Volumn 14, Issue 3, 2005, Pages 356-362

Degradation behavior of Ni3Al plasma-sprayed boiler tube steels in an energy generation system

Author keywords

Coal fired boilers; Erosion; Hot corrosion; Ni3Al; Plasma spray

Indexed keywords

COAL FIRED BOILERS; CORROSION; DEGRADATION; ENERGY RESOURCES; EROSION; NICKEL COMPOUNDS; PLASMA SPRAYING; SPALLING; STOICHIOMETRY;

EID: 23244449526     PISSN: 10599495     EISSN: None     Source Type: Journal    
DOI: 10.1361/10599490523382     Document Type: Article
Times cited : (18)

References (23)
  • 1
    • 0012766569 scopus 로고
    • High temperature oxidation behaviour of nickel aluminide coated mild steel
    • A.U. Malik, R. Ahmad, S. Ahmad, and S. Ahmad, High Temperature Oxidation Behaviour of Nickel Aluminide Coated Mild Steel, Pract. Metallogr., Vol 29, 1992, p 255-268
    • (1992) Pract. Metallogr. , vol.29 , pp. 255-268
    • Malik, A.U.1    Ahmad, R.2    Ahmad, S.3    Ahmad, S.4
  • 2
    • 0034745889 scopus 로고    scopus 로고
    • Cyclic oxidation resistance of Ni-Al alloy coatings deposited on steel by a cathodic arc plasma process
    • J.L. He, K.C. Chen, C.C. Chen, A. Leyland, and A. Matthews, Cyclic Oxidation Resistance of Ni-Al Alloy Coatings Deposited on Steel by a Cathodic Arc Plasma Process, Surf. Coat. Technol., Vol 135, 2001, p 158-165
    • (2001) Surf. Coat. Technol. , vol.135 , pp. 158-165
    • He, J.L.1    Chen, K.C.2    Chen, C.C.3    Leyland, A.4    Matthews, A.5
  • 3
    • 0032785951 scopus 로고    scopus 로고
    • Iron and nickel aluminide composites
    • J.H. Schneibel and P.F. Becher, Iron and Nickel Aluminide Composites, J. Chinese Inst. Eng., Vol 22 (No. 1), 1999, p 1-12
    • (1999) J. Chinese Inst. Eng. , vol.22 , Issue.1 , pp. 1-12
    • Schneibel, J.H.1    Becher, P.F.2
  • 4
    • 0043207255 scopus 로고    scopus 로고
    • 3Al + 5% Cr coatings with and without y doping
    • 3Al + 5% Cr Coatings with and without Y Doping, Oxid. Met., Vol 55 (No. 5-6), 2001, p 481-504
    • (2001) Oxid. Met. , vol.55 , Issue.5-6 , pp. 481-504
    • Liu, Z.1    Gao, W.2
  • 5
    • 2342557236 scopus 로고    scopus 로고
    • High temperature erosion oxidation mechanism MAPS and models
    • R.G. Wellman and J.R. Nicholls, High Temperature Erosion Oxidation Mechanism MAPS and Models, Wear, Vol 256 (No. 9-10), 2004, p 907-917
    • (2004) Wear , vol.256 , Issue.9-10 , pp. 907-917
    • Wellman, R.G.1    Nicholls, J.R.2
  • 6
    • 0016993230 scopus 로고
    • Corrosion-erosion behavior of materials in a coal-gasification environment
    • K. Natesan, Corrosion-Erosion Behavior of Materials in a Coal-Gasification Environment, Corrosion, Vol 32 (No. 9), 1976, p 364-370
    • (1976) Corrosion , vol.32 , Issue.9 , pp. 364-370
    • Natesan, K.1
  • 7
    • 23244435244 scopus 로고
    • Technical note: Corrosion and grain boundary penetration in type 316 stainless steel exposed to a coal gasification environment
    • S. Danyluk and J.Y. Park, Technical Note: Corrosion and Grain Boundary Penetration in Type 316 Stainless Steel Exposed to a Coal Gasification Environment, Corrosion, Vol 35 (No. 12), 1979, p 575-576
    • (1979) Corrosion , vol.35 , Issue.12 , pp. 575-576
    • Danyluk, S.1    Park, J.Y.2
  • 8
    • 0024126315 scopus 로고
    • Corrosion behavior of chromized and/or aluminized 21/4Cr-1Mo steel in medium-BTU coal gasifier environments
    • D. Wang, Corrosion Behavior of Chromized and/or Aluminized 21/4Cr-1Mo Steel in Medium-BTU Coal Gasifier Environments, Surf. Coat. Technol., Vol 36, 1988, p 49-60
    • (1988) Surf. Coat. Technol. , vol.36 , pp. 49-60
    • Wang, D.1
  • 9
    • 2942679487 scopus 로고    scopus 로고
    • Materials for fluidized bed heat exchangers
    • Technical Research Centre of Finland
    • P. Makkonen and M. Makipaa, Materials for Fluidized Bed Heat Exchangers, Valtion Teknillinen Tutkimuskeskus Symposium, Technical Research Centre of Finland, Vol 233, 2004, p 197-207
    • (2004) Valtion Teknillinen Tutkimuskeskus Symposium , vol.233 , pp. 197-207
    • Makkonen, P.1    Makipaa, M.2
  • 10
    • 0024133282 scopus 로고
    • The erosion-corrosion behavior of protective coatings
    • A.V. Levy, The Erosion-Corrosion Behavior of Protective Coatings, Surf. Coat. Technol., Vol 36, 1988, p 387-406
    • (1988) Surf. Coat. Technol. , vol.36 , pp. 387-406
    • Levy, A.V.1
  • 11
    • 0033875119 scopus 로고    scopus 로고
    • The failure of protective oxides on plasma-sprayed NiCrAlY overlay coatings
    • P. Niranatlumpong, C.B. Ponton, and H.E. Evans, The Failure of Protective Oxides on Plasma-Sprayed NiCrAlY Overlay Coatings, Oxid. Met., Vol 53 (No. 3-4), 2000, p 241-258
    • (2000) Oxid. Met. , vol.53 , Issue.3-4 , pp. 241-258
    • Niranatlumpong, P.1    Ponton, C.B.2    Evans, H.E.3
  • 12
    • 0027855139 scopus 로고
    • Coatings resistant to erosive/corrosive and severe environments
    • M.G. Hocking, Coatings Resistant to Erosive/Corrosive and Severe Environments, Surf. Coat. Technol., Vol 62, 1993, p 460-466
    • (1993) Surf. Coat. Technol. , vol.62 , pp. 460-466
    • Hocking, M.G.1
  • 13
    • 0032686417 scopus 로고    scopus 로고
    • 3Al coating on carbon steel surface via the SHS casting route
    • 3Al Coating on Carbon Steel Surface Via the SHS Casting Route, Surf. Coat. Technol., Vol 113, 1999, p 44-51
    • (1999) Surf. Coat. Technol. , vol.113 , pp. 44-51
    • La, P.1    Bai, M.2    Xue, Q.3    Liu, W.4
  • 14
    • 0242499133 scopus 로고    scopus 로고
    • Uniform design method for optimization of process parameters of plasma spray TiN coatings
    • J.F. Li, H. Liao, B. Normand, C. Cordier, G. Maurin, J. Foct, and C. Coddet, Uniform Design Method for Optimization of Process Parameters of Plasma Spray TiN Coatings, Surf. Coat. Technol., Vol 176, 2003, p 1-13
    • (2003) Surf. Coat. Technol. , vol.176 , pp. 1-13
    • Li, J.F.1    Liao, H.2    Normand, B.3    Cordier, C.4    Maurin, G.5    Foct, J.6    Coddet, C.7
  • 15
    • 0031703229 scopus 로고    scopus 로고
    • Improving wear and corrosion resistance of thermal sprayed coatings
    • B. Wielage, U. Hofmann, S. Steinhauser, and G. Zimmermann, Improving Wear and Corrosion Resistance of Thermal Sprayed Coatings, Surf. Eng., Vol 14 (No. 2), 1998, p 136-138
    • (1998) Surf. Eng. , vol.14 , Issue.2 , pp. 136-138
    • Wielage, B.1    Hofmann, U.2    Steinhauser, S.3    Zimmermann, G.4
  • 16
    • 0023165606 scopus 로고
    • Fundamental studies associated with the plasma spray process
    • E. Pfender, Fundamental Studies Associated with the Plasma Spray Process, Surf. Coat. Technol., Vol 34, 1988, p 1-14
    • (1988) Surf. Coat. Technol. , vol.34 , pp. 1-14
    • Pfender, E.1
  • 18
    • 1442354709 scopus 로고    scopus 로고
    • Thermal barrier coatings: Why, how, where and where
    • Nice, France, May 25-29
    • J. Wigren and L. Pejiyd, Thermal Barrier Coatings: Why, How, Where and Where, Proc. of the International Thermal Spray Conf., Nice, France, May 25-29, 1998, Vol 2, p 1531-1542
    • (1998) Proc. of the International Thermal Spray Conf. , vol.2 , pp. 1531-1542
    • Wigren, J.1    Pejiyd, L.2
  • 19
    • 0030286717 scopus 로고    scopus 로고
    • Temperature-variant hardness behavior of plasma sprayed ceramic coatings
    • K. Hyung-Jun and K. Young-Gak, Temperature-Variant Hardness Behavior of Plasma Sprayed Ceramic Coatings, Thin Solid Films, Vol 289, 1996, p 207-212
    • (1996) Thin Solid Films , vol.289 , pp. 207-212
    • Hyung-Jun, K.1    Young-Gak, K.2
  • 20
    • 0037416664 scopus 로고    scopus 로고
    • 3Al coatings on steel in oxidation and molten salt environment at 900°C
    • 3Al Coatings on Steel in Oxidation and Molten Salt Environment at 900°C, Surf. Coat. Technol., Vol 166 (No. 1), 2003, p 89-100
    • (2003) Surf. Coat. Technol. , vol.166 , Issue.1 , pp. 89-100
    • Sidhu, B.S.1    Prakash, S.2
  • 22
    • 23244460181 scopus 로고
    • The reduction of sulphur trioxide by constituents of boiler flue dust
    • H.E. Crossley, A. Poll, and F. Sweett, The Reduction of Sulphur Trioxide by Constituents of Boiler Flue Dust, J. Inst. Fuel, Vol 21, 1948, p 207-209
    • (1948) J. Inst. Fuel , vol.21 , pp. 207-209
    • Crossley, H.E.1    Poll, A.2    Sweett, F.3
  • 23
    • 0035978399 scopus 로고    scopus 로고
    • 2 intermediate on the combination ability of coatings
    • 2 Intermediate on the Combination Ability of Coatings, Surf. Coat. Technol., Vol 140, 2001, p 231-237
    • (2001) Surf. Coat. Technol. , vol.140 , pp. 231-237
    • Wu, X.1    Weng, D.2    Chen, Z.3    Xu, L.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.