메뉴 건너뛰기




Volumn 90, Issue 2, 2007, Pages 541-545

Sliding-wear-resistant liquid-phase-sintered SiC processed using α-SiC starting powders

Author keywords

[No Author keywords available]

Indexed keywords

ELONGATED SIC GRAINS; EQUIAXED SIC GRAINS; LIQUID PHASE SINTERED (LPS) SIC CERAMICS; SIC STARTING POWDERS; YTTRIUM ALUMINUM GARNET (YAG);

EID: 33846521135     PISSN: 00027820     EISSN: 15512916     Source Type: Journal    
DOI: 10.1111/j.1551-2916.2006.01421.x     Document Type: Article
Times cited : (61)

References (34)
  • 1
    • 0035482049 scopus 로고    scopus 로고
    • Micro-and Macro-Tribological Properties of SiC Ceramics in Sliding Contact
    • K.-H. Z. Gahr, R. Blattner, D.-H. Hwang, and K. Pöhlmann, "Micro-and Macro-Tribological Properties of SiC Ceramics in Sliding Contact," Wear, 250 [1-12] 299-310 (2001).
    • (2001) Wear , vol.250
    • Gahr, K.-H.Z.1    Blattner, R.2    Hwang, D.-H.3    Pöhlmann, K.4
  • 3
    • 0036498767 scopus 로고    scopus 로고
    • 4 and SiC under Water Lubrication
    • 4 and SiC under Water Lubrication," Tribol. Int., 35 [3] 129-35 (2002).
    • (2002) Tribol. Int , vol.35 , Issue.3 , pp. 129-135
    • Chen, M.1    Kato, K.2    Adachi, K.3
  • 4
    • 2142711225 scopus 로고    scopus 로고
    • The Critical Condition for the Transition from HL to ML in Water-Lubricated SiC
    • X. L. Wang, K. J. Kato, and K. Adachi, "The Critical Condition for the Transition from HL to ML in Water-Lubricated SiC," Tribol. Lett., 16 [4] 253-58 (2004).
    • (2004) Tribol. Lett , vol.16 , Issue.4 , pp. 253-258
    • Wang, X.L.1    Kato, K.J.2    Adachi, K.3
  • 5
    • 5644279187 scopus 로고    scopus 로고
    • 4 and SiC: Induction Time Analysis
    • 4 and SiC: Induction Time Analysis," Tribol. Lett., 17 [3] 399-407 (2004).
    • (2004) Tribol. Lett , vol.17 , Issue.3 , pp. 399-407
    • Gales, R.S.1    Hsu, S.M.2
  • 6
    • 0030146805 scopus 로고    scopus 로고
    • Wear and Wear Transition in Silicon Carbide Ceramics during Sliding
    • S.-J. Cho, C.-D. Urn, and S.-S. Kim, "Wear and Wear Transition in Silicon Carbide Ceramics during Sliding," J. Am. Ceram. Soc., 79 [5] 1247-51 (1996).
    • (1996) J. Am. Ceram. Soc , vol.79 , Issue.5 , pp. 1247-1251
    • Cho, S.-J.1    Urn, C.-D.2    Kim, S.-S.3
  • 7
    • 0029289227 scopus 로고
    • Wear and Wear Transition Mechanism in Silicon Carbide Ceramics during Sliding
    • S.-.T. Cho, C.-D. Um, and S.-S. Kim, "Wear and Wear Transition Mechanism in Silicon Carbide Ceramics during Sliding," J. Am. Ceram. Soc., 78 [4] 1076-78 (1995).
    • (1995) J. Am. Ceram. Soc , vol.78 , Issue.4 , pp. 1076-1078
    • Cho, S.T.1    Um, C.-D.2    Kim, S.-S.3
  • 8
    • 0035413132 scopus 로고    scopus 로고
    • Microstructural Evolution in Liquid-Phase-Sintered SiC: I, Effect of Starting SiC Powder
    • H. Xu, T. Bhatia, S. A. Deshpande, N. P. Padture, A. L. Ortiz, and F. L. Cumbrera, "Microstructural Evolution in Liquid-Phase-Sintered SiC: I, Effect of Starting SiC Powder," J. Am. Ceram. Soc., 84 [7] 1578-84 (2001).
    • (2001) J. Am. Ceram. Soc , vol.84 , Issue.7 , pp. 1578-1584
    • Xu, H.1    Bhatia, T.2    Deshpande, S.A.3    Padture, N.P.4    Ortiz, A.L.5    Cumbrera, F.L.6
  • 9
    • 0035413155 scopus 로고    scopus 로고
    • Microstructural Evolution in Liquid-Phase-Sintered SiC: Part II, Effects of Planar Defects and Seeds in the Starting Powder
    • S. A. Deshpande, T. Bhatia, H. Xu, N. P. Padture, A. L. Ortiz, and F. L. Cumbrera, "Microstructural Evolution in Liquid-Phase-Sintered SiC: Part II, Effects of Planar Defects and Seeds in the Starting Powder," J. Am. Ceram. Soc., 84 [7] 1585-90(2001).
    • (2001) J. Am. Ceram. Soc , vol.84 , Issue.7 , pp. 1585-1590
    • Deshpande, S.A.1    Bhatia, T.2    Xu, H.3    Padture, N.P.4    Ortiz, A.L.5    Cumbrera, F.L.6
  • 10
    • 0036647165 scopus 로고    scopus 로고
    • Microstructural Evolution in Liquid-Phase-Sintered SiC: Part III, Effect of Nitrogen-Gas Sintering Atmosphere
    • A. L. Ortiz, T. Bhatia, N. P. Padture, and G. Pezzotti, "Microstructural Evolution in Liquid-Phase-Sintered SiC: Part III, Effect of Nitrogen-Gas Sintering Atmosphere," J. Am. Ceram. Soc., 85 [7] 1835-40 (2002).
    • (2002) J. Am. Ceram. Soc , vol.85 , Issue.7 , pp. 1835-1840
    • Ortiz, A.L.1    Bhatia, T.2    Padture, N.P.3    Pezzotti, G.4
  • 11
    • 0028382729 scopus 로고
    • In Situ-Toughened Silicon Carbide
    • N. P. Padture, "In Situ-Toughened Silicon Carbide," J. Am. Ceram. Soc., 77 [2] 519-23 (1994).
    • (1994) J. Am. Ceram. Soc , vol.77 , Issue.2 , pp. 519-523
    • Padture, N.P.1
  • 13
    • 0028529919 scopus 로고
    • Toughness Properties of a Silicon Carbide with In situ-Induced Heterogeneous Grain Structure
    • N. P. Padlure and B. R. Lawn, "Toughness Properties of a Silicon Carbide with In situ-Induced Heterogeneous Grain Structure," J. Am. Ceram. Soc., 77 [10] 2518-22(1994).
    • (1994) J. Am. Ceram. Soc , vol.77 , Issue.10 , pp. 2518-2522
    • Padlure, N.P.1    Lawn, B.R.2
  • 14
    • 0029326204 scopus 로고
    • Contact Fatigue of a Silicon Carbide with a Heterogeneous Grain Structure
    • N. P. Padture and B. R. Lawn, "Contact Fatigue of a Silicon Carbide with a Heterogeneous Grain Structure," J. Am. Ceram. Soc., 78 [6] 1431-38 (1995).
    • (1995) J. Am. Ceram. Soc , vol.78 , Issue.6 , pp. 1431-1438
    • Padture, N.P.1    Lawn, B.R.2
  • 15
    • 33745345069 scopus 로고    scopus 로고
    • Improved Sliding-Wear Resistance in In Situ-Toughened Silicon Carbide
    • O. Borrero-Lopez, A. L. Ortiz, F. Guiberteau, and N. P. Padture, "Improved Sliding-Wear Resistance in In Situ-Toughened Silicon Carbide," J. Am. Ceram. Soc., 88 [12] 3531-34 (2005).
    • (2005) J. Am. Ceram. Soc , vol.88 , Issue.12 , pp. 3531-3534
    • Borrero-Lopez, O.1    Ortiz, A.L.2    Guiberteau, F.3    Padture, N.P.4
  • 16
    • 33846468018 scopus 로고    scopus 로고
    • The Production of fine Silicon Carbide Powder by the Reaction of Gaseous Silicon Monoxide with Paniculate Carbon
    • P. Kennedy and B. North, "The Production of fine Silicon Carbide Powder by the Reaction of Gaseous Silicon Monoxide with Paniculate Carbon," J. Am. Ceram. Soc., 88 [12] 3531-34 (2005).
    • (2005) J. Am. Ceram. Soc , vol.88 , Issue.12 , pp. 3531-3534
    • Kennedy, P.1    North, B.2
  • 17
    • 0003749418 scopus 로고
    • Second Edition. Cambridge University Press, Cambridge, U.K
    • B. R. Lawn, Fracture of Brittle Solids Second Edition. Cambridge University Press, Cambridge, U.K, 1993.
    • (1993) Fracture of Brittle Solids
    • Lawn, B.R.1
  • 18
    • 84987335986 scopus 로고
    • A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: I. direct Crack Measurements
    • G. R. Anstis, P. Chantikul, D. B. Marshall, and B. R. Lawn, "A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: I. direct Crack Measurements," J. Am. Ceram. Soc., 64 [9] 533-38 (1981).
    • (1981) J. Am. Ceram. Soc , vol.64 , Issue.9 , pp. 533-538
    • Anstis, G.R.1    Chantikul, P.2    Marshall, D.B.3    Lawn, B.R.4
  • 19
    • 0032137856 scopus 로고    scopus 로고
    • Indentation of Ceramics with Spheres: A Century after Hertz
    • B. R. Lawn, "Indentation of Ceramics with Spheres: A Century after Hertz," J. Am. Ceram. Soc., 81 [8] 1977-94 (1998).
    • (1998) J. Am. Ceram. Soc , vol.81 , Issue.8 , pp. 1977-1994
    • Lawn, B.R.1
  • 20
    • 0034274218 scopus 로고    scopus 로고
    • Quantitative Phase-Composition Analysis of Liquid-Phase-Sintered Silicon Carbide Using the Rietveld Method
    • A. L. Ortiz, F. L. Cumbrera, F. Sánchez-Bajo, F. Guiberteau, H. Xu, and N. P. Padture, "Quantitative Phase-Composition Analysis of Liquid-Phase-Sintered Silicon Carbide Using the Rietveld Method," J. Am. Ceram. Soc., 83 [9] 228286-94 (2000).
    • (2000) J. Am. Ceram. Soc , vol.83 , Issue.9 , pp. 228286-228294
    • Ortiz, A.L.1    Cumbrera, F.L.2    Sánchez-Bajo, F.3    Guiberteau, F.4    Xu, H.5    Padture, N.P.6
  • 21
    • 0035369844 scopus 로고    scopus 로고
    • X-Ray Powder Diffraction Analysis of a Silicon Carbide-Based Ceramic
    • A. L. Ortiz, F. Sánchez-Bajo, F. L. Cumbrera, and F. Guiberteau, "X-Ray Powder Diffraction Analysis of a Silicon Carbide-Based Ceramic," Mater. Lett., 49 [2] 137-45 (2001).
    • (2001) Mater. Lett , vol.49 , Issue.2 , pp. 137-145
    • Ortiz, A.L.1    Sánchez-Bajo, F.2    Cumbrera, F.L.3    Guiberteau, F.4
  • 22
    • 0033077652 scopus 로고    scopus 로고
    • 2 and C Additives
    • 2 and C Additives," J. Mat. Res., 14 [2] 518-22(1999).
    • (1999) J. Mat. Res , vol.14 , Issue.2 , pp. 518-522
    • Tanaka, H.1    Zhou, Y.2
  • 23
    • 0347567171 scopus 로고    scopus 로고
    • Nonequiaxial Grain Growth and Polytype Transformation of Sintered α-Silicon Carbide and β-Silicon Carbide
    • H. Tanaka, N. Hirosaki, T. Nishimura, D.-W. Shin, and S.-S. Park, "Nonequiaxial Grain Growth and Polytype Transformation of Sintered α-Silicon Carbide and β-Silicon Carbide," J. Am. Ceram. Soc., 86 [12] 2222-24 (2003).
    • (2003) J. Am. Ceram. Soc , vol.86 , Issue.12 , pp. 2222-2224
    • Tanaka, H.1    Hirosaki, N.2    Nishimura, T.3    Shin, D.-W.4    Park, S.-S.5
  • 24
  • 25
    • 33846351913 scopus 로고
    • Grain-Size and R-Curve Effects in the Abrasive Wear of Alumina
    • S.-J. Cho, B. J. Hockey, B. R. Lawn, and S. J. Bennison, "Grain-Size and R-Curve Effects in the Abrasive Wear of Alumina," J. Am. Ceram. Soc., 72 [7] 1249-52(1989).
    • (1989) J. Am. Ceram. Soc , vol.72 , Issue.7 , pp. 1249-1252
    • Cho, S.-J.1    Hockey, B.J.2    Lawn, B.R.3    Bennison, S.J.4
  • 26
    • 44049121717 scopus 로고
    • The Transition from Mild to Severe Wear in Alumina during Sliding
    • S.-J. Cho, H. Moon, B. J. Hockey, and S. M. Hsu, "The Transition from Mild to Severe Wear in Alumina during Sliding," Acta Metal. Mater., 40 [1] 185-92 (1992).
    • (1992) Acta Metal. Mater , vol.40 , Issue.1 , pp. 185-192
    • Cho, S.-J.1    Moon, H.2    Hockey, B.J.3    Hsu, S.M.4
  • 27
    • 0002023796 scopus 로고    scopus 로고
    • Wear and Wear Transition Mechanisms of Ceramics
    • Y. S. Wang and S. M. Hsu, "Wear and Wear Transition Mechanisms of Ceramics," Wear, 195 [1-2] 112-22(1996).
    • (1996) Wear , vol.195
    • Wang, Y.S.1    Hsu, S.M.2
  • 28
    • 10044250907 scopus 로고    scopus 로고
    • Wear-Resistant Ultra-Fine-Grained Ceramics
    • X. Wang, N. P. Padlure, H. Tanaka, and A. L. Ortiz, "Wear-Resistant Ultra-Fine-Grained Ceramics," Acta Mater., 53 [2] 271-77 (2005).
    • (2005) Acta Mater , vol.53 , Issue.2 , pp. 271-277
    • Wang, X.1    Padlure, N.P.2    Tanaka, H.3    Ortiz, A.L.4
  • 30
    • 27644523198 scopus 로고    scopus 로고
    • Effect of Microstructure on Sliding-Wear Properlies of Liquid-Phase-Sintered α-SiC
    • O. Borrero-Lopez, A. L. Ortiz, F. Guiberteau, and N. P. Padlure, "Effect of Microstructure on Sliding-Wear Properlies of Liquid-Phase-Sintered α-SiC," J. Am. Ceram. Soc., 88 [8] 2159-63 (2005).
    • (2005) J. Am. Ceram. Soc , vol.88 , Issue.8 , pp. 2159-2163
    • Borrero-Lopez, O.1    Ortiz, A.L.2    Guiberteau, F.3    Padlure, N.P.4
  • 32
    • 0042266349 scopus 로고    scopus 로고
    • Role of Microstructure in the Grinding and Polishing of α-Sialon Ceramics
    • Z.-H. Xie. R. J. Moon, M. Hoffman, P. Munroe, and Y.-B. Cheng, "Role of Microstructure in the Grinding and Polishing of α-Sialon Ceramics," J. Eur. Ceram. Soc., 23 [13] 2351-60 (2003).
    • (2003) J. Eur. Ceram. Soc , vol.23 , Issue.13 , pp. 2351-2360
    • Xie, Z.-H.1    Moon, R.J.2    Hoffman, M.3    Munroe, P.4    Cheng, Y.-B.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.