Volumn 78, Issue 2, 2006, Pages 393-400

Effects of sandblasting and electrical discharge machining on porcelain adherence to cast and machined commercially pure titanium

Author keywords

3 point bending test; Electrical discharge machining (EDM); Low fusing porcelain; Sandblasting; Titanium

Indexed keywords

ACRYLICS; ADHESION; NICKEL ALLOYS; POLYMERIZATION; PORCELAIN; RESINS; SCANNING ELECTRON MICROSCOPY; TITANIUM;

EID: 33746681253     PISSN: 00219304     EISSN: 15524981     Source Type: Journal    
DOI: 10.1002/jbm.b.30500     Document Type: Article
Times cited : (42)

References (49)
  • 2
    • 0030155746 scopus 로고    scopus 로고
    • Titanium for prosthodontics applications: A review of the literature
    • Wang RR, Fenton A. Titanium for prosthodontics applications: A review of the literature. Quintessence Int 1996;27:401-408.
    • (1996) Quintessence Int , vol.27 , pp. 401-408
    • Wang, R.R.1    Fenton, A.2
  • 3
    • 0034276711 scopus 로고    scopus 로고
    • Corrosion-fatigue life of commercially pure titanium and Ti-6A1-4V alloys in different storage environments
    • Zavanelli RA, Pessanha Henriques GE, Ferreira I, De Almeida Rollo JM. Corrosion-fatigue life of commercially pure titanium and Ti-6A1-4V alloys in different storage environments. J Prosthet Dent 2000;84:274-279.
    • (2000) J Prosthet Dent , vol.84 , pp. 274-279
    • Zavanelli, R.A.1    Pessanha Henriques, G.E.2    Ferreira, I.3    De Almeida Rollo, J.M.4
  • 4
    • 0032991686 scopus 로고    scopus 로고
    • Silicon nitride coating on titanium to enable titaniumceramic bonding
    • Wang RR, Welsch GE, Monteiro O. Silicon nitride coating on titanium to enable titaniumceramic bonding. J Biomed Mater Res 1999;46:262-270.
    • (1999) J Biomed Mater Res , vol.46 , pp. 262-270
    • Wang, R.R.1    Welsch, G.E.2    Monteiro, O.3
  • 5
    • 0004169805 scopus 로고
    • Donachie MJ, editor. Metals Park, OH: ASM International
    • Donachie MJ, editor. Titanium: A Technical Guide. Metals Park, OH: ASM International; 1988. p 28, 69, 71.
    • (1988) Titanium: A Technical Guide , pp. 28
  • 6
    • 0003680998 scopus 로고
    • Technical note 9: Descaling and special surface treatments
    • Boyer R, Welsch G, Collings EW, editors. Materials Park, OH: ASM International
    • Bauccio ML. Technical note 9: Descaling and special surface treatments. In: Boyer R, Welsch G, Collings EW, editors. Materials Properties Handbook: Titanium Alloys. Materials Park, OH: ASM International; 1994. p 1145-1158.
    • (1994) Materials Properties Handbook: Titanium Alloys , pp. 1145-1158
    • Bauccio, M.L.1
  • 7
    • 0021009730 scopus 로고
    • An application of pure titanium to the metal porcelain system
    • Togaya T, Suzuki M, Tsutsumi S, Ida K. An application of pure titanium to the metal porcelain system. Dent Mater 1983;2:210-219.
    • (1983) Dent Mater , vol.2 , pp. 210-219
    • Togaya, T.1    Suzuki, M.2    Tsutsumi, S.3    Ida, K.4
  • 8
    • 0029181886 scopus 로고
    • Bonding characteristics of low-fusing porcelain bonded to pure titanium and palladium-copper alloy
    • Pang IC, Gilbert JL, Chai J, Lautenschlager EP. Bonding characteristics of low-fusing porcelain bonded to pure titanium and palladium-copper alloy. J Prosthet Dent 1995;73:17-25.
    • (1995) J Prosthet Dent , vol.73 , pp. 17-25
    • Pang, I.C.1    Gilbert, J.L.2    Chai, J.3    Lautenschlager, E.P.4
  • 9
    • 0030160162 scopus 로고    scopus 로고
    • Three-point bending strength of ceramics fused to cast titanium
    • Pröbster L, Maiwald U, Weber H. Three-point bending strength of ceramics fused to cast titanium. Eur J Oral Sci 1996;104:313-319.
    • (1996) Eur J Oral Sci , vol.104 , pp. 313-319
    • Pröbster, L.1    Maiwald, U.2    Weber, H.3
  • 10
    • 0028520542 scopus 로고
    • Effects of sandblasting and silica-coating procedures on pure titanium
    • Kern M, Thompson VP. Effects of sandblasting and silica-coating procedures on pure titanium. J Dent 1994;22:300-306.
    • (1994) J Dent , vol.22 , pp. 300-306
    • Kern, M.1    Thompson, V.P.2
  • 11
  • 12
    • 0027828559 scopus 로고
    • Titanium-porcelain system. Part I: Oxidation kinetics of nitrided pure titanium, simulated to porcelain firing process
    • Oshida Y, Hashem A. Titanium-porcelain system. Part I: Oxidation kinetics of nitrided pure titanium, simulated to porcelain firing process. Biomed Mater Eng 1993;3:185-198.
    • (1993) Biomed Mater Eng , vol.3 , pp. 185-198
    • Oshida, Y.1    Hashem, A.2
  • 13
    • 0031116287 scopus 로고    scopus 로고
    • Oxidation behavior of surface-modified titanium for titaniumceramic restorations
    • Wang RR, Fung KK. Oxidation behavior of surface-modified titanium for titaniumceramic restorations. J Prosthet Dent 1997;77:423-434.
    • (1997) J Prosthet Dent , vol.77 , pp. 423-434
    • Wang, R.R.1    Fung, K.K.2
  • 14
    • 0028402743 scopus 로고
    • Bond characteristics of porcelain fused to milled titanium
    • Gilbert JL, Covey DA, Lautenschlager EP. Bond characteristics of porcelain fused to milled titanium. Dent Mater 1994;10:134-140.
    • (1994) Dent Mater , vol.10 , pp. 134-140
    • Gilbert, J.L.1    Covey, D.A.2    Lautenschlager, E.P.3
  • 15
    • 0034328117 scopus 로고    scopus 로고
    • Bond strength of three porcelains to two forms of titanium using two firing atmospheres
    • Atsü S, Berksun S. Bond strength of three porcelains to two forms of titanium using two firing atmospheres. J Prosthet Dent 2000;84:567-574.
    • (2000) J Prosthet Dent , vol.84 , pp. 567-574
    • Atsü, S.1    Berksun, S.2
  • 16
    • 0141608992 scopus 로고    scopus 로고
    • Effects of interfacial variables on ceramic adherence to cast and machined commercially pure titanium
    • Sadeq A, Cai Z, Woody RD, Miller AW. Effects of interfacial variables on ceramic adherence to cast and machined commercially pure titanium. J Prosthet Dent 2003;90:10-17.
    • (2003) J Prosthet Dent , vol.90 , pp. 10-17
    • Sadeq, A.1    Cai, Z.2    Woody, R.D.3    Miller, A.W.4
  • 17
    • 0026247782 scopus 로고
    • Ceramo-metallic bond of cast titanium
    • Böning K, Walter M. Ceramo-metallic bond of cast titanium. Dtsch Zahnärztl Z 1991;46:750-753.
    • (1991) Dtsch Zahnärztl Z , vol.46 , pp. 750-753
    • Böning, K.1    Walter, M.2
  • 19
    • 84989535713 scopus 로고
    • Bond strength of porcelain on cast vs wrought titanium
    • Dérand T, Herø H. Bond strength of porcelain on cast vs wrought titanium. Scand J Dent Res 1992;100:184-188.
    • (1992) Scand J Dent Res , vol.100 , pp. 184-188
    • Dérand, T.1    Herø, H.2
  • 20
    • 0027616999 scopus 로고
    • Titanium and titanium alloys as dental materials
    • Lautenschlager EP, Monaghan P. Titanium and titanium alloys as dental materials. Int Dent J 1993;43:245-253.
    • (1993) Int Dent J , vol.43 , pp. 245-253
    • Lautenschlager, E.P.1    Monaghan, P.2
  • 22
    • 0035000757 scopus 로고    scopus 로고
    • Fusing of dental ceramics to titanium
    • Könönen M, Kivilahti J. Fusing of dental ceramics to titanium. J Dent Res 2001;80:848-854.
    • (2001) J Dent Res , vol.80 , pp. 848-854
    • Könönen, M.1    Kivilahti, J.2
  • 23
    • 0026825389 scopus 로고
    • Electrical discharge machining in dentistry
    • Van Roekel NB. Electrical discharge machining in dentistry. Int J Prosthodont 1992;5:114-121.
    • (1992) Int J Prosthodont , vol.5 , pp. 114-121
    • Van Roekel, N.B.1
  • 24
    • 0026832539 scopus 로고
    • Prosthesis fabrication using electrical discharge machining
    • Van Roekel NB. Prosthesis fabrication using electrical discharge machining. Int J Oral Maxillofac Implants 1992;7:56-61.
    • (1992) Int J Oral Maxillofac Implants , vol.7 , pp. 56-61
    • Van Roekel, N.B.1
  • 25
    • 0031066345 scopus 로고    scopus 로고
    • Correcting the fit of implant-retained restorations by electric discharge machining
    • Evans DB. Correcting the fit of implant-retained restorations by electric discharge machining. J Prosthet Dent 1997;77:212-215.
    • (1997) J Prosthet Dent , vol.77 , pp. 212-215
    • Evans, D.B.1
  • 26
    • 0027630884 scopus 로고
    • Development of fabrication system of prostheses using electric discharge machining
    • Miyazaki T, Kitamura M, Hotta Y, Lee G. Development of fabrication system of prostheses using electric discharge machining. Asian J Aesthet Dent 1993;1:71-79.
    • (1993) Asian J Aesthet Dent , vol.1 , pp. 71-79
    • Miyazaki, T.1    Kitamura, M.2    Hotta, Y.3    Lee, G.4
  • 27
    • 0020451872 scopus 로고
    • Electroerosion in dental technology. Possibilities and limits
    • Rubeling G. Electroerosion in dental technology. Possibilities and limits. Dent Labor (Munch) 1982;30:1697-1702.
    • (1982) Dent Labor (Munch) , vol.30 , pp. 1697-1702
    • Rubeling, G.1
  • 28
    • 0036834297 scopus 로고    scopus 로고
    • Fit of cast commercially pure titanium and Ti-6A1-4V alloy crowns before and after marginal refinement by electrical discharge machining
    • Contreras EFR, Henriques GEP, Giolo SR, Nobilo MAA. Fit of cast commercially pure titanium and Ti-6A1-4V alloy crowns before and after marginal refinement by electrical discharge machining. J Prosthet Dent 2002;88:467-472.
    • (2002) J Prosthet Dent , vol.88 , pp. 467-472
    • Contreras, E.F.R.1    Henriques, G.E.P.2    Giolo, S.R.3    Nobilo, M.A.A.4
  • 29
    • 4444234022 scopus 로고    scopus 로고
    • Effect of casting technique on surface roughness and consequent mass loss after polishing of NiCr and CoCr base metal alloys: A comparative study with titanium
    • Bezzon OL, Pedrazzi H, Zaniquelli O, da Silva TB. Effect of casting technique on surface roughness and consequent mass loss after polishing of NiCr and CoCr base metal alloys: A comparative study with titanium. J Prosthet Dent 2004;92:274-277.
    • (2004) J Prosthet Dent , vol.92 , pp. 274-277
    • Bezzon, O.L.1    Pedrazzi, H.2    Zaniquelli, O.3    Da Silva, T.B.4
  • 31
  • 32
    • 24944544285 scopus 로고    scopus 로고
    • Investigation of the relationship between the white layer thickness and 3D surface texture parameters in the die sinking EDM process
    • Ramasawmy H, Blunt L, Rajurkar KP. Investigation of the relationship between the white layer thickness and 3D surface texture parameters in the die sinking EDM process. Precis Eng 2005;29:479-490.
    • (2005) Precis Eng , vol.29 , pp. 479-490
    • Ramasawmy, H.1    Blunt, L.2    Rajurkar, K.P.3
  • 33
    • 0024345249 scopus 로고
    • Studies of Ti alloys for dental castings
    • Taira M, Moser JB, Greener EH. Studies of Ti alloys for dental castings. Dent Mater 1989;5:45-50.
    • (1989) Dent Mater , vol.5 , pp. 45-50
    • Taira, M.1    Moser, J.B.2    Greener, E.H.3
  • 35
    • 0015371484 scopus 로고
    • Calculation of interfacial stress in dental porcelain bonded to gold alloy substrate
    • Nielsen JP, Tuccillo JT. Calculation of interfacial stress in dental porcelain bonded to gold alloy substrate. J Dent Res 1972;51:1043-1047.
    • (1972) J Dent Res , vol.51 , pp. 1043-1047
    • Nielsen, J.P.1    Tuccillo, J.T.2
  • 38
    • 0033087402 scopus 로고    scopus 로고
    • Comparison of the bond compatibility of titanium and an NiCr alloy to dental porcelain
    • Yilmaz H, Dinčer C. Comparison of the bond compatibility of titanium and an NiCr alloy to dental porcelain. J Dent 1999;27:215-222.
    • (1999) J Dent , vol.27 , pp. 215-222
    • Yilmaz, H.1    Dinčer, C.2
  • 40
    • 0022140001 scopus 로고
    • Der sandstrahlprozeβ und seine einwirkung auf den oberflächenzustand von dentallegierungen (I)
    • Tiller HJ, Magnus B, Göbel R, Musil R, Garschke A. Der Sandstrahlprozeβ und seine Einwirkung auf den Oberflächenzustand von Dentallegierungen (I). Quintessenza 1985;36:1927-1934.
    • (1985) Quintessenza , vol.36 , pp. 1927-1934
    • Tiller, H.J.1    Magnus, B.2    Göbel, R.3    Musil, R.4    Garschke, A.5
  • 41
    • 0022156482 scopus 로고
    • Der sandstrahlprozeß und seine einwirkung auf den oberflächenzustand von dentallegierungen (II)
    • Tiller HJ, Göbel R, Magnus B, Musil R, Garschke A, Lockowandt P, Oden A. Der Sandstrahlprozeß und seine Einwirkung auf den Oberflächenzustand von Dentallegierungen (II). Quintessenza 1985;36:2151-2158.
    • (1985) Quintessenza , vol.36 , pp. 2151-2158
    • Tiller, H.J.1    Göbel, R.2    Magnus, B.3    Musil, R.4    Garschke, A.5    Lockowandt, P.6    Oden, A.7
  • 42
    • 0035342531 scopus 로고    scopus 로고
    • Porcelain adherence to dental cast CP titanium: Effects of surface modifications
    • Cai Z, Bunce N, Nunn ME, Okabe T. Porcelain adherence to dental cast CP titanium: Effects of surface modifications. Biomaterials 2001;22:979-986.
    • (2001) Biomaterials , vol.22 , pp. 979-986
    • Cai, Z.1    Bunce, N.2    Nunn, M.E.3    Okabe, T.4
  • 43
    • 33746688435 scopus 로고    scopus 로고
    • Vita Zahnfabrik, H. Rauter GmbH & Co. KG, Bad Säckingen, Germany
    • VITA TITANKERAMIK working instructions. Vita Zahnfabrik, H. Rauter GmbH & Co. KG, Bad Säckingen, Germany. Available at http://www. vitazahnfabrik.com/resourcesvita/shop/en/en 3050350.pdf.
    • VITA TITANKERAMIK Working Instructions
  • 44
    • 0029338110 scopus 로고
    • Fabrication of titanium implant-retained restorations with nontraditional machining techniques
    • Schmitt SM, Chance DA. Fabrication of titanium implant-retained restorations with nontraditional machining techniques. Int J Prosthodont 1995;8:332-336.
    • (1995) Int J Prosthodont , vol.8 , pp. 332-336
    • Schmitt, S.M.1    Chance, D.A.2
  • 45
    • 84976683428 scopus 로고
    • Microstructure and properties of electro discharge machined surfaces
    • Tomlinson WJ, Adkin JR. Microstructure and properties of electro discharge machined surfaces. Surf Eng 1992;8:283-288.
    • (1992) Surf Eng , vol.8 , pp. 283-288
    • Tomlinson, W.J.1    Adkin, J.R.2
  • 46
    • 0141890027 scopus 로고    scopus 로고
    • Relationship between EDM parameters and surface crack formation
    • Lee HT, Tai TY. Relationship between EDM parameters and surface crack formation. J Mater Process Technol 2003;142:676-683.
    • (2003) J Mater Process Technol , vol.142 , pp. 676-683
    • Lee, H.T.1    Tai, T.Y.2
  • 47
    • 17344374992 scopus 로고    scopus 로고
    • The effect of thermal cycling on the bond strength of low-fusing porcelain to commercially pure titanium and titanium aluminium-vanadium alloy
    • Tróia MG Jr, Henriques GEP, Nóbilo MAA, Mesquita MF. The effect of thermal cycling on the bond strength of low-fusing porcelain to commercially pure titanium and titanium aluminium-vanadium alloy. Dent Mater 2003;19:790-796.
    • (2003) Dent Mater , vol.19 , pp. 790-796
    • Tróia Jr., M.G.1    Henriques, G.E.P.2    Nóbilo, M.A.A.3    Mesquita, M.F.4
  • 49
    • 0043071591 scopus 로고    scopus 로고
    • Adhesion of porcelain to titanium and a titanium alloy
    • Suansuwan N, Swain MV. Adhesion of porcelain to titanium and a titanium alloy. J Dent 2003;31:509-518.
    • (2003) J Dent , vol.31 , pp. 509-518
    • Suansuwan, N.1    Swain, M.V.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.