메뉴 건너뛰기




Volumn 5991, Issue , 2005, Pages

Laser damage initiation and growth of antireflection coated S-FAP crystal surfaces prepared by pitch lap and magnetorheological finishing

Author keywords

Antireflection coating; Damage growth; Damage morphology; E beam; HfO 2; MRF; SiO 2; Yb:S FAP

Indexed keywords

DAMAGE GROWTH; MRF; YB:S-FAP;

EID: 33644599449     PISSN: 0277786X     EISSN: None     Source Type: Conference Proceeding    
DOI: 10.1117/12.638831     Document Type: Conference Paper
Times cited : (20)

References (10)
  • 2
    • 4043102508 scopus 로고    scopus 로고
    • 3F] lasers
    • (The 3rd International Symposium on Laser and NLO Materials) Sept.
    • 3F] Lasers", (The 3rd International Symposium on Laser and NLO Materials) Optical Materials, 26 (4): 391-394 Sept. 2004
    • (2004) Optical Materials , vol.26 , Issue.4 , pp. 391-394
    • Schaffers, K.I.1
  • 5
    • 35448965353 scopus 로고
    • The effects of barrier layers and surface smoothness on 150-ps, 1064-mm laser damage of AR coatings on glass
    • J. H. Apfel, E. A. Enemark, D. Milam, W. L. Smith, and M. J. Weber, "The effects of barrier layers and surface smoothness on 150-ps, 1064-mm laser damage of AR coatings on glass", Nat. Bur. Stand (U.S.), Spec. Publ. 509, 255-259 (1978).
    • (1978) Nat. Bur. Stand (U.S.), Spec. Publ. , vol.509 , pp. 255-259
    • Apfel, J.H.1    Enemark, E.A.2    Milam, D.3    Smith, W.L.4    Weber, M.J.5
  • 6
    • 0019317981 scopus 로고
    • Oxide coatings for one micrometer laser fusion
    • C. K. Carniglia, "Oxide coatings for one micrometer laser fusion", Thin Solid Films 77, 225-238 (1981).
    • (1981) Thin Solid Films , vol.77 , pp. 225-238
    • Carniglia, C.K.1
  • 7
    • 0032651835 scopus 로고    scopus 로고
    • Thermomechanical model of mirror laser damage at 1.06 mm. Part 2: Flat bottom pits formation
    • Laser-Induced Damage in Optical Materials: 1998, G. J. Exarhos, A. H. Guenther, M. R. Kozlowski, K. L. Lewis, and M. J. Soileau, eds.
    • J. Dijon, M. Poulingue, J. Hue, "Thermomechanical model of mirror laser damage at 1.06 mm. Part 2: flat bottom pits formation", in Laser-Induced Damage in Optical Materials: 1998, G. J. Exarhos, A. H. Guenther, M. R. Kozlowski, K. L. Lewis, and M. J. Soileau, eds., Proc. SPIE Eng. 3578, 398-407 (1999).
    • (1999) Proc. SPIE Eng. , vol.3578 , pp. 398-407
    • Dijon, J.1    Poulingue, M.2    Hue, J.3
  • 8
    • 18744401364 scopus 로고    scopus 로고
    • 2 thin films with artificial defects
    • Laser-Induced Damage in Optical Materials: 2004, G. J. Exarhos, A. H. Guenther, N. Kaiser, K. L. Lewis, M. J. Soileau, and C. J. Stolz, eds.
    • 2 thin films with artificial defects", in Laser-Induced Damage in Optical Materials: 2004, G. J. Exarhos, A. H. Guenther, N. Kaiser, K. L. Lewis, M. J. Soileau, and C. J. Stolz, eds., Proc. SPIE 5647, 141-155 (2005).
    • (2005) Proc. SPIE , vol.5647 , pp. 141-155
    • Papernov, S.1    Schmid, A.W.2
  • 9
    • 0038115235 scopus 로고    scopus 로고
    • Role of light intensification by cracks in optical breakdown on surfaces
    • F. Y. Génin, A. Salleo, T. V. Pistor, and L. L. Chase, "Role of light intensification by cracks in optical breakdown on surfaces", J. Opt. Soc. Am. A 18, 2607-2616 (2001).
    • (2001) J. Opt. Soc. Am. A , vol.18 , pp. 2607-2616
    • Génin, F.Y.1    Salleo, A.2    Pistor, T.V.3    Chase, L.L.4
  • 10
    • 0036032068 scopus 로고    scopus 로고
    • Combined advanced finishing and UV-laser conditioning for producing UV-damage-resistant fused silica optics
    • Laser-Induced Damage in Optical Materials: 2001, G. J. Exarhos, A. H. Guenther, K. L. Lewis, M. J. Soileau, and C. J. Stolz, eds.
    • J. A, Menapace, B. Penetrante, D. Golini, A. Slomba, P. E. Miller, T. Parham, M. Nichols, and J. Peterson, "Combined advanced finishing and UV-laser conditioning for producing UV-damage-resistant fused silica optics", in Laser-Induced Damage in Optical Materials: 2001, G. J. Exarhos, A. H. Guenther, K. L. Lewis, M. J. Soileau, and C. J. Stolz, eds., Proc. SPIE 4679, 56-67 (2002).
    • (2002) Proc. SPIE , vol.4679 , pp. 56-67
    • Menapace, J.A.1    Penetrante, B.2    Golini, D.3    Slomba, A.4    Miller, P.E.5    Parham, T.6    Nichols, M.7    Peterson, J.8


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.