1
-
-
4644335450
-
A microstructural observation of near-failure thermal barrier coaling: A study by photostimulated luminescence spectroscopy and transmission electron microscopy
-
B. W. Kempshall, Y. H. Sohn, S. K. Jha, S. Laxman, R. R. Vanfleet, and J. Kimmel, "A Microstructural Observation of Near-Failure Thermal Barrier Coaling: A Study by Photostimulated Luminescence Spectroscopy and Transmission Electron Microscopy,"Thin Solid Films, 466 [1-2] 128-36 (2004).
-
(2004)
Thin Solid Films
, vol.466
, Issue.1-2
, pp. 128-136
-
-
Kempshall, B.W.1
Sohn, Y.H.2
Jha, S.K.3
Laxman, S.4
Vanfleet, R.R.5
Kimmel, J.6
-
2
-
-
0036697965
-
2 gate dielectric deposited on ultrathin silicon capping layer for SiGe metal-oxide-semiconduelor device applications
-
2 Gate Dielectric Deposited on Ultrathin Silicon Capping Layer for SiGe Metal-Oxide-Semiconduelor Device Applications,"Jpn. J. Appl. Phys. 1, 41 [8] 5129-30 (2002).
-
(2002)
Jpn. J. Appl. Phys.
, vol.1-41
, Issue.8
, pp. 5129-5130
-
-
Choi, S.1
Jeon, S.2
Hwang, H.3
Song, Y.J.4
Lim, J.W.5
Shim, K.H.6
Park, K.W.7
-
3
-
-
0037015196
-
3 bicryslals: II, relation of interfacial bonding, chemistry and local plasticity
-
3 Bicryslals: II, Relation of Interfacial Bonding, Chemistry and Local Plasticity,"Acta Mater., 50 [15] 3903-25 (2002).
-
(2002)
Acta Mater.
, vol.50
, Issue.15
, pp. 3903-3925
-
-
Cannon, R.M.1
Korn, D.2
Elssner, G.3
Ruhle, M.4
-
4
-
-
3042754265
-
Interfacial fracture mechanisms in solid solution directionally solidified eutectic oxide composites
-
L. N. Brewer, M. U. Guruz, and V. P. Dravid, "Interfacial Fracture Mechanisms in Solid Solution Directionally Solidified Eutectic Oxide Composites,"Acta Mater., 52 [13] 3781-91 (2004).
-
(2004)
Acta Mater.
, vol.52
, Issue.13
, pp. 3781-3791
-
-
Brewer, L.N.1
Guruz, M.U.2
Dravid, V.P.3
-
5
-
-
0035973445
-
3) emeelics
-
3) Emeelics,"Mater. Sci. Eng. A-Struct., 308 [1-2] 241-9 (2001).
-
(2001)
Mater. Sci. Eng. A-Struct.
, vol.308
, Issue.1-2
, pp. 241-249
-
-
Pastor, J.Y.1
Poza, P.2
Llorca, J.3
Pena, J.I.4
Merino, R.I.5
Orera, V.M.6
-
8
-
-
0023349443
-
Fracture initiation in the direetionally solidified NiO-CaO eutectic
-
M. D. Brumels and B. J. Pletka, "Fracture Initiation in the Direetionally Solidified NiO-CaO Eutectic,"J. Am. Ceram. Soc., 70 [5] 305-10 (1987).
-
(1987)
J. Am. Ceram. Soc.
, vol.70
, Issue.5
, pp. 305-310
-
-
Brumels, M.D.1
Pletka, B.J.2
-
9
-
-
0033276735
-
Interface modification for increased fracture toughness in reaction-formed yttrium aluminum garnet/alumina eutectic composites
-
L. N. Brewer, D. P. Endler, S. Austin, V. P. Dravid, and J. M. Collins, "Interface Modification for Increased Fracture Toughness in Reaction-Formed Yttrium Aluminum Garnet/Alumina Eutectic Composites,"J. Mater. Res., 14 [10] 3907-12(1999).
-
(1999)
J. Mater. Res.
, vol.14
, Issue.10
, pp. 3907-3912
-
-
Brewer, L.N.1
Endler, D.P.2
Austin, S.3
Dravid, V.P.4
Collins, J.M.5
-
11
-
-
0023996616
-
2(CaO) directional composite
-
2(CaO) Directional Composite,"J. Am. Ceram. Soc., 71 [4] 296-301 (1988).
-
(1988)
J. Am. Ceram. Soc.
, vol.71
, Issue.4
, pp. 296-301
-
-
Bonvalotdubois, B.1
Dhalenne, G.2
Berthon, J.3
Revcolevschi, A.4
Rapp, R.A.5
-
13
-
-
0036541119
-
Solid-solution direetionally solidified eutectic oxide composites: Part I. eutectic growth and characterization
-
L. N. Brewer, V. P. Dravid, G. Dhalenne, and M. Velazquez, "Solid-Solution Direetionally Solidified Eutectic Oxide Composites: Part I. Eutectic Growth and Characterization,"J. Mater. Res., 17 [4] 760-7 (2002).
-
(2002)
J. Mater. Res.
, vol.17
, Issue.4
, pp. 760-767
-
-
Brewer, L.N.1
Dravid, V.P.2
Dhalenne, G.3
Velazquez, M.4
-
15
-
-
1042290090
-
Reinforcement by crack-tip blunting in porous ceramics
-
Z. Y. Deng, J. H. She, Y. Inagaki, J. F. Yang, T. Ohji, and Y. Tanaka, "Reinforcement by Crack-Tip Blunting in Porous Ceramics,"J. Eur. Ceram, Soc., 24 [7] 2055-9 (2004).
-
(2004)
J. Eur. Ceram, Soc.
, vol.24
, Issue.7
, pp. 2055-2059
-
-
Deng, Z.Y.1
She, J.H.2
Inagaki, Y.3
Yang, J.F.4
Ohji, T.5
Tanaka, Y.6
-
16
-
-
0242271339
-
Indentation behaviour of porous materials: Application to the vickers indentation cracking of ceramics
-
F. Taneret and F. Oslerslock, "Indentation Behaviour of Porous Materials: Application to the Vickers Indentation Cracking of Ceramics,"Philos. Mag., 83 [1] 125-36 (2003).
-
(2003)
Philos. Mag.
, vol.83
, Issue.1
, pp. 125-136
-
-
Taneret, F.1
Oslerslock, F.2
-
17
-
-
0022911477
-
On the toughening of ceramics by strong reinforcements
-
A. G. Evans and R. M. Mcmeeking, "On the Toughening of Ceramics by Strong Reinforcements,"Acta Metall. Mater., 34 [12] 2435-41 (1986).
-
(1986)
Acta Metall. Mater.
, vol.34
, Issue.12
, pp. 2435-2441
-
-
Evans, A.G.1
Mcmeeking, R.M.2
-
18
-
-
0027573301
-
The mechanics of crack-growth in layered materials
-
M. Y. He, F. E. Heredia, D. J. Wissuchek, M. C. Shaw, and A. G. Evans, "The Mechanics of Crack-Growth in Layered Materials,"Acta Metall. Mater., 41 [4] 1223-8 (1993).
-
(1993)
Acta Metall. Mater.
, vol.41
, Issue.4
, pp. 1223-1228
-
-
He, M.Y.1
Heredia, F.E.2
Wissuchek, D.J.3
Shaw, M.C.4
Evans, A.G.5
-
19
-
-
0026962486
-
The fracture-resistance of metal ceramic interfaces
-
A. G. Evans and B. J. Dalgleish, "The Fracture-Resistance of Metal Ceramic Interfaces,"Acta Metall Mater., 40, S295-306 (1992).
-
(1992)
Acta Metall Mater.
, vol.40
-
-
Evans, A.G.1
Dalgleish, B.J.2
-
20
-
-
0024705950
-
Flow characteristics of highly constrained metal wires
-
M. V. Ashby, F. J. Blunt, and M. Bannister, "Flow Characteristics of Highly Constrained Metal Wires,"Acta Metall. Mater., 37 [7] 1847-5 (1989).
-
(1989)
Acta Metall. Mater.
, vol.37
, Issue.7
, pp. 1847-1855
-
-
Ashby, M.V.1
Blunt, F.J.2
Bannister, M.3
-
21
-
-
0019058952
-
Elastic-plastic indentation damage in ceramics - The median-radial crack system
-
B. R. Lawn, A. G. Evans, and D. B. Marshall, "Elastic-Plastic Indentation Damage in Ceramics - the Median-Radial Crack System,"J. Am. Ceram. Soc., 63 [9-10] 574-81 (1980).
-
(1980)
J. Am. Ceram. Soc.
, vol.63
, Issue.9-10
, pp. 574-581
-
-
Lawn, B.R.1
Evans, A.G.2
Marshall, D.B.3
-
22
-
-
0032472969
-
2(Cubic) interfaces
-
2(Cubic) Interfaces,"Acta Mater., 46 [5] 1801-16 (1998).
-
(1998)
Acta Mater.
, vol.46
, Issue.5
, pp. 1801-1816
-
-
Dickey, E.C.1
Dravid, V.P.2
Nellist, P.D.3
Wallis, D.J.4
Pennycook, S.J.5
|