메뉴 건너뛰기




Volumn 8, Issue 5, 2006, Pages 337-341

Microtensile bond strength of self-adhesive luting cements to ceramic

Author keywords

Ceramic; IPS Empress II; Microtensile; Self adhesive luting

Indexed keywords

ALUMINUM SILICATE; HYDROFLUORIC ACID; IPS EMPRESS CERAMIC; IPS-EMPRESS CERAMIC; MONOBOND S; MULTILINK ADHESIVE SYSTEM; PANAVIA FLUORO; PANAVIA-FLUORO; RELY X UNICEM; RESIN CEMENT; SILANE DERIVATIVE; TOOTH CEMENT;

EID: 33750399912     PISSN: 14615185     EISSN: None     Source Type: Journal    
DOI: None     Document Type: Article
Times cited : (41)

References (29)
  • 1
    • 0038644503 scopus 로고    scopus 로고
    • Resin-ceramic bonding: A review of the literature
    • Blatz MB, Sadan A, Kern M. Resin-ceramic bonding: a review of the literature. J Prosthet Dent 2003;89:268-274.
    • (2003) J Prosthet Dent , vol.89 , pp. 268-274
    • Blatz, M.B.1    Sadan, A.2    Kern, M.3
  • 2
    • 0034230513 scopus 로고    scopus 로고
    • Influence of time and adhesive system on the extrusion shear strength between felpspathic porcelain and bovine dentin
    • Braga RR, Ballester RY, Daronch M. Influence of time and adhesive system on the extrusion shear strength between felpspathic porcelain and bovine dentin. Dent Mater 2000;16:303-310.
    • (2000) Dent Mater , vol.16 , pp. 303-310
    • Braga, R.R.1    Ballester, R.Y.2    Daronch, M.3
  • 3
    • 0036490134 scopus 로고    scopus 로고
    • Are adhesive technologies needed to support ceramics? An assessment of the current evidence
    • Burke FJT, Fleming GJP, Nathanson D, Marquis PM. Are adhesive technologies needed to support ceramics? An assessment of the current evidence. J Adhes Dent 2000;4:7-22.
    • (2000) J Adhes Dent , vol.4 , pp. 7-22
    • Burke, F.J.T.1    Fleming, G.J.P.2    Nathanson, D.3    Marquis, P.M.4
  • 4
    • 0028437167 scopus 로고
    • Fracture resistance of teeth restored with dentin-bonded crowns
    • Burke FJT, Watts DC. Fracture resistance of teeth restored with dentin-bonded crowns. Quintessence Int 1994;25:335-340.
    • (1994) Quintessence Int , vol.25 , pp. 335-340
    • Burke, F.J.T.1    Watts, D.C.2
  • 5
    • 0344083608 scopus 로고    scopus 로고
    • Adhesive permeability affects coupling of resin cements that utilize self-etching primers to dentine
    • Carvalho RM, Pegoraro TA, Tay FR, Pegoraro LF, Silva NRFA, Pashley DH. Adhesive permeability affects coupling of resin cements that utilize self-etching primers to dentine. J Dent 2004;32:55-65.
    • (2004) J Dent , vol.32 , pp. 55-65
    • Carvalho, R.M.1    Pegoraro, T.A.2    Tay, F.R.3    Pegoraro, L.F.4    Silva, N.R.F.A.5    Pashley, D.H.6
  • 7
    • 0032534706 scopus 로고    scopus 로고
    • Moisture-dependent renaturation of collagen in phosphoric acid etched human dentin
    • El Feninat F, Ellis TH, Sacher E, Stangel I. Moisture-dependent renaturation of collagen in phosphoric acid etched human dentin. J Biomed Mater Res 1998;42:549-553.
    • (1998) J Biomed Mater Res , vol.42 , pp. 549-553
    • El Feninat, F.1    Ellis, T.H.2    Sacher, E.3    Stangel, I.4
  • 8
    • 0043130574 scopus 로고    scopus 로고
    • Microtensile bond strength testing of luting cements to prefabricated CAD/CAM ceramic and composite blocks
    • El Zohairy AA, De Gee AJ, Mohsen MM, Feilzer AJ. Microtensile bond strength testing of luting cements to prefabricated CAD/CAM ceramic and composite blocks. Dent Mater 2003;19:575-583.
    • (2003) Dent Mater , vol.19 , pp. 575-583
    • El Zohairy, A.A.1    De Gee, A.J.2    Mohsen, M.M.3    Feilzer, A.J.4
  • 9
    • 0033187284 scopus 로고    scopus 로고
    • Effect of dentin primers on the morphology, molecular composition and collagen conformation of acid-demineralized dentin in situ
    • Eliades G, Vougiouklakis G, Palaghias G. Effect of dentin primers on the morphology, molecular composition and collagen conformation of acid-demineralized dentin in situ. Dent Mater 1999;15:310-317.
    • (1999) Dent Mater , vol.15 , pp. 310-317
    • Eliades, G.1    Vougiouklakis, G.2    Palaghias, G.3
  • 10
    • 0042994075 scopus 로고    scopus 로고
    • Marginal integrity of ceramic inlays luted with a self-curing resin system
    • Ferrari M, Dagostin A, Fabianelli A. Marginal integrity of ceramic inlays luted with a self-curing resin system. Dent Mater 2003;19:270-276.
    • (2003) Dent Mater , vol.19 , pp. 270-276
    • Ferrari, M.1    Dagostin, A.2    Fabianelli, A.3
  • 11
    • 0032149711 scopus 로고    scopus 로고
    • The durability of adhesion to phosphoric acid etched, wet dentin substrates
    • Kato G, Nakabayashi N. The durability of adhesion to phosphoric acid etched, wet dentin substrates. Dent Mater 1998;14:347-352.
    • (1998) Dent Mater , vol.14 , pp. 347-352
    • Kato, G.1    Nakabayashi, N.2
  • 12
    • 0027584741 scopus 로고
    • Wear of ceramic inlays, their enamel antagonists, and luting cements
    • Krejci I, Lutz F, Reimer M, Heinzmann JL. Wear of ceramic inlays, their enamel antagonists, and luting cements. J Prosthet Dent 1993;69:425-430.
    • (1993) J Prosthet Dent , vol.69 , pp. 425-430
    • Krejci, I.1    Lutz, F.2    Reimer, M.3    Heinzmann, J.L.4
  • 13
    • 0142248014 scopus 로고    scopus 로고
    • Tensile bond strength of four resin luting agents bonded to bovine enamel and dentin
    • Mota CS, Demarco FF, Camacho GB, Powers JM. Tensile bond strength of four resin luting agents bonded to bovine enamel and dentin. J Prosthet Dent 2003;89:558-564.
    • (2003) J Prosthet Dent , vol.89 , pp. 558-564
    • Mota, C.S.1    Demarco, F.F.2    Camacho, G.B.3    Powers, J.M.4
  • 15
    • 0037629990 scopus 로고    scopus 로고
    • Dentin bond strengths of two ceramic inlay systems after cementation with three different techniques and one bonding system
    • Ozturk N, Aykent F. Dentin bond strengths of two ceramic inlay systems after cementation with three different techniques and one bonding system. J Prosthet Dent 2003;89:275-281.
    • (2003) J Prosthet Dent , vol.89 , pp. 275-281
    • Ozturk, N.1    Aykent, F.2
  • 18
    • 0032009913 scopus 로고    scopus 로고
    • Effect of cross-sectional surface area on bond strengths between resin and dentin
    • Phrukkanon S, Burrow MF, Tyas MJ. Effect of cross-sectional surface area on bond strengths between resin and dentin. Dent Mater 1998;14:120-128.
    • (1998) Dent Mater , vol.14 , pp. 120-128
    • Phrukkanon, S.1    Burrow, M.F.2    Tyas, M.J.3
  • 19
    • 0032082021 scopus 로고    scopus 로고
    • The influence of cross-sectional shape and surface area on the microtensile bond test
    • Phrukkanon S, Burrow MF, Tyas MJ. The influence of cross-sectional shape and surface area on the microtensile bond test. Dent Mater 1998;14:212-221.
    • (1998) Dent Mater , vol.14 , pp. 212-221
    • Phrukkanon, S.1    Burrow, M.F.2    Tyas, M.J.3
  • 21
    • 3042853580 scopus 로고    scopus 로고
    • Durability of resin dentin interfaces: Effects of surface moisture and adhesive solvent component
    • Reis A, Loguercio AD, Carvalho RM, Grande RHM. Durability of resin dentin interfaces: effects of surface moisture and adhesive solvent component. Dent Mater 2004;20:669-676.
    • (2004) Dent Mater , vol.20 , pp. 669-676
    • Reis, A.1    Loguercio, A.D.2    Carvalho, R.M.3    Grande, R.H.M.4
  • 22
    • 0028476472 scopus 로고
    • Relationship between surface area for adhesion and tensile bond strength - Evaluation of a micro-tensile bond test
    • Sano H, Shono T, Sonoda H, Takatsu T, Ciucchi B, Carvalho R, Pashley D. Relationship between surface area for adhesion and tensile bond strength - evaluation of a micro-tensile bond test. Dent Mater 1994;10:236-240.
    • (1994) Dent Mater , vol.10 , pp. 236-240
    • Sano, H.1    Shono, T.2    Sonoda, H.3    Takatsu, T.4    Ciucchi, B.5    Carvalho, R.6    Pashley, D.7
  • 23
    • 0041419469 scopus 로고    scopus 로고
    • Effect of ceramic surface treatment on the shear bond strengths of two resin luting agents to all-ceramic materials
    • Saygili G, fiahmali S. Effect of ceramic surface treatment on the shear bond strengths of two resin luting agents to all-ceramic materials. J Oral Rehab 2003;30:758-764.
    • (2003) J Oral Rehab , vol.30 , pp. 758-764
    • Saygili, G.1    Fiahmali, S.2
  • 24
    • 0028440877 scopus 로고
    • Effect of cement film thickness on the fracture resistance of a machinable glass-ceramic
    • Sherrer SS, De Rijk WG, Belser UC, Meyer JM. Effect of cement film thickness on the fracture resistance of a machinable glass-ceramic. Dent Mater 1994;10:172-177.
    • (1994) Dent Mater , vol.10 , pp. 172-177
    • Sherrer, S.S.1    De Rijk, W.G.2    Belser, U.C.3    Meyer, J.M.4
  • 26
    • 0036725717 scopus 로고    scopus 로고
    • Shear bond strength of resin cements to both ceramic and dentin
    • Stewart GP, Jain P, Hodges J. Shear bond strength of resin cements to both ceramic and dentin. J Prosthet Dent 2002;88:277-284.
    • (2002) J Prosthet Dent , vol.88 , pp. 277-284
    • Stewart, G.P.1    Jain, P.2    Hodges, J.3
  • 29
    • 0041627676 scopus 로고    scopus 로고
    • Resin-modified glass ionomer cement and self-cured resin composite luted ceramic inlays. A 5-year clinical evaluation
    • Van Dijken JWV. Resin-modified glass ionomer cement and self-cured resin composite luted ceramic inlays. A 5-year clinical evaluation. Dent Mater 2003;19:670-674.
    • (2003) Dent Mater , vol.19 , pp. 670-674
    • Van Dijken, J.W.V.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.