Sato S., Tamura K., and Okuwaki A. Corrosion behaviour of silicon nitride ceramics in caustic alkaline solutions at high temperatures. Br. Ceram. Trans. J. 91 (1992) 117-120
    • (1992) Br. Ceram. Trans. J. , vol.91 , pp. 117-120
    • Sato, T.1    Sato, S.2    Tamura, K.3    Okuwaki, A.4
  • 27
    • 0035479999 scopus 로고    scopus 로고
    • Corrosion of silicon nitride in sulphuric acid aqueous solution
    • Monteverde F., Mingazzini C., Giorgi M., and Bellosi A. Corrosion of silicon nitride in sulphuric acid aqueous solution. Corr. Sci. 43 (2001) 1851-1863
    • (2001) Corr. Sci. , vol.43 , pp. 1851-1863
    • Monteverde, F.1    Mingazzini, C.2    Giorgi, M.3    Bellosi, A.4
  • 29
    • 2742609680 scopus 로고    scopus 로고
    • M. Herrmann, A. Krell, J. Adler, G. Wötting, T. Hollstein, W. Pfeifer. and M. Rombach, Keramische Wälzlager für Anwendungen in korrosiven Medien, VDI-Ber. 1331 (Innovationen für Gleitlager, Wälzlager, Dichtungen und Führungen), 1997, pp. 251-258.


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.